Premature failure of CCA treated vineyard posts from brown rot
1993 - IRG/WP 93-10016
A survey of CCA (AWPA Type C) treated posts used as grape vine trellis supports, to determine the extent and type of decay was carried out at a terraced vineyard in the Hawkes Bay region of the North Island of New Zealand. Of 357 posts examined out of a total of 970 in the vineyard, 47% had moderate to severe decay or had failed, 20% had established decay, 10% had a trace of decay and 23% had no s...
R N Wakeling, A P Singh


Cell wall microdistribution of chloropicrin and methylisothiocyanate in treated spruce
1989 - IRG/WP 3548
Chloropicrin and methylisothiocyanate (MIT) residues were observed using SEM/EDXA and TEM/EDXA in treated spruce wafers that had been exposed to the vapors of the two fumigant preservatives. Chlorinated residues from chloropicrin were found throughout the wood cell wall, even in acetone extracted material. The residues were most heavily concentrated in extractive materials in the rays, but unlike ...
G F Daniel, B Goodell


The nature of osmiophilic particles and their distribution during different stages of brown and white rot decay
1983 - IRG/WP 1213
The distribution of osmiophilic particles during the course of brown and white rot decay was investigated by applying transmission electron microscopic (TEM) methods. It was found that it correlates with the brown and white rot pattern.The osmiophilic particles are produced by the fungus and are supposed to be wood rotting enzymes....
K Messner, H Stachelberger


Preservative treatment of rubber wood (Hevea brasiliensis) to increase its service life
2005 - IRG/WP 05-40320
Rubber wood (Hevea brasiliensis) possess excellent properties for interior designing, wood working and furniture making. But it is very much susceptible to sap stain and mould fungi which decreases the service life. For profitable uses , it is necessary to increase the service life of rubber wood. To protect the rubber wood from wood degrading agents, the sawn timber were treated with Borax – b...
K Akhter


Estimation of the impregnation degree of pine wood by the distribution analysis of active ions concentration in the cross-section
1999 - IRG/WP 99-20174
Samples in the form of pine wood rollers of diversified moisture content of ca. 50, 28 and 12% were impregnated with a water solution of the mixture type CCB with the use of the full-cell process. Moisture content was determined in individual layers from the girth to the pith. In the same way the concentrations of copper and chromium ions with the use of the spectrophotometric method and recalcula...
K Lutomski, B Mazela


Industrial fixation of chromium based wood preservatives
1990 - IRG/WP 3630
Fixation is an abstract and non-defined process. Nevertheless it is a specified requirement in most impregnation standards. The impregnation industry is facing increased pressure to deliver fixed products and to increase the safety of the handling of impregnated products. Industrial fixation of impregnated wood can be obtained by using different methods. The purpose of the process is to transform ...
T Christensen


Extracellular osmiophilic particles in connection with brown rot and white rot
1982 - IRG/WP 1157
The way of attack on Pine woodblocks of two brown-rot fungi (Fomitopsis pinicola, Coniophora puteana) differing in their cellulase activities, and one white-rot fungus (Trametes hirsuta) has been investigated by transmission electron microscopy. Even at early stages of decay, osmiophilic particles were found with all the fungi investigated. In the brown-rotted wood, the osmiophilic particles occur...
K Messner, H Stachelberger


Micromorphology of oak wood degraded by brown rot fungus Coniophora puteana
2000 - IRG/WP 00-10356
To characterize the degradation of hardwood by brown rot fungus, Coniophora puteana was incubated on the wood blocks of Quercus accutissima. For comparison, the same fungus was also incubated on the pine wood blocks of Pinus densiflora. In softwood, the shape of the wood cells and thickness of the cell appeared unchanged even the loss of birefringence in the affected areas. In contrast, oak wood d...
Yoon Soo Kim, Seung-Gon Wi, Kwang-Ho Lee


Cavitation bacteria
1984 - IRG/WP 1235
A form of bacterial wood degradation is described. The term "cavitation bacteria" has been coined in order to describe the discrete cavities that are formed within the wood cell walls. The bacteria observed within the cavities appeared to be polymorphic with rounded as well as filamentous forms recognised. TEM studies suggest that the bacteria produce diffusable wood-degrading enzymes. Cavitation ...
T Nilsson, A P Singh


The development of soft rot decay in bamboo fibres
1992 - IRG/WP 92-1572
The development of decay by soft rot fungus Chaetomium globosum was investigated in young and mature culms of bamboo Phyllostachys virideglaucescens. Soft rot decay was influenced both quantitatively and qualitatively by the differing levels of lignification in the material. Weight loss was significantly greater in the younger culm compared with the older, more heavily lignified culm. The distribu...
O Sulaiman, R J Murphy


Utilisation of carbohydrates by stain fungi in agar culture
1998 - IRG/WP 98-10248
Stain fungi are often defined by their ability to utilise the starch and free sugars found in ray parenchyma cells, and their inability to utilise other wood constituents. However, several species of stain fungi produce bore holes in wood cell walls. This suggests that enzymatic activity capable of degrading structural polysaccharides and/or lignin is associated with the growth of the appressorium...
J Snow, P Vinden, S M Read


Degradation of woods by obligately anaerobic fungi
1990 - IRG/WP 1452
Little is known about the processes occurring during the degradation of wood by obligately anaerobic fungi. When woods from a range of hardwood species were incubated for 11 days with a strain of the Chytrid Neocallimastix frontalis many of the woods were measurably fermented; Fagus sylvatica (23%) was the most highly degraded. Microscopic examination of Populus tremuloides wood after incubation w...
K N Joblin, G E Naylor


Time-of-Flight Secondary Ion Mass Spectrometry Analysis of Polyethylene Glycol Penetration into Wood Cell Walls
2006 - IRG/WP 06-20328
Penetration of high molecular weight polyethylene glycol (PEG) into wood cell walls was investigated in red pine. PEG of different molecular weights (1000, 8000 and 20000) was labelled by bromination and treated samples were analyzed on Time-of-Flight Secondary Ion Mass Spectrometry (TOF-SIMS) in dynamic mode. Both negative and positive spectra of the samples were collected in high spatial (bunche...
D Jeremic, P Cooper, P Brodersen


Copper borate for the protection of engineered wood products
2006 - IRG/WP 06-40334
Copper borate was evaluated for use in protecting oriented strand board (OSB) from mould, decay, and termites. Aspen OSB bonded with either phenolic or isocyanate resin was treated with several formulations of copper borate at various loadings from 0.26 to 4 percent by weight. These panels were then tested to determine the impact of the preservative on mechanical properties as well as resistance ...
R Smart, W Wall


Comparative study between full cell and passive impregnation method of wood preservation for laser incised Douglas-fir lumber
2007 - IRG/WP 07-40359
Many wood species are highly resistant to conventional pressure treatment. To improve the chemical impregnation into Douglas-fir (Pseudotsuga menziesii Franco) lumber, the passive impregnation method had been developed. In this study, ability of the passive impregnation for lumber was compared with a conventional full cell method. Square Douglas-fir lumber with the incising density of 10,000 holes...
Md N Islam, K Ando, H Yamauchi, Y Kobayashi, N Hattori


Micro-Distribution of Micronized Copper in Southern Pine
2008 - IRG/WP 08-30479
For copper-based preservatives to be used in ground contact, penetration of copper into the cell wall is believed to be important to protect the wood from soft rot fungi. Preservatives containing soluble copper are known to do this. It is not known whether preservatives containing particulate copper will also migrate into the cell wall in sufficient quantities to control soft rot decay. An AWPA st...
R Stirling, J Drummond, Jun Zhang, R J Ziobro


Radial flow of Bornmullerian fir (Abies bornmulleriana Mattf.) as affected by wood tapering and the condition of end wall structure of uniseriate ray parenchyma cells
2008 - IRG/WP 08-40441
Amenability to radial permeability of Bornmullerian fir (Abies bornmulleriana Mattf.) was studied on the base of the effects of wood tapering and the structure of end walls of uniseriate ray parenchyma cells. The results showed that the most remarkable culprits of the greatest fluid uptake (as the percentage of void volume filled by the fluid in the radial flow direction, RVVF%) are the lesser woo...
I Usta, S Aslan


Comparison of permeability at different levels of moisture content in Bornmullerian fir (Abies bornmulleriana Mattf.) and Eastern spruce (Picea orientalis L.) impregnated under vacuum/pressure through full-cell method by using CCA and CCB of different concentrations
2007 - IRG/WP 07-40366
In this study, a comparison has been made in terms of the combined, longitudinal, tangential, and radial permeability of the species of Bornmullerian fir (Abies bornmulleriana Mattf.) and Eastern spruce (Picea orientalis L.) with moisture contents of 50 % and 15 %, which were impregnated under vacuum/pressure through full-cell method by using water-borne wood preservatives (impregnation materials)...
I Usta


Effects of concentration and temperature of CCA and CCB on wood strength of Turkish fir (Abies bornmulleriana Mattf.)
2009 - IRG/WP 09-40450
The purpose of this study was to present evidence for the effects of concentration and temperature of solutions of water-borne preservatives (chromated copper arsenate, CCA and chromated copper boron, CCB) on the static bending properties (modulus of elasticity, MOE and modulus of rupture, MOR) of Turkish fir (Abies bornmulleriana Mattf.). Wood samples were mechanically tested after a mild full ce...
I Usta, M Hale


Chapter 11 - Preservation of talla bamboo
2007 - IRG/WP 07-10635-11
Researches revealed that the talla bamboo (Bambusa tulda Roxb.)) in Bangladesh could be full-cell pressure treated with CCA in green and dry conditions. The dry bamboo gives higher loading absorptions than green one when impregnated at same treating conditions. Also higher absorptions are obtained at nodes rather than internodes. Adequate penetration and retention results for ground and wate...
A K Lahiry


Chapter 12 - Treatment Groups of Bamboo
2007 - IRG/WP 07-10635-12
Study on distribution of CCA in three major bamboo species in Bangladesh, full-cell pressure treated at green and dry conditions revealed two treatment groups and some treating principles. Higher adequate treatment for ground and water contact use is only possible by treating problematic bamboo species pre-kiln dried up to half of its FSP and non-problematic species pre-dried up to FSP (20% ...
A K Lahiry


Effects of nano-wollastonite impregnation on fire resistance and dimensional stability of Poplar wood
2012 - IRG/WP 12-40595
The fire-retardant properties of Nano-Wollastonite (NW) in poplar wood (Populus nigra) were determined in this study. Some physical properties such as water absorption, volumetric swelling and Anti-Swelling Efficiency (ASE) were also measured. Specimens were prepared according to the ISO 11925 standard for the fire-retarding properties, and ASTM D4446-2002 standard for the physical properties. Imp...
A Karimi, A Haghighi Poshtir, H Reza Taghiyari, Y Hamzeh, A Akbar Enayati


Cell wall properties of softwood deteriorated by fungi: combined chemical analyses, FT-IR spectroscopy, nanoindentation and micromechanical modelling
2013 - IRG/WP 13-20527
Mechanical properties of wood are determined by its inherent hierarchical microstructure, starting at the nanometer scale, where the elementary components cellulose, hemicelluloses, and lignin build up the wood cell wall material. Fungi cause degradation and decomposition of these components and, thus, alter the mechanical properties of wood. The aim of this study is to gain new insight into these...
L Wagner, T K Bader, K de Borst, T Ters, K Fackler


Visualization of Copper in the Voids and Cell Walls of Treated Wood using X-Ray Micro-Computed Tomography
2013 - IRG/WP 13-40640
This study extends our observations of the distribution of copper in treated wood. A small wood block was cut from a southern pine batten that had been treated with a particulate-copper preservative and similar sized block was cut from a batten that had been treated with a copper-amine preservative. Both blocks were imaged using X-ray micro-computed tomography. We obtained tomograms of each treate...
P D Evans, A Limaye, H Averdunk, M Turner, T J Senden


Scanning Transmission X-ray Microscopy as a tool for examining chemical changes in wood cell walls due to enzymatic activity
2014 - IRG/WP 14-20556
As development of techniques for examining enzymatic activity on solid, complex biological materials, is considered to be an important factor in further development of enzyme applications and for understanding the decay of plant materials, this study explores applicability of Scanning Transmission X-ray Microscope (STXM) for determining chemical changes in enzymatically treated samples at the cell...
D Jeremic, R Goacher, R Yan, C Karunakaran, E R Master


Previous Page | Next Page