IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 3497 documents. Displaying 25 entries per page.


Treatability and natural durability of some lesser used or unused wood species of Bangladesh
2000 - IRG/WP 00-40170
A research study was conducted to determine the natural durability and treatability of heartwood of some lesser used or unused wood species. The treatability of species has been studied along with certain anatomical concepts association with preservative penetrability of the wood. It was observed that grain structure and presence of tyloses appeared to be correlated with penetrability of the wood....
K Akhter, M Younusuzzaman, M H Chowdhury


Durability of exterior natural wood finishes in Brazil
1985 - IRG/WP 3343
Wood finishes systems were evaluated in natural weathering conditions during 5 (five) years, over "Parana-pine" (Araucaria angustifolia). Test samples results show that: - Semitransparent wood preservative stains, based on polimerized linseed oil, provided very good protection to the wood, compared with the one based on alkyd varnish; - Solid color wood preservative stains provided good durability...
D R Macedo


Natural durability of fifty species of Indian timber in Goa waters against marine wood-borers
1989 - IRG/WP 4150
Results of the investigations on the natural durabilitv of fifty species of Indian timber, based on data collected bv exposing test panels at Betim near Panaji (Goa) continuously for a period of 11 months are presented. The study revealed that none of the timber species tested has any natural resistance at this locality and all the panels were completely destroyed within 11 months. Details on the ...
L N Santhakumaran, S Udaya Bhaskar, J C Jain


Non-destructive stress wave measurement of decay and termite attack in experimental wood units
1986 - IRG/WP 2256
The purpose of this study was to determine if stress wave analysis could be used to monitor the degradation of wood specimens exposed to the brown-rot decay fungi (Gloeophyllum trabeum) and of wood specimens subjected to attack by subterranean termites. One hundred fifty 3/4 by 3/4 by 12 in. Southern pine specimens were used for exposure to brown-rot decay fungi and two hundred twenty-five 3/4 by ...
R F Pellerin, R C De Groot, G R Esenther


NIR spectroscopy for rapid estimation of decay resistance
2004 - IRG/WP 04-20294
In Scandinavia Scots pine (Pinus sylvestris L.) is an important commercial tree species. Its heartwood has traditionally been used in constructions exposed to risk of decay. In a laboratory experiment Scots pine wood specimens sampled from inner heartwood, outer heartwood and sapwood were exposed to the brown rot fungus Poria placenta. In general outer heartwood was more resistant than inner heart...
P O Flæte, E Ystrøm Haartveit


Evaluation of the european standard ENV 12038 for durability testing of plywood
2001 - IRG/WP 01-20237
The latest improved version of the standard ENV 12038 drafted as document N44 by CEN Technical Committee 38 (WG 7 - WG 23) is used to evaluate the effect of wood composition and structure on plywood durability. The method described is based on the agar-block test of the EN 113 standard used for the determination of the efficacy of wood preservatives and the assessment of the natural durability of ...
J Van Acker, M Stevens, E De Clercq


Variation of natural durability of sugi (Cryptomeria japonica) wood in 15 clones examined by decay test (Preliminary report)
2004 - IRG/WP 04-10526
Natural durability of wood in 27 trees from 15 clones of sugi (Cryptomeria japonica)  was investigated by an accelerated decay test. Thirty years old trees were collected from a clonal trial in Ibaraki prefecture, Japan. Natural durability is usually evaluated in heartwood. Mass losses of heartwood caused by a brown rot decay fungus, Fomitopsis palustris and a white rot decay fungus, Py...
K Yamamoto, A Tamura, R Nakada


Is laboratory testing of decay resistance questionable as a single criterion for natural durability?
1996 - IRG/WP 96-20096
In a laboratory test set up over 20 hardwood species were evaluated according to the European Standard EN 350-1 including Basidiomycete and soft rot testing. Half of the species used were of a known natural durability. The Basidiomycete testing was carried out using Coriolus versicolor, Gloeophyllum trabeum and Coniophora puteana in a malt agar test similar to EN 113. From this test it was not pos...
J Van Acker, M Stevens, T Van Cauwenberghe, T Seynaeve


Moisture content development in lap-joints of different wood species in outside exposure trials
1998 - IRG/WP 98-20143
Lap-joint trails (following European Standard EN 12037) were set up with 11 different softwood and hardwood species. Half of the number of the lap-joint specimens were coated with an alkyd coating. The moisture development has been followed during a 19 months period. In this paper, the out comes of different moisture contents evaluations are presented. The results show, that the moisture content o...
H Militz, M Broertjes, C J Bloom


Screening techniques for potential wood preservative chemicals. Proceedings of a special seminar held in association with the 10th Annual Meeting of the IRG, Peebles 1978. Report No 136, 1979
1980 - IRG/WP 2138
This paper continues following issues: I. SCREENING INSECTICIDES 1) R W Berry (BRE/PRL, UK): Screen testing of insecticides for use in remedial wood preservatives. 2) D J Cross (FRI, New Zealand): Rapid screening of contact insecticides for use on forest products. 3) C R Coggins; A Forsyth; A E Glaser (Rentokil, UK): Experience in the use of indicative screening techniques for termiticides. ...
Anonymous


Laboratory tests on the natural durability of timber methods and problems
1984 - IRG/WP 2217
In literature a large variety of test methods is mentioned to examine the natural resistance of timber against fungal attack. This concerns the kind of sampling as well as the test procedure, the test fungi, the duration of test, and the classification of the resistance according to the test results. These variations, however, are of great influence on the test result. Long term exposure will lead...
H Willeitner


The comparative resistance to fungi of the wood munika (Pinus heldreichii Christ.), fir (Abies alba Mill.) and spruce (Picea excelsa Poir.) compared with Pinus sylvestris L. and some physical and mechanical characteristics of munika
1981 - IRG/WP 1129
The munika (Pinus heldreichii Christ.) is situated primarily in the Balkans, and partially in the south of the Apenine peninsula. As an endemic species, with a very little annual increment, it has not been used enough as a timber for mechanical conversion up till now, although the oldest trees can grow to 27 m in height, with a diameter at breast height of about 60 cm. According to data of many Ba...
M Petrovic, M Miric


Natural durability of Norwegian wood species for above ground applications – Project presentation and preliminary results
2006 - IRG/WP 06-10594
In Norway exterior wood structures have traditionally nearly exclusively been made of treated and untreated Norway spruce (Picea abies (L.) Karst) and Scots pine (Pinus sylvestris L.). In recent years there has been a tendency that other tree species, like various domestic hardwoods and imported species have been used in exterior above ground applications, often unfinished. For several wood speci...
P O Flæte, G Alfredsen, F G Evans


Durability of heat-treated wood
1999 - IRG/WP 99-40145
Heat-treated wood from the French process were laboratory tested against decay using agar block test and a modified soil block test. Water absorption, bending strength, lignin content and acid number were also determined to evaluate the effect of heat treatment. Heat treated samples exhibit a higher lignin content and a lower acid number compared to untreated control indicating the degradation of ...
D P Kamdem, A Pizzi, R Guyonnet, A Jermannaud


Performance of different treatments and finishes on wood out of ground contact. Preliminary results
1984 - IRG/WP 2221
Pinus and Eucalyptus L-joints treated with CCA, a water dispersable PCP and untreated ones were painted according to seven different finish's schedules and exposed at two sites in State of Sao Paulo. After ten months of exposure, it was possible to verify that preservative treatment improve the performance of both wood and finish. It was also possible to observe that wood substrate, prese...
S Milano


Implications for comparibility of laboratory experiments revealed in studies on the variability in survival and wood consumption between colonies of Coptotermes acinaciformis (Froggatt) (Isoptera: Rhinotermitidae
1983 - IRG/WP 1193
Groups of Coptotermes acinaciformis originating from six colonies, three taken from each of two localities 1500 km apart in northern Australia (Townsville, Darwin), were kept at population densities of 0.005, 0.011 and 0.02 g termites/mL. Survival and wood consumption of the groups after 8 weeks followed a similar pattern in the colonies from both collection areas. Groups were least vigorous at th...
M Lenz


Natural durability transfer from sawmill residues of white cypress (Callitris glaucophylla). - Part 4: Analysis of extracts and treated wood for active components
2000 - IRG/WP 00-20215
In order to facilitate the commercial implementation of a large project aimed at recovering 'waste' durability components from sawmill residues of Callitris glaucophylla, it has been essential to develop analytical methodology for the important bioactive components of the heartwood extract. This methodology will be used 1) to standardise the activity of successive production batc...
Hui Jiang, M J Kennedy, L M Stephens


Evaluating the resistance of wood-based panel products to fungal attack
1995 - IRG/WP 95-20071
At present there is considerable disagreement among national research institutes within Europe and panel product manufacturers on the most appropriate method of testing and indeed the need for specific biological durability testing. This paper seeks to place before a broader international audience, the issues related to development of a European standard for evaluating the resistance to fungal dec...
R G Lea, R W Berry


Field testing of nootkatone and tetrahydronootkatone wood treatments against Coptotermes formosanus Shiraki
2003 - IRG/WP 03-30308
A component of Alaskan yellow cedar, citrus oil, and vetiver oil, nootkatone, and its derivative, tetrahydronootkatone, were tested for their potential as wood treatments against Coptotermes formosanus. Wood treatments dipped in 1% and 5% nootkatone and tetrahydronootkatone in ethanol or vacuum impregnated (5% only) were tested in a natural setting using termite infested bald cypress trees along t...
K E Nix, G Henderson, R Laine


Test methods for wood preservatives against Lyctus: (1) Testing of treated veneer. (2) Testing of glue-line treated plywood. (Laboratory methods)
1977 - IRG/WP 293
Powder-post beetles destroy large quantities of veneer and plywood. Two test procedures are described which can be used to support application-oriented research into veneer and plywood preservatives. These procedures simulate practical conditions on a laboratory scale. Their characteristic feature is that wood species of special susceptibility are used for the tests; the susceptibility of the spec...
S Cymorek


Comparison of performance of wood preservatives in laboratory and field tests of treated commodities
1993 - IRG/WP 93-20010
The purpose of laboratory tests for evaluating efficacy of wood preservatives is usually to establish toxic values against standard strains of wood decay fungi. Exposure conditions are usually chosen as optimal for fungal growth. Toxic values so determined serve as a guide as to expected performance of the preservative in field stake tests or in above ground exposure tests. Test material is select...
M E Hedley


Non-destructive detection of the presence and behaviour patterns of wood-destroying insects
1988 - IRG/WP 2302
An apparatus, designed for the automatic recognition of the presence and of specific behaviour patterns of wood-boring insects, is introduced. From a wood sample, a mixture of noise and action induced substratum vibrations is picked up, amplified, filtered and translated into a sequence of computer-readable numbers which are passed to a microcomputer-based signal-pattern-recognition. If an incomin...
M Pallaske


The effect of alternative pre-conditioning procedures on the durability of wood based board materials to decay fungi
1997 - IRG/WP 97-20105
In the biological testing of wood based board materials it has been shown that exposure of boards in a closed vessel system may lead to inaccurate results due to the build up of volatile substances that inhibit the test fungi. It is thought that this is a transitory effect of freshly manufactured boards. In the European standard for testing fungal durability of board materials which is currently u...
S F Curling, R J Murphy, J K Carey


A soil-less test of treated wood
1978 - IRG/WP 2105
The objective of this work is to devise an accelerated test for preservatives to be used in places away from soil contact. There may be compounds or mixtures which will protect wood or wood derived materials from decay in such articles as sash and doors, boardwalks, steps, laminated arches and the like, and possess properties that make them preferable to the heavy-duty preservatives used for poles...
E A Behr


Status of Work on OECD Test Guidelines for Emissions of Wood Preservatives to the Environment
2005 - IRG/WP 05-50224-3
In April, 2003, OECD published an ESD on wood preservatives that provides guidance on how to estimate emissions: 1) during the wood preservative application processes and storage of treated wood prior to shipment; and 2) from treated wood-in-service. The ad hoc Expert Group that developed the wood preservatives ESD identified the need to develop Test Guidelines to estimate the amount of biocides ...
W Jakob


Previous Page | Next Page