Über Wespen als Holzverderber - Schäden, Ursachen, Bekämpfung
1978 - IRG/WP 189
Observations and a number of actual cases over recent years show that wasps have been associated more frequently with damage to wood. The nature of such damage and the agents involved are as follows: 1. Decay following infestation by Woodwasps (Siricidae). 2. Punctate marks caused by superficial gnawing and also boring into wood by larvae of the Dock sawfly (Tenthredinidae). 3. Damage due to super...
S Cymorek


The Ninth Annual Report of the International Research Group on Wood Preservation 1978-1979
1979 - IRG/WP 579
IRG Secretariat


Working Group I 'Biological Problems' Sub-group 'Insects in dry wood (other than termites)', Scope of work
1976 - IRG/WP 152
S Cymorek


Some aspects of laboratory and field testing methods of antitermite wood preservatives
1973 - IRG/WP 235
Various methods for laboratory testing of antitermite activity of wood preservatives are described. The results of simultaneous tests of three water-borne preservatives, according to the various methods are discussed, and comparison is made with results of field tests on the same three preservatives, showing a fairly good accordance between laboratory results and field results....
M Fougerousse


Assessing the risks from the use of wood preservatives
2001 - IRG/WP 01-50166-07
PPT-Presentation...
C B Welch


A new wood preservative based on polymerized complexes of aminotriazole with copper acetate
1998 - IRG/WP 98-30169
This paper presents the results of preliminary fungitoxicity tests as carried out on new polymerized complexes of aminotriazole with copper acetate (PCC) against Coniophora puteana and Trichoderma viride. Laboratory tests on wood confirmed the findings arrived at in the screening test on agar medium. Deep penetration into pine wood of compounds studied was observed and particularly so at humidity...
K J Krajewski, A Lukasiewicz, J Wazny


Resistance of the wood of Eucalyptus saligna and Paulownia tomentosa against some wood rotting fungi
1997 - IRG/WP 97-10238
Paulownia tomentosa and Eucalyptus saligna are not autochthonous species in Slovenia and we determined the resistance of their wood against our most common wood rotting fungi. The resistance against Coniophora puteana, Gloeophyllum trabeum and Trametes versicolor was determined according to EN 113 and compared to the resistance of beech (Fagus sylvatica) wood. It was stated, that both paulownia an...
F Pohleven, M Petric


An attempt to evaluate wood resistance against fungal decay in non-sterile conditions by measuring the variation of resistance to bending test
1988 - IRG/WP 2308
The main object of this work was to determine the variation of strength on large test specimens of wood (800 x 45 x 45 mm³) when exposed to accelerated fungal attacks close to natural conditions, out of test vessels. The modulus of elasticity (MOE) and the modulus of rupture (MOR) have been assessed. Thereby, the natural resistance of the wood species to fungal decay, the efficiency of preservati...
L N Trong


Determination of the preventive efficacy against wood destroying basidiomycetes fungi, EN V 839 - CEN/TC 38 WG 9
1993 - IRG/WP 93-20015
The WG 9 of CEN TC/38 has presented to EC a mycological test to assess efficacy of preservatives applied by surface process. This method is now an experimental standard (EN V 839) which has to be approved by the different european delegations. The following paper is not the standard as it has been proposed but is a presentation of the principle of the method. The experimental standard specifies a ...
D Dirol


The Tenth Report of the International Research Group on Wood Preservation 1979-1980
1980 - IRG/WP 5110
R Cockcroft


Studies on the infestation behaviour of the powder-post beetle Lyctus brunneus (Steph.) and its physical control in the wood yards of the Caspian forests of Iran
1985 - IRG/WP 1271
Lyctus brunneus (Steph.) is a pest which has not been previously thoroughly studied in Iran. It severely attacks Iranian hardwoods, especially those used in wooden houses and that have not been treated. Research work was necessary to determine the natural resistance of the most important timber species in Iran against this insect....
P Niloufari


The Sixth Annual Report of the International Research Group on Wood Preservation 1974-1975
1975 - IRG/WP 541
IRG Secretariat


Wood Preservation in France. A statement of quality control early 1986
1986 - IRG/WP 3389
A statement of quality control in France early 1986 - Summary of new - Standards criteria for preservatives and treated wood - Aptitude of treated wood for use per class of biological hazard...
M Romeis, G Ozanne


Eco-tax - A new threat for wood preservation? The Belgian experience
1993 - IRG/WP 93-50001-32
At the end of January 1993, a bill was put for Belgian Parliament related to the introduction called "Eco-taxes" on a series of products, such as packaging for drinks (especially on PVC-bottles), non-returnable articles (shavers, small cameras), batteries, pesticides for non-agricultural use and paper....
G Van Steertegem, F De Jaeger


Gloeophyllum trabeum and Gloeophyllum abietinum, the most frequent brown rot fungi in fir wood joinery
1999 - IRG/WP 99-10319
In Croatia the primary raw material for joinery production is silver fir wood (Abies alba Mill). L-joints made of home-grown fir sapwood and prepared according to EN 330: 1993 were used to establish the infection and colonisation of micro-organisms, particularly wood decay fungi, to compare the performance of untreated and 1% TnBTO treated L-joints. The L-joints were coated with two types of coat,...
R Despot, M Glavas


Japanese wood preserving industry
1990 - IRG/WP 3596
Although a great amount of wood is in use in Japan, a little attention has been paid to the significance and importance of wood preservation. The fact reflects that only less than 0.5% of the total wood consumption is treated with wood preservatives today in the country. Over the 20 years before 1970, the annual volume of preservative treated (pressure treatment) wood was relatively at a stable le...
K Tsunoda


Water-based wood preservatives for curative treatement of insect-infested spruce constructions
1998 - IRG/WP 98-30171
On laying down sanitation measures for wooden constructions infested by wood boring insects, we must take into account static risks for the construction - and, thus, for the security of the user - as well as risks for humans and environment due to the chemical preservative compounds of the treated wood. Analyses on many roof constructions made with spruce (Picea abies L.) have revealed that Hylot...
E Graf, P Manser, B Lanz


The resistance of painting materials and consolidants against wood-destroying insects
1997 - IRG/WP 97-10239
Natural and synthetic adhesives, varnishes, painting materials and consolidants were used in investigations of bioresistance against newly hatched larvae and beetles of Hylotrupes bajulus (L.). Animal glues, casein, drying oils and natural resins such as dammar resin and shellac, were not resistant to attack by these larvae. Similarly, semi- and all-synthetic polymers tested including hydroxypropy...
W Unger, H Fritsche, A Unger


Possibility of use of wood species per class of biological risks. Attempt to determine criteria based on Pr EN 350-1/2/3
1992 - IRG/WP 92-2409
M Rayzal


New technique for inoculation of wood wafers with fungi
1997 - IRG/WP 97-20113
A pilot study is described for determining the best possible method for inoculating fungi onto the surface of wood wafers for sapstain control studies. Direct inoculation and spray inoculation are compared on water soaked and malt extract broth soaked wood wafers. The best growth of fungal hyphae across the surface of the wood wafers was achieved following spray inoculation onto malt extract broth...
J Snow, P Vinden


Contribution to the testing of wood based board material
1982 - IRG/WP 2176
R G Lea


Wood preservation in the USA
1982 - IRG/WP 3215
This report is a comprehensive survey of the status of the wood preservation field in the U.S.A. at the start of the 1980s. The importance of wood preservation is discussed and its industry described. Various statistics and analyses regarding the use of treated wood have been compiled. Both pressure and non-pressure applications have been covered, as well as remedial treatments and pest control op...
D D Nicholas, R Cockcroft


Inventory of the use of preservative-treated wood and wood preservatives in Sweden 1900-1997
1999 - IRG/WP 99-50137
The objective of this study was to present an overview of the use of wood preservatives and their active ingredients and industrially preservative-treated wood in Sweden since the beginning of the 20th century. The data presented in the report could for example be used as a basis for different waste management scenarios for preservative-treated wood. Before 1960 railway sleepers and utility poles ...
J Jermer, K Nilsson


Short-term field test method with accelerated infection of Basidiomycetes in wood
1981 - IRG/WP 2155
In the ŠIPAD - IRC Wood Protection Laboratory an attempt has been made to develop a simple short-term method for field testing out-of-ground contact wood using accelerated infections with Basidiomycetes. This method makes it possible to obtain a preliminary assessment of a preservative's quality and to estimate the possibility of achieving promising results in more expensive long-term te...
N Vidovic


Vertical distribution of fouling and wood-boring organisms in the Trondheimsfjord (Western Norway)
1981 - IRG/WP 467
Results of a detailed study on the vertical distribution of fouling and wood-boring organisms of Trondheimsfjord at an interval of 3 m from intertidal level to a depth of 30 m, has been presented, based on data collected from two series of panels, exposed from 15 March 1977 to 15 July 1977 (Series I) and from 22 July 1977 to 13 March 1978 (Series II). The intensity of fouling generally decreased w...
L N Santhakumaran