Characteristics and quantity of impregnated wood waste in Germany
1995 - IRG/WP 95-50041
The disposal of wood waste in Germany is one of the main problems not only for the wood preservation industry but also for all concerned with wood waste. Data on characteristics and quantity of wood waste are still needed. Based on criterions given in a previous paper (IRG/WP 93-50006), several assortments have been characterized with regard to their hazardous potential and their logistical aspect...
A Voss, H Willeitner


Estimation of mycelial biomass by determination of the ergosterol content of wood decayed by Coniophora puteana and Fomes fomentarius
1989 - IRG/WP 1415
The mycelial biomass of fungi decomposing wood materials may be estimated by the use of an ergosterol assay technique.ln decay tests, essentially according to EN 113, estimates made by HPLC analyses on wood decayed by Coniophora puteana and Fomes fomentarius show the increase in biomass in the wood blocks. The ergosterol contents were correlated with dry weight loss determinations. Degradation of ...
K Nilsson, J Bjurman


Leaching from CCA-treated wood submerged in seawater: Effect of high loadings, and a comparison between laboratory and marine conditions
1996 - IRG/WP 96-50080
This study of leaching examined the following variables: CCA loading; marine versus laboratory exposure and length of submergence. Blocks of Pinus sylvestris were treated to a range of nominal retentions from 15 to 50 kg/m³. Each block was then divided into three cubes and all transverse faces were sealed. All cubes were allowed to fix at ambient temperature for a minimum of one week. One set of ...
R M Albuquerque, S M Cragg, J D Icely


Preservative treatment of rubber wood (Hevea brasiliensis) to increase its service life
2005 - IRG/WP 05-40320
Rubber wood (Hevea brasiliensis) possess excellent properties for interior designing, wood working and furniture making. But it is very much susceptible to sap stain and mould fungi which decreases the service life. For profitable uses , it is necessary to increase the service life of rubber wood. To protect the rubber wood from wood degrading agents, the sawn timber were treated with Borax – b...
K Akhter


Influence of surface coating on the leachability of boric acid and bifluorides from spruce wood
1995 - IRG/WP 95-50050
In the Netherlands, window joinery made from non-durable timber species (spruce) are widely protected with preservative rods. These rods contain non-fixing wood preservatives (e.g. bifluorides or boric acid). This reseach was performed to show the possible influence of a coating system to hinder the leaching of the active ingredients. The results of the leaching tests show, that bifluorides and ev...
W J Homan, H Militz


Targeted inhibition of wood decay fungi: degradation of cotton cellulose
1999 - IRG/WP 99-10321
Brown-rot decay is responsible for 80% of the damage and replacement of wood in service. For nearly thirty years, researchers have postulated a one-electron oxidase system combining Fe+2 oxalic acid, and H2O2 in the production of hydroxy radicals which ultimately oxidize cellulose in situ. Recently, researchers have been investigating antioxicants, in combination with biocides (Schultz, et al.,199...
F Green III, T A Kuster


Microemulsion formulations for wood protection chemicals
1993 - IRG/WP 93-30030
A microemulsion is a thermodynamically stable oil-water dispersion system. As a formulation it provides many unique features such as water compatibility for water-insoluble chemicals, formulation stability, good bioavailability and environmental acceptance. This paper discusses the major criteria for the formulations of water-insoluble wood biocides and the comparison in properties between convent...
Bing Yu, L E Leightley


Microwave modification of wood properties - Improvements in wood permeability
2000 - IRG/WP 00-40181
A new method of microwave (MW) wood modification is described. Microwave irradiation of timber provides an improvement in wood permeability mainly in the radial and longitudinal directions. This is achieved by physically modifying ray cells and forming a large number of cavities in the radial - longitudinal planes. More extensive MW irradiation of different species transforms the wood into a new m...
G Torgovnikov, P Vinden


Which substrate to use in a laboratory test with soft rot micro-fungi: vermiculite or unsterile soil?
1991 - IRG/WP 2372
A draft European Standard is being proposed by CEN TC 38 in which a vermiculite-burial and a soil-burial test to be carried out in succession are required. Various experiments with both procedures were set up with CCA, CC and propiconazole-formulations. The results show that vermiculite and unsterile soil yield comparable threshold values against soft rot. This poses the question of whether a two-...
A R Valcke


Site characteristics impacting historic waterlogged wood: A review
2000 - IRG/WP 00-10344
Survival of waterlogged wood from hundreds and in rare cases millions of years presents scientists with a unique opportunity to examine wood specimens which, due to select properties of the wood itself and/or the depostional environment, have not been completely degraded. Although degradation patterns of various types of microbial wood decay have been studied in detail, the site parameters of the ...
B A Jordan, E L Schmidt


Influence of variable lignin content amongst hardwoods on soft-rot susceptibility and performance of CCA preservative
1982 - IRG/WP 1151
This paper presents the outline of an argument, based on both new and established data, which relates varying lignin content to variation of soft-rot susceptibility between hardwood species and of performance of CCA preservatives in controlling soft-rot. Although more data need to be generated to prove this relationship, sufficient evidence exists for the hypothesis to be given close attention, pa...
J A Butcher, T Nilsson


Experiments in accelerated ageing
1984 - IRG/WP 2223
Experiments using a vacuum oven to accelerate the evaporative loss of g-HCH from treated wood blocks have indicated that the method described in this paper has the potential to reproduce in a relatively short time the distributions and loadings of the insecticide that are found during natural ageing. By contrast, the wind tunnel removed the volatile material in a way not found in natural ageing an...
R J Orsler, M W S Stone


Determination of the amine to copper ratio remaining in wood after leaching
2002 - IRG/WP 02-30285
The effectiveness of the protection and the environmental impact of the treated wood are two of the most important aspects that need to be understood for all preservatives. Both are particularly influenced by the loss of biocidal components from treated wood. For amine copper preservatives, copper fixation determines the leaching resistance of the copper and amine compounds formed in wood. Previou...
N Lucas, J N R Ruddick


Effect of moisture and cellulosic substrate on decay of hardwoods by soft-rot fungi
1982 - IRG/WP 2173
The development by Forintek Canada Corp. of standard test procedures for laboratory preservative evaluations using soft-rot fungi was requested by the American Wood Preservers' Association. In Europe, through cooperative studies in the International Research Group on Wood Preservation, several attempts have been made to produce a standard procedure, but variability in results obtained bet...
A Byrne, R S Smith


Wood preservative potential of fractions of wood pyrolysis tar made from Japanese larch
1996 - IRG/WP 96-30102
Wood pyrolysis tar, which was discharged as a waste by-product in the production of charcoal from Japanese larch (Larix leptolepis), was separated into several fractions by solvent extraction using tetrahydrofuran, benzene and aqueous alkali. The fractions obtained were physico-chemically characterized and examined for wood preservative potential. This separation method compared favorably with fra...
T Suzuki, S Doi, M Yamakawa, K Yamamoto, T Watanabe, M Funaki


The treatability of five Indonesian wood species with BFCA preservative
1987 - IRG/WP 3428
This paper deals with a preliminary study on the treatability of five Indonesian wood species, i.e. Altingia excelsa (AE), Rhodoleria teysmanii (CA), Litsea odorivera (LO), Schima wallichii (SW) and Cratoxylon arborescens (CA). Wood samples measuring 4 x 4 x 100 cm³ were dipped into BFCA preservative solution for about 30 seconds. Preservative penetration and the surface area of treated zone were...
Nana Supriana, T K Waluyo


The economics of saving standing wood poles. Labour saving system for pole groundline retreatment
1980 - IRG/WP 3160
This paper consists of 3 contributions First: There are still people who consider wood poles a disposable commodity much the same as paper cups and toilet paper. The idea of conservation is still new in this field, but soon conservation will be a necessity. Only two percent of the forest recources of North America are being replaced. What does it mean? We will run out of poles a lot sooner than ...
W V Inkis


Decay and termite resistance of wood treated with boron-containing quaternary ammonia compound, didecyl dimethyl ammonium tetrafluoroborate (DBF) incorporated with acryl-silicon type resin
2004 - IRG/WP 04-30334
This study evaluates the decay and termite resistance of surface-treated wood with didecyl dimethyl ammonium tetrafluoroborate (DBF) incorporated with acryl-silicon type resin emulsion. DBF is a quaternary ammonia compound and contains boric tetrafluoride (BF4-) as a counter ion in its chemical structure. In the study, DBF was incorporated with an acryl-silicon type resin to increase water-resista...
S N Kartal, W J Hwang, K Shinoda, Y Imamura


Co-operative research project on L-joint testing. Progress report to March 1985
1985 - IRG/WP 2236
It was originally intended that each participant would expose L-joints in the main trial on 1 April 1983 with the first sampling at 8 months (1 December 1983) and the second sampling at 18 months (1 October 1984). In the event, some participants have had to vary this schedule. Results after the first sampling have been received from CTFT (8 months), BAM (12 months) and Sipad-IRC (8 months) and aft...
J K Carey, A F Bravery


IPBC - A new fungicide for wood protection
1984 - IRG/WP 3295
3-iodo-2-propynyl butyl carbamate (IPBC) is presented as a potential low toxic alternative to pentachlorophenol and the sodium chlorophenoxides. Data on its effect against basidiomycetes is shown. Tests according to both the European standard method, EN-113, and American, ASTM D-413, have shown its potential. The chemical gives protection against both the wood destroying fungi, blue stain, mould and algae. It is possible to have it formulated in both water-based and organic solvent-based products. Treatment of wood out of ground contact (vac-vac products, pretreatment products, primers, stains, etc.) and sapstain control are some of the most potential end use areas within wood protection. Besides wood protection, the IPBC is used as a fungicide in paint, adhesives, caulks and sealants, cement, leather, paper, cutting oil, ink and in different roofing materials.
J Hansen


Assessment of untreated Papua New Guinea timbers against subterranean termites. Progress report 2
1993 - IRG/WP 93-10040
Eight species of Papua New Guinea wood including Kwila (Intsia palembanica), Taun (Pometia pinnata), Malas (Homalium foetidum), PNG Walnut (Dracontomelon dao), Calophyllum (Calophyllum sp.), Kamarere (Eucalyptus deglupta), PNG Beech (Nothofagus spp.) and White Cheesewood (Alstonia scholaris) were exposed groun contact for their natural durability against subterranean termites. Inspection after 42 ...
M Rokova, H C Konabe


Potential for using dip/supercritical fluid treatments for wood impregnation
2004 - IRG/WP 04-40276
While supercritical fluid impregnation offers tremendous potential for impregnating wood species that resist conventional liquid preservative treatments, the resulting treatments are often not uniform among samples in a charge or between charges. One factor that influences treatment is the dynamic change in pressure that occurs during introduction of the biocide laden supercritical fluid into the ...
Sung-Mo Kang, J J Morrell


Deterioration of wood viewed from iron nail
1991 - IRG/WP 2368
Deterioration of nail was graded by a five - rank numerical - rating. The rating of nail moisture content and decay of wood were inspected in a mortal-wall of 34-year-old house. The wood was mostly in decay, when the rating of the nail was above about 4, and the moisture content was above about 20%. Nailed wood specimens kept in several humidity room of 20°C for 4 years showed that the rating of ...
H Imamura


Dimensional stability and decay resistance of wood upon modification with some new type chemical reactants
1994 - IRG/WP 94-40028
Solid wood of home grown species can be upgraded by chemical modification with environmentally acceptable chemicals. The best kwown example of modification reaction is acetylation with acetic anhydride. A continued search for reactive chemicals other than acetic anhydride is ongoing, aiming at the improvement of technical properties of wood. This contribution deals with the results of a screening ...
P Goethals, M Stevens


Collaborative soft rot tests: Statistical treatment of results of soil analyses
1971 - IRG/WP 29
Institutes taking part in the collaborative experiments already reported forwarded samples of the soils employed in the tests to the Forest Products Research Laboratory, England. The soils were then autoclaved sterilised under uniform conditions and sent to the Department of Forest Soils, the Royal College of Forestry, Stockholm, Sweden. The results of the soil analyses are given in Table 1, toget...