Evaluation of the effectiveness of three microbiocides in the control of sapstains
1982 - IRG/WP 3212
Results of field test on the effectiveness of BUSAN 30, CAPTAN, FOLPET against mould and sapstain in Pinus elliottii are presented. The viability of use of FOLPET in Brazil as an alternative to sodium pentachlorophenate is also discussed....
S Milano, J A A Vianna Neto


Natural durability transfer from sawmill residues of white cypress (Callitris glaucophylla). - Part 3: Full penetration of the refractory sapwood of white cypress
2000 - IRG/WP 00-40167
The heartwood of white cypress, Callitris glaucophylla, is renowned for its termite resistance and durability against decay. The sapwood, which can represent up to 30% of log volume, is non-durable and refractory to conventional preservative treatment. Previous work ascribes the lack of permeability to oily deposits within tracheids and ray cells. Environmental scanning electron microscopy was use...
M J Kennedy, L M Stephens, M A Powell


Interspecific variability of European oak durability against white rot fungi (Coriolus versicolor): Comparison between sessile oak and peduncle oak (Quercus petraea and Quercus robur)
2001 - IRG/WP 01-10393
The knowledge of wood natural durability against biologic predators enable its external use. The resistance of European oak wood was reported like durable according to the EN 350-2. However, some individuals may contain high durable wood. Our research was focused to understand this variability in oak population that represent the first french species (4.1 millions of ha). Natural durability of Eur...
N Ayadi, B Charrier, M Irmouli, J P Charpentier, C J Allemand, F Feuillat, R Keller


Physical and biological properties of albizzia waferboards modified with cross-linking agents
1995 - IRG/WP 95-40043
Chemically-modified low-density waferboards with cross-linking agents were produced using a fast-growing species of hardwood albizzia (Paraserienthes falcata Becker) as a raw materials and isocyanate resin as a glue adhesive. For the chemical modification, the vapor-phase formalization of the boards and the pad-dry-cure treatment of wafers with cross-linking agents were employed. The vapor-phase f...
S Yusuf, Y Imamura, M Takahashi, K Minato


Rapport sur l'activité du CNE/TC 38 'Méthodes d'essais des produits de préservation du bois'
1980 - IRG/WP 279
G Castan


Blue stain in timber in service. Results of co-operative tests to compare different artificial weathering systems 1981-82
1983 - IRG/WP 2193
The paper describes results of the third phase of co-operative laboratory experiments comparing the effects of different artificial weathering systems on chemicals to control blue-stain in service. Atlas, Xenotest and Marr equipments are shown to give essentially the same results for 5 of the 6 chemicals tested....
A F Bravery, D J Dickinson


Rapport sur l'activité du CEN/TC 38
1983 - IRG/WP 2204
M Pottevin


Working Group II: Sub-group: Methods of testing anti-stain chemicals for protecting sawn lumber during storage, transit
1978 - IRG/WP 2121
R Smith


Extracellular layers of wood decay fungi and copper tolerance
1983 - IRG/WP 1180
Extracellular layers around the hyphae of brown, white and soft rot fungi have been examined using electron microscopy. These layers were isolated for identification. Particular interest was directed towards the extracellular layers of copper-tolerant soft rot fungi....
D M Francis, L E Leightley


Proposed standard laboratory method for testing fungicides for controlling sapstain and mould on unseasoned lumber
1977 - IRG/WP 292
This laboratory method is for determining the effective concentration, or concentration for zero growth (CGo), for fungicides or preparations of fungicides which are potentially useful in protecting packaged or unseasoned lumber in storage and shipment from biodeterioration by sapstain fungi and moulds. The test is rapid and may be completed in three weeks and gives a good indication of the toxici...
A J Cserjesi


Tebuconazole, a new wood-preserving fungicide
1990 - IRG/WP 3634
TEBUCONAZOLE, an anti-fungal triazole compound, has been tested to assess the effectivness as wood preserving fungicide. Tests were made with the active ingredient and also in formulations against basidiomycetes, blue-staining fungi and mould. Results of the DESOWAG laboratories and also from official institutes will be presented. In addition to this there were made different toxicological and eco...
B Wüstenhöfer, H-W Wegen, W Metzner


Basidiosporogenesis by the white-rot basidiomycetes in vitr
1994 - IRG/WP 94-10081
Basidiospores of all forest-inhabiting basidiomycetes are a primary source of infection causing wood decay. However, most studies evaluating wood preservatives have used mycelia or basidiospores obtained from wild mushrooms. The objective of this study was to demonstrate in vitro methods that promote carpogenesis and basidiosporogenesis by the white-rot basidiomycetes, Schizophyllum commune and Tr...
S C Croan


Blue stain in service on wood surface coatings. Part 2: The ability of Aureobasidium pullulans to penetrate wood surface coatings
1992 - IRG/WP 92-1557
The ability of Aureobasidium pullulans to penetrate seven different wood surface coatings was examined. Eight isolates of Aureobasidium pullulans were used. Following penetration, light microscopy was used to examine the effect of the fungus upon the coating, and growth at the wood-film interface. The fungus showed different growth capabilities with different types of surface coatings. Some isolat...
P R Sharpe, D J Dickinson


Electron microscopic detection and chemical analysis of three-lamellar structures in wood-destroying fungi
1984 - IRG/WP 1240
In the course of transmission electron microscopical investigations of pine wood decay by various brown- and white-rot fungi extracellular three-lamellar structures (TLS) formed by the fungi were found in specimens stained with ruthenium red. These structures occured in the lumen of the wood cell surrounding the hypha at the outermost layer of the fungal cell wall. In the course of the investigati...
R Foisner, K Messner, H Stachelberger, M Röhr


Rapport sur l'activité du Comité CEN/TC 38 "Méthodes d'essais des produits de préservation des bois" du Comité Européen de Normalisation (CEN)
1986 - IRG/WP 2266
G Castan


Rapport sur l'activité du CNE/TC 38 'Méthodes d'essais des produits de préservation du bois'
1977 - IRG/WP 288
G Castan


Observations on the penetration of preservatives into green timber
1985 - IRG/WP 3335
Differences in the rate and extent of diffusion of MBT and NaPCP-based preservatives following a short dip treatment were observed. The importance of preservative distribution as well as toxicity to the target organisms in governing the ultimate performance of any anti-sapstain compound is discussed....
G R Williams, R A Eaton, D A Lewis


Methodology challenges in developing a transfer of natural durability from sawmill residues, illustrated by experiences with white cypress (Callitris glaucophylla)
2000 - IRG/WP 00-20203
The transfer of durability-conferring extractives from durable to non-durable wood has been accomplished often, but usually as an educational exercise rather than as a commercially oriented process. In the latter environment, many factors previously overlooked become vitally important. How to study them, in the absence of well-developed methodology and given the shorter timeframes being demanded b...
M J Kennedy, M A Powell


Some physiological characteristics of a non-degradative strain of Postia (=Poria) placenta
1988 - IRG/WP 1341
The decay capacity of 14 strains of the brown-rot fungus Postia (= Poria) placenta was determined using soil-wood block tests. One isolate was identified as being unable to degrade wood and was determined to be monokaryotic. It retained the ability to produce extracellular carbohydrate-degrading enzymes, although regulation of certain enzymes was atypical under certain cultural conditions. It prod...
J A Micales, T L Highley


Movement of boron from fused boron rods implanted in Southern pine, Douglas fir, red oak, and white oak timbers
1995 - IRG/WP 95-30061
This paper reports the distribution of boron from fused boron rods installed into six-inch (15.2 cm) square timbers of Douglas-fir, Southern Pine, red oak and white oak exposed aboveground. The composition and size of rods was: sodium borate and sodium borate-copper oxide (8.5 x 100 mm²); sodium borate-copper, sodium borate and boric oxide-copper oxide (12 x 76 mm²). The boric acid equivalent wa...
T L Highley, L Ferge


Blue-stain fungi (Ceratocystis spp.) found in Spain on pine woods
1989 - IRG/WP 1410
So far, there is only a very limited reported description of the different Ceratocystis spp. present on fresh wood in Spain. So, the main goal of this work has been the identification of species of this genus causing blue-stain on Pinus pinaster A. Ait. and Pinus sylvestris L. woods. We have also investigated the relationship between the species found and their propagation vectors (insects and win...
M T De Troya, A M Navarrete


Final draft of a monographic card for Pole Fungus A, L Harmsen, Rigidoporus vitreus (Fr.) Donk according to the 'Model Questionnaire for preparation of monographic cards for wood-destroying fungi'
1978 - IRG/WP 178
L Harmsen


Antagonistic effect of some mycorrhiza fungi as biological control of blue-stain
1987 - IRG/WP 1314
This report discussed the possibility of using some mycorrhiza fungi as biological control of blue-stain. The results show that new bio-technological possibilities are opening, because, by cultivating antibiosis fungi in fermentor, it is possible to prepare extracts which can then be used as the natural preservative to control the blue-stain in wood....
R Benko


Micromorphology of the decay caused by Chondrostereum purpureum (Pers.:Fr.) Pouzar and Flammulina velutipes (Curt.:Fr.) Singer
1988 - IRG/WP 1358
Two basidiomycetes, Chondrostereum purpureum and Flammulina velutipes, form typical soft rot cavities in hardwoods and softwoods. Cavity formation is prececed by T-branching or bending of hyphae penetrating the wood cell walls. The two fungi also cause erosion of the wood cell walls....
T Nilsson, G F Daniel


Relationship between stacking, location and antisapstain preservatives on visible degrade of Eucalyptus regnans and Pinus radiata boards
1999 - IRG/WP 99-20162
An antisapstain trial was established at a Eucalyptus hardwood sawmill in Victoria, Australia. The trial incorporated two commercial formulations of antisapstain preservatives, used at four different concentrations on both hardwood (Eucalyptus regnans F. Muell) and softwood (Pinus radiata D. Don) boards. The trial also utilised different stacking methods (block-stacked, sticker-stacked, and block-...
J Snow, P Vinden, S M Read