The efficacy of commercial silicones against blue stain and mould fungi in wood
2008 - IRG/WP 08-30471
Scots pine (Pinus sylvestris L.) wood samples were vacuum pressure impregnated with quatsilicone micro emulsion (<40 nm particle size), aminosilicone macro emulsion (110 nm) and silicone macro emulsion with alkyl modified side groups (740 nm) and the resulting material properties were studied. Quatsilicone micro emulsion resulted in maximum bulking (4.8%) and anti-swelling efficiency (21.8%) in...
S C Ghosh, C Mai, H Militz


The Comparison of Fixation and Leachability of Bark, Fruit and Leaf Tannin Extracts with Boron Minerals
2008 - IRG/WP 08-30473
Tannins extracted from several plants have natural durability properties. Due to these properties, some of the researchers have studied them for protecting wood. In this study, Scots pine (Pinus sylvestris) and beech (Fagus orientalis) wood samples were treated with bark, fruit, and leaf extracts as well as water-based wood preservative salts at various concentrations to increase fixation. The pen...
S Sen, C Tascioglu, K Tirak


Performance of wood-based composites in a protected aboveground test in southern Japan
2008 - IRG/WP 08-40391
Five kinds of untreated wood-based composites (medium density fiberboard, hardwood plywood=HP, softwood plywood, particleboard and aspen oriented strand board, hereinafter abbreviated as MDF, HP, SP, PB and OSB, respectively) were exposed to subterranean termites and microbial (decay) attack under protected aboveground conditions in a southern part of Japan (Kagoshima Prefecture) for six years. An...
K Tsunoda


Effect of wood polymers degradation during heat treatment on extracellular enzymatic activities involved in beech degradation by Trametes versicolor
2008 - IRG/WP 08-40392
Effect of heat treatment on extracellular enzymes involved in wood degradation by Trametes versicolor was investigated. Heat-treated and untreated beech blocks were exposed to T. versicolor on malt agar medium and extracellular enzymatic activities investigated. A strong ABTS oxidizing activity has been detected during the first stage of colonization in both cases, while cellulase activities are m...
S Lekounougou, G Nguila Inari, M Pétrissans, S Dumarçay, J P Jacquot, E Gelhaye, P Gérardin


The effect of gamma radiation on selected wood properties
2008 - IRG/WP 08-40394
As an easy, fast, and effective sterilisation method, gamma irradiation changes molecular structures not only in pest’s living cells, but also in wooden cell walls. Radiation-induced depolymerisation causes significant changes in some properties of wood crucial for restoration and for laboratory testing of wood-preservative effectiveness. The influence of gamma radiation concerning total amount ...
R Despot, M Hasan, A O Rapp, C Brischke, C R Welzbacher


Feasibility study on three furfurylated non-durable tropical wood species evaluated for resistance to brown, white and soft rot fungi
2008 - IRG/WP 08-40395
Furfurylation can protect non-durable wood species against biological degradation, but the method used today cannot fully protect the heartwood of Scots pine due to insufficient penetration. In order to test alternative wood substrates for furfurylation, three Malaysian grown wood species (Kelempayan, Rubberwood and Sena) were furfurylated and subjected to soil block decay testing. Their performan...
T Mark Venås, A H H Wong


Preliminary investigation of biological resistance, water absorption and swelling of thermally compressed pine wood panels
2008 - IRG/WP 08-40396
Wood can be modified by compressive, thermal and chemical treatments. Compression of wood under thermal conditions is resulted in densification of wood. This study evaluated decay and termite resistance of thermally compressed pine wood panels at either 5 or 7 MPa and at either 120 or 150?C for one hour. The process caused increases in density and decreases in thickness of the panels; however, lab...
Ö Ünsal, S N Kartal, Z Candan, R Arango, C A Clausen, F Green III


Resistance against basidiomycetes of 1,3-dimethylol-4,5-dihydroxy ethylene urea (DMDHEU)-modified plywood of Pinus sylvestris
2008 - IRG/WP 08-40398
Plywood produced with rotary-cut veneers of Pinus sylvestris impregnated with a solution of 1.3 M 1.3-dimethylol-4.5-dihydroxyethyleneurea (DMDHEU) and glued with a phenolic resin (Prefere 4976 DYNEA) were inoculated with Coniophora puteana, Coriolus versicolor and Pleurotus ostreatus, following the European standard ENV 12038. The specimens were leached following European standard EN 84. The re...
A Dieste, A Pfeffer, S Bollmus, H Militz


Heat treatment, thermal treatment, thermal degradation of wood, carbon nanotubes and Damascus steel swords. What do they all have in common?
2008 - IRG/WP 08-40399
Thermal degradation of wood is a well known phenomenon. Yet heat-treatment of wood can also provide protection for wood against certain environmental hazards. This paper explores some of the aspects of thermal degradation of wood fiber at relatively low temperatures with a surprising result. Carbon nanotubes (CNTs) were produced when a specific heating regime was used to carbonize the wood fiber. ...
Xinfeng Xie, B Goodell, Yuhui Qian, G Daniel


Termite resistance of DMDHEU-treated wood
2008 - IRG/WP 08-40401
Chemical wood modification with dimethyloldihydroxy-ethyleneurea (DMDHEU) or its derivatives are applicable to both solid lumber and wood-based composites. Advantages of DMDHEU-based modification are an increase of dimensional stability and high durability against white, brown and soft rot fungi. At higher chemical loadings, the hardness of the wood is considerably increased. Due to the durabil...
H Militz, S Schaffert, B C Peters, C J Fitzgerald


Effects of bleaching process on the roughness values of wood surfaces of Lebanon cedar (Cedrus libani A. Rich.) and Black poplar (Populus nigra L.) using NaOH (sodium hydroxide), H2O2 (hydrogen peroxide) and Ca(OH)2 (calcium hydroxide)
2008 - IRG/WP 08-40403
Technical progress in the wood industry has been rapid in recent times. In this case, the quality assurance of the consumer products aligned with aesthetics value appears as one of the most important parameters. Because of the outer appearance of goods exert an effect on customers, interest in production of high quality surfaces of wooden commodities has increased essentially based on the surface ...
I Usta, E Aydinlar


Effects of Murgul Copper Process flue gases (SO2) on compression strength parallel to the grain of Beech (Fagus orientalis Lipsky.) wood
2008 - IRG/WP 08-40404
In this study was investigated the effect on the compression strength parallel to the grain as mechanical properties of Fagus orientalis Lipsky. wood exposed to SO2 gas and non-exposed. In the experiments the two of four (total) were obtained from Artvin-Ortaköy region and the other two from Artvin-Murgul region. The compression strength parallel to the grain was calculated at the compare of ...
N Ay, E Topaloglu, A Uncu


Effects of acetic acid and nitric acid pre-treatment on copper content of spruce wood treated with CBA-A and CCA
2008 - IRG/WP 08-40406
This work investigates the effects of nitric acid and acetic acid on compression strength values and copper retention contents of refractory spruce wood (Picea oriental L.) treated with the waterborne preservative Copper azole, (CBA-A, Tanalith-E 3492) and copper / chrom / arsenic (CCA). Before the CBA-A and CCA treatment, the samples were immersed in 500 ml of nitric and acetic acid solutions for...
S Yildiz, E Dizman, Ü C Yildiz


Thermal treatment of Nigerian-grown Albizzia zygia and Funtumia elastica wood in soy oil medium.
2008 - IRG/WP 08-40413
Thermal treatment in soy oil medium is one of the techniques used as a substitute to the chemical treatment in wood preservation. However, the effects of this technique vary from one species to another and hence the need to investigate the response of individual species to it. Thermal treatment of air-dried Nigerian-grown Albizzia zygia and Funtumia elastica wood was carried out in a vessel contai...
L Awoyemi


The Effect of Heat Treatment on Water Absorption and Dimensional Stability of Anatolian Chestnut (Castanea sativa Mill.) wood
2008 - IRG/WP 08-40407
The heat treatment of wood is an environment-friendly method for wood preservation. This process improves wood’s resistance to decay and its dimensional stability. However, mechanical properties decrease in different ration because of density loss as a result of heat treatment. In this study, the effect of heat treatment on water absorption and dimensional stability at different relative humidit...
G Gunduz, D Aydemir


Effects of Moisture Content and Species on Penetration of Liquid in Laser Incised Lumber by the Passive Impregnation Method
2008 - IRG/WP 08-40408
Penetration of liquid by passive impregnation method for Douglas-fir (Pseudotsuga menziesii Franco), sugi (Cryptomeria japonica D. Don) and Japanese larch (Larix leptolepis Gordon) were studied. Effects of initial moisture content of sugi (16, 43 and 70% moisture content) on liquid penetration by the method were also studied. Dried Douglas-fir and sugi, and green Japanese larch and sugi were treat...
N Hattori, M Nazrul Islam, K Ando, H Yamauchi


The effect of treatments in boron steaming medium on boron leaching and strength properties of wood
2008 - IRG/WP 08-40409
The combined effect of boric acid impregnation together with boron steaming and steaming heat treatments were evaluated in this study. Boric acid pre-treated wood samples and untreated ones subjected to steaming heat and direct steaming treatment in a close reactor at 13 bar pressure and 180 ºC for 30 minutes. Compression strength parallel to grain of wood samples, leaching test and pH measuremen...
E D Tomak, Ü C Yildiz, S Yildiz, E Pesman


Changes in hygroscopic, mechanical and surface properties of Scottish-grown Sitka Spruce (Picea sitchensis) wood subjected to dry heat treatment
2008 - IRG/WP 08-40415
Heat-treatment is a wood modification method which has been used to some extent in improving timber quality. However, the main limitation in the use of this technique despite its numerous advantages is the adverse effects on the various properties associated with the use of wood as an engineering material. Dry heat treatment of Scottish-grown Sitka spruce (Picea sitchensis) wood was carried out at...
L Awoyemi, M C Jarvis, A Hapca


Effects of CCB on wood strength of Eastern spruce (Picea orientalis L.)
2008 - IRG/WP 08-40416
The effects of CCB (chromate copper boron) on the static bending properties of Eastern spruce (Picea orientalis L.) based on MOE (modulus of elasticity) and MOR (modulus of rupture) were evaluated after full-cell vacuum/pressure treatment using a 3.0 % concentration followed by kiln-drying at 15 and 30 % moisture contents with heating the preservative at 30 and 40 ºC. The results showed that MOE ...
I Usta, M Hale


COST Action E37. Sustainability Through New Technologies For Enhanced Wood Durability -
2008 - IRG/WP 08-40417
The main overall objective of the Action was to concentrate on the contribution of wood durability to sustainability through the development of systems for quality assurance and performance classification of modified wood and wood products as alternatives to wood treated with traditional preservatives. By this means it seeked to improve and consequently to increase the cost-effective use of compon...
R-D Peek, J Van Acker


Bi-oleothermal treatment of wood at atmospheric pressure: resistance to fungi and insects, resistance to weathering and reaction to fire results
2008 - IRG/WP 08-40418
Bi-oleothermal process is a simple treatment which has been developped by CIRAD in cooperation with FCBA. It allows a deep impregnation of wood with hydrophobic products using cheap facilities. The process includes two steps at atmospheric pressure. The first one is a dipping of wood samples in a hot oil bath (between 110 °C and 200°C) which creates an overpressure inside the wood. The second on...
L Podgorski, I Le Bayon, I Paulmier, J-D Lanvin, V Georges, D Grenier, H Baillères, J-M Méot


The effects of zinc borate treatment of wood strands on some technological properties of oriented strandboard (OSB)
2008 - IRG/WP 08-40419
In this study, influences of zinc borate treatment on some technological properties of oriented strandboard (OSB), from aspen wood (Populus euroamericana cv.) were evaluated. Therefore, a total of nine panels with dimensions of 40 cm by 40 cm by 1.8 cm and with an average target density of 0.65 g/cm3 were manufactured under the laboratory conditions. Experimental panels were manufactured at two di...
A D Çavdar, H Kalaycioglu, G Nemli


Wood plastic composites from modified wood. Part 3. Durability of WPCs with bioderived matrix
2008 - IRG/WP 08-40423
The decay resistance of fully bio-derived wood plastic composites, WPCs, was tested in both laboratory and field tests. The laboratory tests were performed according to modified versions of AWPA E10 (soil-block test) and ENV 807 (tests in three un-sterile soils) and the field tests according to EN 252 (stakes in ground) and EN 275 (resistance to marine borers). The WPC materials for laboratory tes...
M Westin, P Larsson Brelid, B K Segerholm, M Van den Oever


Ecotoxicity of furfurylated wood – Effect of leachate on aquatic bacteria
2008 - IRG/WP 08-50250
Environmental concern regarding the use of toxic preservatives such as CCA (chromated copper arsenate) has been put forward. In the EU, USA and Japan, CCA is now phased out for residential use and for use in water contact. Several ecotoxicological studies of wood treated with conventional preservatives were carried out in the late 1990s. In these studies it was concluded that the main impact is to...
A Pilgård, M Westin


Effect of steam on fixation of Cu-amine preservative treated wood
2008 - IRG/WP 08-50251
The rates of copper fixation in copper amine preservative treated wood were investigated with different fixation conditions (20° with drying and 50° without drying) and post-steaming. We also measured the degree of leaching for other biocide components (azoles, quatz, and Cu-HDO). Treatments conditioned at 20° with drying required 50 days or more to fix in woods. While copper was stabilized i...
Sung-Mo Kang, In-Yong Hwang, Suk-Kuwon Kim