IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 3040 documents. Displaying 25 entries per page.


Effects of surfactants and ultrasonic energy on the treatment of wood with chromated copper arsenate
1977 - IRG/WP 3108
Sugar pine stakes 1'' x 1" x 16" were treated by a hot-water bath followed by soaking in cold CCA solution for 10 to 30 minutes. A similar number of stakes were treated by a cold-cold bath. Half of the stakes were subjected to ultrasonic energy during the CCA bath. The mean absorption for stakes given the hot-cold bath was 18.52 pcf (297 kg/m³) and 4.64 pcf (74 kg/m³) for those...
C S Walters


Decrease in the mechanical resistance of blue stained and "orange stained" Pinus radiata wood
1999 - IRG/WP 99-10313
It is recognised that sapwood attacked by Ceratocystis pilifera increases its permeability to pressure preservative treatments. Since hiphae not only utilise pits, but also the cell wall for crossing from one cell to another, the mechanical resistance of the stained wood might be affected. The orange colour very commonly present in Pinus radiata logs heartwood under water sprinklers, has not recei...
M C Rose, L Reyes, J Alvarez, A Andaur, C Beltran, D Rivera


Properties of hot oil treated wood and the possible chemical reactions between wood and soybean oil during heat treatment
2005 - IRG/WP 05-40304
Thermal treatment with hot oil as the heating media based on the original idea from oil-heat treatment in Germany was investigated. The treatment was mainly carried out at 200ºC and 220ºC for 2 hours and 4 hours, and the wood species were mainly spruce and fir. This paper focuses on the difference between soybean oil and palm oil and the possible chemical reactions between wood and soybean oil. ...
Jieying Wang, P A Cooper


Dimension of lysimeters and the evaluation of the migration of wood preservative components in soil
1996 - IRG/WP 96-50065
In the past, investigations concerning the migration behaviour of wood preservatives were made to a minor extent and no uniform methods of test exist. The migration behaviour of CFB was determined using 5 lysimeters of different dimension. The results of the migration and distribution of the anions in the soil showed considerable differences between both ions. Approximately the whole quantity of c...
E Melcher, R-D Peek


Performance of CCA wood preservative and CCA treated wooden materials (pole, anchor log, cross-arm etc) with special reference to Bangladesh (Series 1)
2005 - IRG/WP 05-40318
Wood is an important renewable natural resources produced by plants which is without question oldest and versatile construction material. It is composed of cellulose, hemicelluloses and lignin. Cellulose and hemicelluloses accounts for about two-thirds of the dry weight of the wood which perform the major structural role. Lignin is the remaining one-third of the wood which holds the cellulose and ...
G N M Ilias


Changes in pore structure and cell wall volume in wood decayed by brown- and white-rot fungi
1991 - IRG/WP 1501
Sweetgum (Liquidambar styraciflua L.) wood blocks were decayed by Postia (=Poria) placenta or Phanerochaete chrysosporium in soil-block cultures. Decay was terminated at various weight losses, and the pore volumes available to probes of various molecular weight and diameter were determined by the solute exclusion technique (Stone, J.E. and A.M. Scallan. 1968. Cellulose Chem. Technol. 2, 343-358.)....
D S Flournoy


Natural Durability of Tropical Species – Variations and Prospects
2005 - IRG/WP 05-10568
The tropical timber resources of the world play an unequivocal role in economic development of both the tropical timber producing and importing regions. This paper describes natural durability as an important and preferred wood quality of tropical species of the world with emphasis on Malaysian hardwoods, the link between various aspects of tropical hardwood durability, hardwood utilization and bi...
A H H Wong, Yoon Soo Kim, A P Singh, Wang Choon Ling


The fungal degradation of quaternary ammonium compounds in wood
1998 - IRG/WP 98-10263
This work focuses on the biodegradation of didecyldimethylammonium chloride (DDAC) by the mould fungus Gliocladium roseum within a woody matrix. Three sawdust types, distinguished by their treatment and amount of DDAC retained, were inoculated with the fungus and their DDAC loss was measured over 11 weeks. The rates of degradation varied depending on the sawdust; however, a significant loss of DDA...
J W Dubois, J N R Ruddick


Accelerated decay tests to investigate postulated effects of tannins on CCA efficacy in wood
1988 - IRG/WP 3497
Five groups of blocks (10 x 10 x 5 mm³) viz., Pinus patula, Pinus patula impregnated to 4% (w/w) tannin; Eucalyptus grandis, Eucalyptus grandis with natural tannins extracted; and extracted Eucalyptus grandis with tannins returned as above; were prepared. Blocks from each group were then treated to 0, 5, 10 and 15 kg/m³ CCA and challenged in four 15-week decay tests, viz., soil burial, and expos...
U L Scherer, A A W Baecker


The implementation of restrictions on the use of arsenic and chromium based wood preservatives in Sweden
1995 - IRG/WP 95-50062
In 1992 the Swedish National Chemicals Inspectorate introduced restrictions on the use of wood treated with arsenic and/or chromium based wood preservatives. Such wood is now in principle only allowed for use in ground contact or in water. These restrictions have had considerable influence on the use of wood preservatives for sawn timber for the Swedish domestic market. Thus only 35% of the preser...
J Jermer, M-L Edlund, K Nilsson


Generic code of good practices for wood preservation facilities
1994 - IRG/WP 94-50037
Wood preservation chemicals are designed to be toxic to wood destroying organisms. This toxicity, however, may not be limited to target organisms but the use of these chemicals can potentially harm various biota and humans as well. This fact dictates that adequate precautionary measures be employed to prevent any harmful effects to humans and the environment. The extensive experience with wood tre...
V N P Mathur, G Das


Délavabilité de bois ronds traités avec un sel CCA dans des conditions réelles de stockage. Incidence pratique de la fixation accélérée par étuvage. Impact effectif sur l'environnement
1993 - IRG/WP 93-50001-23
Un essai de terrain a été organisé pour mesurer concrètement, dans des conditions aussi proches que possibles des conditions réelles de terrain, les pertes effectives en produit de traitement lorsque le bois traité est soumis à des intempéries. L'essai a été conduit sur des bois ronds (poteaux), traités en autoclave par procédé Bethell avec un sel CCA de type C, avec comme fi...
M Rayzal, F Larroze


Biological resistance of aldehyde-treated wood
1994 - IRG/WP 94-40018
Biological resistance of wood treated with aldehyde cross-linking agents such as glyoxal, glutaraldehyde and dimethylol dihydroxy ethyleneurea (DMDHEU) were investigated. Sapwood blocks of Japanese cedar and Japanese beech, measuring 20 x 20 x 10 mm³ (T x R x L), were vacuum-impregnated at room temperature with 5-25% of aldehyde solutions. Blocks were kept in the solution for 1 week to gain the o...
S Yusuf, Y Imamura, M Takahashi, K Minato


Industrial wood preservation in Kenya. Present status – future prospects
2005 - IRG/WP 05-30385
Although some 50 years old, industrial wood preservation in Kenya does not appear to have technically, scientifically, and commercially evolved and contributed to significantly extend service lives of timbers, protect health and the environment, and curb unnecessary over-exploitation of forests. The population of the country has increased by 530% over the past 50 years; regular excisions have red...
R Venkatasamy


Laboratory evaluation of metallic naphthenates as wood preservatives
1991 - IRG/WP 3654
Fungicidal and termiticidal efficacy of copper and zinc naphthenates was appraised according to Japanese standardized laboratory testing methods. Copper and zinc naphthenates succeeded in protecting wood from decay fungi at retentions of 0.5 and 1.0 kg/m³ as metal, respectively. [JIS A 9302 (1976)] when they were applied to vacuum/soak impregnation [JIS A 9301 (1976)]. With respect to the fungici...
K Tsunoda, M Sakurai


Biological detoxification processes - A check list for assessments
1998 - IRG/WP 98-50120
The number of scientific publications on the biological purification of preservative treated wood implies that the biological treatment of wood wastes becomes more and more important. But an information about a successful industrial application is almost missing in all cases. Therefore the applicability of the proposed purification processes is often uncertain. The feasability of such a biological...
H Leithoff, R-D Peek


Protection of rubberwood with modified creosote
1998 - IRG/WP 98-30165
Creosote is a renowned wood preservative but has certain disadvantages like obnoxius odour and colour, with its unpaintability and bleeding from wood surface may create environmental hazards. An effort has been made to isolate chemical fractions from creosote to obtain clean odourless preservative formulations by subjecting to steam distillation (SVC). Rubberwood treated with SVC and tested for it...
H C Nagaveni, H S Ananthapadmanabha, G Vijayalakshmi, M N Sharma, K H Shankaranarayana


Observations on the effect of two preservatives on settlement and development of the marine wood-borer Martesia striata L
1983 - IRG/WP 498
Small heartwood specimens of three tropical hardwoods namely kusia or opepe (Nauclea diderrichii (De Wild) Merrill), emire or idigbo (Terminalia ivorensis A. Chev.) and subaha or abura (Mitragyna stipulose (D.C.) O. Kuntze) were treated with either creosote (BSS 144 type) or a copper-chrome-arsenic preservative and submerged in the sea at Tema, Ghana. They were regularly cleaned of fouling and obs...
J E Barnacle, F F K Ampong


Electrodialytic remediation of CCA-treated wood in larger scale
2005 - IRG/WP 05-50224-20
A pilot plant for the electrodialytic remediation of CCA-treated waste wood has been developed and tested at the Technical University of Denmark. Results from two experiments with different amount of wood chips are presented here. Prior to the electrodialytic remediation the wood was soaked in oxalic acid and phosphoric acid. The main purpose of soaking is to remove the most available fraction fir...
I V Christensen, L M Ottosen, A J Pedersen


Longterm monitoring of termite activity on multiple feeding sites: a laboratory method intended for the determination of attractant/repellent properties of wood preservatives and baits
2001 - IRG/WP 01-20225
A method is introduced allowing the continuous monitoring of the activity of a small laboratory termite- colony at 8 different feeding sites simultaneously. The test assembly consists of a small central polycarbonate-tube containing a colonie of Reticulitermes santonensis (de Feytaud) beeing connected with 8 external feeding sites by small glass-capillaries. The termites passing through the glass ...
M Pallaske, E Graf, H Takiuchi


The degradation of wood surfaces by water
1984 - IRG/WP 3289
Thin radial/longitudinal sections (~100 µ) of Scots Pine (Pinus sylvestris) and lime (Tilia vulgaris), were exposed to deionised water over the temperature range 25-65°C. Losses in wet tensile strength and toughness occurred rapidly at temperatures from about 50°C upwards. After about 2 months' exposure pine lost some 10-30% of its tensile strength and 20-60% of its toughness. For lime...
W B Banks, P D Evans


An attempt to develop a direct and reliable method for testing the preventive action of preservation treatments of wood against fungal decay
1980 - IRG/WP 2139
In wood preservation there are two classical ways for assessing the reliability of preventive treatments against wood decay: the laboratory tests in which the various parameters are evaluated independently and the field tests or service tests in which those parameters are acting together in the natural environment. One has always tried to build bridges between the two types of experiments and to e...
M Fougerousse


Soft rot decay of Belian (Eusideroxylon zwageri) wood
1995 - IRG/WP 95-10119
The heartwood of Belian (Eusideroxylon zwageri), an East Malaysian timber species, is naturally durable due to its certain unique anatomical features and high content of extractives. The timber can tolerate years of exposure to hazardous conditions in ground contact and other situations without any significant loss in its strength. A few Belian transmission poles sampled from one locality in Saraw...
A H H Wong, A P Singh


The influence of copper (II) chemicals on the weathering of treated wood. Part 1: ACQ treatment of wood on its weathering
1994 - IRG/WP 94-30040
Wood weathering can be accelerated by alkylammonium compound (AAC) treatment, and slowed by ammoniacal copper quat (ACQ) treatment. This study aims at investigating the influence of ACQ treatment of wood, especially the present of copper (II), on its weathering. ACQ, CCA and DDAC treated microtomed sections of southern yellow pine earlywood were prepared and naturally weathered for five periods, t...
Ruiying Liu, J N R Ruddick, L Jin


Effect of Scytalidium lignicola on decay resistance and strength of wood
1994 - IRG/WP 94-10061
We reported previously that in laboratory tests, pretreatment of Douglas-fir and Southern Pine blocks with Scytalidium lignicola prevented decay. In the present work, we determined 1) the ability of Scytalidium lignicola to colonize and survive in wood exposed in the field, 2) the decay resistance of blocks removed from previously treated Scytalidium lignicola wood and 3) the effect of Scytalidium...
T L Highley


Previous Page | Next Page