Laboratory testing of wood natural durability - In soil-bed assays
1998 - IRG/WP 98-20141
Laboratory methods for assessing wood decay resistance are being investigated in the framework of an ongoing European research project. This paper summarizes the main results obtained for soil-bed tests based on the European prestandard ENV 807-Test 2. The data suggest that this testing methodology is suitable for evaluating the natural durability of timber species in soil-contact under conditions...
R Sierra-Alvarez, I Le Bayon, J K Carey, I Stephan, J Van Acker, M Grinda, G Kleist, H Militz, R-D Peek


Effect of vapour boron treatment on mechanical properties of wood based board materials
1992 - IRG/WP 92-3727
The mechanical properties of Medium density fibre board, Chipboard and Oriented strand board were investigated after treatment to two retention levels of boric acid applied as a vapour phase system. A range of mechanical properties were investigated. The vapour boron treatment does not have any significant effect on most of the mechanical properties of the boards. The exception is a reduction in i...
R Hashim, D J Dickinson, R J Murphy, J Dinwoodie


Variation of natural durability of sugi (Cryptomeria japonica) wood in 15 clones examined by decay test (Preliminary report)
2004 - IRG/WP 04-10526
Natural durability of wood in 27 trees from 15 clones of sugi (Cryptomeria japonica)  was investigated by an accelerated decay test. Thirty years old trees were collected from a clonal trial in Ibaraki prefecture, Japan. Natural durability is usually evaluated in heartwood. Mass losses of heartwood caused by a brown rot decay fungus, Fomitopsis palustris and a white rot decay fungus, Py...
K Yamamoto, A Tamura, R Nakada


Acceleration of boric acid uptake into the subterranean termite, Coptotermes formosanus Shiraki using steamed larch wood
2000 - IRG/WP 00-10353
Laboratory tests were done to measure the efficacy of addition of steamed larch (Larix leptolepis (Sieb. et Zucc.) Gord.) heartwood extracts for the uptake of boric acid against the termite, Coptotermes formosanus Shiraki. Paper discs were treated with the water-soluble fraction obtained from hot-water extracts of steamed larch wood (S-Water) with or without 0.01-2.0% boric acid, followed by expos...
W Ohmura, S Doi, S Ohara


A review of incising as a means of improving treatment of sawnwood
1994 - IRG/WP 94-40019
The use of incising, perforation of the wood surface, is increased because of the need to treat refractory wood species. This paper reviews the development of incising and shows how the required incising patterns can be determined and specified. Most of the development has been in the area of toothed-roller incisors because of their rapid throughput. Needle, Laser, drill and water jet incisors hav...
P I Morris, J J Morrell, J N R Ruddick


Moisture content development in lap-joints of different wood species in outside exposure trials
1998 - IRG/WP 98-20143
Lap-joint trails (following European Standard EN 12037) were set up with 11 different softwood and hardwood species. Half of the number of the lap-joint specimens were coated with an alkyd coating. The moisture development has been followed during a 19 months period. In this paper, the out comes of different moisture contents evaluations are presented. The results show, that the moisture content o...
H Militz, M Broertjes, C J Bloom


Chemical treatment of ten Amazonian timber species of low natural durability
1991 - IRG/WP 3640
The objective of this work was to evaluate the performance of 10 amazonian wood species of low natural durability, to treatment with CCA preservative (2% concentration): it was concluded that all species studied are easily treated with this preservative. The sapwood showed high absorption and total penetration. The heartwood is relatively easy to preserve, exception to Parkia nitidae (Fava), Quale...
C S Neta, B F Vianez


Treatment of refractory timbers
1993 - IRG/WP 93-40001
Worldover crisis of wood is being felt due to the global environmental problems. Wood preservation technology plays a good role in curtailing the demands of wood for replacement by prolonging the service life of the timber and thus indirectly helps in saving the environment. Some species of timbers which could not be treated to the desired level by virtue of their refractory nature by any of the c...
I Dev, S Kumar


The comparative resistance to fungi of the wood munika (Pinus heldreichii Christ.), fir (Abies alba Mill.) and spruce (Picea excelsa Poir.) compared with Pinus sylvestris L. and some physical and mechanical characteristics of munika
1981 - IRG/WP 1129
The munika (Pinus heldreichii Christ.) is situated primarily in the Balkans, and partially in the south of the Apenine peninsula. As an endemic species, with a very little annual increment, it has not been used enough as a timber for mechanical conversion up till now, although the oldest trees can grow to 27 m in height, with a diameter at breast height of about 60 cm. According to data of many Ba...
M Petrovic, M Miric


Natural durability of Norwegian wood species for above ground applications – Project presentation and preliminary results
2006 - IRG/WP 06-10594
In Norway exterior wood structures have traditionally nearly exclusively been made of treated and untreated Norway spruce (Picea abies (L.) Karst) and Scots pine (Pinus sylvestris L.). In recent years there has been a tendency that other tree species, like various domestic hardwoods and imported species have been used in exterior above ground applications, often unfinished. For several wood speci...
P O Flæte, G Alfredsen, F G Evans


A dynamic approach to assess the modulus of elasticity in wood decay testing
1998 - IRG/WP 98-20139
In this study, the changes in elastic behaviour and mass losses of different hardwood and softwood species exposed to decay in a laboratory soil tests were assessed. Wood decay was monitored using different assessment methods, namely: mass loss and changes in elastic behaviours (MOE) determination. Elastic changes were determined by static and dynamic methods, for the latter, acoustic technique wa...
L Machek, H Militz, R Sierra-Alvarez


Supercritical fluid treatment: Effects on bending strength of white spruce heartwood
1993 - IRG/WP 93-20008
The effects of supercritical carbon dioxide on wood strength were evaluated using white spruce heartwood, a species known to be especially susceptible to collapse during exposure to higher pressures. The effects of pressures of 2000 or 3600 psig and temperatures of 40 or 80°C were evaluated using 30 or 60 minute exposure periods. No significant differences were noted in modulus of rupture or modu...
S M Smith, J J Morrell, E Sahle-Demessie, K L Levien


Natural durability transfer from sawmill residues of white cypress (Callitris glaucophylla). - Part 4: Analysis of extracts and treated wood for active components
2000 - IRG/WP 00-20215
In order to facilitate the commercial implementation of a large project aimed at recovering 'waste' durability components from sawmill residues of Callitris glaucophylla, it has been essential to develop analytical methodology for the important bioactive components of the heartwood extract. This methodology will be used 1) to standardise the activity of successive production batc...
Hui Jiang, M J Kennedy, L M Stephens


Evaluating the resistance of wood-based panel products to fungal attack
1995 - IRG/WP 95-20071
At present there is considerable disagreement among national research institutes within Europe and panel product manufacturers on the most appropriate method of testing and indeed the need for specific biological durability testing. This paper seeks to place before a broader international audience, the issues related to development of a European standard for evaluating the resistance to fungal dec...
R G Lea, R W Berry


On the resistance of consolidated ancient wood against Serpula lacrymans (Wulfen: Fr.) Schroeter
2000 - IRG/WP 00-10348
Structural timbers and other wood objects of cultural value in historical buildings and museums are often attacked by wood-destroying fungi. The aim of conservators is to preserve such damaged timbers and prevent further biodeterioration by impregnation with consolidants. There is little knowledge of the resistance of consolidated timber and art objects to a new attack by wood-destroying fungi. Br...
W Unger, A Unger, U Schiessl


Field testing of nootkatone and tetrahydronootkatone wood treatments against Coptotermes formosanus Shiraki
2003 - IRG/WP 03-30308
A component of Alaskan yellow cedar, citrus oil, and vetiver oil, nootkatone, and its derivative, tetrahydronootkatone, were tested for their potential as wood treatments against Coptotermes formosanus. Wood treatments dipped in 1% and 5% nootkatone and tetrahydronootkatone in ethanol or vacuum impregnated (5% only) were tested in a natural setting using termite infested bald cypress trees along t...
K E Nix, G Henderson, R Laine


Modification of wood by graft treatment
2003 - IRG/WP 03-40257
New water-repellent systems for wood are needed to improve the weathering characteristics. This study found that treatment of wood with chemical grafting systems imparted substantial water repellency. Different direct oxidative grafting systems were examined. Specifically, KMnO4, Fe(NH4)(SO4)2·12H2O, Fe2(SO4)3·5H2O, and (NH4)2Ce(NO3)6 were used as initiators and styrene as the monomer. All the...
M M Morshed, D D Nicholas, C Pittman Jr, T Schultz


Need to develop processing technologies (for value addition) of the species evaluated for their properties and uses
2005 - IRG/WP 05-40307
The demand of timber in India for different industrial as well as domestic applications is ever increasing mostly due to urbanization and industrialization. This demand can only be met either from the imported timber or from the plantation resources outside the reserved and natural forests. There are a number of timber species grown under plantation forestry have their heartwood refractory to any ...
S R Shukla, S K Sharma, Y M Dubey, P Kumar, R V Rao, K S Shashidhar


Evaluation of outdoor weathering performance of modified wood
2004 - IRG/WP 04-20296
Interlace treated, oil treated, silicon treated as well as untreated Scots pine samples have been exposed outdoors. For evaluating the samples on their long term performance an internal standard had been developed. Parameters to be determined were the uptake of liquid water (submersion test), weight variation during exposure, crack performance, surface roughness and colour change. This paper disc...
Y Schulte, S Donath, A Krause, H Militz


Investigation of the suitability of silver fir (Abies alba Mill.) for thermal modification
2004 - IRG/WP 04-40275
In this study the suitability of silver fir (Abies alba Mill.) was examined for thermal modification. Comparative experimental investigations were performed with silver fir and Norway spruce (Picea abies Karst.) after thermal treatments. Besides properties, which characterize the quality of heat treatments, like dimensional stability and resistance against fungal attack, strength properties of the...
C Brischke, A O Rapp


An appraisal of the vertical distribution of attack of untreated and treated wood by warm water sphaeromatids at some tropical sites - A discussion paper
1986 - IRG/WP 4124
Examples of the vertical distribution of burrows of warm water sphaeromatids relative to tide levels and mud line from sites in India, Papua New Guinea and tropical Australia are discussed in detail. These data show clearly that these animals concentrate their attack of resistant natural wood or resistant treated wood in the tidal zone, particularly around Mean Sea Level. Supportive evidence from ...
J E Barnacle, L J Cookson, C N McEvoy


The effect of alternative pre-conditioning procedures on the durability of wood based board materials to decay fungi
1997 - IRG/WP 97-20105
In the biological testing of wood based board materials it has been shown that exposure of boards in a closed vessel system may lead to inaccurate results due to the build up of volatile substances that inhibit the test fungi. It is thought that this is a transitory effect of freshly manufactured boards. In the European standard for testing fungal durability of board materials which is currently u...
S F Curling, R J Murphy, J K Carey


The improvement of wood durability by retification process
1993 - IRG/WP 93-40015
A material with new properties is obtained by retification process. It consists of a light pyrolysis of wood which becomes more stable and especially more resistant to fungal attack with few decrease of mechanical properties. Tests were carried out on three susceptible wood species (Poplar, Spruce, Fir) that are used in construction and are difficult to treat with wood preservatives. Retified wood...
D Dirol, R Guyonnet


Preservative treatment of common timbers and bamboos of Bangladesh for rural electrification infrastructure
1998 - IRG/WP 98-40104
Researches revealed new treatment grades, treatment groups, grading groups, natural durability grades, strength groups and a new preservative combination for remedial treatment and sterilization of most common timbers and bamboos of Bangladesh. The obtained findings are applicable for equivalent timber species having equivalent climatic condition. Sapwoods are always perishable and timbers with wh...
A K Lahiry


Improvement of intrinsic properties of wood by chemical wood densification - Hydrophobic aspects and durability aspects
1999 - IRG/WP 99-40149
To improve the intrinsic properties of Scot pine wood ((1) hydrophobic surface and (2) durability), two ways of chemical modification have been tested. The first one is the chemical modification of hydroxyl groups by active substances like diisocyanate compounds with a copolymerization step. The second way is a densification by an impregnation of resins and a gamma polymerisation. This second way ...
G Labat, Q K Tran, I Le Bayon