IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 3027 documents. Displaying 25 entries per page.


Evaluation of fungal remediation of creosote treated wood
1998 - IRG/WP 98-50101-25
Biotechnological remediation of creosote treated wood may be of interest in connection with novel recycling processes. White rot fungi and/or their ligninolytic enzyme systems are supposed to be valuable tools for such processes. This paper reports about results achieved when creosoted wood was treated in solid substrate fermentation with selected white rot fungi after different extraction procedu...
K Messner, S Böhmer


Evidence for wood cell wall degradation by the blue stain fungus Botryodiplodia theobromae Pat
1994 - IRG/WP 94-10077
Botryodiplodia theobromae Pat., a world wide ubiquitous polyfagus sapstain fungus, was found able to destroy the cell walls of birch fibres (Betula verrucosa Ehrh.) but not Caribbean (Pinus caribaea var. hondurensis Barr. and Golf.) and Scots pine (Pinus sylvestris L.) tracheids. The fungus caused characteristic erosion of fibre cell walls similar to soft rot type 2; destruction of the S1 - S2 int...
O Encinas, G F Daniel


Low-toxicity DNBP wood preservatives
1987 - IRG/WP 3408
Low and very low toxicity single compound preservatives of both excellent insecticidal and fungicidal activity for interior, extrior and ground-contact applications are presented. These are ester derivatives of alkyl dinitrophenols, in particular of 2-sec-butyl-4,6-dinitrophenol (DNBP) and 2-sec-octyl-4,6-dinitrophenol. These esters, of much lower toxicity than DNBP impart to the treated timber co...
A Pizzi, W E Conradie, A Jansen, R Vosloo


Some data on the activity of alternative fungicides for wood preservation
1985 - IRG/WP 3333
Data from laboratory tests against basidiomycete fungi are presented for 9 alternative fungicides in organic solvent formulations and also in water for one product. Results are compared with data for reference preservatives, tributyltin oxide, copper and zinc naphthenates and pentachlorophenol. Of special interest is the apparently better than additive effect of mixing tributyltin naphthenate and ...
A F Bravery, J K Carey


Influence of pre-swelling conditioning on swellometer results for CCA and water repellent additive treated wood
1997 - IRG/WP 97-20125
The pre-test moisture content and conditioning history of wafers cut from wood treated with CCA and an emulsion water repellent additive can dramatically influence swelling curves generated using a standard swellometer apparatus. The rate of water uptake and swelling increased significantly as wafers were dried to lower moisture contents prior to immersion swelling. The pre-swelling conditioning h...
A R Zahora


A technique for determinging the efficacy of wood preservatives for partially treated timber
1988 - IRG/WP 2322
A technique is described for determining the efficacy of wood preservatives either for certain wood species where a full penetration cannot be achieved by normal vacuum-pressure methods or for more permeable species to look at efficacy of treated zone in preventing decay of an untreated core. Both sapwood and heartwood planks of spruce (Picea abies) and pine (Pinus sylvestris) were treated by CCA ...
A J Nurmi


A comparison of inductively coupled plasma spectroscopy and neutron activity analysis for the determination of concentrations in wood
1993 - IRG/WP 93-10048
As wood decays the ionic composition changes, with increases often being seen in the concentrations of Ca, Mg, Fe, Mn and sometimes K. The concentration of eight cations in red spruce sapwood and heartwood samples was determined independently by inductively coupled plasma spectroscopy (ICP) and by neutron activation analysis (NAA) as part of an effort to standardize our analytical procedures and c...
J Jellison, J Connolly, K C Smith, W T Shortle


The new National Directive on wood preservation in the Netherlands
1998 - IRG/WP 98-50101-03
In the Netherlands the major part of treated timber is sold under the KOMO-certificate. The National Directive for vacuum pressure treated timber on which certification is based, is currently being revised. The new National Directive will contain a code of good practice including maximum leaching figures. It incorporates quality requirements for treated timber, existing legislative requirements an...
W J Homan, J K B Kwisthout, J Dubelaar


Volatile losses of wood preservatives
1973 - IRG/WP 236
The purpose of the work we have undertaken so far has been to try to quantify the volatile losses which occur in treated timber, and to examine some of the factors which influence these losses. The preservative compound chosen for the initial part of the programme was the contact insecticide g-BHC. This was attractive for several reasons, not the least of which was that specific and sensitive anal...
J W W Morgan, D F Purslow


Evaluation of the corrosivity of the treated wood - Laboratory vs field test methodologies
2000 - IRG/WP 00-20211
The corrosivity of treated wood to fasteners has been evaluated using laboratory test procedures, including AWPA Standard E12-94. The standard method was modified in order to allow detailed study of commercial metal fasteners in terms of sample types, installation configuration and exposure conditions. Parallel field tests were also performed. The experimental results generated from these tests su...
L Jin, A F Preston


Attractive factors of steam-treated larch wood to termite feeding
1998 - IRG/WP 98-10256
The hot water extractives from steam-treated Japanese larch wood were studied to understand the chemical properties of attractive factors of the treated wood to feeding behavior of a subterranean termite, Coptotermes formosanus. Hot water extractives were fractionated and analyzed using chromatography, gel filtration, and NMR methods. The stimulants yielded by the steam treatment were comprised o...
S Doi, Y Kurimoto, W Ohmura, M Aoyama, S Ohara


A new method for the study of microbiological decay of wood in a strictly anaerobic environment
1988 - IRG/WP 2319
Recent work has suggested that strictly anaerobic bacteria may play a role in the biodeterioration of wood, particularly in aqueous environments. However, no suitable test methods exist for the investigation of this hypothesis. An aqueous minimal medium in specifically adapted conical flasks was sterilised, gassed using a 5.5% H2; 31.8% C02; 62.7% N2 gas mixture to remove oxygen and transferred to...
G M Rogers, A A W Baecker


Management of treated wood waste in Canada - Technical and regulatory solutions
2001 - IRG/WP 01-50166-15
A major problem facing the wood preservation industry in Canada is the management of wastes. This refers to wastes generated during the treatment process as well as waste treated wood that is removed from service. The volume of oil borne preservative treated industrial products to be removed from service in Canada over the next 20 years is expected to be fairly constant at approximately 350,000 to...
B Munson


Copper leaching from Kemwood ACQ and Embalit CBC treated wood products
2000 - IRG/WP 00-50150
TNO has performed a study on the leaching of copper from Kemwood ACQ and Embalit CBC treated wood products, further referred to as ACQ and CBC. The sawn dry wood has been impregnated using an industrial vacuum-pressure process with ACQ (with or without Ultrawood 4) or with CBC, under supervision of Flexchemie B.V. After treatment samples have been transported and subjected to leaching tests at TNO...
P Esser, W L D Suitela, H Trompetter


Natural exposure weathering tests: Their role in the assessment of wood preservative efficacy
1993 - IRG/WP 93-20006
Previous work has demonstrated the potential and usefulness of natural ageing procedures in e evaluation of wood preservative efficacy. This results from the combination of physico-chemical influences and microbiological interactions with both substrate and wood preservative. In this paper, results are presented for a range of biocide types. Discussions are centred on the value of natural exposure...
G R Williams, J Brown


Using DNA probes to characterize the metabolic pathway of pigment production in several wood-staining fungi
1996 - IRG/WP 96-10146
During shipment and storage, lumber is susceptible to sapstain, a wood discoloration caused by fungi. Currently kiln drying and chemical applications are used to control sapstain. However, the chemicals used to protect wood have a broad range of action, and so can affect other organisms. In addition, in Canada most of these chemicals are under temporary registration. Thus there is a need to develo...
R Eagen, S Riecken, J Kronstad, C Breuil


In vitro sporulation of selected wood decay fungi
1978 - IRG/WP 190
Basidiospores produced axenically without laborious attention in the laboratory are useful in studies of wood decay initiation. Such spores presumably approach those collected from natural sporophores in size and germinability (Morton, 1964). Production of spores in vitro by inversion of cultures grown on 2% malt extract agar in deep glass dishes (100x80 mm²) has been the preferred method (Morton...
E L Schmidt, D W French


Wood extractives as carbon sources for staining fungi in the sapwood of lodgepole pine and trembling aspen
1995 - IRG/WP 95-10098
Wood discoloration by sapstaining fungi reduces lumber value. In Canada, the most commonly recorded sapstaining fungi belong to the genera Ophiostoma. This work evaluated the effect that Ophiostoma piceae, Ophiostoma ainoae, and Ophiostoma piliferum used the lipids present in the sapwood of lodgepole pine (Pinus contorta Dougl.) and trembling aspen (Populus tremuloides Michx.). Wood lipids, common...
Yong Gao, C Breuil


Further thoughts on standard principles of testing termiticides and/or wood preservatives
1992 - IRG/WP 92-1530
At the last annual meeting in Kyoto, Japan, there was a special session devoted to the standard principles of testing termiticides. There was definitely a perceived need by researchers and industry for some guidelines that spell out basic procedures required for any methodology in testing termiticidal formulations anywhere in the world. In the testing of new potential active ingredients, considera...
J R J French


Moisture requirements and wood degradation of pine and spruce wood by some Basidiomycetes-fungi
1989 - IRG/WP 1406
The minimum moisture requirements for the growth of the brown rot fungi, Coniophora puteana, Gloeophyllum trabeum and Serpula lacrymans were near or above the fibre saturation point of pine and spruce, sap and heartwood, during 160 days incubation according to the standard method EN 113. The moisture of wood for the optimum growth of Coniophora puteana and Serpula lacrymans was about 35-80% and fo...
H Viitanen, A-C Ritschkoff


Treatability problems - Relationships between anatomy, chemical composition and treatability
2001 - IRG/WP 01-40213
This report documents the results of phase 1 and 2 of a 3-phase research program. In phase 1, two hundred and fifty-six (256) Southern pine (pinus spp.) nominal 2 x 6's (38 mm x 140 mm) from a single mill in Georgia (southeastern US) were evaluated for treatability with CCA preservative. After treatment, 128 pieces representing a broad range of treatment characteristics were selected and ...
J E Winandy, F Green III, D Keefe


Wood preservation in Kenya
2000 - IRG/WP 00-40190
Focussing an Wood Preservation in Kenya, the Report discusses and elaborates on Education and Training, Research, Wood deteriorating organisms, Treatment Plants and Processes, Preserving Chemicals, Specifications, Markets, Health and Safety and Environmental issues. Education and Research is limited to one Institution only, other Institutions involved with the properties and utilization of wood ha...
R Venkatasamy


Durability of Wood Plastic Composites Relative to Natural Weathering and Preservative Treatment With Zinc Borate
2005 - IRG/WP 05-40316
Wood-Plastic Composites (WPCs) used for decking have experienced dramatic increases in North America, averaging 25% growth per annum since 1998. A key factor contributing to this growth has been the successfully communicated message that they are "virtually maintenance free". The common perception being that the wood fiber is completely encapsulated by the thermoplastic resin, minimizing the pot...
M E Mankowski, F M Ascherl, M J Manning


Formation of soft rot cavities in relation to concentric layers in wood fibre walls
1983 - IRG/WP 1185
A large number of timber species attacked by soft rot have been examined using light microscopy. The S2 layers in a large number of the timbers exhibited special structural features in the form of thin concentric layers. Several observations indicate that these layers may be characterised as "weak" zones by being more easily degradable than the surrounding wall layers. The chemical structure of th...
T Nilsson, G F Daniel


Correlation between changes in colour and chemical composition during photo-degradation of wood surfaces
2005 - IRG/WP 05-40301
Changes in colour of wood (yellowing) during photo degradation or weathering reflect chemical changes in wood. Therefore, the relationship between changes in chemical composition and CIELAB colour parameters is very important to characterize photodegradation of lignocellulosic surfaces. In this study, the changes in chemical composition and yellowing due to photo-degradation was studied by expos...
K K Pandey


Previous Page | Next Page