Environmental situations on wood preservation industries in Japan
1995 - IRG/WP 95-50040-21
Because of environmental civil oppinions, Ministry of Agriculture, Forestry and Fisheries in Japan, reviesed "the standards for sawn lumber" in 1994. For the possibilities of the use of preservatives out of CCA, by the using of the hazard levels, new products like ACQ, DDAC and emulsified zinc-naphthenate can be used in the standards. Since 1994, the permitable limit of the arsenic in the waste wa...
K Suzuki


Wood preservation in Iran
1984 - IRG/WP 3270
The report sketches the history of the use of wood in Iran to the establishment of the country's national forest service and gives some figures for Iran's timber needs by the year 2000. Progress in wood preservation has been slow, although items such as railway sleepers and poles have been pressure treated since the first pressure impregnation plant was erected in 1932. Today the...
P Niloufari, R Cockcroft


Wood attacking insects in urban areas in Sao Paulo State - Brazil
1985 - IRG/WP 1267
From 1974 to 1984 the investigators of Wood Division (IPT) inspected, for insect attack, more than 1,500 buildings of several kinds: commercial, residencial and historical buildings, houses and industries. In all cases, IPT was asked to give advices on control and erradication. During that time three papers concerning this problem were published (Cavalcante, 1976; De Lelis, 1978; Zanotto & Can...
P A Zanotto, M D Canedo, D A T Lelis


Possible durability transfer from durable to non durable wood species. The study case of teak wood
2001 - IRG/WP 01-10392
Teakwood is well known for its excellent natural durability, mostly due to its high proportion of extracts. Amongst these extracts, quinones, and more precisely some naphtoquinones (such as lapachol) and anthraquinones (such as tectoquinone) appear to play a crucial role in the resistance to wood decay organisms. At a laboratory scale, sawdust from malaysian teak heartwood has been extracted under...
M-F Thévenon, C Roussel, J-P Haluk


Comparison of thermally modified wood originating from four industrial scale processes – durability
2002 - IRG/WP 02-40229
This study examined the differences in biological wood properties of heat treated wood originating from four different European industrial heat treatment plants. The manufacturers of heat treated material were: PLATO Hout B.V./Netherlands, Thermo Wood/Finland, New Option Wood/France and Menz Holz/Germany where Oil-Heat treated Wood (OHT) is produced. The results of miniblock tests with basidiomyc...
C R Welzbacher, A O Rapp


Management strategies for the disposal of CCA-treated wood
2000 - IRG/WP 00-50155
A two-fold management strategy is presented for the disposal of wood treated with chromated copper arsenate (CCA). The first part focuses on the use of alternative wood treatment preservatives. The second part of the management strategy addresses short-term disposal issues (less than 25 years) by developing new methods to handle the waste. A set of seven alternative wood preservatives were evaluat...
H M Solo-Gabriele, T G Townsend


Resistance of acrylic paints on wood against growth of the rot fungus Dacrymyces stillatus
1990 - IRG/WP 2345
In the last few years the presence of the rot fungus Dacrymyces stillatus has been repeatedly confirmed in external wood panels, particularly from wood painted with water based paints. A laboratory method for testing of the fungal resistance of paint films on wood has been developed.This method has been used to test the efficacy of the fungicides Parmetol DF 18 and Parmetol HF 25 against attack by...
J Bjurman


Method of embedding and staining of wood after biological testing to support the identification of decay type
1998 - IRG/WP 98-20131
A method for preparing wood for microscopic analysis after decay testing is described, with special regard to a novel fast simultaneous staining, which helps to identify different types of decay. The novel staining process is explained as well as the embedding of heavily decayed samples in polyethylene glycol (PEG) and picking up of sections by transparent adhesive tape. Special feature of the int...
A O Rapp


The kinetics of anhydride modification reactions of wood. Experimental results and theoretical modelling
1998 - IRG/WP 98-40125
Although the chemical modification of wood remains a fertile area for research, there has been little work performed on the kinetics of the modification process. The reaction kinetics of a series of linear chain and cyclic anhydrides has been studied and activation energies of the reaction determined. The reaction kinetic profiles are determined by the relative rates of reaction of the reagent wit...
C A S Hill, J G Hillier


Genetic Engineering in tree breeding
1998 - IRG/WP 98-10294
The genetic improvement of forest trees by classical breeding is a slow process in comparison with that of annual crops. Tree breeding however is of great importance and has led to trees with better growth characteristics and better disease resistance. An important wood characteristic which has been neglected in breeding programs is wood durability. The durability of the wood will determine for wh...
J Van Doorsselaere, H Beeckman, M Van Montagu, W Boerjan


The use of light organic solvents in industrial wood preservation - an environmental perspective
1995 - IRG/WP 95-50040-22
The paper examines the evolving regulatory environment concerning the use of hydrocarbon solvents in industry and, in particular, the European wood preserving sector. The implications of the proposed EU Directive on industrial solvent use are explained and possible responses to such regulation examined, including process modification, product changes and emission abatement, where necessary. The de...
G A Ewbank


FLUROX, a new breakthrough in insect control for wood preservation
1995 - IRG/WP 95-30079
FLUROX (flufenoxuron) is an acylurea insecticide which acts as a growth regulator in insects. FLUROX inhibits the production of chitin - the exoskeleton or 'skin' of the insect. When the exposed larva attempt to moult to its next stage of development, it is unable to produce a new skin and dies. FLUROX has been found to be extremely active against wood borers, when applied in a p...
A R Valcke, M Pallaske


IRG test of preservative-treated hardwoods with particular reference to soft rot. Report on condition of specimens installed in Victoria, Australia
1984 - IRG/WP 3318
Over a third of the treated stakes involved in this test have been mechanically damaged. As many of these stakes broke off at or near groundline they could not be reinstalled. So they have been removed from the study despite most exhibiting little or no decay. Because of the mechanical damage to a substantial number of the treated stakes, we propose to terminate the CSIRO part of this study after ...
G C Johnson, J D Thornton


Collaborative soft rot tests: Final Report
1978 - IRG/WP 2106
Since preparation of Document No: IRG/WP/258 results have been received from the remaining collaborators. Thus there is a little further to add to the conclusions already derived, those in Document No: IRG/WP/251 being as follows: 1) the exposure system used sometimes resulted in excessive weight gains in the sterile check blocks. Consequently the corrected loss in weight of the test blocks could ...
J G Savory, J K Carey


On the use of probit analysis for assessing the toxicity of wood preservatives
1974 - IRG/WP 244
To elucidate the general character of the action of the toxic material on the fungus, it is sufficient to carry out preservative tests using the previously described procedure, but in doing so, it is necessary somewhat to change the number of specimens and their arrangement in jars. Five concentrations of toxic material are tested simultaneously. For the testing of one preservative ten jars should...
D A Belenkov


Imaging fungal deterioration of wood using x-ray microtomography
1997 - IRG/WP 97-10240
Nondestructive tomographic images of solid Southern yellow pine (SYP) wood and SYP during deterioration by wood decay fungi were obtained by using a new class of synchrotron X-ray computed microtomography (CMT). The CMT images will provide information about spatial relationship between degrading fungi and wood structures. Wood samples were scanned with synchrotron-generated X-rays at high resoluti...
B Illman, B A Dowd


Minimum inhibitory concentration of methylene bisthiocyanate towards selected wood inhabiting fungi in liquid culture and on radiata pine
2001 - IRG/WP 01-30261
The objective of the current study was to determine the minimum inhibitory concentration (MIC) of methylene bisthiocyanate (MBT) towards wood inhabiting fungi common on unseasoned radiata pine (Pinus radiata D. Don). The fungi used were Ophiostoma floccosum, Leptographium procerum, Sphaeropsis sapinea and Trichoderma viride. Fungi were individually inoculated into nutrient media spiked with differ...
T Singh, B Kreber, C Chittenden, R N Wakeling, A Stewart


Preservative treatment specifications in Fiji
1982 - IRG/WP 3190
The preservative treatment specification used in Fiji is outlined. Reference is made to a basic end use classification and to locally approved treatment processes, preservatives and retention levels. Amenability ratings are defined and penetration requirements for broad commodities indicated. Currently commercial operations rely entirely on pressure treatment with copper-chrome-arsenic multisalts ...
A S Alston


Standard and accelerated testing of boron-additive wood protection systems
2005 - IRG/WP 05-30381
The main objective of this research was to determine the effectiveness of boron-additive protection systems for above ground applications by means of field testing. The two field test procedures used are based on the L-joint test described in the European standard EN 330. For the first set up the boron treated timber was coated in accordance with the standard EN 330 system. The second set up is ba...
A Mohareb, J Van Acker, M Stevens


A quantitative weathering study of wood surfaces modified by chromium VI and iron III compounds
1989 - IRG/WP 2330
Thin veneers of Pinus radiata were treated with dilute aqueous solutions of chromium VI and iron III compounds and exposed to natural weathering for 35 days. Zero-span tensile strength and weight losses of treated veneers were compared with losses observed in untreated specimens In a study designed to demonstrate the applicability of strength and weight loss measurements to the rapid quantitative ...
P D Evans, K J Schmalzl


Co-operative studies on determining toxic values against wood-destroying basidiomycetes: Progress report to April 1990
1990 - IRG/WP 2357
This document reports progress on the co-operative study between nine laboratories, set up following the proposals contained in Document IPG/WP/2316 (1988). Results have been received from eight laboratories. Toxic values data have been established successfully for the test fungus Coniophora puteana with soil, malt agar and vermiculite methods and with the test fungi Gloeophyllum trabeum and Poria...
J K Carey, A F Bravery


Wood detection by the marine isopod Limnoria.markup
1995 - IRG/WP 95-10134
The search for alternative control methods for Limnoria, should perhaps focus on the most vulnerable stage during the isopod life cycle - during dispersal when adulls leave their tunnels to find new wood. Dispersal is known to be triggered by environmental conditions, although how Limnoria locate fresh wood is unknown. Literature available on Limnoria dispersal, their sensory capabilities during d...
S M Henderson, S M Cragg, A J Pitman


The natural history of teredinid molluscs and other marine wood borers in Papua New Guinea
1975 - IRG/WP 410
The teredinids, commonly known as teredos or shipworms, are bivalve molluscs adapted to boring into wood. They are most closely related to the Family Pholadidae, or piddocks, which bore into mud, stone and coral. The teredinids have a relatively small, hemi-spherically shaped shell, the elongated body extending beyond the posterior end of the shell valves. The soft body, protected by the wood and ...
S M Rayner


A new type of biocide suitable for use in different fields of wood preservation
1993 - IRG/WP 93-30014
A new type of polymeric biocides was developed containing quaternary ammonium and boron ester groups as active structure elements, to overcome the disadvantages of AAC's in wood preservation use and to utilise their good performance due to a broad efficacy against fungi on the other hand. The new biocides called polymeric betains have been tested in laboratory and field tests and especial...
V Barth, H Härtner


The durability of wood polymer composites against fungi and insects
2000 - IRG/WP 00-40161
New materials such as wood polymer composites are used more in France. These materials are obtained by mixing wood and thermoplastics in different ratios. These kind of material must be considered as new materials and some characteristics such as durability must be evaluated for outdoor applications. On the other hand, some recycled fibers from wood waste could be used as raw materials. Some woodp...
G Labat, I Le Bayon, J Gerard, F Amin