IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 3576 documents. Displaying 25 entries per page.


Potential toxicants for controlling soft rot in preservative treated hardwoods. Part 4: Evaluation of combined diffusion and toxicity
1979 - IRG/WP 2129
A large number of inorganic and organic preservatives were evaluated as potential soft rot control chemicals, by their degree of inhibition of fungal growth after allowing them to diffuse through a 6 mm thick wood slab. The tests were inoculated with wood powder from soft-rotted CCA treated poles. Pentachlorophenol was unable to diffuse quickly through the wood slab, although formulations with hex...
E W B Da Costa, O Collett


Degradation of the normal fibre walls of rubberwood (Hevea brasiliensis) by the tropical blue-stain fungus Botryodiplodia theobromae
1998 - IRG/WP 98-10286
Rubberwood was examined by light microscopy and transmission electron microscopy (TEM) after exposure to the common tropical sapstain fungus Botryodiplodia theobromae for four weeks to study hyphal colonisation of wood cells and to determine if this fungus also degraded lignified normal fibre cell walls in addition to the walls of non-lignified elements. Light microscopy revealed relatively large ...
A A H Wong, A P Singh


A collaborative test to determine the efficacy of poyurethane coatings on wood samples exposed in the marine environment. 1st Interim Report
1988 - IRG/WP 4145
Wood samples coated with elastomeric polyurethane (ca. 50 mils thick) were exposed for up to 2 years in 12 tropical and temperate marine test sites with known teredinid, pholad and/or crustacean infestations. All uncoated control samples were destroyed or partially destroyed. Polyurethane-coated samples were not attacked, the surfaces of the coating were sound and the polyurethane adhered well to ...
R A Eaton


Production of preservative-treated wood in some countries
1990 - IRG/WP 3598
This report presents figures of the production of preservative-treated wood and wood treated with anti-stain chemicals in 26 and 20 countries respectively from all over the world....
J Jermer


Identification card for Coriolopsis polyzona (Pers.) Ryv
1977 - IRG/WP 161
A Ofosu-Asiedu


An interim report on trials with 'Boliden K33' and 'Celcure A' in water of different salinities in the Baltic Sea and in the UK
1974 - IRG/WP 406
It was felt necessary to undertake field trials using large test samples exposed in natural water of different salinity in order to determine preservative leaching and to assess the degree of biological attack....
R A Eaton, D J Dickinson


Programme Section 3 Wood protecting chemicals
1999 - IRG/WP 99-30210
IRG Secretariat


A method for determining boron diffusion coefficients in wood
1999 - IRG/WP 99-30200
The radial unsteady-state diffusion coefficient for boron in southern yellow pine (Pinus spp.) was determined from measured concentration profiles using Egner's solution, a modified form of Fick's second law. The method uses a slicing technique to accurately determine concentration gradients with time in a single direction. The methodology should be applicable to any diffusible s...
J-B Ra, H M Barnes


Environmental behaviour of treated wood in (semi-)permanent contact with fresh or seawater
1998 - IRG/WP 98-50101-20
This study presents a strategy for the environmental toxicity evaluation of treated wood towards the aquatic compartment, using non target water organisms toxicity tests. A lixiviation process is applied on wood (Pinus sylvestris) treated with several wood preservatives formulations. The lixiviation process is carried out in the laboratory with ultrapure water or synthetic seawater. After chemica...
P Marchal, C Martin


Leaching of inorganic wood preservatives – Investigating the relationship between leachability, dissociation characteristics and long-term leaching potential
2003 - IRG/WP 03-50199
Estimation of the leaching properties of preservative components is greatly affected by the leaching test method applied since not all methods equally consider the physical components responsible for leaching. These include: wetting of the wood and penetration of water (affected by dimensions, amount of end grain, permeability, duration and nature of water exposure); solution of preservative comp...
L Waldron, Y T Ung, P A Cooper


Ground contact performance of wood treated by the MSU process
1990 - IRG/WP 3609
Environmental concerns have prompted a renewed interest in accelerated fixation schemes for CCA-treated wood. Results from stake tests of southern pine (Pinus sp.) treated using a conventional Bethell cycle are compared with matched stakes treated using the MSU Process. The effects of adding boric acid to the preservative formulation are also discussed. Differences among test plots are discussed....
H M Barnes, T L Amburgey, R W Landers


Evaluation and approval of wood preservatives. Unification of European requirements
1988 - IRG/WP 2310
This paper reviews the current activities within the European Homologation Committee for Wood Preservatives (EHC) towards unification of the requirements on evaluation and approval of wood preservatives in Western European countries....
J Jermer


Decay patterns observed in butylene oxide modified ponderosa pine after exposure in unsterile soil
1982 - IRG/WP 3211
Small blocks of ponderosa pine (Pinus ponderosa Laws) chemically modified with butylene oxide to three different weight gains were exposed for 6 weeks in unsterile soil. Severe surface decay caused by soft rot fungi and tunnelling bacteria was observed in blocks with 8 weight percent gain. The soft rot attack was restricted to the outer parts of the radial walls in the latewood tracheids. Bacteria...
T Nilsson, R M Rowell


Laboratory experiments on aerial emissions from wood treated with wood stains
1993 - IRG/WP 93-50001-06
Due to the actual environmental interest in wood preservation, a series of experiments was carried out on the emission of biocides from treated wood. The research focussed on the volatilization of 5 biocides from boards treated with wood preservative finishes containing dichlofluanide (DCF) azaconazole (AZA), pentachlorphenol (PCP), iodopropynylbuthylcarbamate (IPCB) and tributhyltinoxide (TBTO). ...
G M F Van Eetvelde, M Stevens


Disposal of Pressure Treated Wood in Construction and Demolition Debris Landfill
2005 - IRG/WP 05-50235
Pressure treated wood is often disposed in landfills in the US, very frequently in construction and demolition (C&D) debris landfills. C&D debris disposal facilities in many states are not equipped with liner systems to protect underlying groundwater. In this paper, issues associated with the disposal of metal-containing treated wood in C&D debris landfills are discussed. C&D de...
T G Townsend, B Dubey, J Jambeck, H M Solo-Gabriele


Damage by wood-attacking insects in buildings in Sao Paulo State - Brazil. (including errata slip)
1978 - IRG/WP 175
From 1974 to 1978 up to 602 buildings attacked by wood-boring insects were inspected by Instituto de Pesquisas Tecnologicas in Sao Paulo State - Brazil. Damage was caused mainly by subterranean termites, dry-wood termites and wood-attacking beetles. Up to US $ 1000,000 is the amount needed to control such insects in the buildings inspected...
A T De Lelis


End grain sealants for wood preservation studies
1985 - IRG/WP 3341
The results of tests with possible end grain sealants for wood preservation studies are reported. The epoxy resins used gave satisfactory performance on wet or dry Sitka spruce and have been used with success for diffusion treatment studies....
R J Murphy, N A Summers


Status of the Working Group on Preservation of Wood in the Marine Environment - Questionnaire results
1977 - IRG/WP 434
At the joint meeting of the IRG and COIPM dealing with preservation of wood in the marine environment, it was suggested that a Marine Group should be formally recognised within IRG. It was agreed that a questionnaire (Document No: IRG/WP/424) should be circulated to determine the views of the membership on the future status of this group. The results of this questionnaire are presented....
R A Eaton


Quality control of microwave treatment of timber after dry rot attack
2001 - IRG/WP 01-40205
In Denmark microwave treatment of timber has been used during the last 15 years for eradication of dry rot (Serpula lacrymans). About 1500 microwave treatments have been employed in coorporation with Hussvamp Laboratoriet. Previously all the infected timber was removed plus an extra metre as a safety zone. This meant that all casting boards and plaster had to be removed as well and joists replaced...
J Bech-Andersen, J Andreasson, S A Elborne


Disposal of CCA treated waste wood by combustion - An industrial scale trial
1996 - IRG/WP 96-50068
Totally 272 m³ (62.7 t) of CCA treated utility poles were chipped and incinerated at Jalasjärvi Gasification Plant. In average the whole batch of chips contained 57 kg of elementary copper, 95 kg chromium and 76 kg arsenic. During the 56 h combustion trial the measured arsenic emission to the air was 76 g in total. Copper and chromium emission was less than 1 g. The condensing water from the coo...
A J Nurmi


The use of image analysis to quantify soft rot decay
1992 - IRG/WP 92-2410
Image analysis techniques can provide quantitative information from visual images. As part of a wider interest in decay assessment methods we have investigated the application of image analysis techniques for quantifying soft rot decay by Chaetomium globosum in transverse sections of birch wood and bamboo. A method for reducing contamination of the section (and image) by the fungal hyphae and of s...
P J Wickens, R J Murphy


Wood preservation in Kenya
2000 - IRG/WP 00-40191
Current research on wood preservation in Kenya is mainly on the development of biological control of wood-destroying termite species, using mycoinsecticides. The major research institutions include the Kenya Agricultural Research Institute (KARI), Kenya Forestry Research Institute (KEFRI), Moi University and the International Centre for Insect Physiology (ICIPE). Training institutions include Fore...
G Ochiel


A new laboratory technique devised with the intention of determining whether, related to practical conditions, there should be a relationship between growth rate and decay capacity (of different strains) of Serpula lacrymans
1989 - IRG/WP 1384
Most laboratory techniques for the determination of growth rate not only use a medium (agar) unrelated to practice, but also yield values that are often far less than those found in practice. Also, most laboratory techniques for the determination of decay capacity ensure that the whole of a small test block becomes fully surface-colonised within the first few days; whereas in Australian practice S...
J D Thornton


Decay resistance of Scots pine (Pinus sylvestris) heartwood against brown rot
2002 - IRG/WP 02-10433
Natural decay resistance of wood is mainly restricted in the heartwood and based on wood microstructure and chemical composition. The genetic variation in the durability of Scots pine (Pinus sylvestris L.) wood against decay and the relationship between resistance and chemical composition was studied. The laboratory tests of 6 and 8 weeks were carried out with a brown rot fungus Coniophora puteana...
H Viitanen, A M Harju, P Kainulainen, M Venäläinen


Criteria for basidiomycetes testing and ways of defining natural durability classes
1998 - IRG/WP 98-20144
Within the framework of a European research project several laboratories have tested a series of 17 wood species covering the total range of natural durability. Basidiomycete tests are part of the total set up. Although generally based upon standard methods some minor differences in execution of the tests were evaluated for their impact on the results. This variation was superimposed with the fac...
J Van Acker, M Stevens, J K Carey, R Sierra-Alvarez, H Militz, I Le Bayon, G Kleist, R-D Peek


Previous Page | Next Page