Your search resulted in 3272 documents. Displaying 25 entries per page.


Virulence of two Laboratory Test Strains and one Natural Isolate of Rhodonia (Oligoporus) placenta against Thermally Modified Pine and Beech Wood
2013 - IRG/WP 13-20524
Rhodonia (Oligoporus) placenta is known as a relative aggressive basidiomycete fungus against thermally modified timber. In durability lab tests, this often results in a lower durability class, compared to other test fungi. In the reported work, the virulence of three different strains of Rhodonia placenta for untreated and thermally modified timber was determined and compared. Therefore, two lab ...
K Plaschkies, W Scheiding, K Jacobs, N Rangno


Performance testing of DMDHEU-modified wood in Australia
2013 - IRG/WP 13-30613
Chemical wood modification with dimethyloldihydroxy-ethyleneurea (DMDHEU) or its derivatives has been researched for many years and shown to be applicable to improve certain wood properties to both solid lumber and wood-based composites. Earlier research proved a high biological resistance of DMDHEU-modified wood against biological degradation in laboratory and field tests in Europe. Due to the ve...
H Militz, J Norton


Preliminary testing of spiroborate esters as wood preservatives
2013 - IRG/WP 13-30614
Fungicide and insecticide properties of boric acid are known since 30’s of the last century, but high solubility and leachability of inorganic borates limit their use for only applications not directly exposed to liquid water. A number of attempts were made to fixate borate salts into the wood structure but this research topic is still up to date and undiscovered. Water insoluble organoboron est...
D Panov, N Terziev


The effects of impregnation with secondary metabolite extracted from Ipe on durability of Japanese cedar and beech wood
2013 - IRG/WP 13-30618
Ipe wood is known for its high durability; it has been widely used in exterior structures that are exposed to the weather. In this paper, to increase the durability of less durable wood, Japanese cedar and beech specimens were impregnated with a secondary metabolite from Ipe. In a previous study, secondary metabolites extracted by a Soxhlet extraction method showed antifungal properties. Therefore...
T Iida, R Konuma, K Kawarada


Effect of the nature of the inert atmosphere used during thermal treatment on chemical composition, decay durability and mechanical properties of wood
2013 - IRG/WP 13-40625
Wood heat treatment is an attractive alternative to improve decay resistance of low natural durability wood species. Nowadays, several types of thermal treatments of wood exist. These treatments differ mainly by the nature of the inert atmosphere used to avoid wood combustion which may correspond to: nitrogen, vacuum, steam or oil. Decay resistances as well as mechanical properties are strongly co...
K Candelier, S Dumarçay, A Pétrissans, M Pétrissans, P Gérardin


Resistance of WPC against wood destroying fungi
2013 - IRG/WP 13-40627
The investigation of biological durability is a fundamental topic to assess the performance of Wood Plastic Composites (WPC) particularly for outdoor applications. In the last years, different test setups based on existing standards on the field of wood as well as the field of plastics were used for WPC. But the test methodologies give different information about the durability of the tested mater...
A Gellerich, S Bollmus, A Krause


Moisture and Fungal Durability of Wood-Plastic Composites Made With Chemically Modified and Treated Wood Flour
2013 - IRG/WP 13-40648
Evaluating the fungal durability of wood-plastic composites (WPCs) is complicated by the influence of slow moisture sorption. Recently, the American Wood Protection Association (AWPA) Standard Method E10, Testing Wood Preservatives by Laboratory Soil-Block Cultures, was modified to incorporate not only solid wood, but also wood-based composites and WPCs. To simulate long term WPC performance, cond...
B K Segerholm, R E Ibach


Durability of alternatives to CCA-treated wood - Results from field tests after 11 years exposure
2013 - IRG/WP 13-30633
The present study was initiated as a consequence of restrictions against the use of CCA-type wood preservatives in Sweden in the 1990s. New copper-based formulations were introduced on the market and to some extent, also alternatives to preservative-treated wood, such as thermally and chemically modified and linseed oil treated wood as well as heartwood of non-tropical naturally durable wood s...
P Larsson Brelid, M-L Edlund


Estimation of service life of treated wood in ground contact based on early indicators
2013 - IRG/WP 13-20536
A well-known problem with field testing is that it takes a long time before meaningful and reliable results are achieved. Only when a trial has come to an end the so called average life for the samples in a group can be calculated and compared with other samples. The aim of the present study was to investigate if it is possible to get a reasonable and good estimation of the average life long befor...
M Hansson, J Jermer, P Larsson Brelid, N Terziev


Moisture dynamics of wood – An approach to implement wetting ability of wood into a resistance classification concept
2014 - IRG/WP 14-20557
Within the research programmes WoodBuild and PerformWOOD, wetting ability tests have been conducted with 25 wood-based materials. A first attempt has been made to establish factors for calculating the material resistance of wood materials to be implemented into a design guideline for timber structures. The approach looks promising, but further studies are needed to establish more reliable relation...
C Brischke, C Hesse, L Meyer, S Bardage, J Jermer, T Isaksson


An Overview of Western Red Cedar as a Wood Pole Species
2014 - IRG/WP 14-10815
This paper reviews the characteristics of western red cedar, with particular emphasis on its use in utility poles. Western red cedar naturally grows primarily in British Columbia, Alaska, Washington, Oregon, California, Idaho and Montana. Compared to other commercial softwoods it has low density, increased corrosivity, weaker mechanical properties, high dimensional stability, and high natural dura...
M H Freeman, R Stirling


Performance of recent and old Sweet chestnut (Castanea sativa) wood
2014 - IRG/WP 14-10816
Sweet chestnut (Castanea sativa) hardwood is one of the most durable European wood species. In the present research, various aspects that could potentially influence the durability were elucidated, namely: presence of extractives, ring width, and weathering. Simultaneously, properties of wood, which was in outdoor use for 35 years, were elucidated as well. The results indicate that ring width and ...
M Humar, M Žlahtič, N Thaler


Durability and Wood Protection for Historic Covered Bridges in the United States
2014 - IRG/WP 14-10829
A majority of the covered wooden bridges in United States were built in the mid -1800’s. These structures represent a unique cultural and technological heritage from that era. Over time, these bridges have been deteriorated by microorganisms and insects or damaged by acts of vandalism and arson. The National Historic Covered Bridge Preservation (NHCBP) Program sponsored by the Federal Highway Ad...
V W Yang, C A Clausen


Variability in durability of some selected South-American wood species
2014 - IRG/WP 14-10831
Within the scope of sustainable forest management one wants to encourage the proper use of lesser known wood species. Therefore the market has to shift from a demand-driven towards a supply-driven market without loss of wood quality. It is generally known that the durability from pith to bark varies thus, affecting the overall durability of wood species. Consequently, a detailed analysis is necess...
I De Windt, P ’t Hooft, J Van den Bulcke, J Van Acker


Moisture performance testing of wood – Practical experiences
2014 - IRG/WP 14-20546
Different methods are used to characterize the moisture performance of wood and to quantify the effect of moisture loads on the resulting service life. These methods can be divided into direct and indirect methods. Furthermore they can be distinguished by characteristics like continuous or periodical measurements and measuring local or global moisture content (MC). Furthermore each measuring metho...
L Meyer, C Brischke, M Kasselmann, C Rösmann


In-ground durability of wood-based products – Comparative assessment of graveyard field tests and terrestrial microcosms
2014 - IRG/WP 14-20538
Traditionally wood durability and the effectiveness of wood preservatives are determined in so-called graveyard tests (according to EN 252 or AWPA E7). For laboratory testing, terrestrial microcosms (TMC) can serve as an alternative. Both tests have been applied for different types of wood-based materials, preservative treated, modified and unmodified wood. However, the usability of laboratory res...
A Soetbeer, L Meyer, C Brischke, P Larsson-Brelid, J Jermer


Moisture dynamics of wood and wood-based products – Results from an inter-laboratory test
2014 - IRG/WP 14-20539
In the frame of the European research project PerformWOOD in close liaison with the CEN task group TG EN 350 of CEN TC 38 WG 21 in total six research institutes teamed up and initiated an inter-lab trial (Round Robin) to investigate the suitability of different test methods to determine the wetting ability of wood. The moisture performance of wood and wood-based products has been recognized as key...
C Brischke, L Meyer, C Hesse, J Van Acker, I De Windt, J Van den Bulcke, E Conti, M Humar, H Viitanen, M Kutnik, L Malassenet


The development of accelerated test systems to evaluate the durability of framing timber
2014 - IRG /WP 14-20547
Various accelerated decay resistance trials including small simulated wall units, samples exposed in enclosed tanks and ‘I’ samples in stacks have been explored and used to test the durability of treated and untreated radiata pine framing at Scion since 2001. These testing methods have been established to determine the effectiveness of commercial formulations in preventing decay in framing sub...
T Singh, D Page, J van der Waals


Termite resistance of wood modified with short- and long-chain siloxanes
2014 - IRG/WP 14-40660
Scots pine (Pinus sylvestris L.) sapwood specimens modified with short- and long-chain amino-functional siloxane emulsions were exposed to subterranean termites (Reticulitermes flavipes Kollar). Laboratory choice and no-choice tests following the standard EN 117 (2013) were conducted for 8 weeks in order to evaluate the influence of these silicon-based compounds on the termite resistance of treate...
P Gascón-Garrido, M-F Thévenon, H Militz, C Mai


Development of new wood treatments combining boron impregnation and thermo modification - Effect on decay and termites durability
2014 - IRG/WP 14-40666
Environmental pressures appeared in most European countries during the last decade has lead to the development of more environmentally acceptable preservation methods. In this context, wood heat treatment has been one of the most investigated alternative methods during the last years. Treated at temperatures ranging between 180 and 220°C, wood components undergo more or less important chemical mo...
S Salman, A Pétrissans, M-F Thévenon, S Dumarçay, B Pollier, P Gérardin


The Physical Properties of Heat Treated Fir Wood and Outdoor Durability
2014 - IRG/WP 14-40677
Wood might be easily susceptible to degrade by biotic and abiotic factors. Therefore, wood should be protected from fungi, insects and other degradation factors by applying treatment methods. Especially, for the wood have used in the external environment. Chemical treatment methods have some disadvantages such as use of toxic chemicals (Arsenic and chromium) and treatability of refractory wood spe...
O E Özkan, H Vurdu, A Temiz, G Köse


Influence of the moon phase on durability against wood decay fungi of Larix kaempferi and Pseudotsuga menziesii wood species
2015 - IRG/WP 15-10836
The analysis of the natural durability of wood is essential when establishing the level of protection required, depending on the designated end use of timber. On the other hand, there is a popular belief based on the influence of the moon phase in felling timber, recommending the waning moon as the optimum for felling trees. In fact, some companies now offer among their products, sawn timber felle...
M T Troya, M Conde, M J Barriola, F Llinares, V Dorronsoro


Investigations on the durability of several Congo basin wood species
2015 - IRG/WP 15-10840
The sawdust of ten wood species was studied to assess their natural resistance to decay. The extractives and lignin contents were primarily determined (between 2.7-16.0% and 26.8-35.9% respectively) to give an overview of the chemical distribution. Then, a phytochemical screening (colorimetric methods) characterized the different chemical functional groups in all extracts studied. Antioxidant act...
S Mounguengui, J-B Tchinda Saha, M Kor Ndikontar, S Dumarçay, C Attéké, D Perrin, E Gelhaye,


Chemical composition of extractives of different wood compartments of Pinus merkusii and their potential implication in wood durability
2015 - IRG/WP 15-10841
Amounts and nature of extractives differ strongly according to the compartment of wood and to the nature of the wood species. Previous studies reported that knotwood of several European Pinus sp. contains extractives contents much higher than stemwood consisting mainly of lignans which may find valuable applications in cosmetic, nutraceutic or pharmaceutic sectors. Different explanations have been...
A Wijayanto, S Dumarçay, R Kartika Sari, W Syafii, P Gérardin, C Gérardin-Charbonnier


Natural durability of Chilean commercial wood exposed to the action of marine borers
2015 - IRG/WP 15-10849
Results of field experiences of natural durability of ten commercial wood, exposed to the action of Bankia martensi (Stempell) in the South coast of Chile are presented. Tested species were seven types of native wood and three types of exotic ones. Test specimens of standard dimension of 0.02 x 0.045 x 0.23 m with three replications by species were used. The degree of attack was determined accord...
R Carmona C, C Osorio, A Almuna