Recovery of copper chromium and arsenic from old CCA treated commodities
1998 - IRG/WP 98-50118
Due to the expected increase in spent treated wood over the next several decades, numerous means to reuse and recycle preserved wood have been proposed. Burning this wood for cogeneration or recycling of CCA treated wood into reconstituted composites are possible methods, but they are limited to laboratory scale because of environmental air emission issues and the manufacturing process. In the av...
D P Kamdem, Wanli Ma, Jun Zhang, J Zyskowski


Removal of copper, chromium and arsenic from CCA treated wood using boron compounds
2005 - IRG/WP 05-50230
This study evaluates the copper (Cu), chromium (Cr) and arsenic (As) removal from CCA treated wood using boron compounds such as boric acid, borax (sodium tetraborate), and Timbor (DOT, disodium octaborate tetrahydrate) at varying (3 and 5%) concentrations. Remediation processes were taken at 1, 5 and 10 day intervals. Metals in remediated chips or sawdust were then analyzed using ICP and XRF. Res...
B Tarakanadha, T Hata, S N Kartal, W J Hwang, Y Imamura


The difficult choice of the preservation industry when changing to more environmentally acceptable products
2000 - IRG/WP 00-50156
Until recent years the preservation industry in Norway had no problems with the environmental authorities. However, during the last three years the pressure has increased, and the authorities' solution to restrict hazardous chemicals is to introduce green (environmental) taxes for the products containing these chemicals, and also for the pressure-treated wood. The preservation industry ac...
F G Evans


Tributyltin compounds in wood preservation: Health and safety aspects
1986 - IRG/WP 3396
The toxicity of organotin compounds of the general formula RnSnX(4-n) depends strongly on the type of organic substituent R and on the degree of substitution n. The residues X, not bound through a tin-carbon bond, are however of much smaller influence. Furthermore, there is evidence that hydrolysis of tributyltin esters will occur under environmental as well as under physiological conditions to TB...
H Schweinfurth, P Günzel, H A B Landsiedel, R Lang, R Reimann, C Schöbel, F Siegmund


Influence of carboxylic acids on LEACHING of copper amine based preservatives
2005 - IRG/WP 05-30365
The importance of chromium free preservatives is increasing. Leaching of copper from wood preserved with such solutions is still higher compared to leaching from wood impregnated with copper chromium ones. In order to decrease leaching, different carboxylic acids (octanoic, 2-etilheksanoic, decanoic) were added to copper/amine/boron aqueous solutions. Experiment of leaching of copper from Norway s...
M Humar, P Kalan, F Pohleven


Blue stain in service on wood surface coatings. Part 1: The nutritional requirements of Aureobasidium pullulans
1992 - IRG/WP 92-1556
The nutritional requirements of Aureobasidium pullulans was examined with regard to nutrient sources that are potentially available in fresh and weathered wood. The study was designed to determine how far wood cell wall components need to be broken down during weathering before they provide a useful nutrient source for Aureobasidium pullulans. Various carbon sources were tested, with eight differe...
P R Sharpe, D J Dickinson


Temperature and pressure inside wood during creosote impregnation
1991 - IRG/WP 3649
Creosote gives the best protection against decay for sleepers and poles. However, it has a major drawback - bleeding. Modified impregnation processes to reduce bleeding have been tried. For developing such processes it is important to know the actual temperature and pressure inside the wood. This paper describes measurement of temperature and pressure inside wood during creosote impregnation. The ...
Ö Bergman


Comparison of performance of wood preservatives in laboratory and field tests of treated commodities
1993 - IRG/WP 93-20010
The purpose of laboratory tests for evaluating efficacy of wood preservatives is usually to establish toxic values against standard strains of wood decay fungi. Exposure conditions are usually chosen as optimal for fungal growth. Toxic values so determined serve as a guide as to expected performance of the preservative in field stake tests or in above ground exposure tests. Test material is select...
M E Hedley


Fundamentals on steam fixation of chromated wood preservatives
1988 - IRG/WP 3483
Weathering of treated wood directly after impregnation leaches up to 2% of copper-chromate-containing wood preservatives. Almost total fixation of Cr+6 is achieved by steaming the treated wood at 100°C to 120°C, preferably 110°C. To initiate such spontaneous fixation 85°C to 90°C inside the wood are essential, which requires heating times ranging from 20 to 80 min, depending on timber species...
R-D Peek, H Willeitner


Modification of wood by graft treatment
2003 - IRG/WP 03-40257
New water-repellent systems for wood are needed to improve the weathering characteristics. This study found that treatment of wood with chemical grafting systems imparted substantial water repellency. Different direct oxidative grafting systems were examined. Specifically, KMnO4, Fe(NH4)(SO4)2·12H2O, Fe2(SO4)3·5H2O, and (NH4)2Ce(NO3)6 were used as initiators and styrene as the monomer. All the...
M M Morshed, D D Nicholas, C Pittman Jr, T Schultz


Extracellular substance from the white rot basidiomycete Irpex lacteus involved in wood degradation
1992 - IRG/WP 92-1571
Cellulases, phenol oxidase, and a substance that both produced and reduced H2O2 were isolated from cultures containing wood or glucose on which the white-rot fungus Irpex lacteus was growing. The rate of wood degradation by the fungus with different amounts of glucose in the medium was measured. More of the substance that produced and reduced H2O2 was found extracellularly in cultures containing w...
H Tanaka, T Hirano, G Fuse, A Enoki


Valid scientific names of wood-decaying fungi in construction timber and their vernacular names in England, Germany, France, Sweden, Norway and Denmark
1992 - IRG/WP 92-1546
The valid scientific names of 100 species of wood decaying fungi in construction timber are listed, the citation of authors' names is standardized, and an index of the most commonly used synonyms is compiled. For each species vernacular names used in England, Germany, France, Sweden, Norway and Denmark are listed. The list of names is an attempt to update the current use of the most impor...
F Rune, A P Koch


Non-destructive detection of the presence and behaviour patterns of wood-destroying insects
1988 - IRG/WP 2302
An apparatus, designed for the automatic recognition of the presence and of specific behaviour patterns of wood-boring insects, is introduced. From a wood sample, a mixture of noise and action induced substratum vibrations is picked up, amplified, filtered and translated into a sequence of computer-readable numbers which are passed to a microcomputer-based signal-pattern-recognition. If an incomin...
M Pallaske


Role of wood preservation in bioconservation and protection of environment
1997 - IRG/WP 97-50082
In order to meet a revolutionary task of bioconservation and protection of environment through preservation of less important and nondurable timbers from tropical zones, 170 timber species from Bangladesh were screened. Air-dried (12% MC) 170 different species of timbers, full cell pressure impregnated with 5% CCB solution revealed satisfactory treatability of all timbers for long-term indoor uses...
A K Lahiry


Need to develop processing technologies (for value addition) of the species evaluated for their properties and uses
2005 - IRG/WP 05-40307
The demand of timber in India for different industrial as well as domestic applications is ever increasing mostly due to urbanization and industrialization. This demand can only be met either from the imported timber or from the plantation resources outside the reserved and natural forests. There are a number of timber species grown under plantation forestry have their heartwood refractory to any ...
S R Shukla, S K Sharma, Y M Dubey, P Kumar, R V Rao, K S Shashidhar


Evaluation of outdoor weathering performance of modified wood
2004 - IRG/WP 04-20296
Interlace treated, oil treated, silicon treated as well as untreated Scots pine samples have been exposed outdoors. For evaluating the samples on their long term performance an internal standard had been developed. Parameters to be determined were the uptake of liquid water (submersion test), weight variation during exposure, crack performance, surface roughness and colour change. This paper disc...
Y Schulte, S Donath, A Krause, H Militz


Performance of preservative-treated wood not in ground contact
1975 - IRG/WP 254
Experimental sash units of Pinus strobus L. and Pinus resinosa Ait. wood were removed from a test fence at Ottawa, Canada after outdoor exposure of over 20 years. The units were superficially treated, prior to painting, with preservatives containing either copper naphthenate, pentachlorophenol or a combination of zinc naphthenate and pentachlorophenol. Results indicated that all treatments were ef...
J K Shields, J Krzyzewski


Chelator production and cellobiose dehydrogenase activity of wood inhabiting fungi
2000 - IRG/WP 00-10363
Multiple components have been postulated to be involved in the Fenton-based biological degradation of wood by brown rot fungi. Chelators have been implicated in essential iron reduction steps. Cellobiose dehydrogenase activity and quinone reducing activity have also been implicated in brown rot biodegradation. When biochelator production by three white rot fungi, three brown rot fungi and three wo...
Weihong Qi, J Jellison


Chemical Remediation of Beech Condensates
2004 - IRG/WP 04-50221
In the present work, The beech wood condensate are subsequently separated from the aqueous phase. Experimental results reveal the electrostatic interaction between the oppositely charged wood extracts after oxidation and Ca(OH)2. The influence of parameters such as pH, oxidation were studied. The increase in aqueous phase pH resulted in enhanced removal of wood extracts from water. The effect of p...
M Irmouli, J P Haluk


Laboratory studies on control of sapstain and mold on unseasoned wood by bacteria
1991 - IRG/WP 1493
A malt-agar and nonagar laboratory test was used to evaluate the efficacy of bacterial preparations as biological control agents against several sapwood-inhabiting fungi. Both nonsterilized and filter sterilized bacteria preparations prevented attack by the sapwood-inhabiting fungi. Streptomyces rimosus was the most effective bacteria, giving good protection, with a 1-hr soak in a filter-sterilize...
T L Highley, R Benko, S C Croan


Determination of boron levels in solution and in treated wood
1994 - IRG/WP 94-20041
Four methods of measuring boron levels in solutions were investigated. The methods compared included the azomethine-H method which is commonly used in soils and plant tissues, the methods outlined in the Australian Standard AS 1605 (1974) and in Wilson (1958), and the atomic absorption spectrophotometry method. Defect-free radiata pine (Pinus radiata D. Don) sapwood and wood flakes were treated to...
F J Romero, P Vinden, P Kho


Siderophore production by Trichoderma spp. and its importance in the biological control of wood decay fungi
1994 - IRG/WP 94-10070
Competition for iron as well as other micro-nutrients is an essential component of the microbial ecology of many ecosystems. A wide range of micro-organisms including fungi and bacteria have been shown to increase their ability to efficiently capture iron through the production of specialised iron chelating compounds called siderophores. Since iron is in low supply in wood and has been implicated ...
U Srinivasan, A Bruce, T L Highley


An appraisal of the vertical distribution of attack of untreated and treated wood by warm water sphaeromatids at some tropical sites - A discussion paper
1986 - IRG/WP 4124
Examples of the vertical distribution of burrows of warm water sphaeromatids relative to tide levels and mud line from sites in India, Papua New Guinea and tropical Australia are discussed in detail. These data show clearly that these animals concentrate their attack of resistant natural wood or resistant treated wood in the tidal zone, particularly around Mean Sea Level. Supportive evidence from ...
J E Barnacle, L J Cookson, C N McEvoy


Electrochemical removal of Cu, Cr and As from CCA-treated waste wood
2001 - IRG/WP 01-50166-18
CCA-treated waste wood poses a potential environmental problem due to the content of copper, chromium and arsenic. This paper presents the results obtained by electrodialytic remediation of CCA-treated waste wood. It is found that more than 90% Cu, and approximately 85% Cr and As was removed from the wood during the remediation. Thereby the concentration of copper in the wood is reduced from app. ...
I V Kristensen, L M Ottosen, A B Ribeiro, A Villumsen


Leachabilty and efficacy of fatty acid derived boron esters as wood preservatives - leachability and efficacy of fatty acid derived boron esters as wood preservatives
2004 - IRG/WP 04-30351
Borates have many advantages as wood preservatives. However, boron is susceptible to depletion under humid conditions and this restricts its outdoor use. In order to reduce boron leachability in treated wood, one of the anticipative approaches is to use organic fixed boron-based preservatives. This study investigated the leachability of six boron ester compounds as potential preservatives. Scots p...
A Mohareb, J Van Acker, M Stevens