Amine Oxides for Use in Wood Protection: I. A Formulation Adjuvant and Performance Enhancer for Wood
2007 - IRG/WP 07-30425
Amine oxides have great potential for use in the area of wood protection. This paper highlights the advantages of using amine oxides as a formulation adjuvant and performance enhancer for different azoles. It was found that azoles are readily soluble in aqueous amine oxide solutions and form soluble concentrates. These azole/amine oxide concentrates have excellent storage stability and can be dilu...
Xiao Jiang, L Walker


Amine Oxides for Use in Wood Protection: II: Water Repellent Agents for Wood
2007 - IRG/WP 07-30426
Wood treated with cetyl and stearyl amine oxides was evaluated to determine its long term water repellency. Comparative water uptake data, generated during two years of outdoor exposure, illustrated that Lonza’s products, Barlox® 18S (N-octadecyl-N, N-dimethylamine oxide) and Barlox® 16S (N-hexadecyl-N, N-dimethylamine oxide), were effective water repellent agents, imparting lasting water res...
Xiao Jiang, L Walker


Effects of caffeine on growth of wood-decaying fungi
2007 - IRG/WP 07-30427
The wide-used triazoles alter the biosynthesis of ergosterol leading to a disruption of fungal membrane functions. The aim of this study was to investigate the effects of another cell wall perturbing agent, caffeine, in combination with propiconazole on the growth of wood-decaying fungi. 10 mM caffeine inhibits totally the growth of five fungal species. The obtained results showed that caffeine ha...
S Lekounougou, J P Ondo, J P Jacquot, G Nevers, P Gérardin, E Gelhaye


Effects of chlorothalonil (CTN) and butylated hydroxytoluene (BHT) on microbial communities involved in the deterioration of wood using T-RFLP II: Results from field studies
2007 - IRG/WP 07-30429
The effects of Chlorothalonil (CTN) and Butylated Hydroxytoluene (BHT) on microbial species diversity in wood and the surrounding soil are being assessed by Terminal Restriction Fragment Length Polymorphism (T-RFLP). CTN was selected as a trial organic wood preservative, and the non-biocidal BHT was evaluated for its synergistic effects with CTN. ACQ-C was a positive control and untreated SYP sta...
G T Kirker, M L Prewitt, S V Diehl


Laboratory test of blue stain control by chemicals
2007 - IRG/WP 07-30430
8 chemicals and some mixtures against Botryodiplodia theobromae Pat., Fusarium verticillioides(Sacc.)Nirenberg, Trichoderma harzianum Rifai, Trichoderma viride Pers., and Penicillium purpurogenum Stoll were conducted in laboratory by inhibition zone in the paper. The results were shown that: CBZ and benomyl as well as copper oxine alone are much high efficacy for inhibiting most of the 5 fungi tha...
Zhijuan Wang, Zehui Jiang, Mingliang Jiang, Chungen Piao


The effect of wood moisture content and rod dosage on movement of boron through Douglas-fir heartwood
2007 - IRG/WP 07-30431
The potential for moisture sorption by boron rods following application to wood to affect subsequent boron diffusion was investigated in small Douglas-fir blocks conditioned to 30, 60 or 90% moisture content (MC). MCs tended to decline over the 180 day test period, but there was no evidence that the rods acted to draw moisture away from the wood. As expected, boron movement tended to increase with...
Y Cabrera, J J Morrell


Synthesis of boric acid ammonium oleate salt for wood preservation: Leachability and termite resistance test
2007 - IRG/WP 07-30435
A new chemical compound coupling boric acid and oleic acid through a joint of ammonium salt has been produced and its synthesis followed and validated by Fourier Transformed Infra Red (FTIR). This compound named ammonium borate oleate (BAO) combining biocidal properties of boron and water repellence of fatty acids has then been studied as a wood preservative. Synthesis of BAO involved different...
F Lyon, A Pizzi, Y Imamura, M F Thevenon, S N Kartal, J Gril


The influence of pentachlorophenol on mycelial growth of wood decay fungi Trametes versicolor, Grifola frondosa, Hypoxylon fragiforme, and Coniophora puteana
2007 - IRG/WP 07-30437
Polychlorinated phenols have been one of the most commonly used biocides. In recent time they have been increasingly eliminated from the marked. Because of their high stability, they are still present in numerous products, including impregnated wood. In our research we studied in vitro the influences of pentachlorophenol and/or sodium pentachlorophenolate on mycelial growth of four wood degrading ...
F Pohleven, B Boh


Tropical In-Ground Durability of CCB-treated Keruing and other Structural Sarawak Timbers after 8 – 10 Years Exposure
2007 - IRG/WP 07-30439
The heartwood of 12 mainly low-durability native timber species of Sarawak [4 Dipterocarpus (Keruing) species, Anisoptera grossivenia (Mersawa kunyit), Canarium apertum (Seladah), Dacryodes incurvata (Seladah laut), Dryobalanops oblongifolia (Kapur kelansau), Mesua macrantha (Mergasing), Podocarpus micropedunculatus (Kayu cina), Shorea compressa (Engkabang langgai), and Pterospermum javanicum (Ba...
A H H Wong, Ling Wang Choon


Natural Weathering of Coated Oil Heat Treated Wood
2007 - IRG/WP 07-30440
Oil heat-treated (thermally modified) pine wood was coated with 9 different types of solvent- or water-borne exterior finishes. The systems with modified wood substrate as well as unpainted and painted non-modified controls were exposed to weathering (EN 927-3) on two locations with sub-alpine and alpine climate. The influence of natural ageing on surface systems was evaluated after one year of ex...
M Petric, B Kricej, M Pavlic, A Rapp


The effect of brighteners on wood surface aesthetics – exploring the use of various organo-phosphonates based precursors
2007 - IRG/WP 07-30441
Freshly cut hardwood lumber such as white oak, red oak, beech, or redwood are rich in mineral stain (mostly iron and calcium), which provides a strong discoloration of the wood surface significantly influencing the aesthetic of the wood surface and strongly affecting the cost of this lumber. The influence of mineral stain on soft wood discoloration (Southern Yellow Pine, Douglas fir, etc.) is les...
R Craciun, P Mitchell


The Effect of Solar Radiation on the Surface Checking of Wood
2007 - IRG/WP 07-40356
The aim of this research was to investigate whether exposure to solar radiation increases the checking of wood exposed to the weather, and examine the causes and spectral dependency of such an effect. Lodgepole pine samples were exposed outdoors under filters which transmitted selected regions of the solar spectrum while allowing other weathering factors to act on samples. Surface checking in samp...
P Evans, K Urban


The effect of an ionic liquid of imidazolium tetrafluoroborates series on Scots pine wood properties
2007 - IRG/WP 07-40357
Ionic liquids (ILs) of imidazolium tetrafluoroborates series penetrate Scots pine wood very well and are active against wood destroying fungi. The requirement to use ILs as wood preservatives is determined by the liquid influence on the functional properties of wood. Investigations were undertaken to clarify the influence of an ionic liquid, 3-heptyloxymethyl-1-methylimidazolium tetrafluoroborate ...
A Fojutowski, R Szukala, J Pernak


Mold resistance of heat-treated wood
2007 - IRG/WP 07-40358
The resistance of heat-treated sugi sapwood against three mold fungi was evaluated. Wood specimens were first subjected to heat treatments at 180 and 220ºC for 2 and 4 hours. Mold growth on the surface of the specimens was measured 1, 2, 4 and 6 weeks after the inoculation with the fungi in laboratory conditions. Laboratory decay tests were performed using two brown and white-rot fungi along with...
S N Kartal


Comparative study between full cell and passive impregnation method of wood preservation for laser incised Douglas-fir lumber
2007 - IRG/WP 07-40359
Many wood species are highly resistant to conventional pressure treatment. To improve the chemical impregnation into Douglas-fir (Pseudotsuga menziesii Franco) lumber, the passive impregnation method had been developed. In this study, ability of the passive impregnation for lumber was compared with a conventional full cell method. Square Douglas-fir lumber with the incising density of 10,000 holes...
Md N Islam, K Ando, H Yamauchi, Y Kobayashi, N Hattori


Micro-Distribution of Metals in Wood Treated with a Nano-Copper Wood Preservative
2007 - IRG/WP 07-40360
The microdistribution of copper in southern pine treated with a newly-developed nano-copper wood preservative was examined to determine if it differed from that reported for wood treated with conventional copper-based wood preservatives. Field Emission Scanning Electron Microscopy (FE-SEM) in combination with x-ray microanalysis (EDX) revealed the presence of nano-sized copper and iron particles i...
H Matsunaga, M Kiguchi, P Evans


Fire, flame resistance and thermal properties of oil thermally-treated wood
2007 - IRG/WP 07-40361
Oil thermal treatment, first developed by German scientists, is a promising technology for improving the durability and dimensional stability of wood for outdoor above-ground residential uses such as siding and shingles. The present authors’ previous research showed that 220ºC is an optimal treatment temperature, with 2 hours’ treatment producing wood with significantly improved moisture and ...
Jieying Wang, P Cooper


Effects of sodium hypochlorite on compression strength and copper retention of spruce wood treated with copper azole and alkaline copper quat
2007 - IRG/WP 07-40362
This work investigates the effects of sodium hypochlorite on compression strength values and copper retention ratios of refractory spruce wood (Picea oriental L.) treated with the waterborne preservative Copper Azole, (CBA-A, Tanalith-E 3492) and alkaline copper quat (ACQ-2200). Before the copper azole and alkaline copper quat treatment, the samples were immersed in 500 ml of sodium hypochlorite s...
S Yildiz, E Dizman, A Temiz, Ü C Yildiz


Effect of ozone treatment on survival of termites and wood decay fungi
2007 - IRG/WP 07-40365
There is increased concern about the potential for transport of invasive pests on or in untreated wood. Current regulations utilize heating or fumigation as mitigation tools, but both have drawbacks that have stimulated interest in new phytosanitation methods. Ozone fumigation has been shown to control insects, fungi and bacteria on a variety of agricultural products. Systems for the controlled g...
A M Taylor, L J Mason, J J Morrell


Multivariate analysis of infrared spectra for the prediction of the mechanical performance and dimensional stability of thermally modified wood
2007 - IRG/WP 07-40367
The use of calibrated mid-infrared Fourier transform (FTIR) spectroscopy for predicting the main bending strength parameters of thermally modified wood is described for the first time. The analysis is based on the handling of OSC-filtered FTIR data from control and treated wood samples, using partial least squares (PLS) regression. Sets of Norway spruce, Scots pine and Beech wood samples were th...
M M González-Peña, M D C Hale


Refinement of emission values for preserved wood in the ‘Storage Scenario’, for use in the environmental risk assessment of Wood Preservatives under the Biocidal Products Directive
2007 - IRG/WP 07-50244
The evaluation of an active substance or a biocidal product under the Biocidal Products Directive (BPD) requires that an environmental risk assessment is carried out. The risk assessment for wood preservatives includes a scenario for the treated wood in storage after treatment, in which the predicted environmental concentration (PEC) in soil, surface water and groundwater is calculated, using emis...
E F Baines


The effect of additives on copper losses from alkaline copper treated wood
2007 - IRG/WP 07-50246
The replacement of chromated copper arsenate (CCA) by alkaline copper compounds has heightened awareness of the potential impact of copper losses on aquatic organisms. While there remains a healthy debate concerning the actual risk of copper leaching from wood preservatives into aquatic ecosystems, it is clear that reducing these losses will be necessary to avoid continued regulatory actions aga...
J Mitsuhashi, J J Morrell, L Jin, A F Preston


Construction of an ITS sequence database for the identification and classification of wood rot fungi
2007 - IRG/WP 07-10626
Developing a database that contains information about wood rot fungi is important in improving technologies about wood preservation as well as advances in understanding wood decay. On the other hand, with rapid spread of the Internet, establishment of a system for the swift precise access to information are required for the computerization of the research information. In the present study, genetic...
S Horisawa, Y Honda, S Itakura, S Doi


Control of Moisture Content in Wood Materials for Mold Growth
2007 - IRG/WP 07-10630
Mold growth on wood materials is a major concern for house owners, as it can cause health and aesthetic problems. Mold fungi, present everywhere, usually appear as black or gray patches on wood surfaces in humid environments, and are common in houses. Like any living organism, molds need food, water, oxygen, and a specific temperature range in order to grow. To avoid mold growth on wood materia...
Dian-Qing Yang


White Rot in Eucalyptus Wood: Anatomical Changes and Density Variation by X-Ray Densitometry
2007 - IRG/WP 07-10631
Wood samples of the hybrid Eucalyptus grandis x urophylla attacked by white rot fungi were characterized. Microscopically, the colonization of the fungi was observed in the vessels and radial parenchyma, however the cell walls of the some fibers were attacked, indicating susceptibility to this fungi. Zone lines were observed as a result of interaction and compartmentalization of the fungi. Microsc...
M Tomazello Fo, S Brazolin, M P Chagas