The influence of the location of a wood defect on the modulus of elasticity determination in wood durability testing
2004 - IRG/WP 04-20287
This study investigates the influence of the location of a wood failure in stakes upon elastic changes observed in beech specimens with the resonance vibration technique. Natural failures were simulated by artificially created defects at different locations of the test stake. The results indicate that the location of an attack in a stake is important for the measurement outcome. When the attack is...
L Machek, H Militz


Borates as wood preservatives - an environmental, health and safety perspective
1993 - IRG/WP 93-50001-03
Boron compounds are highly effective wood preservatives and have an established safe use in the timber treatment industry. Their widespread background occurrence in nature, low acute mammalian toxicity and useful properties make them versatile active ingredients within today's environmentally aware society. A critical review of health, safety and environmental data on the borates, their u...
J B Rainer


Fungi causing sap stain in wood
1980 - IRG/WP 199
The present paper is a revised edition of former Document No: IRG/WP/125. It contains some additions and an explanation of terminology, as was suggested at a previous meeting of the Group. The paper is a compilation based mainly on available literature. Some of my own unpublished results have been added together with other unpublished data which have been received from the Bundesanstalt für Mater...
A Käärik


Influence of CCA and TnBTO on wood decay, under different oxygen levels and various initial moisture content
2001 - IRG/WP 01-10415
Fagus sylvatica (beech) and Pinus sylvestris (Scots pine) were impregnated by TnBTO (tributyl-tin oxide) and CCA (chromated copper arsenate). In wood blocks two levels of moisture content (50% and 100% of saturation point) were used. Three levels of oxygen concentrations (10, 21, and 50%) were chosen. Treated and untreated wood were exposed to three fungi (C. versicolor a white rot, C. puteana, a ...
S M Kazemi, R J Murphy, D J Dickinson


Examination of algal and wood extracts for the control of marine borers
1999 - IRG/WP 99-10306
Extracts obtained from a marine alga and white cypress pine (Callitris glaucophylla J. Thompson & L.J. Johnson) were examined for their ability to control marine borers. In a two week laboratory bioassay, filter papers were soaked in 0-8% extract concentrations, dried, and placed with Limnoria quadripunctata Holthuis in Petri dishes containing seawater. The 8% algal extract virtually prevented...
D Scown, L J Cookson, R De Nys


Metal Leaching from Pressure Treated Wood in Sanitary Landfill Leachate
2004 - IRG/WP 04-50220
Pressure treated wood products contain heavy metals to prevent biological decay. Scrap treated wood from construction activities and demolished structures containing treated wood are typically disposed in landfills. To examine the potential mobility of metals from pressure-treated wood disposed in landfills, wood samples were leached using leachate from lined landfills and the concentrations of ar...
B Dubey, T G Townsend, H M Solo-Gabriele


Resistance of wood inorganic material composites against decay fungi and subterranean termites
1996 - IRG/WP 96-40062
Double diffusion process was applied to the treatment of small sound sapwood specimens [20(T) x 20(R) x 10(L) mm³] of Cryptomeria japonica D. Don. The specimens were consecutively dipped in the two kinds of acqueous solutions to form water insoluble deposits within the wood after an expected reaction between the solutes. Following the comparison of deposits formed and treating conditions (tempera...
K Tsunoda, T Yoshimura, M Takahashi, S Hirao, H Usui


The Efficacy of Wood Preservative Treatments in Laboratory Soil-Bed Test
2004 - IRG/WP 04-20289
The efficacy of wood preservatives were determined in laboratory soil-bed test. Pine and alder wood samples (10 x 10 x 10 mm) were treated with CCA (1, 2%), ACQ-1900 (2, 3%), ACQ-2200 (1, 2%), Tanalith E 3491 (2, 2,8%), Wolmanit CX-8 (1, 2%). The leached and unleached samples were exposed 76 days at Simlångsdalen soil and determined mass loss. The results of this study showed that mass losses o...
A Temiz, T Nilsson, Ü C Yildiz, E D Gezer, S Yildiz


Efficacy of anhydrides as wood protection chemicals
1997 - IRG/WP 97-30162
Wood samples treated with anhydrides of various compositions have been examined for their decay resistance and moisture behaviour. For this purpose two brown rot fungi (Coniophora puteana and Gloeophyllum trabeum) and two white rot fungi (Trametes versicolor and Pycnoporus sanguineus) were used in conventional and modified soil block tests. The modified soil block tests conformed to the method as ...
S C Forster, M D C Hale, G R Williams


The colonisation pattern of anaerobic fungi in wood
1989 - IRG/WP 1403
Timber foundations may be degraded in service in anaerobic conditions. The present work was conducted to investigate whether anaerobic fungi could colonise wood, using rumen fungi as test microorganisms. Strictly anaerobic fungi were isolated and purified from cow dung and goat and sheep rumen fluids respectively. Colonisation of Eucalyptus grandis and Pinus patula by these fungi and Neocallimasti...
A H Wiederhold, M Morrison, A A W Baecker


Modèles de laboratoire et évaluation des risques. Protocole pour l'étude physiqo-chimique et toxicologique de la thermolyse de bois, de matériaux composites et de végétaux arbustifs
1995 - IRG/WP 95-50040-03
Thermolysis of samples is achieved inside an oven called "Fire model", designed to simulate fire conditions. This fire model was previously designed by the LEMD at the occasion of studies carried out for the purpose of toxicity studies on materials in the conditions occurring at the building level. This model essentially a cubic chamber takes into account the energy of radiation reflexed on the wa...
R Capron, E Leghouchi, M Guerbet, E Dittmar, J M Jouany


Resistance of acetylated wood to basidiomycetes, soft rot and blue stain
1994 - IRG/WP 94-40021
Poplar (Populus spp.), beech (Fagus sylvatica) and pine sapwood (Pinus sylvestris) samples were acetylated in a semi-industrial acetylation plant and tested for durability according to European standards. Resistance to Gloeophyllum trabeum, Coniophora puteana and Coriolus versicolor could be reached at a weight percent gain (WPG) of 12%. Susceptibility of acetylated pine to Poria placenta was high...
E P J Beckers, H Militz, M Stevens


Ponding of radiata pine (Pinus radiata) - 1. The effect of bacteria on wood
1998 - IRG/WP 98-10265
Radiata pine (Pinus radiata) wood panels which had been ponded for periods ranging from 2 to 12 weeks were examined by light microscopy, confocal laser scanning microscopy (CLSM), scanning electron microscopy (SEM) and transmission electron microscopy (TEM) for bacterial colonisation of wood and degradation of pit membranes. After 2 weeks of ponding bacteria colonised the outer few cells of wood, ...
A P Singh, Y S Kim, U Schmitt, B S Dawson


Extracellular hydrogen peroxide producing and hydrogen peroxide reducing compounds of wood decay fungi
1991 - IRG/WP 1516
Extracellular H2O2-producing and H2O2-reducing compounds were isolated from wood-containing cultures of all the white-rot and brown-rot fungi and Ascomycetes which well degraded wood, but were not detected in the culture of the fungi which degraded little wood. The compounds are glycopeptides with a low molecular weight, require H2O2 for one-electron oxidation, catalyze the redox reaction between ...
A Enoki, G Fuse, H Tanaka


A technique for the rapid assessment of wood surface degradation during weathering
1987 - IRG/WP 2281
Radiate pine (Pinus radiata D. Don) sapwood samples taken from four trees were converted into thin strips 100 x 10 x 0.085 (85 µm) mm³, (longitudinal x radial x tangential) in size and exposed in preweighed hatches to the weather inclined at 45° facing equatorially for 10, 20, 40, 60, 80 and 100 days. Significant (P < 0.001) weight losses occurred with time over the exposure period. Differen...
P D Evans, D Abbott, S Thein


A novel guide for the determination of the physical properties of wood including kiln drying and full-cell preservative treatment
2004 - IRG/WP 04-20298
An ideal flow chart for the sequential experimental determination of a range of physical properties relevant to wood drying and subsequent preservation was designed as a novel guide to assist wood scientists. In this manner, data assembly and experimental processing are shown. This was designed according to experience and published literature. Aspects emphasised in this review were the physical p...
I Usta, M D C Hale


Leaching from CCA-impregnated wood to food, drinking-water and silage
1987 - IRG/WP 3433
During the last years The Norwegian Institute of Wood Technology (NIWT) has analysed different foodstuff for contamination by copper, chrome and arsenic from CCA-impregnated wood. There has been some interest for using CCA-impregnated wood in contact with food and drinking-water. Before giving their permission the Norwegian Health Authorities want results from experiments. NIWT therefore started t...
F G Evans


A reliable spot test for TCMTB in wood
1992 - IRG/WP 92-2391
Test specimens of slash pine (Pinus elliottii) and spotted gum (Eucalyptus maculata) were treated with aqueous emulsions of Busan 30WB and Busan 31, containing the fungicide TCMTB (2-(Thiocyanomethylthio)benzothiazole), or with solutions of TCMTB in toluene. These and matching untreated specimens were subjected to a wide range of procedures in an attempt to reveal TCMTB penetration patterns. Most ...
D E Ferlazzo, M J Kennedy


Development of wood retification process at the industrial stage
1998 - IRG/WP 98-50101-16
Wood is a natural composite material which exhibits outstanding properties from the technical as well as from the ecological point of view. However, it is an anisotropic, hygroscopic material sensitive to biological attacks. We have to stabilise and preserve it if we want to ensure its market shares faced with competing synthetic material, whilst taking the new environmental rules into account. T...
P Gohar, R Guyonnet


Ecotoxicological behaviour of leachates from superficially treated timber as an approach for a test strategy of environmental risk assessment in wood preservation
1998 - IRG/WP 98-50101-09
At present for wood preservatives, which in Germany are subject to the quality mark of the RAL-Gütegemeinschaft Holzschutzmittel, health and safety as well as environmental aspects are evaluated by official authorities, as BgVV (Federal Institute for Consumer Health Protection and Veterinary Medicine) and the UBA (Federal Environmental Agency). From the environmental point of view to day there a...
H W Wegen, U J Lucks


Applications of the shower test. Part A: Results from CCA type C treated wood: influence of fixation process
1993 - IRG/WP 93-50009
This report outlines the results of shower tests conducted on CCA type C treated wood. The results indicate the inherent good fixation of CCA type C, as judged by the leaching limits within the Environmental Regulations. The shower test has proven to be a useful quality control and research test. It determines reasonably accurately the leaching under simulated conditions and, admittedly from a lim...
W J Homan, H Militz, D A Lewis


Co-incineration of CCA-treated wood and Municipal Solid Waste in MSWI plant
2005 - IRG/WP 05-50224-19
The Norwegian Association of Energy Users and Suppliers (Norsk Energi) have carried out incineration tests with addition of 10 % by weight CCA-treated wood waste to municipal solid waste in a MSWI plant. The objective with the test was to determine emissions and composition of bottom ash. The incineration test was done at the Klemetsrud plant in Oslo The main conclusions are: -No significant inc...
D Borgnes, B Rikheim


Kinetics and mechanism of fixation of Cu-Cr-As wood preservatives. Part 5: Effect of wood species and preservative composition on the leaching during storage
1975 - IRG/WP 354
Conversion reactions during storage of CCA treated wood take place even at and below the fiber saturation point as long as ion transport is possible. Increase in drying temperature increases the final pH of the treated wood and the leachability of Cu and decreases slightly the leachability of Cr, while the leachability of As is not affected. This temperature effect is considered to be of no techni...
S-E Dahlgren


Optimun storage period for the boron diffusion treatment of rubber wood
1996 - IRG/WP 96-30121
The study determined the maximum thickness of rubber wood that can be diffusion treated and the effect of diffusion storage period on the distribution of chemicals in treated wood of various thicknesses. Wood of thickness up to 50 mm can be easily diffusion treated with 10% boric acid equivalent (BAE) solution to adequate loading of chemicals. The optimum diffusion storage period to get uniform an...
T K Dhamodaran, R Gnanaharan


Confocal Laser Scanning Microscopy (CLSM) of decayed wood
1998 - IRG/WP 98-10273
Confocal laser scanning microscopy (CLSM) is currently being used to examine biodegraded wood and is proving to be a useful new technique in this area of work. Non-invasive optical sectioning within a thick specimen (20 - 50 µm), coupled with post image processing techniques allows manipulation of images and 3-D reconstruction from serial sections. Glutaraldehyde can cause cell autofluorescence,...
Ying Xiao, R N Wakeling, A P Singh