Testing wood in ground contact: An artificial soil
1977 - IRG/WP 280
This document is an interim report on the development of the artificial soil medium. It includes some information on the relationship between soil, wood and water which is of relevance in testing....
E F Baines, D J Dickinson, J F Levy


A review of environmental emissions from building and construction materials in comparison with preserved wood
2005 - IRG/WP 05-50224-11
A review of the public domain literature concerning emissions to the environment from materials which are used in the construction of buildings (e.g. Concrete, Asphalt, Galvanised Steel), in comparison with preserved wood, and a review of the approaches taken by the construction sector in assessing the risk from environmental emissions, in comparison with the approaches taken by the wood preservat...
E F Baines


Disposal of treated wood - Canada
1990 - IRG/WP 3563
It is estimated that treated wood removed from service each year in Canada contains about 16,000 tonnes of creosote, 1000 tonnes of pentachlorophenol and 245 tonnes of CCA or ACA. The amount of CCA treated wood for disposal is expected to increase more than ten-fold by the year 2020. At present, most treated wood is disposed of in landfills, burned (creosote only) or recycled as other products. Ot...
P A Cooper


How to determine what is a realistic emission from treated wood - basic reflections
1998 - IRG/WP 98-50105
Emissions from treated wood occur by evaporation and by leaching. Up to date by far more experience exists on leaching tests than on evaporation test. The methods applied will be of interest to give answers to the questions about the quantity of possible emissions. Standardisation on leaching started very early. One of the first attempts to quantify the effect of leaching on the remaining efficacy...
H Willeitner, R-D Peek


Variation in Canadian bluestain fungi: Tolerance to DDAC and DOT
1999 - IRG/WP 99-10303
Bluestain in Canadian wood products results in significant and unpredictable losses each year. In order to develop rational methods to eliminate or reduce the sapstain problem, a more complete knowledge of the causal organisms must be gained. This includes a knowledge of the variability in tolerance of different fungal species and strains to commercially used chemicals. In British Columbia, the ma...
J Dubois, A Byrne, J E Clark, A Uzunovic


A field test with Benzotar, an industrial residue, as a wood preservative
1985 - IRG/WP 3349
Benzotar, a residue of production of benzoic acid, was tested in field as a wood preservative. Results, after 6.5 years of exposure, showed that this product presents properties that improve the performance of wood in ground contact. This paper describes these results and presents a discussion an some aspects of its potential utilization in Brazil....
S Milano, L R Silva


Checking of sodium pentachlorophenate fixation in wood
1990 - IRG/WP 3620
In order to estimate the volatilization of sodium pentachlorophenate from treated wood, wood samples treated with pentachlorophenate were analysed after various durations of an EN 73 weathering The results giving no clear evidence of volatilization, treated wood samples were put in a test chamber with precise climatic conditions, the air used in the experiment being analysed. The pentachlorophenat...
M Lamour, H Sageot


The permanence of permethrin in wood preservation
1984 - IRG/WP 3288
The permanence of the synthetic pyrethroid permethrin in treated wood has been assessed for double vacuum and immersion treated Scots pine sapwood and whitewood using a 0.5% m/m solution of the insecticide in a hydrocarbon solvent. It is concluded that for all but the outermost 0.5 mm of the treated battens the distribution of the permethrin is relatively permanent. The outermost 0.5 mm appears vu...
R J Orsler, M W S Stone


The effects of heat treatment on anatomical changes of beech wood
2004 - IRG/WP 04-40284
The effects of heat treatment on anatomical changes of beech wood (Fagus orientalis) naturally grown and intensively used in forest products industry in Turkey were studied. The wood samples were cut into 2x2x3 cm and than conditioned at 25 °C and 65 % relative humidity for 3 weeks. Heat treatment was than applied to the wood samples at four different temperatures (130 °C, 150 °C, 180 °C and ...
Ü C Yildiz, Z Gerçek, B Serdar, S Yildiz, E D Gezer, E Dizman, A Temiz


Timber Preservation and Sustainable Construction in Australia
2005 - IRG/WP 05-50224-14
Sustainable development has been described as meeting the needs of the present without compromising the ability of future generations to meeting their own needs. (Bruntland 1987) To achieve the sustainable development goal therefore, the maximum performance has to be obtained from existing resources (timber) so that the remaining resource is protected from over-exploitation. Clearly, wood preserva...
J Norton


Inspection of tropical hardwood window frames in Nigeria for decay presence
1987 - IRG/WP 2294
A method of in situ inspection of hardwood window frames for expression of decay is discussed in this paper. The results show that about 6% of the frames inspected or 23% of the volume of wood in all the frames sampled in buildings erected between 1920 and 1984, exhibited evidence of advanced decay. Protection by the length of the eaves, species of the framing timber used, length of exposure to se...
M A Odeyinde, M A Amakiri, E B Lucas, J O Eyenike, S Akanni


Metal carboxylates for wood pest control
1996 - IRG/WP 96-30109
Metal carboxylates have been used as wood preservatives for more than fifty years. Predominantly salts of naphtenic acids have been commercially applied so far. They have water repellent as well as fungicidal and insecticidal properties. In the last years, metal carboxylates of saturated fatty acids were introduced. Fatty acids with 7-10 carbon atoms already have fungicidal activity by themselves....
F Pohleven, M Petric


The more important wood-destroying insects found in buildings in Poland
1974 - IRG/WP 128
In the different regions (voievodships) of the country Anobium punctatum and Anobium pertinax were to be found in the range of 47.7 to 63.5%. These insects were the main pests in urban buildings. In the second place came Hylotrupes bajulus occurring in the range of 25.9 to 45.1%. The other insects were to be found within the limits of 0.1 to 10.0%; only in a single instance did the amount reach 24...
J Dominik, J Wazny, M Czajnik


The First Annual Report of the International Research Group on Wood Preservation 1969-1970
1970 - IRG/WP A 7
IRG Secretariat


Some observations on miniaturised soil/block tests
1988 - IRG/WP 2317
Results are presented for miniaturised soil/block tests carried out in 120 ml capacity glass jars. The four test fungi (Coniophora puteana, Coriolus versicolor, Gloeophyllum trabeum and Poria placenta) reacted differently to different moisture regimes established by varying the soil moisture content. Acceptable levels of decay were achieved by the three brown rot fungi with soil at 110% whc; howev...
J K Carey


The use of zirconium as an inert fixative for borates in preservation
2001 - IRG/WP 01-30256
Stand-alone borates have been used in internal protected situations as wood preservatives for about 60 years. They have not been deemed acceptable for external situations because of their leaching characteristics. Work carried out to reduce the leachability of borates has been reviewed briefly here, and a specific fixation agent based on zirconium has been tested in standard leaching and decay tes...
J D Lloyd, J L Fogel, A Vizel


Performance of chromated copper arsenate-treated aspen fence posts installed in Forintek's Eastern test plot from 1951 to 1963
1984 - IRG/WP 3272
Aspen poplar fence posts were pressure treated by the full cell process using three formulations of copper chrome arsenate wood preservative. A total of one hundred and fifty nine of the posts were installed in service in Forintek's Chalk River post plot from 1951 to 1962. During the 1982 general inspection of the post plot all 159 posts were still in service. A groundline inspection was ...
C D Ralph


Cleaner prodiction and the wood preserving industry
1995 - IRG/WP 95-50040-29
H Carr-Harris, C R Coggins


Work program of CEN/TC 38 (January 1994). Durability of wood and derived materials
1994 - IRG/WP 94-20019
R Hüe


The most important wood-destroying insects in various countries (Results of questionnaire)
1981 - IRG/WP 1136
M-M Serment


Standardisation of tests of toxicity of preservatives to soft rot fungi
1978 - IRG/WP 2119
J G Savory


Report on biological control of decay in poles
1977 - IRG/WP 149
The following its a brief report on a preliminary experiment carried out for the United Kingdoms Midland Electricity Board during 1974-1975 to establish, under laboratory conditions, the potential controlling value of some non-decay fungi against Lentinus lepideus. Lentinus lepideus has been confirmed to be the commonest Basidiomycete causing decay in poles in the Boards area....
T A Oxley


Risk assessment and the approval of wood preservatives in the United Kingdom
1995 - IRG/WP 95-50040-23
An approval system operates in the United Kingdom (UK) for the regulation of wood preservatives. The regulatory authority uses a risk assessment approach to evaluate how far the potential for harm to people and the environment from wood preservatives is likely to be realised in practise, and hence the controls required for products to be, used safely. The evaluation for approval purposes also take...
R M Turner


Questionnaire: Facility for accelerated stake tests in unsterile soil
1981 - IRG/WP 2166
An acceptable name for this type of test facility has not yet been devised, but it has previously been referred to as a FUNGUS CELLAR or as a TROPICAL DECAY HOUSE. The attached pamphlet (What's New in Forest Research No.65) describes in broad terms the facility used for this purpose at FRI in New Zealand. Over the last two or three years several laboratories and commercial firms have inst...
J A Butcher


Wood preservation research at the Technical University in Zvolen - Slovakia
2004 - IRG/WP 04-10538
Presented paper gives basic information about wood protection in Slovakia and research in the field of wood preservation at the Technical University in Zvolen – the Faculty of Wood Sciences and Technology. The degradation processes in wood and wooden composites caused by fungi, environmental factors and fire, the identification of these processes, the protection of wood with fungicides and ot...
L Reinprecht