IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 179 documents. Displaying 25 entries per page.


Moisture content levels and decay of hemlock
1986 - IRG/WP 1287
As a model of decay conditions of wooden members in wooden houses, a decay test was set up in which samples of western hemlock (Tsuga heterophylla) under 4 moisture levels were examined. Each week the samples were weighed and if the weights indicated that their moisture contents were lower than the expected levels, distilled water was added. Every 8 weeks 3 samples from each condition were oven dr...
K Suzuki


Effects of acetylation on the dimensional stability and decay resistance of kenaf (Hibiscus cannabinus L.) fiberboard
1996 - IRG/WP 96-40059
The objective of this study was to investigate the influence of the acetylation treated kenaf fiber, Phenol formaldehyde resin content level, and three fungi species on the dimensional stability and decay resistance of high density non wood composition boards. A standard ASTM method was used to evaluate weight loss and thickness change. The linear shrinkage and expansion of each species were also ...
P Chow, T Harp, R Meimban, J A Youngquist, R M Rowell


Collaborative soft rot tests: PRL tests of Cu/Cr/As preservative using method of Document No: IRG/WP/208
1973 - IRG/WP 223
These tests were undertaken as a preliminary to the next series of collaborative soft rot tests. An interim report has already been presented at Berlin in 1972 as Document No: IRG/WP/211...
J K Carey, J G Savory


On Donkioporia expansa (Desm.) Kotl. & Pouzar
1986 - IRG/WP 1285
Donkioporia expansa is found more often in houses than realised until now. Virulence tests according to EN 113 show not only an attack of oak, but also of other hardwoods and even soft-woods....
G Buchwald


Soil virulence tests using Scots pine sapwood
1973 - IRG/WP 222
Following the tests reported in Document No: IRG/WP/210, in which soils from different laboratories were investigated for virulence, supplementary tests have been carried out using Scots pine sapwood and an extended incubation period....
J K Carey, J G Savory


Comparison of the agar-block and soil-block methods used for evaluation of fungitoxic value of QAC and CCA wood preservatives
1994 - IRG/WP 94-20039
The modyfied agar-block and soil-block methods were used for comparing the fungitoxic value of QAC and CCA type preservatives against Coniophora puteana and Coniophora olivacea The mass loss and moisture contents of wood were analysed....
J Wazny, L J Cookson


The biostatic effect of copper on decay of fire retardant-treated mining timber
1991 - IRG/WP 1507
Blocks of Eucalyptus grandis were treated with 20kg/m³ ammonium sulphate as fire retardant and challenged with Coriolus versicolor. Replicates were soil buried. A second set of blocks was treated with retardant and copper at 6.6 kg/m³ (ie 1% w/w), and challenged similarly. After 8 weeks weight losses produced by Coriolus versicolor in untreated, retardant treated and copper supplemented blocks w...
G D Shelver, E A Shelver, A A W Baecker


Temperature influence on the growing velocity and cellulolytic activities of Poria placenta strains from several locations
1986 - IRG/WP 2263
The differences observed on the FPRL 280 Poria Placenta strain at several Research European Laboratories for determining up the fungicide effectiveness of wood preservative has carry us to do a comparative study about the cellulolytic activity and growth velocity of each of this strains at different temperatures (22, 24 and 28°C). The results show significative differences when the temperature is...
A M Navarrete, M T De Troya


Collaborative soft rot tests: Interim report on PRL tests of Cu/Cr/As preservative using method of Document No: IRG/WP/208
1972 - IRG/WP 211
Preservative: Tanalith CT.106 - Results obtained with beech are given in the table and indicate a toxic limit of 16.7-19.2 kg/m³ - The initial soil moisture content was adjusted to 27.8% (the water holding capacity). Noticeable drying out has occurred in some of the test bottles....
J G Savory


Contribution to the testing of wood based board material
1982 - IRG/WP 2176
R G Lea


Proposals for a vermiculite burial soft rot test method
1980 - IRG/WP 283
J G Savory, J K Carey


Collaborative soft rot tests: 2nd interim report
1975 - IRG/WP 258
J G Savory, J K Carey


Virulence testing of cultures of different origins of the test fungus Coriolus versicolor strain CTB 863 A
1986 - IRG/WP 2267
The virulence of cultures of different origins of Coriolus versicolor CTB 863 A - a strain which is mentioned in EN 113 - was tested. Standard blocks of beech wood were used at temperatures of 20-22°C and 26-28°C and particleboard was tested at 26-28°C. The decay capacity of the different inoculations varied widely, as could be expected it was greatest at the higher temperature level....
W Kerner


Evaluation of the decay caused by Chaetomium globosum Kunze, in the course of time
1987 - IRG/WP 2288
The main research done on soft rot has been directed to determining, by microscopic study, the different stages of penetration into the wood of the fungi that cause it. On the basis of the information furnished by this research, in this work we have tried to quantify its effect, by evaluating the weight loss caused by Chaetomium globosum Kunce in wood of Pinus sylvestris L. and Fagus sylvatica L. ...
M T De Troya, A M Navarrete


Detection of incipient brown rot decay in wood by fourier transform infrared spectrometry
1987 - IRG/WP 2275
Fourier transform infrared spectrometry was evaluated as a possible method for detecting different levels of brown-rot decay in pine sapwood. By using first derivative spectra and regression analysis, an equation based on 4 absorption peaks, normalized with an internal standard peak, was developed. The correlation between weight loss and absorption was highly significant indicating that this is a ...
D D Nicholas, T Schultz


Results from soft rot tests in vermiculite jars
1976 - IRG/WP 272
T Vihavainen


About the relations between the natural durability of some tropical species and their extractives content
1983 - IRG/WP 1208
G R Y Déon


The performance of wood preservatives in soil-bed soft rot tests
1993 - IRG/WP 93-20007
Testing the efficacy of wood preservatives in soil is recognised as a fundamental part of the assessment of long-term wood protection in ground contact. Laboratory based tests can provide a hazardous environment in which a preservative can be challenged by a range of micro-organisms. This paper presents the results of tests carried out to investigate the performance of wood preservatives in a wet ...
G R Williams, S Caswell


On the use of % weight loss as a measure for expressing results of laboratory decay experiments
1992 - IRG/WP 92-2394
It is suggested that careful consideration should be given for the presentation of data from laboratory decay experiments, especially when comparisons are being made from experiments involving wood blocks of varying densities. Percent weight loss can be used for comparisons of durability even if wood blocks vary in density. It is suggested that the absolute weight loss for a given volume (g/cm³) ...
T Nilsson, G F Daniel


Termiticidal effectiveness of synthetic pyrethroids, carbaryl and chlordane in wood-block test
1985 - IRG/WP 3356
The results of some wood-block tests with allethrin, permethrin, fenvalerate, carbaryl and chlordane against Coptotermes formosanus are tabled and compared against some organophosphates, chlorpyrifos, fenitrothion, phoxim, tetrachlorvinphos and acephate. The treatment of the wood blocks was exactly as described in Document No: IRG/WP/3330. Among the pyrethroids tested, permethrin was the most effe...
K Tsunoda


Virulence tests with fungal strains used in EN 113 CEN ring test. Results with Coniophora puteana (Schum.ex Fr.) Karst
1986 - IRG/WP 2249
D Dirol


Collaborative soft rot experiments 1974. Preliminary analysis of results
1975 - IRG/WP 251
J K Carey, J G Savory


Evaluation and approval of wood preservatives in Japan
1988 - IRG/WP 2303
Japanese standardized decay test methods, performance requirements and approving system are briefly described. JIS (Japanese Industrial Standard) A 9302, which is related to a testing method for evaluating effectiveness of wood preservatives when applied to pressure treatment, is fundamentally a sand-block laboratory test method. According to performance requirements in JIS A 9201, mean percentage...
K Tsunoda


Laboratory evaluation of organophosphates as termiticides
1985 - IRG/WP 3330
In accordance with Japan Wood Preserving Association Standard 11(1) laboratory evaluations of five organophosphate insecticides and chlordane were conducted. Superficially treated sapwood of Pinus densiflora Sieb. et Zucc. (10 x 10 x 20 mm³) was compulsorily exposed to the attacks of 150 workers and 15 soldiers of Coptotermes formosanus Shiraki for 21 days at 28±2°C in the dark. Percentage weig...
K Tsunoda, K Nishimoto


Biodegradation of acetylated southern pine and aspen composition boards
1994 - IRG/WP 94-40020
This objective of this study was to investigate the influence of the acetylation treated wood fiber, Phenol-formaldehyde resin content level, two wood fiber species, three fungi species on the dimensional stability and decay resistence of high density composition boards. A standard ASTM method was used to evaluate weight loss and thickness change. The linear shrinkage and expansion of each species...
P Chow, T Harp, R Meimban, J A Youngquist, R M Powell


Next Page