A new technique for testing decay resistance of framing lumber
2002 - IRG/WP 02-20247
Model house frame units (two studs, top and bottom plates and a central “dwang”) were constructed using short (500-600 mm) lengths of framing timber. Constructed frames were impregnated with water using a mild pressure schedule to raise the initial moisture content to 35-40 % mc. The back face of each unit was then covered with black polyethylene. Two locations at the stud/dwang and stud/botto...
M E Hedley, D Page, B E Patterson


Moisture requirements and wood degradation of pine and spruce wood by some Basidiomycetes-fungi
1989 - IRG/WP 1406
The minimum moisture requirements for the growth of the brown rot fungi, Coniophora puteana, Gloeophyllum trabeum and Serpula lacrymans were near or above the fibre saturation point of pine and spruce, sap and heartwood, during 160 days incubation according to the standard method EN 113. The moisture of wood for the optimum growth of Coniophora puteana and Serpula lacrymans was about 35-80% and fo...
H Viitanen, A-C Ritschkoff


Wood preservation in Kenya
2000 - IRG/WP 00-40190
Focussing an Wood Preservation in Kenya, the Report discusses and elaborates on Education and Training, Research, Wood deteriorating organisms, Treatment Plants and Processes, Preserving Chemicals, Specifications, Markets, Health and Safety and Environmental issues. Education and Research is limited to one Institution only, other Institutions involved with the properties and utilization of wood ha...
R Venkatasamy


Formation of soft rot cavities in relation to concentric layers in wood fibre walls
1983 - IRG/WP 1185
A large number of timber species attacked by soft rot have been examined using light microscopy. The S2 layers in a large number of the timbers exhibited special structural features in the form of thin concentric layers. Several observations indicate that these layers may be characterised as "weak" zones by being more easily degradable than the surrounding wall layers. The chemical structure of th...
T Nilsson, G F Daniel


Microbial breakdown mechanisms. Mini-Symposium at the 18th IRG meeting, Honey Harbour, Ontario, Canada
1987 - IRG/WP 1327
An understanding of how micro-organisms cause chemical alternation to wood is essential for effective wood preservation. Investigation of the Microbial Breakdown of wood is a very dynamic research field and is increasing in importance as several biocides are being examined as alternativesw to classic wood preservatives. These biocides often do not possess broad spectrum activity. It is esential th...
L E Leightley


Correlation between changes in colour and chemical composition during photo-degradation of wood surfaces
2005 - IRG/WP 05-40301
Changes in colour of wood (yellowing) during photo degradation or weathering reflect chemical changes in wood. Therefore, the relationship between changes in chemical composition and CIELAB colour parameters is very important to characterize photodegradation of lignocellulosic surfaces. In this study, the changes in chemical composition and yellowing due to photo-degradation was studied by expos...
K K Pandey


Evaluating the natural durability of native and tropical wood species against Reticulitermes flavip
2004 - IRG/WP 04-10539
Environmental pressures to eliminate arsenate from wood preservatives has resulted in voluntary removal of CCA for residential applications in the United States. A new generation of copper organic preservatives has been formulated to replace CCA for decking and in-ground applications but there is no guarantee that these preservatives represent a permanent solution to all related problems. There...
R A Arango, F Green III, K Hintz, R B Miller


Acetylated solid wood. Laboratory durability test (part 2) and field trials
1995 - IRG/WP 95-40048
Degradation of acetylated beech, pine and poplar by soft rot fungi was related to strength loss in a laboratory test. No strength loss was noticed for poplar acetylated to a weight percent gain (WPG) of more than 11.2% and beech with a WPG of 12.8%. Several field trials were set up to determine the durability of acetylated products in practice. They included a field test to determine the durabilit...
E P J Beckers, H Militz, M Stevens


Wood-based composites exposed to fungal degradation: Laboratory results
2001 - IRG/WP 01-40215
Oriented strandboard (OSB) and laminated veneer lumber (LVL) are widely used as residential construction materials. The durability of OSB and LVL against biological degradation has not been studied comprehensively. The objective of this research was to investigate the durability of OSB and LVL when exposed to wood decay fungi. Fourteen brown-rot and eight white-rot wood decay fungi were screened f...
V W Yang, B Illman, L A Ferge, R J Ross


The possible role of mobile CCA components in preventing spore germination in checked surfaces, in treated wood exposed above ground
2001 - IRG/WP 01-30263
Untreated check surfaces are often exposed in CCA-treated lumber of refractory species used above ground since, during weathering, some checks develop beyond the preservative penetrated zone. However, decay is seldom observed in these checks even after many years of exposure. It is hypothesized that minor amounts of mobile CCA preservative components redistribute during weathering into checks, and...
S Choi, J N R Ruddick, P I Morris


Evaluating possibilities of leaching of deltamethrin and TCMTB (insecticides and fungicide for protecting wood) by rain water or by soaking in water
1988 - IRG/WP 3464
Deltamethrin and TCMTB have been subjected to several field leaching tests on freshly fallen trees and in the laboratory, using standard EN 84. All the trials gave the same results and confirm that Deltamethrin and TCMTB are not washed out after they have been allowed to penetrate the trunk surface properly. According to the EN 84 standard, less than 1% Deltamethrin and less than 1.7% TCMTB were r...
J S Duguet, V Dartigues


Improvement of some technological and biological properties of poplar wood by impregnation with aqueous macromolecular compounds
1992 - IRG/WP 92-3721
Poplars (Populus spp) belong to the most important tree species in afforestation programs of the Netherlands. Due to their rapid growth, the wood quality is usually low. Therefore, studies were performed to elucidate whether some technological properties and the resistance against fungal attack could be improved by impregnation with water-soluble resins. The results showed that swelling and shrink...
R D Peek, H Militz, J J Kettenis


A suggestion for the improvement of the chemical protection of wooden poles
1987 - IRG/WP 3445
Insufficient drying of white poles in Sweden causes inadequate penetration of the impregnation compounds, CCA salts and creosote, in a varying proportion of the treated poles, and with pretreatment decay present, sooner or later, internal fungal attack in the ground-line zone of the standing poles is the result. The application of a diffusing fungicide in the ground-line zone in connection with th...
H Friis-Hansen


The compatability of tributyltin fungicides and synthetic pyrethroid insecticides as wood preservatives
1987 - IRG/WP 3414
The stability of three synthetic pyrethroids, cypermethrin, deltamethrin and permethrin, to selected tributyltin compounds, Bu3SnX {where X = OSnBu3, Cl, 02CC6H5, O2C (Naphthenyl), OSO2Et}, (Bu3SnO)3PO and {NBu4} {Bu3SnCl2}, in toluene solution was investigated by infra-red spectroscopy over a six month period. It was found that only (Bu3Sn)2O reacted with the pyrethroids and that their order of r...
S J Blunden, R Hill


ATP assay for the determination of mould activity on wood at different moisture conditions
1992 - IRG/WP 92-2397
To determine fungal responses to fungicides and environmental conditions and for detection of microbial activity in wood, sensitive and objective methods are needed. We have developed a suitable assay based on analysis of adenosine triphosphate (ATP) by using the luciferin-luciferase reaction. With the aid of this assay the activity of Penicillium brevicompactum on wood at different RH levels was ...
J Bjurman


Chlorpyrifos as a wood treatment temiticide
1994 - IRG/WP 94-30047
Chlorpyrifos, O,O-diethyl O-(3,5,6-trichloro-2-pyridyl) phosphorothioate, is a broad-spectrum insecticide used worldwide for the control of many insect pests. As a wood preservative, chlorpyrifos is registered with the United States Environmental Protection Agency for protection of seasoned and green lumber and logs from attack by wood destroying insects such as termites, carpenter ants, ambrosia ...
R D Fears


Utility pole recycling and disposal in Eastern Canada
1990 - IRG/WP 3587
Increasing public awareness, prompted by environmental groups such as Greenpeace, concerning the use and disposal of treated wood is becoming a serious issue in Canada. Producers and user groups of treated Pentachlorophenol (PCP) utility poles are at the forefront of public, government and media attention. If, as expected, further limitations on the use and disposal of PCP by the public are impose...
S D Henry


Using image analysis to rate wood stain trials
1993 - IRG/WP 93-10034
Assessing the extent of fungal discoloration on wood during laboratory trials is a subjective process which provides an opportunity for considerable variation between individual evaluators of specimens. The development of reliable systems for automatically assessing discoloration would minimize evaluator bias and permit comparisons between results from different laboratories. The use of image anal...
C M Sexton, A G Maristany,C C Brunner, J J Morrell


Effects of surfactants and ultrasonic energy on the treatment of wood with chromated copper arsenate
1977 - IRG/WP 3108
Sugar pine stakes 1'' x 1" x 16" were treated by a hot-water bath followed by soaking in cold CCA solution for 10 to 30 minutes. A similar number of stakes were treated by a cold-cold bath. Half of the stakes were subjected to ultrasonic energy during the CCA bath. The mean absorption for stakes given the hot-cold bath was 18.52 pcf (297 kg/m³) and 4.64 pcf (74 kg/m³) for those...
C S Walters


Decrease in the mechanical resistance of blue stained and "orange stained" Pinus radiata wood
1999 - IRG/WP 99-10313
It is recognised that sapwood attacked by Ceratocystis pilifera increases its permeability to pressure preservative treatments. Since hiphae not only utilise pits, but also the cell wall for crossing from one cell to another, the mechanical resistance of the stained wood might be affected. The orange colour very commonly present in Pinus radiata logs heartwood under water sprinklers, has not recei...
M C Rose, L Reyes, J Alvarez, A Andaur, C Beltran, D Rivera


Dimension of lysimeters and the evaluation of the migration of wood preservative components in soil
1996 - IRG/WP 96-50065
In the past, investigations concerning the migration behaviour of wood preservatives were made to a minor extent and no uniform methods of test exist. The migration behaviour of CFB was determined using 5 lysimeters of different dimension. The results of the migration and distribution of the anions in the soil showed considerable differences between both ions. Approximately the whole quantity of c...
E Melcher, R-D Peek


Performance of CCA wood preservative and CCA treated wooden materials (pole, anchor log, cross-arm etc) with special reference to Bangladesh (Series 1)
2005 - IRG/WP 05-40318
Wood is an important renewable natural resources produced by plants which is without question oldest and versatile construction material. It is composed of cellulose, hemicelluloses and lignin. Cellulose and hemicelluloses accounts for about two-thirds of the dry weight of the wood which perform the major structural role. Lignin is the remaining one-third of the wood which holds the cellulose and ...
G N M Ilias


Natural Durability of Tropical Species – Variations and Prospects
2005 - IRG/WP 05-10568
The tropical timber resources of the world play an unequivocal role in economic development of both the tropical timber producing and importing regions. This paper describes natural durability as an important and preferred wood quality of tropical species of the world with emphasis on Malaysian hardwoods, the link between various aspects of tropical hardwood durability, hardwood utilization and bi...
A H H Wong, Yoon Soo Kim, A P Singh, Wang Choon Ling


The fungal degradation of quaternary ammonium compounds in wood
1998 - IRG/WP 98-10263
This work focuses on the biodegradation of didecyldimethylammonium chloride (DDAC) by the mould fungus Gliocladium roseum within a woody matrix. Three sawdust types, distinguished by their treatment and amount of DDAC retained, were inoculated with the fungus and their DDAC loss was measured over 11 weeks. The rates of degradation varied depending on the sawdust; however, a significant loss of DDA...
J W Dubois, J N R Ruddick


A study of the decay type potential of seven soils
1992 - IRG/WP 92-1539
The aim of this experiment was to determine the significance of the fungal inoculum potential and physico-chemical properties of five field trial test site soils, a garden compost known to cause white rot in copper treated fence palings, and soil from a zone between 2 and 15 centimetres from a CCA treated post with brown rot, in causing differential decay type in Pinus radiata and Poplus deltoides...
R N Wakeling