Spruce lumber treatments with ammoniacal solutions of inorganic preservatives
1977 - IRG/WP 391
As a part of our work in the Wood Preservation group at the Eastern Forest Products Laboratory in Ottawa to facilitate exploitation of spruce, which is a large timber resource in Canada, we have been studying the treatability of spruce roundwood. A report on this subject was presented to this group last year. More recently, another commodity - spruce timber - has been rapidly gaining the interest ...
R Rak


Physical and biological properties of albizzia waferboards modified with cross-linking agents
1995 - IRG/WP 95-40043
Chemically-modified low-density waferboards with cross-linking agents were produced using a fast-growing species of hardwood albizzia (Paraserienthes falcata Becker) as a raw materials and isocyanate resin as a glue adhesive. For the chemical modification, the vapor-phase formalization of the boards and the pad-dry-cure treatment of wafers with cross-linking agents were employed. The vapor-phase f...
S Yusuf, Y Imamura, M Takahashi, K Minato


Micromorphology of the decay caused by Chondrostereum purpureum (Pers.:Fr.) Pouzar and Flammulina velutipes (Curt.:Fr.) Singer
1988 - IRG/WP 1358
Two basidiomycetes, Chondrostereum purpureum and Flammulina velutipes, form typical soft rot cavities in hardwoods and softwoods. Cavity formation is prececed by T-branching or bending of hyphae penetrating the wood cell walls. The two fungi also cause erosion of the wood cell walls....
T Nilsson, G F Daniel


Characterization of glycopeptide from white-, brown- and soft rot fungi
2002 - IRG/WP 02-10424
Extracellular low-molecular-weight substances that catalyze a redox reaction between O2 and electron donors to produce hydroxyl radicals have been isolated from wood degrading cultures of white-rot, brown-rot, and soft-rot fungi. They contained protein, neutral carbohydrate, and Fe(II). These substances were glycosylated (glycated) peptides and suggested to form Amadori product (ketoamine). The...
H Tanaka, S Itakura, A Enoki


Ibuprofen inhibits in vitro growth of brown-rot fungi
1996 - IRG/WP 96-10160
Ibuprofen, a phenyl propionic acid derivative (2-(4-isobutylphenyl)propionic acid) inhibited growth in vitro of 17 brown-rot fungi at a concentration of 100 µg/mL, while exhibiting no growth inhibition for 8 white-rot fungi at the same concentration. Propionic acid did not inhibit fungal growth in vitro. Morphological changes were noted in fungi that were able to grow in the presence of ibuprofen...
C A Clausen


Local preservation with difluoride pills: Life-time of preservative
1998 - IRG/WP 98-40127
A brief history of the situation in the Netherlands with respect to the preservation of joinery is given. Already in the eighties in the Netherlands many spruce window frames were treated with difluoride pills. One of the possible disadvantages of this kind of diffusing preservatives is the high leaching rate found in laboratory situations. The leaching rate in practice is influenced by many facto...
W J Homan, C Blom, B W Holleboom


Water-based wood preservatives for curative treatement of insect-infested spruce constructions
1998 - IRG/WP 98-30171
On laying down sanitation measures for wooden constructions infested by wood boring insects, we must take into account static risks for the construction - and, thus, for the security of the user - as well as risks for humans and environment due to the chemical preservative compounds of the treated wood. Analyses on many roof constructions made with spruce (Picea abies L.) have revealed that Hylot...
E Graf, P Manser, B Lanz


Basidiosporogenesis by the white-rot basidiomycetes in vitr
1994 - IRG/WP 94-10081
Basidiospores of all forest-inhabiting basidiomycetes are a primary source of infection causing wood decay. However, most studies evaluating wood preservatives have used mycelia or basidiospores obtained from wild mushrooms. The objective of this study was to demonstrate in vitro methods that promote carpogenesis and basidiosporogenesis by the white-rot basidiomycetes, Schizophyllum commune and Tr...
S C Croan


Electron microscopic detection and chemical analysis of three-lamellar structures in wood-destroying fungi
1984 - IRG/WP 1240
In the course of transmission electron microscopical investigations of pine wood decay by various brown- and white-rot fungi extracellular three-lamellar structures (TLS) formed by the fungi were found in specimens stained with ruthenium red. These structures occured in the lumen of the wood cell surrounding the hypha at the outermost layer of the fungal cell wall. In the course of the investigati...
R Foisner, K Messner, H Stachelberger, M Röhr


The influence of formulation on the behaviour of LOSP's during industrial impregnation of spruce
1986 - IRG/WP 3387
Evidence is presented that the comparative behaviour of two LOSP formulations during impregnation treatment of spruce cannot be predicted purely on the basis of their physical characteristics (viscosity, surface tension and contact angle) nor on the extent of their 'passive' penetration into pine sapwood....
L D A Saunders, D M Zuvencko


Defining fungal decay types - Final proposal
1988 - IRG/WP 1355
The term soft rot is proposed for all forms of decay caused by Ascomycetes and non-basidiomyceteous Fungi imperfecti. The terms brown rot and white rot should be used only for decay caused by Basidiomycetes. Brown rot is characterized by extensive depolymerization of the cellulose and limited lignin degradation. White rot is characterised by significant degradation of the lignin component in wood....
T Nilsson


Methodology challenges in developing a transfer of natural durability from sawmill residues, illustrated by experiences with white cypress (Callitris glaucophylla)
2000 - IRG/WP 00-20203
The transfer of durability-conferring extractives from durable to non-durable wood has been accomplished often, but usually as an educational exercise rather than as a commercially oriented process. In the latter environment, many factors previously overlooked become vitally important. How to study them, in the absence of well-developed methodology and given the shorter timeframes being demanded b...
M J Kennedy, M A Powell


Some physiological characteristics of a non-degradative strain of Postia (=Poria) placenta
1988 - IRG/WP 1341
The decay capacity of 14 strains of the brown-rot fungus Postia (= Poria) placenta was determined using soil-wood block tests. One isolate was identified as being unable to degrade wood and was determined to be monokaryotic. It retained the ability to produce extracellular carbohydrate-degrading enzymes, although regulation of certain enzymes was atypical under certain cultural conditions. It prod...
J A Micales, T L Highley


Movement of boron from fused boron rods implanted in Southern pine, Douglas fir, red oak, and white oak timbers
1995 - IRG/WP 95-30061
This paper reports the distribution of boron from fused boron rods installed into six-inch (15.2 cm) square timbers of Douglas-fir, Southern Pine, red oak and white oak exposed aboveground. The composition and size of rods was: sodium borate and sodium borate-copper oxide (8.5 x 100 mm²); sodium borate-copper, sodium borate and boric oxide-copper oxide (12 x 76 mm²). The boric acid equivalent wa...
T L Highley, L Ferge


Above ground performance of CCA-treated fingerjointed lumbe
1993 - IRG/WP 93-40003
Studs made from short lengths by finger jointing are becoming more commonly used in North America. Recently Forintek has received enquiries about the performance of such material in a treated form. Treated and untreated nominal 2x4 inch² spruce-pine-fir (SPF) studs exposed above ground for 12 years in southwestern British Columbia were evaluated for evidence of decay. Despite shallow preservative...
P I Morris, G E Troughton


Evaluation of Barrier Wrap Systems after 71 Months of Exposure
2013 - IRG/WP 13-40631
A 71 month study of the performance of booted samples in ground contact was conducted in AWPA hazard zone 4. Data indicated that excellent performance of wrapped systems, even over untreated wood, could be obtained. Instances of decay colonization or termite attack could all be attributed to some breaking of the integrity of the barrier system. Good performance for treatment below ground contact...
H M Barnes, M G Sanders, G B Lindsey, C McIntyre


Treatment of dried sawn spruce and redwood building timbers with water-borne preservatives under a scheme for the quality control of the preservation and preserved wood in the Netherlands
1978 - IRG/WP 3123
Treatment of dried sawn spruce and redwood Building Timbers with water-borne preservatives under a scheme for the quality control of the preservation and preserved wood in the Netherlands. The aim of this article is to give the reader a modest description of the evaluation of fundamental research in wood preservation into a practical application....
H F M Nijman, N Burgers


Improved resistance of Scots pine and Spruce by application of an oil-heat treatment
2000 - IRG/WP 00-40162
Spruce (Picea abies L. Karst.) and Scots pine (Pinus sylvestris L.) were subject to a heat treatment which was carried out in an oil-bath. The aim was to improve the dimensional stability of the treated wood and its resistance against fungi. The bath of vegetable oil provides a uniform heat transfer at temperatures of 180°C, 200°C and 220°C and protects the submersed wood from oxygen. Heat trea...
M Sailer, A O Rapp, H Leithoff


Synergistic effects between 2-HPNO, Irganox 1076 and EDTA on the inhibition of wood degradation by Coriolus versicolor
2004 - IRG/WP 04-30331
The efficiency of 2-hydroxypyridine-N-oxide (2-HPNO) as wood preservative has been investigated. As shown using classical experiments as well as using response surface methodology, the efficiency of 2-HPNO as wood preservative is strongly improved in presence a chelator like EDTA and/or of Irganox 1076 an industrial antioxidant. In these conditions, wood preservative efficiency of the mixture the ...
A Mabicka, S Dumarçay, N Rouhier, M Linder, J P Jacquot, P Gérardin, E Gelhaye


Multiple-Phase Pressure (MPP) Process: One-stage CCA treatment and accelerated fixation process. 5. Treatment of Sitka spruce and Scots pine
1999 - IRG/WP 99-40136
The suitability of the MPP Process for CCA treatment and accelerated fixation of species other than Radiata pine was assessed by pilot plant trials on UK-grown Sitka spruce (Picea sitchensis) and Scots pine (Pinus sylvestris). Pressure and vacuum kickbacks of spruce (14 l/m3) and Scots' pine (122 l/m3) were both substantially lower than that generated during treatment of radiata pine (369...
M E Hedley, K Nasheri, G Durbin


Analysing the characteristic role of moisture content for drying and fluid flow in Sitka spruce. - Part 1: The drying process of sapwood and heartwood of two different thickness of Sitka spruce using a kiln. - Part 2: Effects of moisture content on longitudinal permeability of Sitka spruce in vertical variation of the tree
2000 - IRG/WP 00-40173
The characteristic role of the moisture content in Sitka spruce (Picea sitchensis (Bong.) Carr.) that grown in the United Kingdom was examined by this study on the basis of (1) the reduction of moisture content in two different thickness of sapwood and heartwood by kiln drying process, and (2) the effects of moisture content to the longitudinal void volume filled of tanalith-C by the full-cell pro...
I Usta


The effects of heat treament on the specific gravity of beech and spruce wood
2003 - IRG/WP 03-40254
The effects of heat treatment on specific gravity of beech (Fagus orientalis) and spruce wood (Picea orientalis) naturally grown and intensively used in forest products industry in Turkey were studied. The wood samples were cut into 2 x 2 x 3 cm. Heat treatment was than applied to the wood samples at four different temperatures (130 °C, 150 °C, 180 °C and 200 °C) and three different durations...
S Yildiz, Ü C Yildiz, G Colakoglu, E D Gezer, A Temiz


Changed susceptibility of the chemically and thermally degraded spruce wood to its attack by the dry rot fungus Serpula lacrymans
1999 - IRG/WP 99-10322
In buildings, some intentional or unintended situations can occur at which some wood products are exposed to aggressive chemicals and also to higher temperatures. Occasional activity of fungi on such pre-attacked wood products can be either higher or lower. This paper deals with changes in the susceptibility of spruce wood (Picea abies L. Karst.) to attack by the dry rot fungus Serpula lacrymans, ...
L Reinprecht


The influence of previous anti-blue-stain preservative treatments on the fixation of CC in spruce
1997 - IRG/WP 97-30134
Freshly cut and kiln dried spruce boards were treated with 4 different anti-blue stain preservatives (ABP). After a period of 10 days allowing the samples to dry and fixate, the samples were treated with CC (chromium, copper formulation) using a vacuum pressure cycle. After impregnation the wood was steam fixed. A submersion leaching test showed differences in the leachable quantity of copper and ...
M Van der Zee, W J Homan


Susceptibility of angiosperm sapwood to white-rot fungal colonization and subsequent degradation: a hypothesis
1997 - IRG/WP 97-10211
It has long been recognized that angiosperm sapwood in nature is relatively easily and preferentially degraded by white-rot fungi. This susceptibility to white-rot fungi is generally believed to be mainly caused by the structure and concentration of angiosperm lignin. However, an explicit explanation as to why lignin structure makes a particular wood vulnerable to white-rot colonisation and subseq...
T Schultz, D D Nicholas