IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 3410 documents. Displaying 25 entries per page.


Vapour boron treatment of wood based panels: Mechanism for effect upon impact resistance
1994 - IRG/WP 94-40036
Samples of medium density fibreboard, chipboard and oriented strandboard (OSB) were treated to two retentions of boric acid by a vapour phase treatment. The results of a range of mechanical tests were reported by Hashim et al. (1992, 1993) in which a small reduction in impact resistance was observed. Several investigations were carried out to study how and where this loss in impact resistance occu...
R Hashim, R J Murphy, D J Dickinson, J Dinwoodie


Ammoniacal wood preservative for use in non-pressure treatment of spruce and aspen poplar. Part 1
1984 - IRG/WP 3273
End-matched lumber of Picea glauca (Moench)Voss (white spruce) and Populus tremuloides Michx. (aspen poplar) timbers was treated by a thermal diffusion process in open tank treating vessels using an ammoniacal copper-arsenate wood preservative. The process proved technically feasible with respect to controlling the vapourization of ammonia from open tanks during treatment at high temperatures. Tre...
C D Ralph, J K Shields


Canadian code of good practices - Recommendations for design and operation of wood preservation facilities
1990 - IRG/WP 3582
The rationale and procedures for the development of a set of recommendations for design and operation of wood preservation facilities in Canada are discussed. Multi stake holders involvement in problem identification, problem assessment, state of the art knowledge database, implementation and periodic assessment procedures are important considerations for the successful development of a Code of Go...
V N P Mathur, G Das


Issues Facing Wood Preservation in New Zealand Today
2003 - IRG/WP 03-30326
In New Zealand, the three major issues facing the wood preservation industry today are: Extension of use of LOSP preservatives, chiefly tributyltin naphthenate, for treatment of products in Hazard Class H3 exposed to the weather for which LOSP have not been traditionally used. Concerns have been expressed about the long-term durability of such products. Restrictions on the use of CCA preservativ...
M E Hedley


Effects of heat treatment on water repellence and anti-swelling efficiency of beech wood
2002 - IRG/WP 02-40223
The heating of solid wood to higher temperatures is the simplest and the cheapest means for stabilizing its dimensions. For the investigation of the effect of thermal treatment on water repellency effectiveness and anti-swelling efficiency of beech wood (Fagus orientalis Lipsky), air-seasoned samples of beech wood were heated in presence of air at temperatures of 130 C, 150 C, 180 C and 200 C for ...
S Yildiz


Decrease of the antidecay resistance of beech wood treated with organotin fungicides after its natural ageing
1998 - IRG/WP 98-30185
The antidecay resistance of beech-wood samples (120 x 8.5 x 8.5 (MM)) treated with tributyltin fungicides gradually decreased due to prolongation of their natural ageing: tributyltin fungicides (TBTO, TBTS, TBTCA, TBT-DEDTK were applied by pressure impregnation technique in ethanole solutions (c = 0. 1%, 0.33% or 1%); treated beech-wood samples were naturally aged without their contact with grou...
L Reinprecht


Study of the degradation of retified wood through ultrasonic and gravimetric techniques
1994 - IRG/WP 94-40030
One of the non-polluting processes that increase the natural durability of wood is a thermal treatment in an atmosphere poor in oxygen, producing what is normally denominated "retified wood". In this study the validity of a non-destructive technique (ultrasound) in order to determine the biodegradation suffered by wood across time has been studied. For this reason, the behavior of a wood species (...
D T De Troya, A M Navarrete


Resistance of Teak, Balau, keruing and Chengal Wood species against marine borers attack
2004 - IRG/WP 04-10513
Wood samples of Teak (Tectona grandis) , Keruing (Dipterocarpus alatus),Yellow Balau (Shorea laevis) and Chengal (Balanocarpus heimii) were treated by Creosote, using Ruping method. The dimension of samples were 200 x 75 x 20 mm and the retention were 188, 186, 331, 40 kg /m3 respectively. Both treated and untreated samples were installed in sea water (Mahshar in Persian gulf and Bandar Torkman an...
A Rezanejad


Treatment of wood-based panel products with volatile borate
1990 - IRG/WP 3616
The paper presents recent developments in the use of volatile borate esters for the preservative treatment of wood based board materials. Several advances on previous reports are discussed. In laboratory studies, treatment times of approximately ten minutes at 20°C on boards at equilibrium moisture content provided full penetration and retentions of 1% wt/wt boric acid. Biological tests have been...
P Turner, R J Murphy, D J Dickinson


A comparison between the effects of ACC & CFK on the durability of beech, hornbeam and cottonwood by using Dipping & Bethel methods in the North of Iran
1997 - IRG/WP 97-40089
From the economical point of view, increasing the lumber durability by the application of preservative treatments is very important. In this study, samples were randomly selected from Fagus orientalis Lipsky., Carpinus betulus L. and Populus deltoides Bartr. in two forms (Board & Squared cross-section) and have been treated with ACC & CFK by using Dipping & Bethel methods. The matched ...
D Parsapajouh, V Etemad, K Pourtahmasebi


Microwave conditioning of Pinus radiata D. Don for preservative treatment
2000 - IRG/WP 00-40182
This paper reviews the effect of pressure steam conditioning on the permeability and treatability of green radiata pine heartwood and the potential for substituting microwave conditioning for steaming. The penetration of liquids into radiata pine occurs mainly in the radial tissue. The permeability of green radiata pine improves following steam conditioning by blowing out the soft radial tissue. T...
P Vinden, G Torgovnikov, J Romero


Sampling rates and the probability of detecting defective treatment in the sampling of preservative treated timber
1987 - IRG/WP 2277
When attempting to enforce standards of penetration and retention set for treated timber, the regulating authority must establish a sampling or inspection scheme which will prevent large quantities of substandard product entering the market. On the other hand, the scheme should not penalise treaters for the small quantities of such material which are inevitably produced by any industrial process. ...
M J Kennedy, L E Leightley


Inhibition of termite damage by N'N-napthaloylhydroxyamine (NHA): Reticulotermes flavipes (Kollar) vs. Coptotermes formosanus Shiraki
2000 - IRG/WP 00-10354
The calcium precipitating agent NHA has been shown to protect southern yellow pine (SYP) from wood decay and termite damage comparable to CCA in field tests (Gulfport, MS) for two years (Crawford and Green, 1999). In a collaborative study, SYP wood blocks were vacuum treated with three concentrations of aqueous NHA and exposed in a no-choice test to Eastern subterranean termites (FPL, USA) and For...
F Green III, S T Lebow, T Yoshimura


Treatment of wood with formaldehyde. Acid catalysis of the reaction between formaldehyde and wood
1980 - IRG/WP 3146
Formaldehyde reacts with the free OH-groups in wood forming cross-linking bonds. The reaction can be brought about without any catalyst but in that case the activation energy is very high and high temperatures and long reaction times are needed. Normally, the reaction is catalysed by different acids. Acid catalysts, however, tend to degrade the cellulose and the wood matrix causing reduction in th...
T Vihavainen, K Piispanen, P Mansikkamäki


Practical consequences of the clarification of the chemical mechanism of CCA fixation to wood
1983 - IRG/WP 3220
Practical consequences derived from the chemical investigation of the mechanism of fixation of CCA to the wood constituents are discussed. Among these, formulas for the calculation of the time of hexavalent chrome fixation are presented. Furthermore, three parameters are shown to be important to the long-term effectiveness of CCA-treated timber: (i) the temperature of treatment, (ii) the initial p...
A Pizzi


Environmental situation on wood preservation industries in Bangladesh
2000 - IRG/WP 00-50148
The hazard that wood preservative chemicals pose to people and the environment is serious. The lack of information, legislation and awareness create an unfavorable situation on wood preservation industries. In this regard, three wood preservation industries have been visited to collect the information about pollution. It was observed that different steps have been taken to minimize the contaminati...
K Akhter


The treatment of sawn whitewood with organic solvent wood preservative
1982 - IRG/WP 3192
The impregnation schedules approved in the UK for the treatment of sawn European whitewood (Picea abies) with organic solvent borne preservatives result in comparitively high loadings relative to the limited depth of penetration they achieve. Results are presented, which show how substantial reduction in the overall loading may be achieved without concomitant reduction in penetration. A model for ...
L D A Saunders


The foreign exchange situation and fate of wood preservation in Nigeria
1989 - IRG/WP 3558
Up to about 15 years ago, wood utilization industry in Nigeria gave no serious thoughts to wood preservation. After this period however, as a result of escalated local demand for sawn timber, logs with wider sapwood and mainly of secondary tree species requiring protection of the sawn timber became dominant in the local timber scene. Preservatives both for protection in and out of ground contacts ...
M A Odeyinde, S C Ifebueme


Wood protection by surface treatment of two borate preservatives, TIM-BOR® and BORA-CARE®, for the formosan subterranean termite and eastern subterrean termite
1993 - IRG/WP 93-10044
TIM-BOR® (disodium octaborate tetrahydrate: DOT, Na2B8O134H2O) and BORA-CARE® (40% DOT in ethylene glycol) are two borate products marketed for treating wood in use by brushing or spraying onto the wood surface. The active ingredients presumably diffuse into wood by the 10-15% existing wood moisture. Few data, however, are available to demonstrate the diffusion rate. Su & Scheffrahn (1991) s...
M Toroko, N-Y Su


Laboratory evaluation of borate formulations as wood preservatves to control the subterranean termite coptotermes acinaciformis (isoptera: Rhinotermitidae) in Australia
2001 - IRG/WP 01-30266
The termiticidal efficacy of Borocol (sodium octaborate tetrahydrate), boric acid, bore-ester-7 and tri- methyl borate was evaluated in laboratory bioassays against Coptotermes acinaciformis (Froggatt). Seasoned sapwood blocks of Pinus radiata D. Don, and Eucalyptus regnans (F. Muell) were impregnated with the various borate compounds. There were marked differences in mass loss and mortality rate ...
B M Ahmed, J R J French, P Vinden


Some data on the activity of alternative fungicides for wood preservation
1985 - IRG/WP 3333
Data from laboratory tests against basidiomycete fungi are presented for 9 alternative fungicides in organic solvent formulations and also in water for one product. Results are compared with data for reference preservatives, tributyltin oxide, copper and zinc naphthenates and pentachlorophenol. Of special interest is the apparently better than additive effect of mixing tributyltin naphthenate and ...
A F Bravery, J K Carey


A technique for determinging the efficacy of wood preservatives for partially treated timber
1988 - IRG/WP 2322
A technique is described for determining the efficacy of wood preservatives either for certain wood species where a full penetration cannot be achieved by normal vacuum-pressure methods or for more permeable species to look at efficacy of treated zone in preventing decay of an untreated core. Both sapwood and heartwood planks of spruce (Picea abies) and pine (Pinus sylvestris) were treated by CCA ...
A J Nurmi


The new National Directive on wood preservation in the Netherlands
1998 - IRG/WP 98-50101-03
In the Netherlands the major part of treated timber is sold under the KOMO-certificate. The National Directive for vacuum pressure treated timber on which certification is based, is currently being revised. The new National Directive will contain a code of good practice including maximum leaching figures. It incorporates quality requirements for treated timber, existing legislative requirements an...
W J Homan, J K B Kwisthout, J Dubelaar


Wood preservation in Kenya
2000 - IRG/WP 00-40190
Focussing an Wood Preservation in Kenya, the Report discusses and elaborates on Education and Training, Research, Wood deteriorating organisms, Treatment Plants and Processes, Preserving Chemicals, Specifications, Markets, Health and Safety and Environmental issues. Education and Research is limited to one Institution only, other Institutions involved with the properties and utilization of wood ha...
R Venkatasamy


Durability of Wood Plastic Composites Relative to Natural Weathering and Preservative Treatment With Zinc Borate
2005 - IRG/WP 05-40316
Wood-Plastic Composites (WPCs) used for decking have experienced dramatic increases in North America, averaging 25% growth per annum since 1998. A key factor contributing to this growth has been the successfully communicated message that they are "virtually maintenance free". The common perception being that the wood fiber is completely encapsulated by the thermoplastic resin, minimizing the pot...
M E Mankowski, F M Ascherl, M J Manning


Previous Page | Next Page