Wood preservation research in Tanzania: Priorities and challenges
1988 - IRG/WP 3462
Tanzania provides some of the highest rates of wood deterioration in service leading to alarming economic losses and yet no serious concern is shown in search for solutions to the problem. The paper attempts to point out some of the priority areas in the field of wood preservation research that demand urgent attention if timber is to be used judiciously in this country. An account is given of the ...
K K Murira, R Cockcroft


Treatment groups and remedies for CCA treated hardwood and softwood poles
1999 - IRG/WP 99-40142
Different hardwood and softwood species from Bangladesh and Bhutan was investigated regarding density, green fiber stress, natural durability of heartwood and CCA treated sapwood, CCA treatability grades, sapwood thickness, and kiln-drying properties for long term use as electric poles. These properties along with the past service records for nineteen years, separated ten heardwood and five softwo...
A K Lahiry


The effect of stilbenes on decay fungi of birch and aspen
2000 - IRG/WP 00-10364
Fourteen species of decay fungi, mainly species growing on birch and aspen, one leaf spot fungus of birch and the pine canker fungus Gremmeniella abietina were used to investigate how the stilbenes resveratrol and pinosylvin influence their relative growth on malt agar. With some species the ability to decay with stilbenes impregnated wood was also studied. The concentration of pinosylvin needed t...
L Syrjälä, K Von Weissenberg, A Pappinen, L Paajanen


Wood injurers found at wood processing plants in SR Sloveni
1981 - IRG/WP 1140
This report describes the stating of damages on wood and taking stock of wood injurers found in the warehouses of wood processing plants in SR Slovenia. The results of this research show that in the process of manufacture vast quantities of spruce-wood, pine-wood, beech wood, oak-wood, and poplar-wood are exposed to numerous injurers, both fungi and insects. The reasons for such a state lie in con...
R Benko


Preservation of coppice wood for the fabrication of glued beams or panels
1987 - IRG/WP 3427
In this survey we will examine the specific problems concerning the conservation and the preservation of timber (issued from trunks of small diameter corresponding to products of clearings or coppices) destined for the fabrication of solid reconstituted elements. Thus for six metropolitan species of wood, we first characterized the biological deteriorations which occur after felling and their kine...
G R Y Déon, R Schwartz


Preliminary investigation on the natural durability of Guayule (Parthenium argentatum)-based wood products
2000 - IRG/WP 00-40154
Conventional preservatives used to protect wood from insect and microbial damages are presently of major concern to human health and the environment. Finding alternative and economical preservatives has not been successful. Previous studies have shown that the resinous material extracted from the guayule plant (Parthenium argentatum, Gray) has both insect- and microbial-resistant properties. Unfor...
F S Nakayama, P Chow, D S Bajwa, J A Youngquist, J H Muehl, A M Krzysik


List of fungi in soft-rot tests
1975 - IRG/WP 105
This list gives information on the terrestrial and marine species and strains of fungi tested for soft-rot ability in pure culture with data on their decay activity in untreated wood. An index of the timber species tested is added. The compilation is based on 1) the list of soft-rot fungi of the former OECD Group (Doc.No. 27/DAS/CSI/M/559), Oct. 1968, prepared by R. Rösch and W. Liese, 2) informa...
G Seehann, W Liese, B Kess


Durability of Sugi (Cryptomeria japonica D.DoN ) wood treated in high temperature liquid paraffin
2002 - IRG/WP 02-40221
Sugi(Cryptomeria japonica D.DoN )wood was subject to a heat treatment in high-temperature liquid paraffin for the purpose of improving the resistance against fungi and termites without chemicals. The bath of paraffin liquid, which can provide a uniform heat transfer (±2?), was used at temperatures of 90?,120?and 150?.?ecay resistance according to JIS K 15711) was evaluated using a brown rot fungu...
Y Matsuoka, W Ohmura, S Fujiwara, Y Kanagawa


An analysis of the effects of some factors on the natural durability of pine (Pinus sylvestris L.) and spruce (Picea abies Karst.)
1986 - IRG/WP 1279
The effects of some factors on the natural resistance of pine and spruce sapwood against fungal decay and against attack of house-longhorn beetle larvae have been studied in laboratory tests and the results are evaluated by analysis of variance and regression analysis. Following conclusions were reached: Wood from summer-felled trees did not have a lower inherent natural durability against fungal ...
J B Boutelje, T Nilsson, S Rasmussen


Defining fungal decay types - A proposal for discussion
1985 - IRG/WP 1264
The present definitions of the fungal decay types, white rot, brown rot, and soft rot are somewhat vague. The definitions are based on a mixture of criteria involving morphological and chemical aspects of decay as well as taxonomic affiliation of the responsible fungal species. The present vague definitions have led some fungi being erroneously places in a wrong decay type. Furthermore, some fungi...
T Nilsson


Durability of some alternatives to preservative treated wood
2004 - IRG/WP 04-30353
The environmental discussion in Sweden has lead to an increasing use of naturally durable domestic wood species and wood treated according to alternative methods for use above ground. A number of these alternatives have been tested according to field- and laboratory tests and compared to wood treated with preservatives for above ground use. Seven untreated wood species, four alternative wood treat...
M-L Edlund


Degradation of resin constituents in various wood species by the white rot fungus Bjerkandera sp. strain BOS55
1999 - IRG/WP 99-10301
In previous studies, the white-rot fungus Bjerkandera sp. strain BOS55 was shown to cause extensive degradation of lipophilic extractives (resin) in Scots pine wood. Further research was carried out in order to investigate the ability of Bjerkandera sp. for reducing resinous constituents in various softwood (Douglas fir, larch and spruce) and hardwood species (birch, beech and poplar). The greates...
J Dorado, T A Van Beek, F W Claassen, R Sierra-Alvarez


Effect of fungal degradation on the chemical composition of acetylated beech wood
2003 - IRG/WP 03-40267
This study investigated the impact of fungal attack on the chemical composition of acetylated wood. Beech wood acetylated to different degrees was exposed to decay by the white-rot fungus Trametes versicolor under solid-state fermentation conditions. Laboratory soil-bed assays were also conducted to study the degradation of acetylated wood by soft rot fungi and other soil-inhabiting microorganisms...
H Militz, Dong-won Son, L Gómez-Hernández, R Sierra-Alvarez


Wood preservation in Japan
1982 - IRG/WP 3218
The report indicates the importance of wood preservation in Japan, which is the world's largest importer. The main hazards of timber are listed, fungi, insects and marine borers. Besides wood preservation fire protection treatments are also important in Japan. Classifications are given of the durability and treatability of the timbers used. In describing the wood preservation industry, th...
S Amemiya, R Cockcroft


Partial characterization of inhibitors extracted from pine (Pinus sylvestris) sapwood active against germination of wood rotting fungi
1988 - IRG/WP 1351
Germination inhibitors in pine sapwood could be extracted and separated with the aid of solvent partitioning and chromatography on silicic acid. The inhibitory action was tested by three different bioassays. Active fractions have been characterized by TLC and HPLC. Inhibitory activity could be correlated with phenolic compounds. The minimum active concentration of inhibitors have been determined....
J Bjurman


Shorter-term biological control of wood decay in pre-seasoning pine roundwood as an alternative to chemical methods
1992 - IRG/WP 92-1555
Previous studies on the long-term control of decay in creosoted transmission poles, using Trichoderma and other antagonistic moulds, have met with limited success. However, it is possible biological control is more suited to control of decay on shorter time scales. An earlier study, focusing on pre-seasoning treatment of transmission poles showed that favourable porosity increases could be brought...
M W Schoeman, D J Dickinson


The use of fumigants for controlling decay of wood: a review of their efficacy and safety
1989 - IRG/WP 3525
Volatile agricultural chemicals (fumigants) such as chloropicrin (trichloronitromethane) and sodium n-methyldithiocarbamate have been used in the United States for controlling internal decay of large dimension wood products for over 20 years. This usage has been concentrated in the electric utility industry, but fumigants are increasingly applied to protect bridge timbers, marine piling, and even ...
J J Morrell


Selecting fumigants for treatment of internal decay in wood
1986 - IRG/WP 3370
A number of potential fumigants were screened with respect to their toxicity to decay fungi, (Poria carbonica, and Lentinus lepideus) and their sorption characteristics on Douglas Fir (Pseudotsuga menziesii Mirb. Franco) wood. Wafers of infected wood were exposed to different fumigant concentrations for various times then cultured to determine viability. The lethal concentration X time (ct) factor...
P A Cooper


Moisture Adsorption Behaviour of Rubber Wood Decayed by Brown and White rot Fungi
2005 - IRG/WP 05-40306
Moisture adsorption behaviour of rubber wood blocks decayed by each brown rot and white rot fungi was studied. The adsorption isotherms of decayed wood were compared with the isotherm of undecayed wood. The wood decayed by brown rot adsorbed less moisture as compared to sound or undecayed wood at all humidity levels. No significant difference was observed in adsorption behaviour of white rot dec...
S S Chauhan, H C Nagaveni


Collaborative soft rot tests: Specific gravity loss resulting from soft rot
1973 - IRG/WP 227
It was proposed at the 5th meeting of Working Group II of the IRG in June 1973 in Lahti, Finland, that the specific gravity (swollen volume basis) of test blocks used in the IRG Collaborative Soft Rot Tests should be determined on all the blocks at the completion of the exposure period. Specific gravity determined on the basis of the oven dry weight and water swollen volume was selected because (1...
C R Levy


Characterization of wood decay enzymes by MALDI-MS for post-translational modification and gene identification
2002 - IRG/WP 02-10442
The recent sequencing of the Phanerochaete chrysosporium genome presents many opportunities, including the possibility of rapidly correlating specific wood decay proteins of the fungus with the corresponding gene sequences. Here we compare mass fragments of trypsin digests, determined by MALDI-MS (Matrix Assisted Laser Desorption Ionization-Mass Spectrometry), with predicted mass fragments derive...
T H de Koker, P J Kersten


Water transfer in wood in relation to fungal attack in building - Effect of condensation and diffusion
1992 - IRG/WP 92-1543
Wood is continuously exchanging moisture with the surrounding atmosphere, the temperature and relative humidity are important factors. Wood moisture in this case is not enough to provoque decay by fungi. However, when, during the night, condensation appears cyclically, wood absorbs water and moisture content may be sufficiently high to allow development if drying does not take place. The water tra...
D Dirol, J-M Vergnaud


Bethoguard; A new wood protecting fungicide for use in metal free ground contact wood preservatives
2002 - IRG/WP 02-30301
Research has identified the limitations in both the spectrum of activity and permanence of organic biocides placed in wood in high hazard environments, particularly in the absence of heavy metals such as copper. More specifically, the control of soft rot decay in wood in soil contact has proven to be most problematic. The new organic biocide, Bethoguard; an oxathiazine, has demonstrated excellen...
S C Forster, G R Williams, M Van Der Flaas, M Bacon, J Gors


Soft rot - Soil burial - Tests. Influence of the addition of nitrogen compounds to the soil on wood decay by soft rot
1972 - IRG/WP 213
The decay of wood specimens buried in soil is influenced by various factors. Decisive are the water content, the content of organic substances, the pH-value, the content of mineral nutritive salts, nitrogen content, etc. of the soil. These tests were carried out in order to investigate if the decay of wood in the soil will be influenced by additions of various nitrogen-compounds in different conce...
O Wälchli


Leaching tests on CCA-treated wood using inorganic salt solutions
1984 - IRG/WP 3310
Pinus radiata sapwood treated to approximately 10 kg/m³ with Tanalith NCA or Tanalith C-type CCA preservatives was ground to a fine powder and samples were then leached with solutions of calcium chloride, calcium nitrate, magnesium nitrate, or a mixture of potassium di-hydrogen orthophosphate and di-potassium hydrogen orthophosphate, at 0.03M-1.00M solution concentrations. Leached wood samples we...
D V Plackett