CCA Chemistry
1983 - IRG/WP 3268
A Pizzi


Soil chemistry and wood decay
1978 - IRG/WP 2109
Soil is a most complex biological, chemical and physical material; its study is effectively a separate branch of science but almost entirely in relation to ist ability to grow plants - this paper is intendet just to note some known facets that might have relevance to the decay of wood and the performance of wood preservatives....
E A Hilditch


Alternative technologies for wood wastes recycling - Part B: Biotreatment of PCP- and creosote-treated wood
1998 - IRG/WP 98-50101-18 b
Alternative technologies have been investigated to detoxify treated wood. Two classes of organic compounds are studied. Creosote-treated wood are classified in France as dangerous wood wastes. A conventional incineration could be provided for these wood wastes but the cost of this elimination could be very high (> 2000 FFR/ton). For these reasons, we have tested two kinds of new processes as al...
S Legay, P Marchal, G Labat


Accelerated laboratory soil contact decay test using soil amended with composted wood
2004 - IRG/WP 04-20284
The effect of amending soil with wood compost on the decay rate of wood wafers in contact with the unsterile soil, as measured by radial compression strength loss, was explored. It was found that the addition of composted wood to the soil significantly increased the wood decay rate. The reason for this acceleration in wood decay is not entirely clear, but appears to be at least partially associate...
D D Nicholas, H Borazjani, T Schultz


Natural weathering of wood in a sunny climate effects on surface chemistry and paint adhesion
1997 - IRG/WP 97-20109
Radiata pine veneers and blocks were exposed to natural weathering under Australian summer conditions over a period of 30 days. Infrared spectroscopy revealed that there was perceptible surface delignification after 4 hours exposure, substantial surface delignification after 3 days exposure and almost complete surface delignification after 6 days. Viscometry determinations on holocellulose samples...
P D Evans, P D Thay, K J Schmalzl


Alternative technologies for wood wastes recycling - Part A: Supercritical extraction of PAH compounds from wood wastes
1998 - IRG/WP 98-50101-18 a
Alternative technologies have been investigated to detoxify treated wood. Two classes of organic compounds are studied. Creosote-treated wood are classified in France as dangerous wood wastes. A conventional incineration could be provided for these wood wastes but the cost of this elimination could be very high (> 2000 FFR/ton). For these reasons, we have tested two kinds of new processes as al...
L Schrive, C Perre, G Labat


Natural Durability studies and Changes in wood chemistry of some Ghanaian hardwoods during decay by white- and brown-rot fungi
2004 - IRG/WP 04-10542
The natural decay resistance of Esa (Celtis mildbraedii), Wawabima (Sterculia rhinopetela) and Dahoma (Piptadeniastrum africanum) obtained from Ghana was determined according to BS EN 113 (1997). Esa was found not durable to the white-rot, but very durable to the brown-rot; Wawabima was very durable to both white- and brown-rots; and Dahoma was durable to the white-rot, and very durable to the bro...
Zeen Huang, K Maher, S A Amartey


On the nature of the tertiary wall in wood cells. Summary of lecture given at 9th Annual Meeting, Noordwijk-aan-Zee, Holland
1977 - IRG/WP 169
During recent discussions on the possible causes of failure of treated hardwood species by soft rot fungi, the uneven micro distribution of toxic components was found to be of importance; this might be attributed to a restricted diffusion of the preservative from the cell lumina into the cell wall.·In this context, the nature of the tertiary wall as the inner lining of wood cells merits special a...
W Liese


Effect of soil chemistry and physical properties on wood preservative leaching
1998 - IRG/WP 98-50111
When treated wood is placed in contact with soil, complicated mass transfer and chemical reactions occur which causes the preservative components to leach from the wood. There are several factors that are known to affect the amount of chemical leached from wood. These are properties of the preservative and carrier, preservative retention, degree of fixation, exposure time, grain orientation, surfa...
Joan-Hao Wang, D D Nicholas, L S Sites, D E Pettry


Chelator-Mediated Fenton Chemistry in Wood Degraded by Fungi
2007 - IRG/WP 07-10618
Wood specimens were colonized by individual isolates of brown rot, white rot, soft rot and blue (sap) stain fungi. Ethyl acetate extracts of the ground wood were analyzed for their iron-reducing capabilities using a ferrozine-based assay. Extracts from wood colonized by brown rot fungi showed a significantly greater iron-reducing capability than extracts from wood colonized by white rot fungi or n...
B Goodell, G Daniel, J Jellison, Yuhui Qian


Chemical Analysis in Production Quality Control at Wood Treatment Plants
2008 - IRG/WP 08-20396
Analysis methods for quality control analysis in wood treatment plants have evolved with the changes in treatment preservative chemistries and analytical instrument technology. The basic hydrometer specific gravity measurements used for solution strength and classic wet chemistry methods for wood have given way to instrumental techniques such as X-ray fluorescence, automatic titrator, and HPLC. No...
P Walcheski, L Jin


Vacuum drying of European oakwood: Color, chemistry and anti-oxidant potency of wood. Improving appearance in forest value added products
2008 - IRG/WP 08-40432
In hardwoods used for decorative and appearance purposes, wood colour is one of the most important factors of wood quality; in addition colour is related with durability and biological decay of wood. Wood discolouration during drying is mainly affected by heat, light, physiological reactions, combinations of reactions, biochemical and chemical reactions, and micro-organisms attack. In freshly fell...
S Sandoval, W Jomaa, F Marc, J-R Puiggali


New insights from NMR, FTIR, X-ray diffraction and physical chemistry into digestive processes in the wood-boring marine crustacean Limnoria quadripunctata
2010 - IRG/WP 10-10732
This paper summarises preliminary findings of a multi-technique exploration of the degradation of lignocellulose in the marine isopod Limnoria quadripunctata. Scanning electron microscopy revealed connections between the digestive gland and the hindgut that would permit the exchange of fluids between the two organs while the food mass is retained in place within the hindgut. This enables enzymes t...
G P Malyon, S LaBarre, N Kervarec, P Carey, J McGeehan, X Xie, A Klüppel, S M Cragg


A comparison of the chemistry of alkaline copper and micronized copper treated wood
2010 - IRG/WP 10-30528
This paper discusses the chemistry of the reaction of alkaline copper and micronized copper with wood. The objective of this study is to examine the copper species produced in wood during the fixation reaction using electron paramagnetic resonance (EPR) spectroscopy. The initial experiments (phases 1 to 2) were designed to confirm the effect of time of treatment and solution concentration on the s...
Wei Xue, P Kennepohl, J N R Ruddick


The chemistry of wood degradation by Basidiomycetes studied in a van Krevelen diagram
2013 - IRG/WP 13-10805
The atomic composition ratios of decayed wood by Basidiomycetes are mapped in a van Krevelen diagram. It is shown that the wood residue after decay is chemically reduced, rather than oxidized. A previously developed and verified theoretical model for thermal wood modification, relating atomic composition ratios to moisture sorption and fungal resistance properties has tentatively been applied to w...
W Willems, H Militz


Chemistry of copper preservative treated wood
2014 - IRG/WP 14-30651
The reaction chemistry of micronized copper wood preservatives is fundamentally different from any previous inorganic preservative system. In order to study the chemistry, analytical procedures had to be developed which allowed the determination of the total copper as well as the copper which reacted with the wood forming copper-wood complexes. With the success of this approach it also became poss...
Wei Xue, P Kennepohl, J N R Ruddick


The potential of 2D NIR imaging for wood protection research
2015 - IRG/WP 15-20566
Investigating wood and wood-based materials using infrared spectroscopy has since long been explored. Recently, image-based systems have been developed that are used in food and pharmaceutical industries for rapid screening. Such hyperspectral cameras are able to collect spatial and spectral information simultaneously, resulting in a volume with a spectral profile for each pixel of the image. We p...
J Van den Bulcke, N Defoirdt, W Li, J Van Acker


Enhancing Our Understanding of Brown Rot Mechanisms through Catalytic Pretreatment and Cellulase Cocktail
2018 - IRG/WP 18-10909
A catalytic mechanism, described as the “chelator-mediated Fenton” (CMF) mechanism, is proposed to mimic the non-enzymatic action of brown rot fungi. A CMF treatment was used together with an enzymatic cocktail to study how wood was deconstructed and solubilized. This was done in-part to determine if the treatment mimicked the action of brown rot fungi, but also to explore improved treatment p...
S Tabor, L Orjuela, D Contreras, G Alfredsen, J Jellison, S Renneckar, B Goodell


Wood chemistry completes natural durability as criteria for shorting best provenances in the improvement of teakwood quality: case of five provenances from Ivorian Séguié’s trial
2018 - IRG/WP 18-10920
In order to determine the best provenance for continuing breeding program in Côte d’Ivoire, five provenances of teak planted in 1970 at Séguié’s trial (Agboville, in the south of Côte d’Ivoire), were compared. Fifteen trees (three trees per provenance) composed the sample. Decay resistance and the chemical content especially, non-structural carbohydrates, total phenolics and quinone comp...
F B Niamke, N Amusant, A A Adima, A A Kadio, G Chaix, C Jay-Allemand


Decay capacity and degradation patterns of Xylaria hypoxylon on different wood species
2022 - IRG/WP 22-10985
A host of physical and environmental factors may influence fungal decay including the wood substrate, temperature, moisture, oxygen, light, pH, and nitrogen. Understanding the effects of these factors on fungal decay is important for the effective utilization of wood decay fungi in biotechnological processes and for understanding the role of these organisms in global carbon cycling. The ascomycete...
E Bari, G Daniel, A Singh, J J Morrell


Danish wood preservatives approval system with special focus on assessment of the environmental risks associated with industrial wood preservatives
2001 - IRG/WP 01-50166-01
The following is a description of the procedure used by the Danish Environmental Protection Agency to assess the environmental risks associated with preservatives used in the pressure impregnation of wood. The risk assessment covers issues considered to be of significance for the environment and which are adequately documented so as to allow an assessment. Such issues are persistence and mobility ...
J Larsen


Data sheet on wood-boring insects. Apate monachus Fabricius. 2. Position systématique, nomenclature, identification et distribution - Espèces végétales attaquée
1981 - IRG/WP 1105
R L A Damoiseau


Confocal laser scanning microscopy of a novel decay in preservative treated radiata pine in wet acidic soils
1997 - IRG/WP 97-10215
Light microscopy of radiata pine (Pinus radiata D. Don) field test stakes (20x20x500mm3) exposed in wet acidic (pH 3-4) soil for 12 - 24 months showed predominance of an unusual type of decay characte-rised by tunnelling attack of wood cell walls. After two years decay was moderate to severe in wood treated to ground contact CCA specifications and also equivalent retentions of creosote, and a numb...
R N Wakeling, Ying Xiao, A P Singh


Effect of acetylation on decay resistance of wood against brown-rot, white-rot and soft-rot fungi
1989 - IRG/WP 3540
Effect of acetylation on decay resistance of wood was investigated using wood blocks of Cryptomeria japonica, Pinus densiflora, Albizia falcata and Fagus crenata. Blocks were treated with uncatalyzed acetic anhydride for different lengths of time and exposed to Tyromyces palustris, Serpula lacrymans, Coriolus versicolor and unsterilized soil. The action of OH-radical on acetylated wood was also ex...
M Takahashi, Y Imamura, M Tanahashi


The IRG..Chanelling information and ideas into the mainstream of wood preservation technology
1985 - IRG/WP 5241