IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 3079 documents. Displaying 25 entries per page.


Charring of Norway spruce wood surface – an alternative surface modification technique?
2019 - IRG/WP 19-40870
Charring is an old wood surface treatment technique, mainly performed on wooden façade elements with the aesthetical aims, but also with the purpose of protection. This flame treatment method can be grouped into heat treatment processes. Below the top charred layer of damaged wood there is a layer which is during flame treatment exposed to high temperatures in anoxic or semi-anoxic conditions. Th...
M Petric, M Pavlic, J Zigon


Improvement of wood decay and termite durability resulting from combined treatments based on borax/phenol-formaldehyde impregnation followed by thermal modification
2019 - IRG/WP 19-40871
This study determined the factors influencing the boron content after leaching of pine blocks impregnated with aqueous solution of phenol-formaldehyde (PF) resin with or without borax and subjected to heat treatment by response surface methodology. An experimental design permits to analyze the effects of heat treatment temperature (150, 185 and 220°C), curing time (5, 12, 5 and 20 hours), resin c...
S Salman, M-F Thevenon, A Petrissans, S Dumarcay, P Gerardin


Biofinish: A Functional Wood Surface Treatment based on Aureobasidium
2020 - IRG/WP 20-40903
Xyhlo Biofinish is a natural and environmentally friendly wood protection concept based on linseed oil impregnation and a fungal-based coating. It emerged in the late 1990s and has been developed over the past 15 years into an industrially applicable process in the Netherlands. The combination of linseed oil impregnation and a surface treatment with the living fungus Aureobasidium extends the serv...
S Rensink, M Sailer, S Roukens, J Gerber, H van der Mel, K Potgieter, J Spit, R Bulthuis, C Struck, M Bennink


The influence of chemical compounds on wood cell wall to surface cracks
2020 - IRG/WP 20-40908
Degradation due to cracking and dimensional changes caused by drying, have a significantly negative impact on the preservation and durability of wood. Therefore, the prevention of surface cracking, which tends to occur during the drying process, is vital. High temperature set drying is one of the most effective methods for preventing wood surface cracking. It begins with softening the wood at a hi...
R Suzuki, Y Mori, K Yoshihiro, K Yamashita, M Kiguchi


Plasma treatment of wood - a review of 15 years of research in Göttingen
2021 - IRG/WP 21-40913
Wood is an important renewable resource and can be found omnipresent in everyday life. Its natural properties offer numerous advantages regarding physical, mechanical but also aesthetic aspects, but also challenges that one has to address with various modification methods. Driven by the desire to promote the use of promising new technologies using plasmas, there has been a close research network ...
P Sauerbier, R Köhler, G Avramidis, W Viöl, H Militz


Influence of weathering on surface roughness of thermally modified wood
2021 - IRG/WP 21-40915
Thermally modified wood is exposed to weathering similarly as other wood-based building materials. It has been reported that if thermally modified wood is exposed to weathering, its moisture performance might decrease fairly fast. The aim of this study was to determine whether this phenomenon is associated with crack formations or roughness. Norway spruce, thermally modified spruce, wax-treated th...
E Kerzic, B Lesar, M Humar


Surface morphology and short-term water uptake of charred and coated wood
2021 - IRG/WP 21-40916
Charring of the wood surface represents a traditional alternative surface treatment technique with the purpose of aesthetics and protection. By the treatment with flame the surface of wood becomes carbonized and a few millimetres thick charred layer is formed on the top of the wooden element. Further, the charred layer can be removed by brushing, which accentuates the structure of the surface. Add...
J Zigon


Dynamics of fungi colonization on the surface of Scots pine wood during natural weathering in different European climate zones
2022 - IRG/WP 22-10984
Wood The presence of fungi leads to biomaterial decay and/or changes in aesthetical appeal. The start of fungi colonization as well as the following growth on wood are primarily influenced by four factors: ambient temperature, moisture history of the object, access to oxygen, and intrinsic properties of the exposed wood, considered here as a source of nutrients for microorganisms. A prevalence of ...
F Poohphajai, O Myronycheva, O Karlsson, L Rautkari, J Sandak, A Sandak


Impact of wetting agents on polyelectrolyte complex impregnation for wood fire-retardancy
2022 - IRG/WP 22-30768
Wood fire performance is a great concern in interior finishing due to the high risk of flame spread. To increase the use of wood in high building while ensuring the safety of building occupants, fire retardant (FR) treatments are required. Traditionally, two fireproofing strategies are employed: impregnation and coatings. They have been widely studied but they, respectively, are time and chemicals...
M Soula, J B Grenier, S Duquesne, F Samyn, V Landry


Surface chemical wood densification through in situ electron beam polymerization: description and dose study
2022 - IRG/WP 22-40933
Traditional wood chemical densification processes can be used to improve wood mechanical properties by increasing density of the material throughout its thickness. While mechanical surface densification has heavily been investigated, surface treatments involving impregnation of monomers remain unexplored. This study describes a new material, surface densified through lateral impregnation of acryla...
J Triquet, P Blanchet, V Landry


Comparative study of the properties of silicate coatings with different mineral pigments (titanium dioxide, iron (III) oxide, copper (II) oxide) on the surface of wood
2022 - IRG/WP 22-40936
Silicate coatings are attractive alternatives to conventional organic-based coatings for wood protection. In this work, silicate coatings were prepared with a potassium silicate binder modified with a methyl siliconate solution, and three types of mineral pigments titanium dioxide, iron (III) oxide and copper (II) oxide. The coatings were applied on beech wood and cured under ambient conditions. T...
A M Cheumani Yona, M Petrič


Optimized composition of alkyd emulsion with nanoparticles of iron oxide for enhancing protection of thermally modified wood
2022 - IRG/WP 22-40940
Thermal treatment is acknowledged as an environmentally friendly method to improve durability of wood and some of its properties, such as biological resistance, dimensional stability, reduced hygroscopy. Despite these improvements, when used outdoors, also thermally treated wood is subjected to the action of environmental factors, like solar radiation, moisture, precipitations, temperature, etc., ...
E Sansonetti, D Cīrule, I Andersone, B Andersons, E Kuka


Effect of nano-particle characteristics and concentration on UV protection of timber: A field exposure test
2022 - IRG/WP 22-40941
Wood has a well-known susceptibility to ultra-violet light degradation, leading to premature replacement. A variety of products have been developed to protect against this damage, but most provide less than 12 months of protection and must be regularly reapplied. Developing improved coatings would help reduce wood losses and reduce maintenance costs. Nano-particles have a variety of attractive pro...
T Yi, J J Morrell


The influence of thermal modification and surface charring to different levels on wettability of Norway spruce wood
2022 - IRG/WP 22-40942
The wood can alternatively be protected from water absorption by thermal modification and charring. Both techniques cause certain chemical and physical changes in the wood, the extent of which depends on the level of temperature applied. The objective of this study was to determine how the combination of charring to different levels and thermal modification affects the chemical, morphological, and...
J Žigon, C Gerardin, M E P Wålinder, P Gerardin


Accelerated surface mould testing for exterior wood treatment in Temperate, Tropical and Laboratory environments
2023 - IRG/WP 23-20699
Mould attack is a very common cause of discoloration on wooden surfaces and can subsequently promote development of wood decay by other organisms. Prevention of mould growth is relevant for both pigmented wood paints as well as more transparent systems with a high or low amount of binder. The use of commercial biocides has led to effective microbiological inhibition in many contexts, but the incre...
A Nazeri, J Stenbaek, T R Laursen, A H H Wong, B M Hasnul


Effects of preservative impregnations on wettability and surface free energy properties of Eucalyptus grandis wood
2023 - IRG/WP 23-40978
Wettability and surface free energy (SFE) are crucial parameters for evaluating the adhesion thermodynamics of solid surfaces. Hence, this study investigated the effects of copper azole (CA) and disodium octaborate tetrahydrate (DOT) preservative impregnations on Eucalyptus grandis wood wettability and SFE. Wettability was determined in terms of contact angles with polar (water) and non-polar (dii...
A A Alade, C B Wessels, H Stolze, H Militz


Starch modified with silanes – high hydrophobic surface treatment for wood protection
2023 - IRG/WP 23-40981
The great potential of silanes for starch modification and their utility as surface wood protection is still not sufficiently assessed. The work aimed to analyze the crosslinking process's effect on starch modification with silane and tested the hydrophobic properties of surface-treated wood. The starch treatment was modified with methyltrimethoxysilane or N-octyltriethoxysilane. SEM-EDX with a cr...
W Perdoch, M Bajstok, B Mazela, I Siemińska, B Peplińska


A novel treatment for increasing UV stabuility of wood based on citric acid and urea
2024 - IRG/WP 24-30811
Wood, a fundamental material in the Built Environment, faces challenges related to durability and weathering, notably UV degradation leading to colour changes. This study explored a novel treatment method utilising citric acid and urea to enhance the UV stability of wood. The reaction between these compounds forms fluorescent species and insoluble nanoparticles upon thermal treatment. Two treatmen...
S Jué, A Scharf, C-F Lin, R Moutou Pitti, D Sandberg, D Jones


Danish wood preservatives approval system with special focus on assessment of the environmental risks associated with industrial wood preservatives
2001 - IRG/WP 01-50166-01
The following is a description of the procedure used by the Danish Environmental Protection Agency to assess the environmental risks associated with preservatives used in the pressure impregnation of wood. The risk assessment covers issues considered to be of significance for the environment and which are adequately documented so as to allow an assessment. Such issues are persistence and mobility ...
J Larsen


Data sheet on wood-boring insects. Apate monachus Fabricius. 2. Position systématique, nomenclature, identification et distribution - Espèces végétales attaquée
1981 - IRG/WP 1105
R L A Damoiseau


Confocal laser scanning microscopy of a novel decay in preservative treated radiata pine in wet acidic soils
1997 - IRG/WP 97-10215
Light microscopy of radiata pine (Pinus radiata D. Don) field test stakes (20x20x500mm3) exposed in wet acidic (pH 3-4) soil for 12 - 24 months showed predominance of an unusual type of decay characte-rised by tunnelling attack of wood cell walls. After two years decay was moderate to severe in wood treated to ground contact CCA specifications and also equivalent retentions of creosote, and a numb...
R N Wakeling, Ying Xiao, A P Singh


Effect of acetylation on decay resistance of wood against brown-rot, white-rot and soft-rot fungi
1989 - IRG/WP 3540
Effect of acetylation on decay resistance of wood was investigated using wood blocks of Cryptomeria japonica, Pinus densiflora, Albizia falcata and Fagus crenata. Blocks were treated with uncatalyzed acetic anhydride for different lengths of time and exposed to Tyromyces palustris, Serpula lacrymans, Coriolus versicolor and unsterilized soil. The action of OH-radical on acetylated wood was also ex...
M Takahashi, Y Imamura, M Tanahashi


The IRG..Chanelling information and ideas into the mainstream of wood preservation technology
1985 - IRG/WP 5241
IRG Secretariat


JWPA method for testing effectiveness of surface coatings with preservatives against decay fungi
1981 - IRG/WP 2164
In 1979 JWPA established a new method for testing effectiveness of surface coatings in accordance with practical use of preservative-treated lumber. Comparing the new testing method with JIS A 9302, a few new trials - size of wood specimen, weathering procedure, and decay-test procedure - are incorporated....
K Tsunoda


Wood preservation in Poland
2004 - IRG/WP 04-30362
Dynamic growth of market demand for wooden elements and articles, generated in Poland increase of interest in industrial preservation. Today, Poland is a substantial producer and exporter of wood made products. Majority of exported wood - approximately 70% - is scotch pine (Pinus silvestris L.), which, due to its natural durability, requires preservation....
A Kundzewicz


Previous Page | Next Page