Corrosion of fastener and connector in contact with alkaline copper treated wood – it is a problem
2008 - IRG/WP 08-40437
For many decades, chromated copper arsenate (CCA) was the most common wood preservative used in North America for residential and industrial applications. Since December 31, 2003, the use of CCA for residential application was voluntarily terminated. One of the most widely accepted alternative wood preservatives in Western Canada is Alkaline Copper Quaternary Compound (ACQ). This paper will compar...
J N R Ruddick


Vacuum drying of European oakwood: Color, chemistry and anti-oxidant potency of wood. Improving appearance in forest value added products
2008 - IRG/WP 08-40432
In hardwoods used for decorative and appearance purposes, wood colour is one of the most important factors of wood quality; in addition colour is related with durability and biological decay of wood. Wood discolouration during drying is mainly affected by heat, light, physiological reactions, combinations of reactions, biochemical and chemical reactions, and micro-organisms attack. In freshly fell...
S Sandoval, W Jomaa, F Marc, J-R Puiggali


Opportunities and Needs with Treatments for the Protection of Plantation Species
2008 - IRG/WP 08-40438
The future of the wood treating industry lies increasingly on the treatment of wood derived from plantation forests. Plantation softwoods and hardwoods both provide significant opportunity for utilization coupled with protection technologies, but development programs will require much more focus and funding than is currently available. Manufacturing and treating of products from plantation fores...
A F Preston


Chemical modification of Scots Pine Sawdust by mixed anhydrides
2008 - IRG/WP 08-40439
By making react mixtures containing acetic-fatty anhydrides on Scots pine sawdust (SPS) without any solvent or catalyst; we synthesized mixed acetic-fatty esters of SPS. Such mixtures were synthesized by reaction between a carboxylic acid and acetic anhydride. These mixtures were obtained after reaction of acetic anhydride and a fatty acid that yields at equilibrium a mixture of five compounds: ac...
J Peydecastaing, E Borredon, S El Kasmi


Effect of different ASAs (alkenyl succinic anhydrides) on the treatment of biological protection of wood in use class 4
2008 - IRG/WP 08-40440
The alkenyl suscinic anhydrides (ASAs) used in this work are adducts resulting from the maleinization reaction of fatty acid alkyl esters. Various products with different alkyl groups were synthesized from rapeseed (Brassica napus) oil esters, rich in oleic acid. The liquids obtained showed a viscosity similar to that of vegetable oils and a brown color. When applied into wood, a thermal treatment...
C Vaca-Garcia, O Pignolet


Wood preservative obtained by recycling – preliminary selection of leaching inhibitor
2008 - IRG/WP 08-50252
Based on recycling of used household batteries, a process was developed to enable the recovery of major manufacturing components, leading to a solution of zinc (32 g.l-1) and manganese (15 g.l-1) salts, free of heavy metals. The potential use of the above solution as wood preservative was demonstrated by means of assays both of fungicidal activity -using white and brown rot fungi- and of insectici...
C Ibáñez, C Mantero, G Cecchetto, M Rabinovich, M Cerdeiras


Natural Durability of Some Heartwood from European and Tropical African Trees against Marine Organisms
2009 - IRG/WP 09-10682
This study aims to investigate the natural marine durability of some tropical and domestic wood species in marine environment. A total of 33 tree species, comprising 18 European and 15 tropical originated trees were exposed to marine conditions in 6 meters depth for a period of 14 months at east and west Black sea, Mediterranean, Aegean, and Marmara coasts. The results indicated that wood species...
S Sen, H Sivrikaya, M Yalçın


The amazing wooden churches from Northern Romania - learning from the past, restoring for the future, preserving the present valuable heritage of forgotten wood building tradition
2009 - IRG/WP 09-10683
The beauty and the uniqueness of the north-western region of Romania called “Maramureş” are well known in Europe. Surrounded by mountains, the region remained to some extend isolated from modern influences, preserving the local village architecture and craftsman traditions learnt and passed on from generation to generation. Local folklore and past heritage sets you back centuries ago when...
R Craciun, R Möller


Mechanical and chemical properties of blue stained wood
2009 - IRG/WP 09-10686
Discoloration of wood is frequently caused by blue-staining fungi. In the previous researches there was general opinion that blue-stain fungi do not influence mechanical properties. On the other hand, there were some opposite results reported as well. In order to elucidate this issue, specimens made of Pinus sylvestris sapwood were exposed to two the most frequent and important blue stain fungi Au...
M Humar, V Vek, B Bučar


The involvement of hydroxyl-radical-producing glycoprotein from the white-rot basidiomycete Ceriporiopsis subvermispora in wood decay
2009 - IRG/WP 09-10688
White-rot decay can be divided into two subtypes. One type involves the simultaneous degradation of all wood components through the formation of erosion troughs with a progressive thinning of wood cell walls. This type of decay is consistent with a model in which several polymer-degrading enzymes act on the exposed surfaces of the wood cell walls, producing progressive erosion from the lumen to th...
H Tanaka, Y Inoue, T Morikawa, S Itakura, A Enoki


Discovering anti-fungal agents in New Zealand native plants for use in wood protection
2009 - IRG/WP 09-10692
Extracts from Hinau (Elaeocarpus dentatus) leaves were tested in the laboratory for antifungal activity. In addition, the anatomical structure of the leaf was also examined by a combination of light and scanning electron microscopy. Chemical characterisation of the extracts and investigation into potential use of its components for wood protection is underway. A combination of light microscopy (...
C Rickard, T Singh, A Singh, R Newman


Prevelence of termite infestation and wood preferences in Pakistan
2009 - IRG/WP 09-10695
In order to know about prevalence of termite infestation in Pakistan, A study was carried out to know the intensity of infestation of different species of termites to different types of woods used in buildings as well as in the forests. Heterotermes indicola was the most notorious species of termite present in buildings, grounds throughout the year while Odontotermes obesus was most common in for...
F Manzoor, S Asma Malik


The effect of different foundation systems against fungal flora in the crawl space of a new wooden Japanese house
2009 - IRG/WP 09-10700
In order to establish novel preventive measures against damage of wooden houses by decay fungi with less-use or no-use of chemicals, we periodically monitored the fungal flora in the crawl space of a new wooden Japanese house build with recyclable and low-environmental load materials at the Research Institute for Sustainable Humanosphere, Kyoto University. We employed either a layer of concrete or...
A Toyoumi, S Horisawa, T Yoshimura, S Doi,Y Imamura


Postia placenta gene expression of oxidative and carbohydrate metabolism related genes during growth in furfurylated wood
2009 - IRG/WP 09-10701
A range of studies the last decade have shown that modified wood can provide excellent protection against a range of wood deteriorating organisms, including decay fungi. However, we still lack information about why the modified wood is protected from microbial attack. Several hypotheses have been put forward e.g. inhibition of action of specific enzymes, but they still need testing. An understandi...
G Alfredsen, C G Fossdal


Gene expression of selected decay enzymes produced during biodeterioration of three wood types
2009 - IRG/WP 09-10702
Comparative studies were conducted on the expression of several decay enzyme genes during the decay of pine, cedar, and ACQ treated pine over 10 months. Measurements of MOE, decay rating, and moisture control were monitored for physical properties. Identification of decay fungi and the detection of decay enzymes were carried out before gene expression levels were measured. The MOE of wood stakes d...
Young-Min Kang, L Prewitt, S Diehl


Isolation and identification of stain fungi and mould fungi on bamboo wood in China
2009 - IRG/WP 09-10703
One hundred and seventeen isolations were isolated from 150 specimens of mildewed or stained bamboo wood and bamboo products from 9 locations in north, south and central China. The molecular (ribosomal DNA Internal Transcribed Spacer, rDNA-ITS) and morphological identification results showed these fungi could be categorized 2 phyla, 2 classes, 4 subclasses, 10 orders, 15 families, 22 genera, 56 sp...
Xingxia Ma, Mingliang Jiang, Daochun Qin


Natural Durability Variations of Malaysian Timbers from Sarawak after 26 Years Exposure by Stake Test
2009 - IRG/WP 09-10704
An extensive graveyard stake test site was established in 1977 in Sibu, Sarawak, Malaysia, to evaluate the in-ground durability of 132 Sarawak wood species, mainly hardwoods. Test samples were planted at 100 x 50 cm spacing. Authenticated wood specimens from 3 trees of each of 132 species were processed into 20 replicated outer heartwood (or else undifferentiated heartwood) stakes of 19 x 19 x 457...
A H H Wong, Ling Wang Choon


Accelerated weathering of nine tropical wood species from Cameroon
2009 - IRG/WP 09-10705
The natural durability of tropical species for building components has been a subject of recent concern and questioning, mainly the resistance to weathering. Weathering resistance of nine tropical species from Cameroon, namely Azobe, Bilinga, Bubinga, Teak, Dousie, Moabi, Musanga, Sipo and Padauk were evaluated using an accelerated weatherometer for 2016 hours. Measurement of moisture fluctuation,...
S Pankras, Jinzhen Cao, D P Kamdem


Effects of cold treatment on wood destroying fungi important in cultural heritage
2009 - IRG/WP 09-10706
The dry rot fungus Serpula lacrymans (Wulfen:Fr.) Schroeter is notorious in building environments for its vitality, destructive potential, and the huge costs associated with remediation of damage caused to wood of cultural heritage. Due to the potentially adverse of effects of chemical treatment methods such as have been attempted in the past, more benign physical methods of treatment, e.g. heat t...
M Lüdicke, W Unger, G Binker


Moisture adsorption isotherms of wood studies using a dynamic vapour sorption apparatus
2009 - IRG/WP 09-20398
Five types of wood including two Malaysian hardwoods acacia mangium (Acacia mangium) and sesenduk (Endospermum malaccense), two temperate softwoods, Sitka spruce (Picea sitchensis), radiata pine (Pinus radiata) and Accoya (commercially modified wood) were studied to determine their moisture sorption behaviour using a Dynamic Vapour Sorption (DVS) apparatus. The isotherm plot for each species teste...
J Zaihan, C A S Hill, S Curling


Degradation of wood veneers by Fenton’s reagents: effects of low molecular weight phenolic compounds on hydrogen peroxide decay and tensile strength loss
2009 - IRG/WP 09-20400
Pine wood (Pinus sylvestris) veneers strips were incubated in acetate buffer containing hydrogen peroxide and iron to mimic mechanisms of brown rot decay and assess the degradation of cellulose through analysis of the tensile properties of the decayed wood. The tensile properties of thin wood strips treated with Fenton system reagents or precursors were determined and correlated to weight loss as ...
Yanjun Xie, R Well, Zefang Xiao, B Goodell, J Jellison, H Militz, C Mai


Service Life Prediction of Wood Claddings by in-situ Measurement of Wood Moisture Content: Status after 5 years of Outdoor Exposure
2009 - IRG/WP 09-20401
The Danish Technological Institute is in co-operation with industry partners running a project aiming at predicting the service life of different wood protecting systems. The project focuses on examining the moisture reducing effect of different protecting systems for timber claddings and the ability of these to maintain the appearance of the surfaces, when the wood is used in service class 3 (EN ...
E Tang Engelund, B Lindegaard, N Morsing


Wart Morphology can Distinguish White Cypress Pine from the Less Durable Species, Black Cypress Pine
2009 - IRG/WP 09-20406
White cypress pine (Callitris glaucophylla) wood is durable enough to be used outdoors, but occasionally there are reports of its premature failure in ground contact, which may be due to its substitution by the less durable species, black cypress pine (C. endlicheri). It has been difficult to prove this, however, because the woods of both species are very similar in structure and cannot be separat...
R Heady, R Cunningham, P Evans


Evaluation of exposure conditions for wooden facades and decking
2009 - IRG/WP 09-20408
During their functional life, building components are exposed to moisture and other environment stress conditions in numerous ways. This is a fact that should be taken into account during manufacture, product development, designing and work execution of building components. For wood material, moisture stress and biological factors like mould and decay fungi are often critical in cladding and decki...
H Viitanen, T Toratti, R Peuhkuri, T Ojanen, L Makkonen


Evaluation of variables that influence dynamic MOE in wood decay studies
2009 - IRG/WP 09-20409
The effect of wood moisture content (MC) and outdoor exposure of southern pine lap-joint components on dynamic MOE values was investigated. The use of dynamic MOE as a method of measuring progressive biodeterioration of above ground test samples shows promise, but the accuracy of this method for evaluating test samples subjected to fluctuating environmental conditions has not been reported. The re...
D Nicholas, J Shi, T Schultz