Wood decay in Danish buildings
1985 - IRG/WP 1261
At Technological Institute identification of fungi and advisory activity concerning repair of damages has taken place since 1935. Statistical analyses based on material from 1982 and 1983 are compared to earlier investigations worked out by L. Harmsen. The material shows that building traditions influence the diversity and frequency of fungal species. Many fungal damages in the last decade have sh...
A P Koch


Lignin degradation by wood-degrading fungi
1986 - IRG/WP 1310
The wood-degrading white-rot fungus Phanerochaete chrysosporium, has been the subject of intensive research in recent years and, based upon isolation of the extracelluar enzyme ligninase, major advances have now been made toward elucidating the mechanism by which this fungus degrades lignin. From these developments, a model emerges which could explain the process by which wood-degrading fungi in g...
P J Harvey, H E Schoemaker, J M Palmer


Surface coatings for impregnated wood
1992 - IRG/WP 92-3684
The use of proper surface coatings enhances the aesthetic and protective properties of impregnated wood. Good results with especially water-borne coatings have been obtained for class-A impregnated L-joints and claddings in field tests started in 1982....
L Kotama


Ultrastructural observations on wood-degrading erosion bacteria
1986 - IRG/WP 1283
G F Daniel, T Nilsson


CCA Chemistry
1983 - IRG/WP 3268
A Pizzi


Re Questionnaire: The use of computers in wood preservation research
1985 - IRG/WP 2239
A questionnaire (Document No: IRG/WP/2240) concerning the use of computers in wood preservation research is introduced. Completing and returning the questionnaire will allow information to be collated on the usage of computers and computer programmes...
E F Baines


Termiticidal effectiveness of synthetic pyrethroids, carbaryl and chlordane in wood-block test
1985 - IRG/WP 3356
The results of some wood-block tests with allethrin, permethrin, fenvalerate, carbaryl and chlordane against Coptotermes formosanus are tabled and compared against some organophosphates, chlorpyrifos, fenitrothion, phoxim, tetrachlorvinphos and acephate. The treatment of the wood blocks was exactly as described in Document No: IRG/WP/3330. Among the pyrethroids tested, permethrin was the most effe...
K Tsunoda


An Australian test of wood preservatives. - Part IV: The condition, after 35 years' exposure, of stakes treated with creosote oils and oilborne preservatives
2000 - IRG/WP 00-30241
This paper contains the first results dealing with creosote oils and oilborne preservatives from this in-ground field trial in Australia. The substrates impregnated with preservative were Pinus radiata D. Don sapwood and Eucalyptus regnans F. Muell. heartwood and sapwood. Data are reported from stakes exposed for 35 years at three Australian sites (Innisfail, Sydney, Walpeup). Comparisons were mad...
G C Johnson, J D Thornton


Biocides - Efficacy assessment and doses for wood preservatives (product type 8). Local/geographical aspects. Termite control as case study
1999 - IRG/WP 99-20181
Currently, the efficacy of a wood preservative, as biocidal product type 8, is assessed as a ‚critical value' (CV), an efficient dose (retention in wood at a given depth of penetration). CVs are planned to be adapted for exposure to basic target organisms (5 hazard classes) and additional requirements concerning the occurrence of local target organisms in relation with climate, building...
G Ozanne


Creosote movement from treated wood immersed in fresh water: Initial PAH migration
2003 - IRG/WP 03-50201
Creosote has a long history of successful use as a wood preservative, but polycyclic aromatic hydrocarbons (PAHs) in this preservative have raised environmental concerns, particularly when creosote-treated wood is used in aquatic environments. A number of models have been developed to predict the risk of creosote use in aquatic environments, but one limitation of these models is a lack of data o...
Sung-Mo Kang, J J Morrell, J Simonsen, S T Lebow


Data sheet on wood-boring insects: Ptilinus pectinicornis (Linnaeus)
1987 - IRG/WP 1334
S Cymorek, M-M Serment


Determination of toxic limits of wood preservatives towards wood-destroying Basidiomycetes. Investigation on the effect of the use of two impregnated wood blocks and of one impregnated and an untreated block respectively in Kolle jars on the toxic limits of wood preservatives
1973 - IRG/WP 225
O Wälchli


300 years water-logged wood: Treatability with CCA-C
1998 - IRG/WP 98-40103
The treatability of 300 years water-logged and recent wood (Abies bornmülleriana M.) was assessed by dip treatment and vacuum and pressure cycling with CCA-C. Treatment runs were evaluated on the basis of weight gain retention and radial and tangential penetration measurements. The preservative penetration and retention levels in the 300 years water-logged wood were higher than in the recent wood...
S N Kartal, N Yilgör


Copper based water-borne preservatives: The biological performance of wood treated with various formulations
1987 - IRG/WP 3451
Wood samples treated with the various components of CCA preservative singly and in combination were tested against a soft rot organism, a copper tolerant brown rot organism and in soil burial both unleached and after leaching. The results suggest that, of the elements tested, fixed copper is essential for preventing soft rot attack and fixed arsenic is essential for preventing attack by a copper t...
S M Gray, D J Dickinson


Implications for comparability of laboratory experiments revealed in studies on the variability in survival and wood consumption between colonies of Coptotermes acinaciformis (Froggatt) (Isoptera: Rhinotermitidae
1983 - IRG/WP 1196
(Summary of paper 1193) Groups of Coptotermes acinaciformis, originating from six colonies, three taken from each of two localities, 1500 km apart, in northern Australia (Townsville, Darwin) were kept at population densities of 0.005, 0.01 and 0.02 g termites/mL. Survival and wood consumption of the groups after 8 weeks followed a similar pattern in the colonies from both collection areas. Groups were least vigorous at the lowest population density; their performance reached a maximum at a population density of 0.01 g/mL. The subsequent decline in vigour was less marked as the highest population density was approached. However, the actual values for survival and wood consumption varied widely between colonies, irrespective of their origin. It is recommended that in all laboratory experiments which use survival and wood consumption as indicators of termite vigour, controls of a favourable as well as an unfavourable food type are included which would serve to monitor the vigour of the termites. Results from termite sources whose vigour falls below a certain threshold value would have to be treated with caution and could not be used in definative data, as e.g. in defining critical retentions of wood preservatives.
M Lenz


Seasonal effects of the field evaluation on wood preservatives against mold fungi
1996 - IRG/WP 96-20087
For the purpose of the amelioration of field test methods, commercial preservatives against mold fungi were tested under two different seasons, in winter and in summer. The specimens were bundled and set over the water bath and all these systems were covered with plastic film. At top of the system under film, black films for regeneration of sunlight were put in, and windows for changing air were r...
K Suzuki, Y Sugai, K Ryugo, D Watanabe


Estimation of service life of durable timber species by accelerated decay test and fungal cellar test
2002 - IRG/WP 02-20249
Many kinds of durable wood species for outdoor uses has been imported from all over the world to Japan. However information on the natural durability of these species is not sufficient to estimate the service life of them in the climate of Japan. Highly durable species such as Jarrh, Teak, Ipe, Ekki, Selangan batu, Red wood, Western red cedar showed no significant percent mass losses by accelerate...
K Yamamoto, I Momohara


Draft of a mongraphic card for Serpula himantioides (Fr.) Karst. according to the 'Model Questionnaire for preparation of monographic cards for wood-destroying fungi'
1978 - IRG/WP 174
L Harmsen


Trends in environmental management in industry. Implications for wood preservation activities
1993 - IRG/WP 93-50001-34
J A De Larderel


Monographic information on Serpula (Poria) incrassata according to the "Model Questionnaire for preparation of monographic cards for wood-destroying fungi"
1980 - IRG/WP 160
J G Palmer, W E Eslyn


Some statistics on the Brazilian Wood Preservation Industry: 1980-81
1982 - IRG/WP 3214
Statistical data on the production of pressure treated wood and on the consumption of wood preservatives are given for the years of 1980 and 1981 in Brazil....
M S Cavalcante, F C Geraldo, A R De Freitas


Wood preservation and the environment: A Canadian perspective
1990 - IRG/WP 3577
The non-pressure (surface) and pressure treatment of wood impacts on the environment in four ways. These are: through the production of treated wood at sawmills and pressure treating facilities; during the storage of treated wood prior to use; when the pressure treated wood is placed in service; and finally, when the treated product reaches the end of its useful life and must be disposed. By refer...
J N R Ruddick


Effects of some essential oils on wood destroying organisms
1993 - IRG/WP 93-10047
Three wood destroying fungi: Botryodiplodia theobromae Pat. (stain), Gloeophyllum sepiarium (brown rot), and Pycnoporus sanguineus (white rot) were exposed to six plant essential oils: the peppermint, kaffir lime or leech lime, lavender, tarragon, holy basil, and the eucalyptus. The peppermint oil showed most effective to inhibit fungal growth, while eucalypus oil was the least effective. The othe...
K Atisongkroh, C Anantachoke, P Lekuthai, S Pensook, T Kittirattrakarn


Lignin-copper, a new wood preservative without arsenic and chromium
1992 - IRG/WP 92-3702
A more environmentally sound treatment for wood with preservatives containing no arsenic or chromium, has been developed and studied on a laboratory scale. The method involves a first step impregnation with an aqueous solution containing modified, water-soluble kraft lignin followed by a second step involving impregnation with a copper salt solution to give fixation of the lignin into a water-inso...
B Ohlsson, R Simonson


A comparison between methods for evaluating the water repellency of wood
1989 - IRG/WP 2328
Wood specimens treated with a number of water repellent formulations have been tested for their water repellency according to four laboratory test methods, based on weight increase, swelling and contact angle measurements, in order to assess the degree of agreement between the different methods. Treatments representing formulations with a wide range of water repellent efficiency were tested both i...
R Nussbaum