IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 3145 documents. Displaying 25 entries per page.


Radio frequency heating times for sterilization radiata pine solid piles
2017 - IRG/WP 17-40815
In this work was sterilized wood packaging material of radiata pine, stacked as solid piles without stickers, for determining the heating times using radiofrequency treatment. The experiments were performed in a radio frequency semi-industrial equipment. The results showed that the radio frequency heating times increases with wood volume and that radio frequency treatments were faster than convent...
H Esquivel, V Sepúlveda, J Torres, L Salvo, R A Ananías


Leaching of CCA preservative from treated timber in marine environment
2001 - IRG/WP 01-30254
Knowledge on the amount of preservatives leaching out of treated wood is essential to optimise the chemical loading in various species of timber required for different end uses. In order to gain more insight into this aspect, the residual CCA content in 40 treated timber panels belonging to 14 species removed on destruction by marine organisms from a series of durability tests conducted in Kochi w...
M V Rao, V Kuppusamy, K S Rao, L N Santhakumaran


Volumes and weights of different CCA-C treated wood poles, anchor logs and crossarms of REB at air dry condition
1996 - IRG/WP 96-40073
Researches revealed the unit volumes and weights at air-dry condition (12% MC) of different poles, anchor logs and crossarms species of REB from this world. The softwood products are lighter than hardwood products. Inversely the unit volumes of softwood poles are higher than those of hardwood poles. Red pine (Pinus resinosa), radiata pine (Pinus radiata), blue pine (Pinus wallichiana), fir (Abies ...
A K Lahiry


Copper-resistant fungi on pressure impregnated wood in Denmark
1994 - IRG/WP 94-10078
The occurence of Amorphotheca resinae Parbery and its asexual stage Cladosporium resinae (Lindau) de Vries on CCA and CCB treated wood has previously been shown. In the autumn 1993 some other blue stain fungi were found on CCP and CCB treated pine timber, such as Ophiostoma minus (Hedgc.) H. and P. Sydow, Ophiostoma pilifera (Fr.) H. and P. Sydow and Ophiostona piceae (Munch) H. and P. Sydow. The ...
J Bech-Andersen, S A Elborne


Leaching of CCA components from treated wood under acidic conditions
1993 - IRG/WP 93-50004
The leaching of CCA components from treated wood under acidic conditions were investigated. Western hemlock treated with three types of CCA and two levels of target retention was subjected to leaching at four different levels of pH. After leaching tests, leached samples were subjected to laboratory decay and soft rot tests. The amount of CCA components leached was dependent on acidity of leaching ...
Jae-Jin Kim, Gyu-Hyeok Kim


The IRG48 Scientific Conference on Wood Protection - Poster abstracts
2017 - IRG/WP 17-60414
IRG Secretariat


Programme. IRG48 Scientific Conference on Wood Protection, 4-8 June 2017
2017 - IRG/WP 17-60415
IRG Secretariat


The IRG49 Scientific Conference on Wood Protection. Poster abstracts
2018 - IRG/WP 18-60433
IRG Secretariat


Programme. The IRG49 Scientific Conference on Wood Protection
2018 - IRG/WP 18-60434
IRG Secretariat


The IRG50 Scientific Conference on Wood Protection. Poster abstracts
2019 - IRG/WP 19-60454
IRG Secretariat


Programme. The IRG50 Scientific Conference on Wood Protection
2019 - IRG/WP 19-60455
IRG Secretariat


Programme. The IRG51 webinar on Wood Protection
2020 - IRG/WP 20-60471
IRG Secretariat


Utilization of plasma treatments in the field of wood protection
2021 - IRG/WP 21-40912
Plasma treatments have been used for modification of surfaces of wood and wood-based materials for some decades and solutions were developed to apply it for wood protection. This contribution aims to present the background, introduce the available plasma technology, and to give an overview on the typical applications and benefits....
S Dahle, H Militz


Status of wood preservation in India
2005 - IRG/WP 05-30386
Wood, despite the advent of other modern materials, continues to play an important role in man’s day to day life. Usage of wood ranges from fuelwood to engineered wood products and demand for it is increasing which has resulted in depletion of forests and diminishing wood supplies. Future needs are required to be met from plantation timbers after adopting processing technologies for their life...
S C Gairola, P K Aggarwal


Artificial drying of impregnated wood
1987 - IRG/WP 3448
Sawn timber (Pinus Sylvestris) of dimension 50x150 mm was impregnated with CCA by a full-cell process. The timber was then dried in a conventional kiln or a special vacuum kiln where the timber was dried by circulating superheated steam. Drying time was 16 days and 2 days respectively. The aim of the investigation was to compare the physical appearence of the wood after drying by the two methods w...
M-L Edlund


A novel defaunation method of the protozoa to investigate cellulose metabolism in Coptotermes formosanus Shiraki (Isoptera: Rhinotermitidae)
1994 - IRG/WP 94-10050
The largest protozoa in the hindgut of workers of Formosan subterranean termite, Coptotermes formosanus Shiraki, was selectively eliminated by forced-feeding on low-molecular weight cellulose (LC) with a mean DP of 17. Although one week's feeding on LC caused perfect disappearance of Pseudotrichonympha grassii Koidzumi, the selective defaunation method itself had no detrimental effect on ...
T Yoshimura, K Tsunoda, M Takahashi


Inhibition of wood decay and termite damage by calcium precipitation
1996 - IRG/WP 96-30111
Fungal decay of wood in service, especially brown rot, results in billions of dollars (US) of losses annually. Recent environmental restrictions, both U.S. and international, are limiting or eliminating the use of broad spectrum biocides for wood preservation, primarily due to problems with disposal. In order to design new, environmentally benign methods for control of wood decay fungi, it is esse...
F Green III, T A Kuster, L Ferge, T L Highley


Programme. The IRG53 Scientific Conference on Wood Protection
2022 - IRG/WP 22-60501
IRG Secretariat


Exploring the potential for plasma-assisted coating at atmospheric pressure for wood protection
2023 - IRG/WP 23-40982
J Profili, G Laroche


Programme. The IRG54 Scientific Conference on Wood Protection
2023 - IRG/WP 23-60518
IRG Secretariat


In service performance of wood sound abatement barriers
2024 - IRG/WP 24-41006
Sound abatement barriers made form treated hem-fir in service near Vancouver, Canada were inspected after about 10-12 years in service. The barriers appeared in good condition and no boards were to the point of needing replacement. The sound abatement decibel readings at all locations indicate they perform as well as concrete barriers and exceed the 5 dBA regulatory requirement for noise reduction...
S Kus, D Wong, R Stirling


The course of fixation of Cu-Cr-As wood preservatives
1972 - IRG/WP 307
Copper-chrome-arsenic (CCA) preservatives in contact with wood result in an instant extensive increase of pH, because of ion-exchange and adsorption reactions with the wood. During precipitation of the active elements the pH continuously increases but reaches a maximum, when all chrome is consumed. Some of the early reaction products are unstable and slowly convert via dissolution into stable comp...
S-E Dahlgren


Effects of artificial UV weathering and soft rot decay on heat treated wood
2005 - IRG/WP 05-40302
Oil and inert gas oven heat treated pine wood strips 100 µm thick were mildly heat treated (200°C, 30 mins linseed oil, 120 mins oven). Following treatment, specimens were exposed to UV weathering (300 hours) and decay by the soft rot fungus, Chaetomium globosum. The effects of each treatment were assessed by zero span tensile testing, microscopy and by FTIR. Tensile testing of heat treated s...
M D C Hale, S C Ghosh, M J Spear


Three dimensional computer representations of growth of microbial populations in wood
1984 - IRG/WP 1243
Creosoted distribution poles inoculated with either Lentinus lepideus, biological control organisms including Triochoderma or combinations of both were extensively sampled to monitor the spread of organisms. A computer program which enabled the results to be portrayed in a three dimensional graphic form was developed and is illustrated. Results showed that computer mapping of this type usefully en...
A Bruce, B King, C Bruce, G M Smith


Programme. The IRG55 Scientific Conference on Wood Protection
2024 - IRG/WP 24-60534
IRG Secretariat


Previous Page | Next Page