Comparative investigations between thermal and microwave assisted digestion as a novel tool for the chemical analysis of inorganic wood preservative components
2011 - IRG/WP 11-20461
The correct chemical impregnation of wood requires an internal as well as external quality control of the treated wood. The active is located in a solid matrix, therefore it is often difficult to analyse such material since most analytical procedures are based on liquid systems. Because of this quite a number of methods – like extraction or thermal digestion - were developed in order to transfer...
H Ahl, J Fromm, E Melcher


Quantitative design guideline for wood outdoors above ground applications
2011 - IRG/WP 11-20465
This paper describes the background and principles behind an engineering design guideline for wood in outdoor above ground applications, i.e. use class 3 according to EN 335. The guideline has been developed in the European research project WoodExter and can be seen as a first prototype for a quantitative design tool in the area of wood durability. It is based on a defined limit state for onset of...
S Thelandersson, T Isaksson, E Suttie, E Frühwald, T Toratti, G Grüll, H Viitanen, J Jermer


Methods of field data evaluation - time versus reliability
2011 - IRG/WP 11-20466
Field testing of wood and wood-based products is so far the most reliable way to get information on performance with respect to durability and expected service life. However, field trials are extremely time and cost consuming. The main objective of the present study was to investigate possible correlations between early stages of decay, preferably during the first 5 years, and the actual service l...
P Larsson Brelid, C Brischke, A O Rapp, M Hansson, M Westin, J Jermer, A Pilgård


Investigating extraction of bifenthrin from composite wood products
2011 - IRG/WP 11-20467
Bifenthrin is added to resin prior to lay-up of plywood and laminated veneer lumber to provide termite protection. Analysis of this chemical in resins can be challenging. The potential for using ground wood in place of sawn material to recover bifenthrin was investigated using laminated veneer lumber composed of Douglas-fir veneers analyzed by three laboratories. Although the results differed amo...
J J Morrell, L Bell, J Norton, C Shaw


Improving our understanding of moisture and other durability-related properties of wood in building envelope performance prediction
2011 - IRG/WP 11-20468
Building science has become an increasingly important field in recent years with rapid changes in construction methods, building materials and consumer expectations. The field has also been brought to prominence by a few large-scale premature building envelope failures in a few regions across the world. Considerable effort has been put into developing hygrothermal models to simulate heat, air, vap...
Jieying Wang, P Morris


Decay initiation in plywood, OSB and solid wood under marginal moisture conditions
2011 - IRG/WP 11-20469
Hygrothermal models are increasingly used as research tools by building scientists and and design tools by designers to simulate heat, air, vapour, and water movements within and through building envelope and even to predict the consequences in terms of mould/decay growth and metal corrosion. This work was designed to generate data on decay initiation under marginal moisture conditions to support...
Jieying Wang, P Morris


Aesthetic service life of coated and uncoated wooden cladding - influencing factors and modelling
2011 - IRG/WP 11-20470
Mould growth on exterior coated cladding façades is an undesirable element and will often shorten the aesthetical service life. Mould growth on painted surfaces is influenced by type and concentration of film fungicides, the paint formulation and the wood substrate itself, and wooden cladding may experience exponential fungal deterioration caused by variation in the climatic factors, often within...
L Ross Gobakken, O A Høibø


Classification of wood materials using Fourier Transform Near Infrared Spectroscopy and multivariate analysis
2011 - IRG/WP 11-20471
A distinction between preservative-treated wood and non-treated wood can be demonstrated by the combination of Fourier Transform-Near Infrared Spectroscopy (FT-NIRS) and Multivariate Analysis (MVA). This technique is non-destructive, quick, easy to use and can be portable. The calibration models for different heavy metals are set up using principal component analysis (PCA) to classify species of t...
M A Bouslamti, M A Irle, C Belloncle, V Salvador, S Hulot, B Caron, E M Qannan


Sample Origin Influencing the Leachability of Wood Preservatives
2011 - IRG/WP 11-20474
The aim of this study is to see if the raw material influences fixation and leachability of wood preservatives. Moving towards more eco-friendly and –concious society, the wood industries must adjust itself to new rules and regulations. Greener solutions in wood protection are being tested and introduced, older systems are being improved, but questions still arise concerning some elements curren...
K Kängsepp. E Larnøy, P Meier


Slice - Cut and Analyze Laser Microdissection (LMD): A method to produce sample material from modified wood for chemical quality analysis
2011 - IRG/WP 11-20478
Wood modification with its various systems is an established way to enhance a wood products’ service life in outdoor applications. Per definition, selected material properties are enhanced by means of modification without producing toxic substances or residues during service life and combustion afterwards. The systems of impregnation modification include a physical and often chemical alteration ...
K Zimmer, E Larnøy, A Treu, M Fongen


Non-destructive evaluation of wood decay
2011 - IRG/WP 11-20479
Evaluation of wood decay is often prone to subjective assessment. Standard rating scales are based on human perception of decay, often in addition to weight loss measurements. Especially the assessment of graveyard specimens or other long term testing material that has to be monitored regularly on a non-destructive basis, is challenging. In this paper two techniques are presented that can deliver ...
J Van den Bulcke, I De Windt, N Defoirdt, J Van Acker


LOSP for glulam, when should the treatment be applied?
2011 - IRG/WP 11-30555
Treatment options for outdoor above-ground (H3) exposed glulam of Pinus radiata and P. elliottii were examined. Beams were treated with azole LOSP (containing a zinc tracer) aiming for retentions of 35-40 l/m3 or 70-80 l/m3. Treatment was conducted either before or after gluing. TBTN LOSP and CCA were included as comparative treatments. Test specimens for exposure were cut after treatment, while w...
L J Cookson


Influence of wood swelling agents on penetration and copper leaching of copper-ethanolamine based wood preservatives
2011 - IRG/WP 11-30556
Copper ethanolamine based preservatives are currently the most important solutions for impregnation of wood in ground contact in Europe. One of the issues related to those and similar water based solutions is insufficient penetration to refractory wood species like Norway spruce. In order to elucidate this issue, commercial copper ethanolamine based solution was supplemented with five different wo...
M Humar, N Thaler, B Lesar


Ten Year Field Tests of Borate-Treated Wood Against Subterranean Termites
2011 - IRG/WP 11-30557
In the mid 1990s, Forintek Canada Corp. initiated a study of the termite resistance of borate-treated lumber above ground, protected from rain in Canada, Japan and Hawaii. Predominant termite species at three test were Reticulitermes flavipes in Canada, and Coptotermes formosanus in both Japan and Hawaii. The material included hemlock and amabilis fir lumber treated with disodium octaborate tetrah...
P I Morris, J K Grace, K Tsunoda


Phytosanitary standards and the potential for acceptance of chemical treatments as a phytosanitary measure
2011 - IRG/WP 11-30558
Regulations governing international trade in forest products must balance the economic and social benefits of trade with the potential risks of transporting invasive species. The International Plant Protection Convention (IPPC) is an international agreement intended to manage this process. It develops international phytosanitary standards (ISPMs) that are recognised by the World Trade Organisation...
A Uzunovic, R Stirling, J J Morrell, P I Morris, C F Schauwecker


Effect of P/F ratio, PF concentration and treating method on boron leaching from wood treated with PF modified boron compounds
2011 - IRG/WP 11-30559
In order to immobilize boron in wood, three kinds of resol-type phenol-formaldehyde (PF) resin with different P/F ratios were synthesized in laboratory and incorporated with three types of boron compounds to treat wood. The used boron compounds included boric acid (BA), borax (BX) and disodium octaborate tetrahydrate (DOT). The leaching test of boron from wood blocks was performed according to the...
Liping Yu, Jinzhen Cao


Characterisation and evaluation of various chitosan oligomers, and decay resistance
2011 - IRG/WP 11-30562
Chitosan, a polymer of D-glucosamine, is known for its antimicrobial activity. However, the physicochemical properties of chitosan depend upon three principal factors, i.e. source of raw material, molecular weight and degree of deacetylation. Here, we report synthesis and characterization of chitosan oligomers prepared by deaminative depolymerization of chitosan (s) obtained from Sigma Aldrich and...
I Hussain, C Chittenden, T Singh


Comparison of rates of wood decay from four different field test protocols following 4-5 years exposure at a site in New Zealand
2011 - IRG/WP 11-30565
The rate of decay of Pinus radiata was evaluated using four different field test protocols at a site near New Plymouth, New Zealand. The average Scheffer index was 86 over the five year period of testing. The field tests were an in-ground stake test (AWPA Std E7-01) and three above ground tests – lap-joint (AWPA Std E16-98), decking (AWPC protocol) and ground proximity tests (AWPA Std E18-06) T...
P Lobb, K Day, A Siraa


Copper Nanoparticles in Southern Pine Wood Treated with a Micronised Preservative: Nanodistribution of Copper in the Pit Membrane and Border of an Earlywood Bordered Pit
2011 - IRG/WP 11-30566
Copper nanoparticles can penetrate the cell walls of unlignified parenchyma cells in southern pine wood treated with a micronised wood preservative, but they are excluded from lignified tracheid walls. This paper extends these observations to include the cell wall layers of the bordered pit. Focused ion beam and ion milling were used to make an ultra-thin section of the cell wall layers of an earl...
H Matsunaga, Y Kataoka, M Kiguchi, P Evans


The potential for using CuO nanoparticles as a wood preservative
2011 - IRG/WP 11-30569
The potential for using nano-copper particles for wood protection was investigated using mini-agar slant and wood block tests with Gloeophyllum trabeum or Trametes versicolor. Nano-copper was more effective against G. trabeum than T. versicolor, although neither of these fungi would be considered copper tolerant. Nano-copper solutions were stable over a 17 week storage period, but precipitated w...
I S Weitz, K Knani, M Maoz, C Freitag, J J Morrell


Protective Levels of Borates in timber Foundation Piles 5 – 18 Years after In-situ Remedial Treatment in Areas with Wet Clay Ground Conditions. The Jerbor and Eurobor Protocol, Part 1.
2011 - IRG/WP 11-30571
Timber has been used as foundation piles and grillages for decades or even centuries. Since the late 1970s a method for investigate, analyze and treat building timber foundations in soft clay grounds against decay fungus with a biocide have been developed and used by the late professor Allan Jerbo. Settling of buildings in soft clay grounds is continuously monitored and if damages to the building ...
M Theorin, K-M Bandh


The study of fungicidal values und sorption processes of ionic liquids- potential wood preservatives on soils
2011 - IRG/WP 11-30572
In the paper, the fungicidal activity of new ionic liquids structures, N,N-dimethylalkylamines derivatives, containing a spacer built of 7 or 10 methylene groups with nitrate(V) and tetrafluoroborate anions, didecyldimethylammonium and benzalkonium nitrate(V) were presented. The research was also conducted on the sorption of cations of ammonium ionic liquids on five types of podzolic, humic alluvi...
W Przybylska, J Zabielska-Matejuk, A Stangierska, A Skrzypczak


Effectiveness of Water Based Bentonite-Borate Slurry for In-situ Remedial Protection of Historic Wooden Piles: The Eurobor Protocol, Part 2
2011 - IRG/WP 11-30574
The study of the biocide product Eurobor®, water mixture of boric acid, borax and sodium bentonite, aimed to verify previous findings regarding borates penetration from a clay-water mixture of foundation timber. The product was applied on samples from 100 year old timber foundation from the city of Göteborg. Although in ground for this long the timber was in acceptable god condition due to groun...
M. Theorin, K. Fimmerstad, K-M. Bandh


Biological and mechanical performances of particleboard panels made from maritime pine (Pinus pinaster) and glued with cornstarch-mimosa tannin-urea formaldehyde adhesive
2011 - IRG/WP 11-40542
The objective of this work was to demonstrate the utility of cornstarch-mimosa tannin-based resins designed for application as an adhesive in the particleboard production. Bond qualities of cornstarch-mimosa tannin- urea formaldehyde (UF) (10:4:86, weight ratios) resins and commercial UF resin were assessed by using an automatic bonding evaluation system, prior to production of particleboard panel...
A Moubarik, F Charrier, A Pizzi, A Allal, B Charrier


Acetylation Properties of Southern Pine and Radiata Pine
2011 - IRG/WP 11-40543
The chemical modification of wood via acetylation with acetic anhydride has been a well investigated technology and is of current commercial interest due to improved properties such as dimensional stability as well as resistance to termites and resistance to rot and decay fungi. Despite this, the acetylation of a board substrate requires further investigation in order to assess board properties a...