Ultrastructure of degraded, CCA-treated Pinus radiata wood from a marine pile
1990 - IRG/WP 1461
During an inspection of marine piles, 12 years after installation, severe degradation was noted on one of them in the vicinity of a corroded eye-bolt. The wood was dark brown in colour and tended to crumble easily. Wood fragments were examined by light microscopy and scanning and transmission electron microscopy and were also analysed for carbohydrates and lignin. Light microscopy showed numerous ...
A P Singh, M E Hedley


Investigation of microwave as a means of eradicating dry rot attack in buildings
1992 - IRG/WP 92-1545
A microwave-apparatus developed for treatment of building-structures infested by dry rot was tested in the laboratory. The test-conditions simulated treatment of either infested timber or infested brickwork. Sawdust samples, both wet and dry, infested by viable mycelium of Serpula lacrymans were packed in glass-tubes. The tubes were then placed in the middle of either 20 cm thick wooden beams or 3...
C Kjerulf-Jensen, A P Koch


Methyl bromide eradication of the oak wilt fungus in logs. Laboratory and field fumigation
1981 - IRG/WP 3168
Concern over accidental introduction of the oak wilt fungus (Ceratocystis fagacearum) into oak-importing nations has prompted a study supported by the U.S. National Lumber Exporter's Assn. to assess the efficacy of methyl bromide fumigation to eradicate the fungus from logs and lumber. Laboratory and field fumigation trials to develop a reliable and realistic treatment were performed on r...
E L Schmidt, M M Ruetze, D W French


The performance of CCA treatment in bamboo against decay fungi
1993 - IRG/WP 93-30027
Samples of culm wall material from young (< 6 month age) and mature (> 3 years age) culms of the bamboo, Phyllostachys virideglaucescens were treated to equivalent% w/w retentions of a CCA preservative. After fixation and leaching the treated samples were exposed to decay by Chaetomium globosum FPRL S70K, Coriolus versicolor FPRL 28A and Coniophora puteana FPRL 11E. Thin section samples of u...
O Sulaiman, R J Murphy


The evaluation of the occurrence of soft rot in creosoted wooden poles
1988 - IRG/WP 1368
The occurrence of soft rot decay in creosoted wooden poles for overhead power lines was investigated by collection of field samples, their subsequent microscopic examination and statistical analysis of the data collected. Examination of samples collected from 296 poles revealed that approximately 15% of the pole population studied (Eastern Electricity Board) showed the presence of soft rot decay. ...
A Wylde, D J Dickinson


Novel observations on the micromorphology of soft rot attack of wood
1996 - IRG/WP 96-10176
Electron microscopic examinations of decaying Pinus radiata horticultural posts which had been treated with CCA preservative prior to being placed in service about nine years ago showed the presence of soft rot fungi and tunnelling bacteria. Some novel observations on the micromorphology of the soft-rotted areas of tracheid walls are described here. The micromorphology of soft-rotted areas was hig...
A P Singh, R N Wakeling


Oxalate production and calcium oxalate accumulation by Gloeophyllum trabeum in buffered cultures
1994 - IRG/WP 94-10075
Most basidiomycetous fungi produce oxalic acid as a result of their metabolic activities and nutrient procurement. There is currently a renewed interest in the role that oxalic acid may play in the decomposition of wood by basidiomycete fungi. It has been observed that although most wood degrading fungi have the capacity to produce oxalic acid, not all of these organisms express this capacity equa...
J H Connolly, J Jellison


High CCA retentions and the protection of eucalypt power poles
1983 - IRG/WP 3226
Tasmanian power pole material treated to high retentions, was analysed to accurately determine the amount of CCA preservative in the timber. Material from the same disc was subsequently exposed in unsterile soil in order to determine the effectiveness of treatment. Results showed that even at high retention levels, soft-rot attack was not prevented. Fourteen further poles were sampled, but this ti...
L E Leightley, J Norton


Soft rot tests
1983 - IRG/WP 2206
At the IRG meeting in Turkey it was proposed that developments in testing preservative-treated wood in unsterile soil according to techniques variously described as "fungus cellar", "soil-bed", or "accelerated field simulation" be considered along with conventional laboratory procedures as the basis for a standard test. Before formulating any co-operative test programme it is essential to examine ...
J A Butcher


Degradation of the gelatinous-layer in aspen and rubber wood by the blue stain fungus Lasiodiplodia theobromae
1996 - IRG/WP 96-10168
Studies on the degradative ability of the blue stain fungus Lasiodiplodia theobromae Pat. have shown several strains to cause significant weight losses (i.e. ca 20%) in the temperate and tropical wood species, aspen (Populus tremula) and rubber wood (Hevea brasiliensis). In addition to the consumption of soluble carbohydrates and extractives, major changes in the ultrastructure of fibre cell walls...
O Encinas, G F Daniel


The possible significance of the lignin content and lignin type on the performance of CCA-treated timber in ground contact
1988 - IRG/WP 1357
The lignin in wood samples of Alstonia scholaris, Octomeles sumatrana and a Simaruba species have been analysed. These timbers are characterised by a high lignin content and low syringyl:guaiacyl ratios. Decay tests with two soft rot fungi showed that the timbers were less susceptible than timbers with a low lignin content and higher syringyl:guaiacyl ratios. Numerous data for field performance of...
T Nilsson, J R Obst, G F Daniel


Soft rot studies on CCA treated eucalypt power transmission poles
1981 - IRG/WP 1132
Initial results found for sixty CCA treated eucalypt poles, from a soft-rot survey are discussed. Retentions of CCA within above and below ground pole samples were variable. The variation was attributed mostly to biodegradation and effect of soil environment, rather than leaching. Bacterial decay was found in many poles and was severe in some cases. Although found in the presence of soft-rot decay...
L E Leightley


Soil-bed studies. Part 2: The efficacy of wood preservative
1983 - IRG/WP 2205
Various methods of decay assessment were investigated. Three stages or phases of decay were identified which could be used to describe the efficacy of a preservative system or virulence of a soil-bed testing medium. These included the lag, decay, and senescent phase. Premature senescence could arise if wood samples became waterlogged. It was concluded that time to failure was unsuitable as a metho...
P Vinden, J F Levy, D J Dickinson


Soft-rot problems with treated hardwoods: A paper for discussion and establishment of a programme of work
1974 - IRG/WP 331
At the 5th meeting of IRG in Lahti (June 1973) it was decided that an ad hoc group should be formed to study these problems. It was decided that it&apos;s activity could be usefully directed in two main areas; a) in the encouragement and direction of existing research in this field, and b) in the organising of a collaborative field trial involving interested parties using locally important har...
D J Dickinson


Optimum growth conditions for the metal-tolerant wood decay fungus, Meruliporia incrassata TFFH 294
1999 - IRG/WP 99-50142
There is a worldwide need for alternative methods for the treatment and disposal of CCA-treated waste wood. Illman and Highley (IRG/WP 96-10163) reported the isolation of a unique strain of Meruliporia incrassata (TFFH 294) with tolerance to CCA. The strain is capable of degrading CCA treated waste wood, giving a 40% weight loss in the ASTM soil block test. The strain is an ideal candidate for deg...
V W Yang, B Illman


Practical consequences of the clarification of the chemical mechanism of CCA fixation to wood
1983 - IRG/WP 3220
Practical consequences derived from the chemical investigation of the mechanism of fixation of CCA to the wood constituents are discussed. Among these, formulas for the calculation of the time of hexavalent chrome fixation are presented. Furthermore, three parameters are shown to be important to the long-term effectiveness of CCA-treated timber: (i) the temperature of treatment, (ii) the initial p...
A Pizzi


Fungus cellar and field tests with tall oil derivatives. Final report after 11 years' testing
1993 - IRG/WP 93-30007
Two derivatives of tall oil were tested as wood preservatives in a fungus cellar and in ground contact (field test). Stakes of Pinus sylvestris sapwood were used in the tests. For the field test the size of the stakes was 20 x 50 x 500 mm³ and for the fungus cellar test 20 x 20 x 250 mm³. The stakes were vacuum-pressure treated with the two products and exposed in 1981. The field test site used ...
J Jermer, Ö Bergman, T Nilsson


Worldwide in-ground stake test of acetylated composite boards
1997 - IRG/WP 97-40088
Acetylated wood composite stakes are being tested in ground contact (graveyard test) in seven fields around the world. Three types of acetylated wood composites were prepared: spruce fiberboard in Sweden, aspen fiberboard in Madison and rubber wood particle board in Indonesia. Two levels of acetylation were used, a high level of ~20% acetyl content and a low level of 10% acetyl content. Control bo...
R M Rowell, B S Dawson, Y S Hadi, D D Nicholas, T Nilsson, D V Plackett, R Simonson, M Westin


Evaluation of substituted isothiazolone as a potential new wood preservative
1984 - IRG/WP 3306
Laboratory decay tests were carried out with isothiazolone (4,5-dichloro-2-n-octyl-4-isothiazolone-3-one) treated wood. This compound was found to be extremely effective against three common wood decaying brown-rot fungi, exhibiting toxic threshold values in the range of 0.37 to 0.50 kg/m³. For the white-rot fungus, Coriolus versicolor, the toxic threshold values for treated pine and sweetgum wer...
D D Nicholas, A F Preston, D E Greenley, S V Parikh


An illustrated comment on the soft rot problem in Australia and Papua New Guinea
1977 - IRG/WP 296
A brief survey of soft rot is presented, with particular reference to attack of preservative treated hardwood transmission poles in Australia. Possible explanations of why the preservatives are failing to protect the poles are discussed, together with current efforts to produce control measures. Examples of soft rot in variously treated eucalypt or pine specimens are shown to illustrate the morpho...
H Greaves


Changed permeability and surface properties of hornbeam wood due to its degradation by erosive strain of Phanerochaete chrysosporium
2004 - IRG/WP 04-40290
Specimens of hornbeam wood were submitted to a medium-term degradations by erosive fungus Phanerochaete chrysosporium. Biodegradations of specimens resulted in their apparent structural alterations, changes in permeability and increased intensity of interactions with polar liquids. Modified physical properties of biodegraded wood may significantly influence its penetration with polar media and che...
R Solár, S Kurjatko, L Reinprecht, M Mamon, V Vacek


CCA modifications and their effect on soft rot in hardwoods. Part 2
1983 - IRG/WP 3244
The work outlined in this document is a continuation of that presented in Document No: IRG/WP/3201. The findings described in the previous paper are summarised below: a double treatment of CCB followed by arsenic (CCB+A) is more effective than a double treatment of boron followed by CCA (B+CCA) or a single treatment of CCA, CCB or CCAB in controlling soft-rot due to Chaetomium globosum in birch. C...
S M Gray, D J Dickinson


Supplementary experiment to the main trial (IRG/WP/367, 384) to determine the performance of preservative treated hardwoods with particular reference to soft rot
1977 - IRG/WP 3101
The field experiment being carried out by the IRG (described in document IRG/WP/367) is designed to obtain information on the performance of a preservative in different hardwoods in ground contact. A total of 57 timber species is being examined and 36 different field sites are involved representing a complete range of climatic conditions. IRG document WP/384 describes the treatment details of the ...
F W Brooks, C R Coggins, D J Dickinson


The natural durability assessment of secondary hardwood species - laboratory tests
1998 - IRG/WP 98-10295
Laboratory tests have been undertaken to assess the natural durability of 16 species of lesser known hardwoods, or hardwoods from non-traditional sources, including teak from three different plantations. Resistance to decay by both basidiomycetes and soil-inhabiting micro-fungi has been established. ´The data indicated that published information on the durability of these timbers should be treat...
J K Carey, S J Hendry


Assessment of the toxicity of some copper-, zinc- and boron-based wood preservatives to the cellar fungus Coniophora cerebella Schröet
1974 - IRG/WP 242
This article reports the use of a method based on the determination of the probability of the protection of timber against destruction by fungi. By converting the probability values to probit values and plotting them as a function of the amount of preservative retained in the timber, curves of the toxic effect are obtained, enabling any timber protection probability to be assessed....