Volumes and weights of different CCA-C treated wood poles, anchor logs and crossarms of REB at air dry condition
1996 - IRG/WP 96-40073
Researches revealed the unit volumes and weights at air-dry condition (12% MC) of different poles, anchor logs and crossarms species of REB from this world. The softwood products are lighter than hardwood products. Inversely the unit volumes of softwood poles are higher than those of hardwood poles. Red pine (Pinus resinosa), radiata pine (Pinus radiata), blue pine (Pinus wallichiana), fir (Abies ...
A K Lahiry


Copper-resistant fungi on pressure impregnated wood in Denmark
1994 - IRG/WP 94-10078
The occurence of Amorphotheca resinae Parbery and its asexual stage Cladosporium resinae (Lindau) de Vries on CCA and CCB treated wood has previously been shown. In the autumn 1993 some other blue stain fungi were found on CCP and CCB treated pine timber, such as Ophiostoma minus (Hedgc.) H. and P. Sydow, Ophiostoma pilifera (Fr.) H. and P. Sydow and Ophiostona piceae (Munch) H. and P. Sydow. The ...
J Bech-Andersen, S A Elborne


Leaching of CCA components from treated wood under acidic conditions
1993 - IRG/WP 93-50004
The leaching of CCA components from treated wood under acidic conditions were investigated. Western hemlock treated with three types of CCA and two levels of target retention was subjected to leaching at four different levels of pH. After leaching tests, leached samples were subjected to laboratory decay and soft rot tests. The amount of CCA components leached was dependent on acidity of leaching ...
Jae-Jin Kim, Gyu-Hyeok Kim


Exploring the potential for plasma-assisted coating at atmospheric pressure for wood protection
2023 - IRG/WP 23-40982
J Profili, G Laroche


Programme. The IRG54 Scientific Conference on Wood Protection
2023 - IRG/WP 23-60518
IRG Secretariat


In service performance of wood sound abatement barriers
2024 - IRG/WP 24-41006
Sound abatement barriers made form treated hem-fir in service near Vancouver, Canada were inspected after about 10-12 years in service. The barriers appeared in good condition and no boards were to the point of needing replacement. The sound abatement decibel readings at all locations indicate they perform as well as concrete barriers and exceed the 5 dBA regulatory requirement for noise reduction...
S Kus, D Wong, R Stirling


Programme. The IRG55 Scientific Conference on Wood Protection
2024 - IRG/WP 24-60534
IRG Secretariat


Status of wood preservation in India
2005 - IRG/WP 05-30386
Wood, despite the advent of other modern materials, continues to play an important role in man’s day to day life. Usage of wood ranges from fuelwood to engineered wood products and demand for it is increasing which has resulted in depletion of forests and diminishing wood supplies. Future needs are required to be met from plantation timbers after adopting processing technologies for their life...
S C Gairola, P K Aggarwal


Artificial drying of impregnated wood
1987 - IRG/WP 3448
Sawn timber (Pinus Sylvestris) of dimension 50x150 mm was impregnated with CCA by a full-cell process. The timber was then dried in a conventional kiln or a special vacuum kiln where the timber was dried by circulating superheated steam. Drying time was 16 days and 2 days respectively. The aim of the investigation was to compare the physical appearence of the wood after drying by the two methods w...
M-L Edlund


A novel defaunation method of the protozoa to investigate cellulose metabolism in Coptotermes formosanus Shiraki (Isoptera: Rhinotermitidae)
1994 - IRG/WP 94-10050
The largest protozoa in the hindgut of workers of Formosan subterranean termite, Coptotermes formosanus Shiraki, was selectively eliminated by forced-feeding on low-molecular weight cellulose (LC) with a mean DP of 17. Although one week's feeding on LC caused perfect disappearance of Pseudotrichonympha grassii Koidzumi, the selective defaunation method itself had no detrimental effect on ...
T Yoshimura, K Tsunoda, M Takahashi


The effect of high temperature and long pressing time on the dimensional stability and decay resistance of OSB
2002 - IRG/WP 02-40237
The exterior use of OSB is restricted because when it is exposed to wet conditions swelling, loss of internal bond strength (IB) and decay occur. In this study an alternative process of pressing which results in the production of dimensionally stable and a more decay resistant strandboard was investigated. Boards were pressed at elevated temperatures for prolonged pressing cycles and their physi...
G J Goroyias, M D C Hale


The course of fixation of Cu-Cr-As wood preservatives
1972 - IRG/WP 307
Copper-chrome-arsenic (CCA) preservatives in contact with wood result in an instant extensive increase of pH, because of ion-exchange and adsorption reactions with the wood. During precipitation of the active elements the pH continuously increases but reaches a maximum, when all chrome is consumed. Some of the early reaction products are unstable and slowly convert via dissolution into stable comp...
S-E Dahlgren


Effects of a formaldehyde and sulphur dioxide treatment on decay and mechanical properties of aspen waferboard
1983 - IRG/WP 3242
Aspen wafers were sequentially treated under vacuum with formaldehyde and sulfur dioxide gas and pressed into waferboard bonded with powdered phenol formaldehyde resin. Decay resistance and strength properties were determined before and after simulated weathering. The water resistance of the phenol bonding system was lost in board made from the gas-treated wafers. This white rot fungus Coriolus ve...
E L Schmidt


Three dimensional computer representations of growth of microbial populations in wood
1984 - IRG/WP 1243
Creosoted distribution poles inoculated with either Lentinus lepideus, biological control organisms including Triochoderma or combinations of both were extensively sampled to monitor the spread of organisms. A computer program which enabled the results to be portrayed in a three dimensional graphic form was developed and is illustrated. Results showed that computer mapping of this type usefully en...
A Bruce, B King, C Bruce, G M Smith


Estimation of effective diffusion path lengths in wood by swelling studies
1989 - IRG/WP 3524
The effective average distance that a solute must diffuse to penetrate the cell wall matrix following pressure treatment is estimated from the rate of swelling of wood, vacuum treated with water. It is assumed that the diffusion paths are similar for water and a solute such as a wood preservative component. Since bound water diffusion coefficients for water in wood have been estimated by others, t...
P A Cooper, R Churma


Movement and persistence of chloropicrin, Vapam, Dazomet and methylisothiocyanate in red and white oak timbers
1992 - IRG/WP 92-3728
This study describes the movement and persistence of four fumigants in sawn red and white oak timbers exposed out of ground contact for 2 years. Chloropicrin moved the furthest from the point of application, and was the most persistent. Vapam was next best, followed by Dazomet. Methylisothiocyanate (MIT), applied as pellets, was not effective, probably because MIT was lost from pellets prior to tr...
T L Highley


Changes to New Zealand Timber Treatment Specifications
2004 - IRG/WP 04-20288
Changes have been made to the New Zealand timber treatment specifications in response to frequent incidences of decay in framing timber and doubts about the long-term performance of tributyltin formulations when used in exposed situations. Changes have been made to Hazard Class H1 to allow a level of treatment to provide short to medium decay resistance to framing which would protect it, should l...
M E Hedley


Testing method for the treatability of wood
1994 - IRG/WP 94-40031
In order to test and classify the treatability of wood species in pressure treatment processes with water-based solutions, a laboratory method was developed which allows the testing of small samples and limited sections of a stem, e.g. sapwood. The penetration of different liquids was determined separately concerning the three anatomical directions of wood. The common parameters for pressure impre...
A O Rapp, R-D Peek


Waste management of wood products in life cycle assessment
2000 - IRG/WP 00-50154
Within the framework of the European project LIFE SYS WOOD (contractnr. FAIR CT95-7026) TNO has performed a study on the waste management of wood demolition waste for inclusion in Life Cycle Assessment. In LIFE SYS WOOD one of the main aims was to develop a consistent LCA methodology for wood products. LCA case studies have been performed by partners on wood as raw material, glulam contructions, O...
P Esser, P Eggels, A Voss


The effect of creosote and Basilit on the boards of 4 wood species against destructive fungi in Northern Iran
1989 - IRG/WP 3555
The results of the experiments conducted on the boards of maple, hornbeam, alder and beech, show that under the humid and moderate climate condition of Northern Iran, after 30 months, the witness samples were about 10% destructed by fungi, especially by Schyzophyllum commune and Coriolus versicolor. The impregnated samples by Creosote Basilite using Rueping and Bethell methods, were quite intact. ...
D Parsapajouh


Laboratory evaluation of fipronil (a phenyl pyrazole) as a candidate termiticide in the protection of wood against the subterranean termite, Coptotermes acinaciformis (Froggatt) Rhinotermitidae
1997 - IRG/WP 97-10225
In this laboratory evaluation, radiata pine wood blocks (50 x 25 x 15 mm3) were impregnated with fipronil (a phenyl pyrazole) at various concentrations (0, 5, 10, 20, 40, 80, 100 and 200 ppm). Half the treated blocks underwent a leaching schedule for 5 days, while the remainder were unleached after treatment. Five replicates per treatment regime were presented to the test termite, Coptotermes acin...
B M Ahmed, J R J French, P Kwint, G Webb


The attack of naturally durable and creosote treated timbers by Limnoria tripunctata Menzies
1995 - IRG/WP 95-10132
Limnoria tripunctata was found tunnelling in creosote treated Douglas fir (Pseudotsuga menziesii) pilings and naturally durable greenheart (Ocotea rodiaei) gate seals at two sites on the south coast of the United Kingdom. Examination of thc creosote-treated wood showed that Limnoria tunnels were concentrated at a depth of 2-3 cm from the timber surface, where creosote loading was lower. Fewer tunn...
A J Pitman, G S Sawyer, G F Daniel


Alternative technologies for wood wastes recycling - Part B: Biotreatment of PCP- and creosote-treated wood
1998 - IRG/WP 98-50101-18 b
Alternative technologies have been investigated to detoxify treated wood. Two classes of organic compounds are studied. Creosote-treated wood are classified in France as dangerous wood wastes. A conventional incineration could be provided for these wood wastes but the cost of this elimination could be very high (> 2000 FFR/ton). For these reasons, we have tested two kinds of new processes as al...
S Legay, P Marchal, G Labat


Iron in stone wool - one reason for the increased growth and decay capacity of Serpula lacrymans
1992 - IRG/WP 92-1537
The chemical compositions of stone wool and glass wool were analysed. There was more iron in the stone wool than in the glass wool. It was found that iron present in stone wool was easily dissolved by oxalic acid that Serpula lacrymans is able to produce. The stone wool promoted the decay of pine wood by Serpula lacrymans. The glass wool had no effect on the decay capacity of Serpula Iacrymans. Th...
L Paajanen, A-C Ritschkoff


Durability of wood in the area of wood-inhabiting termites in Slovenia
1981 - IRG/WP 1139
This report describes a research dealing with resistance and durability of five different species of wood. The experiment was made in natural conditions in the Slovene area of wood-inhabiting termites. The results of our experimental field, which correspond to the results of the former laboratory experiments, show a very weak resistance of spruce-wood, fir-wood, and beech-wood. They also show thei...