Natural resistance of twenty-six Guianese wood species against marine borers
1988 - IRG/WP 4144
This note is a contribution on the study of the natural resistance of some wood species from French Guiana, some of which could be found too in the neighbourhood. Here are presented the results after one year exposure in the marine environment....
L N Trong


Report on a field demonstration of methods for detecting defects in wood poles
1984 - IRG/WP 2232
P I Morris, H Friis-Hansen


Detection of brown rot decay in wood by ion mobility spectrometry
1991 - IRG/WP 2377
A test method for the detection of brown rot decay in wood is described and involves a two-step procedure: thermal release of vapours from wood samples followed by analysis using Ion Mobility Spectrometry (IMS), with results being obtained in 5-10 seconds. The advantages, limitations as well as the detection limit of the technique are presented....
A H Lawrence, T Nilsson


Short term preconditioning of preservative-treated wood in soil contact in relation to performance in field trials
2000 - IRG/WP 00-20185
The effect of pre-exposure to primary colonising micro-organisms on preservative-treated wood, prior to a basidiomycete decay test, was determined by preconditioning in two soil types. Scots pine EN 113 blocks treated with 3 model systems (a triazole, a copper quaternary compound and a copper boron triazole) were leached according to EN 84 and subjected to 6 weeks and 8 weeks burial in either John...
S Molnar, D J Dickinson


Reliability-based service life prediction methodology for assessment of water protection efficiency for coatings on wood
2003 - IRG/WP 03-20268
Assessment of water protection efficiency according to EN 927-5 has been shown to give significant differences in water absorption values for different types of coatings on wood. It is shown that the combination of EN 927-5 and an artificial weathering procedure gives more information regarding expected durability and long-term performance than a single measurement of water absorption on fresh, un...
J Ekstedt


Fungal defacement of water-stored softwoods
1993 - IRG/WP 93-10009
Sapstain, mould and basidiomycete defacement of untreated sawn boards of Scots and Corsican pine was recorded during a 14 week field trial. Boards were cut from freshly felled logs and from logs previously maintained under water sprinklers for 6 months and ca. 4 years. The incidence of sapstain defacement or the freshly felled wood was very servere aftcr 2 weeks and remained so throughout the boar...
M A Powell, R A Eaton


The resistance of fifteen Indonesian tropical wood species to the powder post beetle Heterobostrychus aequalis
1990 - IRG/WP 1429
A preliminary laboratory test on the resistance of 15 tropical wood species to Heterobostrychus aequalis has been carried out using small samples of 7.5 x 5 x 1.5 cm³. The results reveal that Pinus merkusii and Agathis borneensis are very susceptible to Heterobostrychus aequalis. Other 13 species vary between susceptible to resistance There is no signifisant relation between starch content and th...
Jasni, Nana Supriana


Preventive action against fungal decay: A comparative experiment on the effects of natural and artificial infection of wood by Basidiomycetes
1981 - IRG/WP 2160
M Fougerousse


Report on Sub-group 5 in Raleigh, 6 May 1980
1980 - IRG/WP 1123
S Cymorek


United States Federal Committee on Wood Protection
1971 - IRG/WP 43
A C Jewett


Elimination of alternative explanations for the effect of iron on treated wood
1993 - IRG/WP 93-30006
Amounts of iron which had previously been found in stakes removed from ground contact reduced decay of untreated wood by four brown-rot fungi. This suggested that the effect of iron may be on the preservative. Analysis of the leachates from CCA- and ACA-treated wood blocks first exposed to rusting iron, then to a brown-rot fungus, showed that the increased decay found in the laboratory for wood ex...
P I Morris, J K Ingram, D L Gent


Natural durability and basic physical and mechanical properties of secondary commercially less accepted wood species from Brazil
2002 - IRG/WP 02-10451
The natural durability towards basidiomycete fungi and termites of several secondary timber from Brazil (Vatairea sp., Hymenolobium sp., Inga sp., Manilkara sp., Caryocar sp., Terminalia sp., Apuleia sp.) has been evaluated according to the EN 350-1. Some basic physical and mechanical properties (density, shrinkage, hardness, colour, static strength in flexion and compression) were also measured a...
M-F Thévenon, A Thibaut


Improved resistance of Scots pine and Spruce by application of an oil-heat treatment
2000 - IRG/WP 00-40162
Spruce (Picea abies L. Karst.) and Scots pine (Pinus sylvestris L.) were subject to a heat treatment which was carried out in an oil-bath. The aim was to improve the dimensional stability of the treated wood and its resistance against fungi. The bath of vegetable oil provides a uniform heat transfer at temperatures of 180°C, 200°C and 220°C and protects the submersed wood from oxygen. Heat trea...
M Sailer, A O Rapp, H Leithoff


Some wood-destroying Basidiomycetes. Volume 1 of a collection of monographs
1981 - IRG/WP 1121
One of the first tasks of the International Research Group on Wood Preservation, when it began its work in 1969, was to compile a series of reports on the common decay fungi which can attack wood. This volume, which contains the first of these reports, has been compiled with the help of mycologists and wood preservation specialists in France, Ghana, the Federal Republic of Germany, the Netherlands...
R Cockcroft


Synergistic effects between 2-HPNO, Irganox 1076 and EDTA on the inhibition of wood degradation by Coriolus versicolor
2004 - IRG/WP 04-30331
The efficiency of 2-hydroxypyridine-N-oxide (2-HPNO) as wood preservative has been investigated. As shown using classical experiments as well as using response surface methodology, the efficiency of 2-HPNO as wood preservative is strongly improved in presence a chelator like EDTA and/or of Irganox 1076 an industrial antioxidant. In these conditions, wood preservative efficiency of the mixture the ...
A Mabicka, S Dumarçay, N Rouhier, M Linder, J P Jacquot, P Gérardin, E Gelhaye


Marine borers and marine wood protection - Some answers and some outstanding questions - A comment
1990 - IRG/WP 4163
A brief description of the nature of hazards encountered in different parts of the marine environment is given. An attempt is then made to assess what were the essential findings of selected areas of research in the marine wood protection field and what still needs to be done. That is, if we are to more adequately understand what we are attempting to do in this field of study!...
J E Barnacle


Depletion of wood preservatives after four years' marine exposure in Mt. Maunganui harbour, NZ
1994 - IRG/WP 94-50036
This paper reports on chemical analysis of marine test samples exposed in Mt. Maunganui harbour, New Zealand from 1977 to 1981. Depletion data for a Class II CCA, a CCA-A formulation, acid copper chromate and ammoniacal copper arsenate are presented. The results suggest differences in the rate of loss of individual preservative components among the four formulations and redistribution of individua...
K J Archer, A F Preston, C M Chittenden, D R Page


The Fifth Annual Report of the International Research Group on Wood Preservation 1973-1974
1974 - IRG/WP 531
IRG Secretariat


Model questionnaire for preparation of monographic cards for wood-destroying fungi
1972 - IRG/WP 103
C Jacquiot


Microscopic characteristics of Pinus radiata wood veneers weathered outdoors for one yea
1993 - IRG/WP 93-10018
Radiata pine (Pinus radiata) wood veneers glued to solid wood hacking strips were exposed outdoors at 45° north-facing for one year and then examined by light microscopy (LM) and transmission electron microscopy (TEM). As expected, the exposed wood surfaces were colonised by a variety of microorganisms; however, wood decay was not observed. Ultlaviolet (UV light) radiation and water were the main...
A P Singh, R A B Sweeney, E A Dunningham, D V Plackett


Marine borers as wood degraders in Bangladesh and their protection
1996 - IRG/WP 96-10186
Field study on timber piles used in Bangladeshi brackish waters revealed that untreated and pentachlorophenol treated piles drastically degraded by the attack of molluscs and pholads (marine borers). Adequately CCA-C impregnated (30 kg/m³ or 6% W/W dry oxide retention) timber piles can protect the attack of molluscs. It is very difficult to protect pholads which can invade naturally very durable ...
A K Lahiry


About the water and biological resistance of some new chemically modified wood composites
1997 - IRG/WP 97-40077
As well known, wood represents a valuable natural composite material with a very large utilisation as solid wood or in wood based composite materials. Its qualities but also its defects as the dimensional instability, the susceptibility to biological attack, the anisotropy, are due to its complex structure. Research has demonstrated that the chemical modification of wood, meaning the involving of ...
M C Timar, M D Mihai, G Baciu


A note on testing the efficacy of wood preservatives above ground
1995 - IRG/WP 95-20078
A number of test methods have been used to evaluate the performance of wood preservatives in above ground situations. These have included EN 113 tests following natural exposure weathering (NEWT), L-joint or T-joint tests, lap-joint tests, and decking tests. A new test referred to as the A-frame test has been developed and is under evaluation. This is based on a sandwich-type test in which a thin ...
G R Williams, J A Drysdale, R F Fox


A bibliography of organic solvent-based wood preservatives
1973 - IRG/WP 322
H Alliot


The role of communication in the field of environment protection: A case study "Wood Protection"
1990 - IRG/WP 3574
L Wöss