Copper naphthenate treatment for wood pols - a review and update
2012 - IRG/WP 12-30600
This paper reviews copper naphthenate (CuNap) and its utility as a treatment for wooden utility poles. One of the principal reasons that CuNap has gained market acceptance, in addition to its efficacy against decay fungi and wood-destroying insects, is its low mammalian toxicity. CuNap is a well-proven non-restricted use preservative, used extensively and specified for environmental reasons by ut...
J A Brient, M H Freeman


Study of the use of organosolv lignin as bio-preservative of wood
2012 - IRG/WP 12-30603
The service life of wood depends on the species, use and environmental conditions of exposure. The treatment of wood protects it against degradation by xylophagous agents, enhancing the durability of material up to 10 times, and reducing the deforestation around 12.5%. In this way, the use of treatments is necessary because increases the service life of material and protect against xylophagous age...
P S B dos Santos, A Garcia, P H G de Cademartori, D A Gatto, J Labidi


Effectiveness of CCA-C and CCB preservatives after a 30 years stake test
2012 - IRG/WP 12-30606
The objective of this experiment was to assess the durability of four pine species treated with waterborne preservatives. In order to determinate this, a stake field test, following the IUFRO (International Union of Forestry Research Organizations) recommendations, was installed at Experimental Station of Luiz Antonio (21º 32’ S and 47º 42’ W), State of São Paulo, Brazil. Species under t...
I PJankowsky, E S Lepage, C Salvela, J M Vidal, S Takeshita


Microwave Treatment of Frozen Wood Packaging Material
2012 - IRG/WP 12-40609
As part of the wood packaging material (WPM) regulation in international trade, the dielectric heating (DH) is soon to be included in ISPM15 (IPPC 2009) as an approved phytosanitary treatment. It has been considered that when using dielectric radiation (i.e. microwaves or radio-frequencies), reaching 60°C or more throughout the entire profile of the wood during at least 60s (i.e. 60°C/60s) ensur...
J-M Henin, A Bauduin, V Leemans, M Leyman, B Jourez, J Hébert


The effect on moisture content of water trapped in wood joints
2012 - IRG/WP 12-40613
To predict the service life of a structure, a model where the exposure of a structure is compared to its resistance can be used. Which exposure and resistance parameters that are relevant depend on which materials the structure consist of. This approach, with an exposure and a resistance parameter, is similar to the one used in structural engineering where a load (exposure) is compared to the bear...
M Fredriksson, L Wadsö, P Johansson


Differences between heat treated Pinus pinaster heartwood and sapwood
2012 - IRG/WP 12-40617
Heat treatment is a well known process to improve the durability and dimensional stability of less noble woods. The treatment can be applied for heartwood unlike the traditional treatments based on impregnation due to the difficulty of impregnating heartwood. Pure sapwood and pure heartwood samples were treated in an oven at 190ºC and 200ºC for 2h, 4h and 6h. Dimensional stability, measured a...
B Esteves, L Nunes, I Domingos, H Pereira


Transferable Durability: Enhancing decay resistance of non-durable species with extractives from durable wood species
2013 - IRG/WP 13-10808
Extractive content and composition is a vital component of naturally durable woods; however, variability in extractives can limit their usefulness in the field. Two extractive-free, non-durable wood species were pressure treated with ethanol-toluene extractives from 8 durable wood species. Extracted Southern pine, Paulownia and unextracted Southern pine blocks were treated and challenged in soil b...
G T Kirker, A B Blodgett, S Lebow, C A Clausen


Focus on the European standardization - Towards a revision of the EN 350 natural durability standard: a different approach to the inherent resistance and performance of wood and wood-based materials
2013 - IRG 13-10811
The European standard EN 350 “Natural durability of solid wood”, Parts 1 and 2, is one of the fundamental standards developed by the CEN/TC 38 “Durability of wood and wood-based products”. This standard is widely used by wood industries as the reference document which provides information on the resistance of wood species used in mainly the construction sector against decay fungi, wood-bor...
M Kutnik


Determination of the natural durability of solid wood against wood-destroying fungi - a European round-robin test
2013 - IRG/WP 13-20511
In Europe the durability of wood against wood-destroying basidiomycetes is tested according to CEN/TS 15083-1 (2005). Hitherto existing experience with this standard is quite heterogeneous and results from previous round-robin tests have stayed unreported or have been reported incompletely. In particular the need for natural pre-weathering of the test specimens to allow potential detoxification of...
C Brischke, C R Welzbacher, A Gellerich, S Bollmus, M Humar, K Plaschkies, W Scheiding, G Alfredsen, J Van Acker, I De Windt


Virulence of two Laboratory Test Strains and one Natural Isolate of Rhodonia (Oligoporus) placenta against Thermally Modified Pine and Beech Wood
2013 - IRG/WP 13-20524
Rhodonia (Oligoporus) placenta is known as a relative aggressive basidiomycete fungus against thermally modified timber. In durability lab tests, this often results in a lower durability class, compared to other test fungi. In the reported work, the virulence of three different strains of Rhodonia placenta for untreated and thermally modified timber was determined and compared. Therefore, two lab ...
K Plaschkies, W Scheiding, K Jacobs, N Rangno


Moisture distribution in glulam beams with natural cracks observed with CT Scanning before and after rain
2013 - IRG/WP 13-20534
The way cracks in outdoor wooden constructions affect durability is an interesting topic, since a certain amount of cracks can always be found naturally in wood and glued laminated wood. The question in this was, can cracks lead water into the wood and thereby increase the risk for decay and reduce strength and service life. Moisture balance, i.e., water absorption and water distribution were stud...
K Sandberg


Methylene Chloride compared with white spirit as a treatment solvent for wood preservation – results from decay and termite studies
2013 - IRG/WP 13-30611
Non-aqueous solvents have a long history in the treatment of wood products in various parts of the world. The most familiar solvent treatment is the ‘light organic solvent preservative’ (LOSP) treatment based on low density solvents such as white sprit. Until recently white spirit was the only non-aqueous solvent approved for use in wood preservation in New Zealand. Australia also permitted...
A Siraa, P Lobb, C Molloy


Performance testing of DMDHEU-modified wood in Australia
2013 - IRG/WP 13-30613
Chemical wood modification with dimethyloldihydroxy-ethyleneurea (DMDHEU) or its derivatives has been researched for many years and shown to be applicable to improve certain wood properties to both solid lumber and wood-based composites. Earlier research proved a high biological resistance of DMDHEU-modified wood against biological degradation in laboratory and field tests in Europe. Due to the ve...
H Militz, J Norton


Preliminary testing of spiroborate esters as wood preservatives
2013 - IRG/WP 13-30614
Fungicide and insecticide properties of boric acid are known since 30’s of the last century, but high solubility and leachability of inorganic borates limit their use for only applications not directly exposed to liquid water. A number of attempts were made to fixate borate salts into the wood structure but this research topic is still up to date and undiscovered. Water insoluble organoboron est...
D Panov, N Terziev


The effects of impregnation with secondary metabolite extracted from Ipe on durability of Japanese cedar and beech wood
2013 - IRG/WP 13-30618
Ipe wood is known for its high durability; it has been widely used in exterior structures that are exposed to the weather. In this paper, to increase the durability of less durable wood, Japanese cedar and beech specimens were impregnated with a secondary metabolite from Ipe. In a previous study, secondary metabolites extracted by a Soxhlet extraction method showed antifungal properties. Therefore...
T Iida, R Konuma, K Kawarada


Hygroscopicity of wood after polyethylene glycol (PEG) impregnation and/or heat treatment
2013 - IRG/WP 13-40623
The hygroscopicity of wood after polyethylene glycol (PEG) impregnation and/or heat treatment was investigated by testing the water uptake, equilibrium moisture content (EMC) at various relative humidity levels, and contact angle of the poplar wood surface. The results showed that: (1) At the first moment, the heat treatment at temperatures lower than 160 ℃ did not reduce the water uptake be...
Weiyue Xu Yuan Zhu, Jinzhen Cao


Resistance of WPC against wood destroying fungi
2013 - IRG/WP 13-40627
The investigation of biological durability is a fundamental topic to assess the performance of Wood Plastic Composites (WPC) particularly for outdoor applications. In the last years, different test setups based on existing standards on the field of wood as well as the field of plastics were used for WPC. But the test methodologies give different information about the durability of the tested mater...
A Gellerich, S Bollmus, A Krause


Influence of Heat Treatment Medium on Fungal Resistance of Beech Wood
2013 - IRG/WP 13-40643
Hydrothermal treatment of beech wood (Fagus orientalis) performed in acidic, neutral and alkaline buffered mediums in 160 and 180°C. White rot fungi (Coriolus versicolor) and brown rot fungi (Coniophora puteana) were used to determine the influence of heat treatment mediums on the behaviour of fungal resistance. White rot of wood digest lignin rather than cellulose; while brown rot digests the ce...
A Talaei, A Karimi, M-F Thévenon


Investigation of Nanocopper-Hygrothermally Treated Wood Properties
2013 - IRG/WP 13-40644
Nanometals with high thermal conductivity can be considered as modifiers, especially in thermal modification of wood. This study was aimed to investigate some physical and mechanical properties of nanocopper impregnated Iranian beach (Fagus orientalis Lipsky), which was hygrothermally treated. For this purpose, nanocopper solution (400 ppm) was used for impregnation process. Hygrothermal treatment...
G Rassam, B Jamnani, A Faraji Heris


Moisture and Fungal Durability of Wood-Plastic Composites Made With Chemically Modified and Treated Wood Flour
2013 - IRG/WP 13-40648
Evaluating the fungal durability of wood-plastic composites (WPCs) is complicated by the influence of slow moisture sorption. Recently, the American Wood Protection Association (AWPA) Standard Method E10, Testing Wood Preservatives by Laboratory Soil-Block Cultures, was modified to incorporate not only solid wood, but also wood-based composites and WPCs. To simulate long term WPC performance, cond...
B K Segerholm, R E Ibach


Estimation of service life of treated wood in ground contact based on early indicators
2013 - IRG/WP 13-20536
A well-known problem with field testing is that it takes a long time before meaningful and reliable results are achieved. Only when a trial has come to an end the so called average life for the samples in a group can be calculated and compared with other samples. The aim of the present study was to investigate if it is possible to get a reasonable and good estimation of the average life long befor...
M Hansson, J Jermer, P Larsson Brelid, N Terziev


Moisture dynamics of wood – An approach to implement wetting ability of wood into a resistance classification concept
2014 - IRG/WP 14-20557
Within the research programmes WoodBuild and PerformWOOD, wetting ability tests have been conducted with 25 wood-based materials. A first attempt has been made to establish factors for calculating the material resistance of wood materials to be implemented into a design guideline for timber structures. The approach looks promising, but further studies are needed to establish more reliable relation...
C Brischke, C Hesse, L Meyer, S Bardage, J Jermer, T Isaksson


An Overview of Western Red Cedar as a Wood Pole Species
2014 - IRG/WP 14-10815
This paper reviews the characteristics of western red cedar, with particular emphasis on its use in utility poles. Western red cedar naturally grows primarily in British Columbia, Alaska, Washington, Oregon, California, Idaho and Montana. Compared to other commercial softwoods it has low density, increased corrosivity, weaker mechanical properties, high dimensional stability, and high natural dura...
M H Freeman, R Stirling


Performance of recent and old Sweet chestnut (Castanea sativa) wood
2014 - IRG/WP 14-10816
Sweet chestnut (Castanea sativa) hardwood is one of the most durable European wood species. In the present research, various aspects that could potentially influence the durability were elucidated, namely: presence of extractives, ring width, and weathering. Simultaneously, properties of wood, which was in outdoor use for 35 years, were elucidated as well. The results indicate that ring width and ...
M Humar, M Žlahtič, N Thaler


Durability and Wood Protection for Historic Covered Bridges in the United States
2014 - IRG/WP 14-10829
A majority of the covered wooden bridges in United States were built in the mid -1800’s. These structures represent a unique cultural and technological heritage from that era. Over time, these bridges have been deteriorated by microorganisms and insects or damaged by acts of vandalism and arson. The National Historic Covered Bridge Preservation (NHCBP) Program sponsored by the Federal Highway Ad...