Implications for comparability of laboratory experiments revealed in studies on the variability in survival and wood consumption between colonies of Coptotermes acinaciformis (Froggatt) (Isoptera: Rhinotermitidae
1983 - IRG/WP 1196
(Summary of paper 1193) Groups of Coptotermes acinaciformis, originating from six colonies, three taken from each of two localities, 1500 km apart, in northern Australia (Townsville, Darwin) were kept at population densities of 0.005, 0.01 and 0.02 g termites/mL. Survival and wood consumption of the groups after 8 weeks followed a similar pattern in the colonies from both collection areas. Groups were least vigorous at the lowest population density; their performance reached a maximum at a population density of 0.01 g/mL. The subsequent decline in vigour was less marked as the highest population density was approached. However, the actual values for survival and wood consumption varied widely between colonies, irrespective of their origin. It is recommended that in all laboratory experiments which use survival and wood consumption as indicators of termite vigour, controls of a favourable as well as an unfavourable food type are included which would serve to monitor the vigour of the termites. Results from termite sources whose vigour falls below a certain threshold value would have to be treated with caution and could not be used in definative data, as e.g. in defining critical retentions of wood preservatives.
M Lenz


Seasonal effects of the field evaluation on wood preservatives against mold fungi
1996 - IRG/WP 96-20087
For the purpose of the amelioration of field test methods, commercial preservatives against mold fungi were tested under two different seasons, in winter and in summer. The specimens were bundled and set over the water bath and all these systems were covered with plastic film. At top of the system under film, black films for regeneration of sunlight were put in, and windows for changing air were r...
K Suzuki, Y Sugai, K Ryugo, D Watanabe


Estimation of service life of durable timber species by accelerated decay test and fungal cellar test
2002 - IRG/WP 02-20249
Many kinds of durable wood species for outdoor uses has been imported from all over the world to Japan. However information on the natural durability of these species is not sufficient to estimate the service life of them in the climate of Japan. Highly durable species such as Jarrh, Teak, Ipe, Ekki, Selangan batu, Red wood, Western red cedar showed no significant percent mass losses by accelerate...
K Yamamoto, I Momohara


Wood preservation and the environment: A Canadian perspective
1990 - IRG/WP 3577
The non-pressure (surface) and pressure treatment of wood impacts on the environment in four ways. These are: through the production of treated wood at sawmills and pressure treating facilities; during the storage of treated wood prior to use; when the pressure treated wood is placed in service; and finally, when the treated product reaches the end of its useful life and must be disposed. By refer...
J N R Ruddick


Lignin degradation by wood-degrading fungi
1986 - IRG/WP 1310
The wood-degrading white-rot fungus Phanerochaete chrysosporium, has been the subject of intensive research in recent years and, based upon isolation of the extracelluar enzyme ligninase, major advances have now been made toward elucidating the mechanism by which this fungus degrades lignin. From these developments, a model emerges which could explain the process by which wood-degrading fungi in g...
P J Harvey, H E Schoemaker, J M Palmer


Surface coatings for impregnated wood
1992 - IRG/WP 92-3684
The use of proper surface coatings enhances the aesthetic and protective properties of impregnated wood. Good results with especially water-borne coatings have been obtained for class-A impregnated L-joints and claddings in field tests started in 1982....
L Kotama


Lignin-copper, a new wood preservative without arsenic and chromium
1992 - IRG/WP 92-3702
A more environmentally sound treatment for wood with preservatives containing no arsenic or chromium, has been developed and studied on a laboratory scale. The method involves a first step impregnation with an aqueous solution containing modified, water-soluble kraft lignin followed by a second step involving impregnation with a copper salt solution to give fixation of the lignin into a water-inso...
B Ohlsson, R Simonson


A comparison between methods for evaluating the water repellency of wood
1989 - IRG/WP 2328
Wood specimens treated with a number of water repellent formulations have been tested for their water repellency according to four laboratory test methods, based on weight increase, swelling and contact angle measurements, in order to assess the degree of agreement between the different methods. Treatments representing formulations with a wide range of water repellent efficiency were tested both i...
R Nussbaum


The variation in electrical resistance in the CCA-treated wood during the fixation
1989 - IRG/WP 3554
The curve commonly used in Scandinavia for describing the fixation period at different temperatures for CCA-impregnated wood is based on investigation by Dahlgren on the pH-variations in a mixture of sawdust and preservative solution. As far as we know there is no such investigation on solid wood. We have therefore measured the electrical resistance in CCA-treated solid wood to see if this will di...
F G Evans, B Nossen


Antagonistic effect of some mycorrhiza fungi as biological control of blue-stain
1987 - IRG/WP 1314
This report discussed the possibility of using some mycorrhiza fungi as biological control of blue-stain. The results show that new bio-technological possibilities are opening, because, by cultivating antibiosis fungi in fermentor, it is possible to prepare extracts which can then be used as the natural preservative to control the blue-stain in wood....
R Benko


Ultrastructural observations on wood-degrading erosion bacteria
1986 - IRG/WP 1283
G F Daniel, T Nilsson


CCA Chemistry
1983 - IRG/WP 3268
A Pizzi


Re Questionnaire: The use of computers in wood preservation research
1985 - IRG/WP 2239
A questionnaire (Document No: IRG/WP/2240) concerning the use of computers in wood preservation research is introduced. Completing and returning the questionnaire will allow information to be collated on the usage of computers and computer programmes...
E F Baines


Data sheet on wood-boring insects: Ptilinus pectinicornis (Linnaeus)
1987 - IRG/WP 1334
S Cymorek, M-M Serment


Use of Transverse Compression Properties as a Measurement of Wood Biodeterioration, Part 1 of 2 - Effect of White-Rot on Yellow-Poplar
2002 - IRG/WP 02-40239
The soil block and agar block test methods are used extensively as a screening process for potential and modified wood preservatives. The extent of decay in standard screening tests, indicative of preservative efficacy, is currently based on mass loss. Mass loss techniques, due to their limit of sensitivity in detecting significant mass loss vis-à-vis decay, require an extended fungus exposure ...
S Janzen, D D Nicholas


Effect of asphyxiation on wood decay fungi treated with argon and nitrogen gas
2002 - IRG/WP 02-10452
The effects of low-oxygen conditions, achieved with either argon or nitrogen gas, on the viability of wood decay fungi Coniophora puteana, Antrodia vaillantii and Trametes versicolor, cultivated on PDA medium and infected wood samples, were examined. The fungal cultures were exposed to low oxygen concentration (below 10 ppm) for one to five weeks in hermetically sealed vessels. Anoxic treatment di...
C Tavzes, F Pohleven, M Janisek, R J Koestler


Use of fluorescent-coupled lectins as probes for studying fungal degradation of wood
1986 - IRG/WP 1288
The ability of the fluorescent-coupled lectins wheat germ agglutin (WGA) and Concanavalin A (Con A) to react with selected Basidiomycetes, Ascomycetes, and Fungi Imperfecti was evaluated using pure cultures of 35 fungi grown on malt extract agar. WGA, which binds specifically to the n-acetylglucosamine residues found in fungal chitin, reacted with nearly all hyaline fungal structures but did not r...
J J Morrell, R L Krahmer, L C Lin


Determination of toxic limits of wood preservatives towards wood-destroying Basidiomycetes. Investigation on the effect of the use of two impregnated wood blocks and of one impregnated and an untreated block respectively in Kolle jars on the toxic limits of wood preservatives
1973 - IRG/WP 225
O Wälchli


300 years water-logged wood: Treatability with CCA-C
1998 - IRG/WP 98-40103
The treatability of 300 years water-logged and recent wood (Abies bornmülleriana M.) was assessed by dip treatment and vacuum and pressure cycling with CCA-C. Treatment runs were evaluated on the basis of weight gain retention and radial and tangential penetration measurements. The preservative penetration and retention levels in the 300 years water-logged wood were higher than in the recent wood...
S N Kartal, N Yilgör


Draft of a mongraphic card for Serpula himantioides (Fr.) Karst. according to the 'Model Questionnaire for preparation of monographic cards for wood-destroying fungi'
1978 - IRG/WP 174
L Harmsen


Tests on preservation of wood against marine borers
1976 - IRG/WP 417
The Instituto del Legno has carried out for some years a series of trials about the biodeterioration of wood in the sea. The investigations included the settlement and activity of marine borers, the natural durability of indigenous and tropical woods and the preservation of wood for marine use. This paper reports the trials on the effectiveness of some preservatives in protecting wood against mari...
A Gambetta, E Orlandi


Thirty-four year test of on-site preservative treatments to control decay in wood above ground
1993 - IRG/WP 93-30015
This research was initiated in 1958 to investigate efficacy of various preservatives and treating methods for new lumber going into exterior structures of buildings. Post-rail units (2x4 inches) constructed of Southern Pine sapwood, Douglas-fir heartwood, and mill run western hemlock were dip- or brush-treated before or after assembly. Units were trested with pentachlorophenol in various petroleum...
T L Highley, T C Scheffer


Safety clearance of wood preservatives in United Kingdom
1977 - IRG/WP 398
In the United Kingdom the principal route of control of pesticides is through the Pesticides Safety Precautions Scheme (PSPS) which is a non-statutory scheme agreed between government ministries and departments (referred to as "Departments") and associations representing the pesticide industries. The scheme formally began in 1957 covering those pesticides and related substances used in agriculture...
J M Baker


Termite field test results of preservative treated and modified woods in Kumamoto, Japan
2001 - IRG/WP 01-30275
Various preservative treated or modified wood stakes other than CCA, were buried in the soil, maximum for six years in Kumamoto, south west side of Japan. In this area, two main termite species, Coptotermes formosanus and Reticulitermes speratus, are distributed. After two years in field, untreated sapwood of sugi (Cryptomeria japonica) were observed severe attacks by termites, but the preservativ...
K Suzuki


Trends in environmental management in industry. Implications for wood preservation activities
1993 - IRG/WP 93-50001-34
J A De Larderel