Collaborative experiments in testing the toxicity of wood preservatives to soft rot fungi
1970 - IRG/WP 25
Eight Institutes from seven countries, Austria, England, France, Germany, Holland, Sweden and Switzerland have collaborated in an attempt to assess the suitability of various laboratory test procedures for acceptance as standard methods of determining the toxicity of wood preservatives to the cellulose-attacking micro-fungi which cause 'soft rot' of wood. Pure culture methods wit...
J G Savory, A F Bravery


Volatile borates in the treatment of wood and wood based panel products against subterranean termites
1995 - IRG/WP 95-30094
Blocks of pine solid wood, oriented strand board and plywood were treated with trimethyl borate by vapour treatment. It was meant to obtain either a full impregnation of the specimens or a shell treatment of the outer three millimetres. The efficacy of the treatments against subterranean termites (Reticulitermes lucifugus) was evaluated using an European Standard method....
L Nunes, D J Dickinson, R J Murphy


The present classification of wood degradation factors
1994 - IRG/WP 94-10071
The revised version of classification of wood degradation factors is presented after discussion and remarks sended by IRG-Members. The classification contains the biotic and abiotic factors in two aspects: etiological and symptomatical....
J Wazny


A collaborative test to determine the efficacy of polyurethane coatings on wood samples exposed in the marine environment
1984 - IRG/WP 4113
Aims are: a) to determine the effectiveness of elastomeric polyurethane as a protective coating against marine wood boring animals in a range of tropical and tempreate sites; b) to compare the adhesion of polyurthane coatings on different wood species exposed in seawater; c) to record the severity of attack in failed samples and to identify the causal marine organisms....
R A Eaton


Preservative-treated wood as a component in the recovered wood stream in Europe – A quantitative and qualitative review
2004 - IRG/WP 04-50218
Wood preservatives have been used for the protection of timber products in the European market in appreciable quantities for about 100 years. Between the 1960s up to the present day this usage has been particularly noticeable. The aim of this paper is to present quantitative and qualitative data on the volumes of preservative treated wood placed on the market in the UK and Sweden and to evaluate t...
R J Murphy, P Mc Quillan, J Jermer, R-D Peek


Current and future options for managing used preservative-treated wood
1995 - IRG/WP 95-50042
The amount of preservative-treated wood available for disposal will continue to increase exponentially in the next several decades as landfill availability declines. At the same time, recent legal ruling on competitiveness among utilities and disposal of ash has clouded the economic outlook for combustion of treated wood for energy recovery. This report identifies current and future options for ma...
R C De Groot, C Felton


Treatment of dried sawn spruce and redwood building timbers with water-borne preservatives under a scheme for the quality control of the preservation and preserved wood in the Netherlands
1978 - IRG/WP 3123
Treatment of dried sawn spruce and redwood Building Timbers with water-borne preservatives under a scheme for the quality control of the preservation and preserved wood in the Netherlands. The aim of this article is to give the reader a modest description of the evaluation of fundamental research in wood preservation into a practical application....
H F M Nijman, N Burgers


Evaluation of wood treated with copper-based preservatives for Cu loss during exposure to heat and copper-tolerant Bacillus licheniformis
1999 - IRG/WP 99-20155
Copper-based wood preservatives need to be effective against exposure to all types of microorganisms. Wood treated with six copper-based preservatives was exposed to 121°C and 20 psi pressure for 15 minutes under standard autoclave conditions and the copper-tolerant bacterium, Bacillus licheniformis CC01, for 10 d at 28°C and 150 rpm. Sixteen to 37 percent of the copper was released from the woo...
D M Crawford, C A Clausen


Evaluation of polystyrene as a protective of wood in sea-water
1986 - IRG/WP 4129
A test is described on the biological protection of wood by treatment with polystyrene. The results, obtained in marine trials, after 18 months, show that the treatment with polystyrene is not all that effective in preventing the attack of marine borers....
A Gambetta


European standardization for wood preservation
1990 - IRG/WP 2359
G Castan


On the problem "House Longhorn Beetle" in hardwoods and an aid to distinguish between Hylotrypes bajulus and Hesperophanes cinereus larvae
1981 - IRG/WP 1141
S Cymorek


Influence of storage on mould susceptibility of wood at relative humidity values lower than 100%
1989 - IRG/WP 1413
It is well known that wood material changes with time because of different environmental influences. The effects of such changes on the subsequent mould susceptibility are less known. In this paper we report on increased mould susceptibility of pine wood after storage. Mould growth was detected by indirect methods....
J Bjurman


Short term preconditioning of preservative-treated wood in soil contact in relation to performance in field trials
2000 - IRG/WP 00-20185
The effect of pre-exposure to primary colonising micro-organisms on preservative-treated wood, prior to a basidiomycete decay test, was determined by preconditioning in two soil types. Scots pine EN 113 blocks treated with 3 model systems (a triazole, a copper quaternary compound and a copper boron triazole) were leached according to EN 84 and subjected to 6 weeks and 8 weeks burial in either John...
S Molnar, D J Dickinson


Reliability-based service life prediction methodology for assessment of water protection efficiency for coatings on wood
2003 - IRG/WP 03-20268
Assessment of water protection efficiency according to EN 927-5 has been shown to give significant differences in water absorption values for different types of coatings on wood. It is shown that the combination of EN 927-5 and an artificial weathering procedure gives more information regarding expected durability and long-term performance than a single measurement of water absorption on fresh, un...
J Ekstedt


Tentative method of testing wood preservatives against blue staining
1977 - IRG/WP 259
The blue stain of sawn wood is still a real problem in Poland. Although a preservative based on sodium orthophenylphenoxide has been introduced into sawmill practice, and the technology of wood protection developed with it, new information has been obtained concerning blue stain in wood material destined for export. In order to select new chemicals or to improve the effectiveness of the ones in cu...
E Tarocinski, O Lewandowski, M H Zielinski


The resistance of fifteen Indonesian tropical wood species to the powder post beetle Heterobostrychus aequalis
1990 - IRG/WP 1429
A preliminary laboratory test on the resistance of 15 tropical wood species to Heterobostrychus aequalis has been carried out using small samples of 7.5 x 5 x 1.5 cm³. The results reveal that Pinus merkusii and Agathis borneensis are very susceptible to Heterobostrychus aequalis. Other 13 species vary between susceptible to resistance There is no signifisant relation between starch content and th...
Jasni, Nana Supriana


Natural durability and basic physical and mechanical properties of secondary commercially less accepted wood species from Brazil
2002 - IRG/WP 02-10451
The natural durability towards basidiomycete fungi and termites of several secondary timber from Brazil (Vatairea sp., Hymenolobium sp., Inga sp., Manilkara sp., Caryocar sp., Terminalia sp., Apuleia sp.) has been evaluated according to the EN 350-1. Some basic physical and mechanical properties (density, shrinkage, hardness, colour, static strength in flexion and compression) were also measured a...
M-F Thévenon, A Thibaut


Natural resistance of twenty-six Guianese wood species against marine borers
1988 - IRG/WP 4144
This note is a contribution on the study of the natural resistance of some wood species from French Guiana, some of which could be found too in the neighbourhood. Here are presented the results after one year exposure in the marine environment....
L N Trong


Report on a field demonstration of methods for detecting defects in wood poles
1984 - IRG/WP 2232
P I Morris, H Friis-Hansen


Detection of brown rot decay in wood by ion mobility spectrometry
1991 - IRG/WP 2377
A test method for the detection of brown rot decay in wood is described and involves a two-step procedure: thermal release of vapours from wood samples followed by analysis using Ion Mobility Spectrometry (IMS), with results being obtained in 5-10 seconds. The advantages, limitations as well as the detection limit of the technique are presented....
A H Lawrence, T Nilsson


Baiting techniques for subterranean termite control
1983 - IRG/WP 1205
The use of artificial baits, with and without toxins, have proved effective in attracting large numbers of non-mound and mound building subterranean termites in both urban and rural areas. An outline is presented of a termite baiting program which emphasises concurrent laboratory and field investigations on termite ecology, behaviour and physiology...
J R J French, J P Robinson


Improved resistance of Scots pine and Spruce by application of an oil-heat treatment
2000 - IRG/WP 00-40162
Spruce (Picea abies L. Karst.) and Scots pine (Pinus sylvestris L.) were subject to a heat treatment which was carried out in an oil-bath. The aim was to improve the dimensional stability of the treated wood and its resistance against fungi. The bath of vegetable oil provides a uniform heat transfer at temperatures of 180°C, 200°C and 220°C and protects the submersed wood from oxygen. Heat trea...
M Sailer, A O Rapp, H Leithoff


Synergistic effects between 2-HPNO, Irganox 1076 and EDTA on the inhibition of wood degradation by Coriolus versicolor
2004 - IRG/WP 04-30331
The efficiency of 2-hydroxypyridine-N-oxide (2-HPNO) as wood preservative has been investigated. As shown using classical experiments as well as using response surface methodology, the efficiency of 2-HPNO as wood preservative is strongly improved in presence a chelator like EDTA and/or of Irganox 1076 an industrial antioxidant. In these conditions, wood preservative efficiency of the mixture the ...
A Mabicka, S Dumarçay, N Rouhier, M Linder, J P Jacquot, P Gérardin, E Gelhaye


Microscopic characteristics of Pinus radiata wood veneers weathered outdoors for one yea
1993 - IRG/WP 93-10018
Radiata pine (Pinus radiata) wood veneers glued to solid wood hacking strips were exposed outdoors at 45° north-facing for one year and then examined by light microscopy (LM) and transmission electron microscopy (TEM). As expected, the exposed wood surfaces were colonised by a variety of microorganisms; however, wood decay was not observed. Ultlaviolet (UV light) radiation and water were the main...
A P Singh, R A B Sweeney, E A Dunningham, D V Plackett


Preventive action against fungal decay: A comparative experiment on the effects of natural and artificial infection of wood by Basidiomycetes
1981 - IRG/WP 2160
M Fougerousse