IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 3122 documents. Displaying 25 entries per page.


Wood preservation in Kenya
2000 - IRG/WP 00-40191
Current research on wood preservation in Kenya is mainly on the development of biological control of wood-destroying termite species, using mycoinsecticides. The major research institutions include the Kenya Agricultural Research Institute (KARI), Kenya Forestry Research Institute (KEFRI), Moi University and the International Centre for Insect Physiology (ICIPE). Training institutions include Fore...
G Ochiel


Vapour boron treatment of wood based panels: Further studies on mechanical properties
1993 - IRG/WP 93-30028
Samples of medium density fibreboard, chipboard and oriented strandboard were treated to two retentions of boric acid by vapour phase methods. The results of short term mechanical tests on this material were discussed by Hashim et al. (1992). The present paper discusses results with long term studies on bending and impact resistance with panel types. Long term tests of impact resistance showed no ...
R Hashim, R J Murphy, D J Dickinson, J Dinwoodie


Sustainability Through New Technologies for Enhanced Wood Durability. COST Action E37 – A New Action in the Forestry Domain
2004 - IRG/WP 04-40293
The main overall objective of the action is to concentrate on the contribution of wood durability on the sustainability through the development of systems for quality assurance and perfoamance of modified wood and wood products as alternatives to wood treated with traditional preservatives. By this means it seeks to improve and consequently increase the cost-effective use of sustainably produced E...
R-D Peek


Novel wood modification processes for window and cladding products
2004 - IRG/WP 04-40285
Because of the low natural durability and low dimensional stability of European wood species, the usage of wood for window frames has decreased dramatically during the last decade. In a joint project of several German research institutes and the window industry, following wood modification systems were compared. heat treatment (3 different materials from 2 companies) acetylation (pine sapwood an...
A Krause, C Hof, H Militz


Waste management of wood products in life cycle assessment
2000 - IRG/WP 00-50154
Within the framework of the European project LIFE SYS WOOD (contractnr. FAIR CT95-7026) TNO has performed a study on the waste management of wood demolition waste for inclusion in Life Cycle Assessment. In LIFE SYS WOOD one of the main aims was to develop a consistent LCA methodology for wood products. LCA case studies have been performed by partners on wood as raw material, glulam contructions, O...
P Esser, P Eggels, A Voss


Vapour boron treatment of wood based panels: Mechanism for effect upon impact resistance
1994 - IRG/WP 94-40036
Samples of medium density fibreboard, chipboard and oriented strandboard (OSB) were treated to two retentions of boric acid by a vapour phase treatment. The results of a range of mechanical tests were reported by Hashim et al. (1992, 1993) in which a small reduction in impact resistance was observed. Several investigations were carried out to study how and where this loss in impact resistance occu...
R Hashim, R J Murphy, D J Dickinson, J Dinwoodie


Health and safety aspects of the use of wood preservatives in Sweden
1977 - IRG/WP 396
The Act on products Hazardous to Health and to the Environment (Swedish Code of Statutes SFS 1973:329) came into force on 1st July 1973. The Act cancelled and superseded the Poison Act, the Pesticides Act and the PCB Act from 1962, 1962 and 1971 respectively. Regulations for the implementation of the Act are contained in the Ordinance on Products Hazardous to Health and to the Environment (SFS 197...
B Henningsson


Risk reduction from curative treatments, restoration and maintenance of building and individual housing - simple precautions that make the difference
2005 - IRG/WP 05-50224-15
This document explores the potentialities of risk reduction, from activities of remediation in construction, developped at small scale by professionals or individuals on targets like moulds, rots, termites and other wood destroying insects, with products distributed for professional or do-it-yourself purposes. At the first stage, an inventory of the type / interest of products / processes is carri...
G Ozanne


Performance of copper-based wood preservatives in above ground and ground contact tests
1994 - IRG/WP 94-30057
The relative performance of a range of copper-based wood preservatives was compared using above ground and ground contact procedures. The data, accumulated after several years' testing, show that on an equivalent active ingredient basis, differences in performance of the preservative systems tested can vary quite markedly. The contribution of co-biocides to the overall performance of thes...
A F Preston, K J Archer, L Jin, W Metzner, D Seepe


Assessment of the toxicity of some copper-, zinc- and boron-based wood preservatives to the cellar fungus Coniophora cerebella Schröet
1974 - IRG/WP 242
This article reports the use of a method based on the determination of the probability of the protection of timber against destruction by fungi. By converting the probability values to probit values and plotting them as a function of the amount of preservative retained in the timber, curves of the toxic effect are obtained, enabling any timber protection probability to be assessed....
V N Sozonova, D A Belenkov


Experiences with penetration of copper-based wood preservatives
2001 - IRG/WP 01-20233
In the Nordic countries there is a long tradition of result type based specifications for preservative-treated wood. A common Nordic standard for treated pine (Pinus sylvestris) wood was published in 1976. After a revision in 1989 this standard, then named INSTA 140, defined four classes of treated wood: M, A, AB and B. Treaters producing according to this standard had to be affiliated to a qualit...
J Jermer, F G Evans, I Johansson


Copper leaching from Kemwood ACQ and Embalit CBC treated wood products
2000 - IRG/WP 00-50150
TNO has performed a study on the leaching of copper from Kemwood ACQ and Embalit CBC treated wood products, further referred to as ACQ and CBC. The sawn dry wood has been impregnated using an industrial vacuum-pressure process with ACQ (with or without Ultrawood 4) or with CBC, under supervision of Flexchemie B.V. After treatment samples have been transported and subjected to leaching tests at TNO...
P Esser, W L D Suitela, H Trompetter


Wood-based composites exposed to fungal degradation: Laboratory results
2001 - IRG/WP 01-40215
Oriented strandboard (OSB) and laminated veneer lumber (LVL) are widely used as residential construction materials. The durability of OSB and LVL against biological degradation has not been studied comprehensively. The objective of this research was to investigate the durability of OSB and LVL when exposed to wood decay fungi. Fourteen brown-rot and eight white-rot wood decay fungi were screened f...
V W Yang, B Illman, L A Ferge, R J Ross


Contradiction between uptake of preservative in practical situation and laboratory testing
1992 - IRG/WP 92-2392
By brush treatment water- and solvent-based products were applied on boards of Scots pine and Norway spruce to achieve an uptake of 100 and 200 g/ml. In addition the scope of work to achieve the required uptake of preservative was determined under practical conditions for both product groups. EN 113 (RAL-GZ 830) tests were carried out to test the biological efficacy of products. After 18 months ex...
R Gründlinger, O Janotta, M Melzer


The implementation of restrictions on the use of arsenic and chromium based wood preservatives in Sweden
1995 - IRG/WP 95-50062
In 1992 the Swedish National Chemicals Inspectorate introduced restrictions on the use of wood treated with arsenic and/or chromium based wood preservatives. Such wood is now in principle only allowed for use in ground contact or in water. These restrictions have had considerable influence on the use of wood preservatives for sawn timber for the Swedish domestic market. Thus only 35% of the preser...
J Jermer, M-L Edlund, K Nilsson


Distinguishing isolates of Aureobasidium on the basis of their ability to utilise lignin breakdown products as a sole carbon source
1996 - IRG/WP 96-10151
Wild isolates of Aureobasidium were obtained by dilution plating from a ca 20 year old painted pine window frame. Four isolates were obtained from the paint/wood interface region and four isolated from regions deep in the wood. The isolates were then used to inoculate liquid cultures containing ferulic acid, a lignin breakdown product, present as the sole carbon source. Ability of the isolates to ...
M W Schoeman, D J Dickinson


Serpula lacrymans, The Dry Rot Fungus and its Tolerance towards Copper-based Wood Preservatives
2005 - IRG/WP 05-10555
Serpula lacrymans (Wulfen : Fries) Schröter, the dry rot fungus, is considered the most economically important wood decay fungus in temperate regions of the world i.e. northern Europe, Japan and Australia. Previously copper based wood preservatives were the most commonly used preservatives for pressure treatment of wood for building constructions. Because of a suspicion about tolerance toward cop...
A C Steenkjær Hastrup, F Green III, C A Clausen, B Jensen


Observations on the performance of copper-based wood preservatives in fungal cellar (soil-bed) tests
1994 - IRG/WP 94-20047
Fungal cellar (soil-bed) tests are considered to be an important tool for the evaluation of the performance of ground contact wood preservatives. Facilities of this type have been established world wide although caution has been exercised in their introduction into standard testing methods for the approval of wood preservatives. This is the result of concerns over the variability in the biological...
G R Williams, D Rudolph, M E Hedley, J A Drysdale, R F Fox


Risk assessment of energetic valorization of treated wood - wooden recycling
1996 - IRG/WP 96-50072
The most useful method for the valorization of wood wastes and wooden wastes is energetic valorization. In France the percentage of wood treated by antisaptain products is around 30%. Currently with the growing regulation, there is a need for cleaner methods and technology to allow sustainable valorization. The preservatives concerned are common organochlorine compounds (NaPCP) less used nowadays ...
G Deroubaix, P Marchal, G Labat


Environmental fate of copper-based wood preservatives in different soil substrates - Part 2: Study of the metal sorption and migration potential under simulated rainfall
1998 - IRG/WP 98-50101-21 b
In order to examine the potential environmental impact of spillages of the saltborne wood preservative CCA in treatment plants, four large scale experiments are set-up so as to follow the water transport and ion mobility in various field soils. A plastic container is filled with a sand, silt, clay and potting soil, made up at their respective bulk density and wetted to a given moisture content. U...
G M F Van Eetvelde, R Hartmann, J M Mwangi, H S Öztürk, M Stevens


Pest control products act. An overview of regulation of heavy duty wood preservatives
1995 - IRG/WP 95-50040-30
The regulation of pesticides in Canada is carried out under the authority of the Pest Control Products Act and Regulations. Products which control, prevent, destroy, mitigate, attract or repel a pest are required to undergo a presale assessment for safety, merit and value. This review will determine whether a product, when used according to label directions, can be used both safely and will be eff...
K McCullogh


The EWPMG proposal for the environmental risk assessment of wood preservatives
2001 - IRG/WP 01-50166-09
This paper reviews the protocol prepared by the European Wood Preservative Manufacturer's Group, which could be used by an applicant for product approval under the Biocidal Products Directive 98/8/EC, to produce a risk assessment for an active substance or product in the Product Type 8 Wood Preservatives, in support of the application. The background and scope of the protocol are reviewed...
E F Baines


A field method for determining the above-ground resistance of wood and wood products to attack by subterranean termite
1994 - IRG/WP 94-20035
A method for determining the above-ground resistance of wood and wood products to subterranean termites in the field is described. Termites are aggregated in 20-litre steel drums, each containing a highly susceptible timber substrate. At the centre of each drum, specimens of the test material under evaluation are sandwiched, using circular sections of wire mesh, between two layers of the substrate...
J W Creffield


Effectiveness of the new chemical wood preservative Borosol 9? against a house longhorn beetle Hylotrupes bajulus
2004 - IRG/WP 04-30355
Chemical wood preservative Borosol 9, consisting of boric acid - alkanolamine complex, is a new wood preservative with proven efficacy against wood decay fungi. However, we were interested in its efficacy against larvae of house longhorn beetle (Hylotrupes bajulus). Thus, experiment according to the EN 46 procedure was performed. Specimens made of Norway spruce wood (Picea abies) were ...
G Babuder, M Petric, F Cadež, M Humar, F Pohleven


Tolerance of Wood Decay Fungi to Commercial Copper Based Wood Preservatives
2002 - IRG/WP 02-30291
Due to the use of copper based preservatives like CCB or CCA for more than a century, copper tolerant fungi have appeared in some European countries in recent times. It is therefore important to find out whether this phenomenon is specific for only classical copper ingredients, or generally for all copper based formulation. Thus, we tested the tolerance of three commercial copper based pres...
F Pohleven, M Humar, S A Amartey, J Benedik


Previous Page | Next Page