Grading the Performance of 18 Common Bamboo Species
2010 - IRG/WP 10-10723
A grading method for assessing the performance of 18 common bamboo species was introduced in this article. The method was based on 4 grade levels with corresponding scores of 4 reference indexes of bamboos including culm diameter, culm-wall thickness, natural durabiliy and preservative treatability. In comparison with the traditional utlilization of bamboo, the grading results showed that this gra...
Chen Lifang, Su Haitao, Zhang Yanjun, Wang Yuxia, He Xuexiang, Ma Hongxia, Xie Guijun


Early detection of colonisation by blue stain and mould on modified wood using PCR technique
2010 - IRG/WP 10-10730
The aim of this research was the early detection of fungal attack on the surfaces of modified and unmodified wood after natural weathering. The investigation was carried out by molecular techniques and the development and establishment of genus/species specific PCR for important moulds and sapstain fungi was part of this work. After adaption of the method, a monitoring of the succession of Ascomyc...
A Steitz, B Schmöllerl, N Pfabigan, S Bollmus, G Grüll


The Relative Performance of an Organic Preservative System under UC3A and UC3B Conditions using Two Test Methods
2010 - IRG/WP 10-20429
Coated L-joints have been used for decades to evaluate the performance of wood preservatives in protected environments. This study was conducted using matched coated and uncoated L-joints to simulate above ground protected and unprotect exposures. When exposed to constant moisture in a greenhouse environment, coated and uncoated L-joints give very similar performance results. In contrast, exposi...
C F Schauwecker, A Zahora, A F Preston


The Use of Micro-Tensile Testing to Assess Weathering Decay and Oxidative Degradation of Wooden Items
2010 - IRG/WP 10-20433
This paper presents a method to study the weathering performance of wooden items and to assess the oxidative degradation of wood via the Fenton reaction. Weathering resistance and photo-stability of wood was tested using pine wood (Pinus sylvestris) veneer strips measuring approximately 60 µm in thickness. The veneer strips were treated using a reactive chemical to impart surface protection. The ...
C Mai, Yanjun Xie, Zefang Xiao, P D Evans, H Militz


Profiling fungal community in wood decay ecosystem by Denaturing High-Performance Liquid Chromatography
2010 - IRG/WP 10-20443
A DNA-based fingerprinting technique, Denaturing High Performance Liquid Chromatography (DHPLC) was developed to profile fungal communities colonizing indoor timber. Molecular fungal diversity was assessed using amplification based on the Internal Transcribed Spacer (ITS1) rDNA of 74 wood samples collected from infected buildings in France. Due to its high sensitivity, the PCR-DHPLC technique was ...
S Maurice, G Le Floch, M Le Bras-Quéré, J P Rioult, G Barbier


The biological durability approach for wood product performance and service life prediction
2010 - IRG/WP 10-20457
The performance of wood-based products under conditions that enable biodegradation are of concern to all who envisage sustainable use of forest based products. This concern is also the basis of classification of wood species on the basis of their biological durability. Engineers are looking for options to transfer such classification into practical service life values for constructions and related...
J Van Acker, J Van den Bulcke, L De Boever


Finite Element Modelling of the Checking of Wood Exposed to Accelerated Weathering
2010 - IRG/WP 10-20459
The surface checking that develops when wood is exposed to the weather reduces the visual appeal of treated wood products and can reduce the effectiveness of preservative treatments. There is strong interest in developing solutions to this problem and also a growing realization that such solutions may evolve from a deeper understanding of the mechanisms responsible for surface checking. In this pa...
S G Ribarits, P D Evans


Biological performance of wood treated with tar-oil recovered during slow pyrolysis of macadamia nut shells
2010 - IRG/WP 10-30523
This study evaluated decay and termite resistance of wood treated with tar oil obtained from a commercial pyrolysis process of macadamia nut shells. Vacuum-treated pine wood specimens were subjected to various brown and white rot fungi based on the soil-block test method specified by the American Wood Protection Association (AWPA) after leaching process. Treated specimens were also subjected to th...
S Nami Kartal, E Terzi, C Kose, J Hofmeyr, Y Imamura


Photostabilization of Wood with Higher Molecular Weight UV Absorbers
2010 - IRG/WP 10-30524
Higher molecular weight UV absorbers were created by reacting the epoxy-functionalized UV absorber 2-hydroxy-4(2,3-epoxypropoxy)-benzophenone (HEPBP) with maleic, phthalic or succinic anhydride. The ability of the UV absorbers to photostabilize wood was then examined. FTIR-spectroscopy confirmed that HEPBP reacted with phthalic anhydride to create a polyester that preserved the UV-absorbing benzop...
P D Evans, M J Chowdhury


Distribution and availability of preservative components in ACQ treated wood - effects of coatings and weathering
2010 - IRG/WP 10-30537
Copper and quaternary ammonium compound (quat) distributions across lumber (gradients) and availability, as measured by amount removed by intensive leaching of wood flour, were measured in ACQ treated southern pine lumber. Samples were evaluated just after treatment and stabilization, or after 3 years of laboratory storage, or after 3 years of natural weathering exposure. The objective was to in...
T Ung, M Nejad, P Cooper


A Comparison of the Performance of Related Copper Based Preservatives against Soft Rot
2010 - IRG/WP 10-30540
The performance of pine and beech wood treated with either a soluble copper + quat (ACQ type D) preservative system or a particulate copper + quat system was evaluated in unsterile soil using the European standard ENV 807 soft rot decay test procedure. In addition, to compare soft rot performance of soluble and particulate copper directly without the influence of co-biocides, beech and pine test...
M Ray, D Dickinson, K Archer


Accelerated L-joint performance testing of organosilicon treated wood
2010 - IRG/WP 10-30551
In this research Scots pine sapwood L-joints were treated with organosilicons and organosilicons in combination with biocides. These L-joints were prepared and exposed according to the accelerated L-joint method. They were inspected each season for fungal discolouration and removed from the rack after three years outdoor exposure. Subsequently the moisture content, mass loss and decaline uptake we...
L De Vetter, J Van Acker


Effect of 4 Preservatives on Physical, Mechanical and Mold-Resistant Properties of Bamboo Oriented Strand Boards
2010 - IRG/WP 10-40483
This study investigated the effects of 4 preservative systems on physical, mechanical and mold-resistant properties of bamboo oriented strand board (OSB) panels bonded with urea formaldehyde resin. Preservative A (Zinc Borate), B (IPBC), C (AAC+Borate) and D (carbendazim + prochloraz) were incorporated with strands during blending at three loading levels. The results showed that the mechanical and...
Juwan Jin, Daochun Qin, Wanshu Wei, Kuan Fan


The Effects of Natural Weathering on the Properties of Heat Treated Alder Wood
2010 - IRG/WP 10-40484
Heat treatment is an effective method to improve the dimensional stability and biological durability of wood. The heat treatment technology and the heat treated wood products were recently introduced to Turkey. However, only a few studies have been reported on the effect of natural weathering on the properties of heat treated wood in both Turkey and the world. In this study, heat treated alder (Al...
S Yildiz, Ü C Yildiz, E D Tomak


Comparison of colour change in wood clear-coating systems including inorganic and organic UV absorbers for exterior use
2010 - IRG/WP 10-40499
The aim of this work is to compare the performance of inorganic and organic UV absorbers used in a wood coating application against weathering. Our study has investigated the colour changes of selected UV absorbers; hombitec 402 RM from the Sachtleben Company as an inorganic UV absorber, tinuvin 477 DW from the Ciba Company as an organic UV absorber. The study was carried out on two wood species; ...
Ö Özgenç, B Forsthuber, A Teischinger, C Hansmann


Study of Microscopy Properties of Modified Wood During Weathering Process
2010 - IRG/WP 10-40517
In this study spruce (Picea excelsa) and Beech (Fagus orientalis) wood acetylated and has been subjected of artificial weathering in difference times (0, 50,150&300 h), then wood surface analyzed using Scanning Electron Microscopy (SEM). The SEM results shown that the surface of wood exposed to weathering undergoes distinct physical changes and the surface degradation appears to be directly propor...
M Akhtari


Effect of Coatings on the Durability of Birch and Spruce Plywood. Part 2: Biological Durability
2010 - IRG/WP 10-40527
Several different coated birch and spruce plywood types were investigated in Finland using the combination of outdoor weathering and decay test EN 12038. The most important factor to affect on the biological performance of birch plywood, coated and uncoated, was edge sealing. For spruce plywood edge sealing had a smaller effect. However, in spite of positive effect against decay, edge sealing did ...
A Nurmi, H Viitanen


Lignin blocking effects on weathering process of wood plastic composites
2010 - IRG/WP 10-40529
The weathering of wood–plastic composites (WPC) causes discoloration which affects their aesthetic aspects. It has been proved that these discolorations are due to lignin degradation. Effects of blocking the susceptible structure of lignin assessed by chemical treatment such as acetylation and methylation are reported in this study. Surface chemical change of wood plastic composite (WPC) formula...
P Darabi, A Naghi karimi, S Ahmade Mirshokraie, M-F Thévenon


Silicon compounds as additives improving alkyd-based wood coatings performance
2010 - IRG/WP 10-40531
The reactivity of cellulose with solvent-born alkyd-based wood coatings supplemented with organosilanes was analyzed. Structural analysis of cellulose subjected to the reaction with organosilanes and following extraction with water was performed using Fourier-transform infrared spectroscopy (FTIR). The analyzed IR spectra comprise bands 1250 cm-1 typical for the SiC group and 800 cm-1 typical for ...
B Mazela, I Ratajczak, K Wichłacz-Szentner, P Hochmańska


Decay hazard mapping for Europe
2011 - IRG/WP 11-20463
In this study, two different dose-response models for above-ground decay as well as a model transferring macro climate data to wood climate data are presented. The models base on data from field trials, which had been conducted at 28 European test sites, and were used to calculate the relative risk for decay caused by climate variability in Europe. The two dose-response models give coherent result...
C Brischke, E Frühwald Hansson, D Kavurmaci, S Thelandersson


Service life prediction of wooden components - Part 3: Approaching a comprehensive test methodology
2011 - IRG/WP 11-20464
This paper is the third in a series on 'service life prediction' of wooden components and should be considered as a discussion paper. The authors tried to analyze the topic with a look from a distance and comment sometimes with a smile on the current controversial discussion about SLP issues. Nevertheless, the viewpoints of different groups, such as natural scientists, engineers, approva...
C Brischke, C R Welzbacher, L Meyer, T Bornemann, P Larsson Brelid, A Pilgård, E Frühwald-Hansson, M Westin, A O Rapp, S Thelandersson, J Jermer


Improving our understanding of moisture and other durability-related properties of wood in building envelope performance prediction
2011 - IRG/WP 11-20468
Building science has become an increasingly important field in recent years with rapid changes in construction methods, building materials and consumer expectations. The field has also been brought to prominence by a few large-scale premature building envelope failures in a few regions across the world. Considerable effort has been put into developing hygrothermal models to simulate heat, air, vap...
Jieying Wang, P Morris


The Effectiveness of Machined Profiles at Reducing the Checking of Wooden Decking
2011 - IRG/WP 11-40541
This study tests the hypothesis that ‘the ability of surface profiling to reduce checking of deck boards exposed to weathering will vary with wood species and profile type’. Southern pine (Pinus sp.) and Pacific silver fir (Abies amabilis) deck boards were machined to produce three different types of surface profiles: flat (control), ribbed (V-shaped grooves), and rippled (U-shaped grooves). B...
P Evans, I Cullis, P Morris


Evaluation of an optimized industrial process aiming to improve the natural durability and mechanical behavior of bamboo for outdoor use
2011 - IRG/WP 11-40554
Mao Bamboo (Phyllostachys pubescens) is characterized by high contents of sugar and starch and by high hygroscopicity, which makes it susceptible to biodegradation, and specifically to fungal decay. Still, many bamboo based products regularly enter the European wood construction market, competing with traditional solid wood products used for outdoor decking and cladding. The performance of a heat ...
F Simon, M Kutnik, I Le Bayon, G Moisset, V Gatimel


Wet and dry adhesion of coatings on modified and unmodified wood: influence of 18 months of natural weathering on the pull-off test and cross-cut test results
2011 - IRG/WP 11-40569
The objective of this paper is to study the influence of several types of modification (acetylation, furfurylation, heat treatment) on coatings adhesion after 18 months of natural weathering according to EN 927-3 in Vienna (Austria). The paper compares two methods for assessing the adhesion: the cross-cut test (EN ISO 2409) which is the conventional method used and recommended in EN 927-3 and th...