The field performance of CCA-C treated sawn refractory softwoods from North America
1997 - IRG/WP 97-40085
Approximately 15% of the total volume of wood treated in the United States consists of difficult to treat softwoods known as "refractory softwoods". The long term positive performance record of CCA treated sawn material is based upon the testing of yellow pine sapwood stakes with only limited field data available for sawn refractory softwoods. As a result, the existing North American wood preserva...
M J Richards, W S McNamara


Field performance of novel antisapstain formulations
1997 - IRG/WP 97-30125
The effectiveness as antisapstain formulations of combinations of oxine copper (Cu-8), carbendazim, hexaconazole, cyproconazole, flusilazole, didecyldimethyl ammonium chloride (DDAC), an alkanolamine borate (SB), benzalkonium chloride (BAC), 2-n-octylisothiazolin -3-one (isothiazoline) and p-chlorophenyl-3-iodopropagilformal (CPIPF) was determined for freshly sawn, block-stacked radiata pine in th...
D R Eden, R N Wakeling, C M Chittenden, J G Van der Waals


L-joint trials: Part 1: Observations on the process of colonisation and decay
2002 - IRG/WP 02-20250
The first trials using the small L-joint, later adopted for use in BS EN 330 and AWPA Standard E9-97 were exposed at BRE in 1975 but all were assessed destructively during the early stages of exposure. The longest running trial which included replicates for long-term exposure will have been exposed for 20 years in July 2002. This paper provides an overview of the results of testing during that p...
J K Carey


A technique for the rapid assessment of wood surface degradation during weathering
1987 - IRG/WP 2281
Radiate pine (Pinus radiata D. Don) sapwood samples taken from four trees were converted into thin strips 100 x 10 x 0.085 (85 µm) mm³, (longitudinal x radial x tangential) in size and exposed in preweighed hatches to the weather inclined at 45° facing equatorially for 10, 20, 40, 60, 80 and 100 days. Significant (P < 0.001) weight losses occurred with time over the exposure period. Differen...
P D Evans, D Abbott, S Thein


IUFRO rating system compares favourably to weight loss for soil-bed testing
1990 - IRG/WP 2343
The soil-bed/small stake test is commonly used for rapidly evaluating the performance of new, more environmentally acceptable, preservatives. In a 1.5 year experiment with three copper-based waterborne preservatives, visual evaluation and probing using the IUFRO performance rating scale (0-4) gave very similar toxic thresholds to those derived from measurement of weight loss at the end of the expe...
P I Morris


Characterization of checks and cracks on the surface of weathered wood
2000 - IRG/WP 00-40153
The surface roughness of unweathered and untreated pine; unweathered copper chromium arsenate type C (CCA) - treated pine; weathered CCA-treated pine; and weathered CCA-plus-water-repellent (WR) - treated pine was evaluated by a stylus tracing method. Surface roughness parameters Ra, Rz, Rmax, Rk, Rpk, and Rvk were measured. Ra, Rpk, and Rvk were the most appropriate parameters for describing modi...
D P Kamdem, Jun Zhang


Durability of exterior natural wood finishes in Brazil
1985 - IRG/WP 3343
Wood finishes systems were evaluated in natural weathering conditions during 5 (five) years, over "Parana-pine" (Araucaria angustifolia). Test samples results show that: - Semitransparent wood preservative stains, based on polimerized linseed oil, provided very good protection to the wood, compared with the one based on alkyd varnish; - Solid color wood preservative stains provided good durability...
D R Macedo


Effect of kerfing on performance of Douglas-fir utility poles in the Pacific Northwest
1990 - IRG/WP 3604
Preservative treatment produces an external layer of protection in Douglas-fir poles, but the development of deep checks as the wood dries after treatment can permit entry by fungi and insects. A variety of remedial treatments can arrest this decay; however, it is far more efficient to prevent checking. Kerfing represents one potential method for limiting the development of deep checks. In previou...
J J Morrell


Performance trials of treated hardwood fences
2002 - IRG/WP 02-30281
This paper examines the performance of the traditional hardwood paling fence used in Australia, after preservative treatment. Unseasoned rails, palings and plinths of the low natural durability species Eucalyptus regnans (mountain ash) and E. obliqua (messmate) were treated with PEC (pigment emulsified creosote) or PROCCA (an oil emulsion of CCA). Treated posts of these species were also compared ...
L J Cookson D Scown, B Iskra


Performance of preservative-treated timber against biodeterioration in Indian waters
1984 - IRG/WP 4106
Results on the investigation on the durability of panels of 32 timber species, pressure-treated with various preservatives and exposed along the Indian coast for varying periods upto a maximum of 15 years, are summarised. Panels of even non-durable timber gave excellent results against biodeterioration after treatment. Their life was comparable to that of treated durable timber. The preservative t...
L N Santhakumaran, J C Jain, M C Tewari


Performance of borate-treated sill plates (dodai) in a protected, above-ground field test in Japan
2002 - IRG/WP 02-30278
This document is supplemental to the previous IRG document (IRG/WP 2000-30239). An experiment to simulate the dodai (sill plate) of the Japanese houses was conducted at the termite field test site of the Wood Research Institute in Kagoshima, Japan where two economically important subterranean termite species [Coptotermes formosanus Shiraki and Reticulitermes speratus (Kolbe)] are established. DOT...
K Tsunoda, A Adachi, A Byrne, P I Morris, J K Grace


Non-destructive stress wave measurement of decay and termite attack in experimental wood units
1986 - IRG/WP 2256
The purpose of this study was to determine if stress wave analysis could be used to monitor the degradation of wood specimens exposed to the brown-rot decay fungi (Gloeophyllum trabeum) and of wood specimens subjected to attack by subterranean termites. One hundred fifty 3/4 by 3/4 by 12 in. Southern pine specimens were used for exposure to brown-rot decay fungi and two hundred twenty-five 3/4 by ...
R F Pellerin, R C De Groot, G R Esenther


Disodium octaborate tetrahydrate, alone and in conjunction with a selected isolate of Trichoderma viride, reduces decay of fresh felled pine independent of the effect of weathering
1994 - IRG/WP 94-10054
Unpeeled billets of Corsican pine were treated with the following: 5% aqueous disodium octaborate tetrahydrate (DOT) solution; 5% DOT solution with an isolate of Trichoderma viride with a low susceptibility to borate; the Trichoderma viride isolate alone. Half of the billets in each treatment group were also placed in large-diameter plastic pipes to protect the billets from the weather. All three ...
M W Schoeman, D J Dickinson, J F Webber


Timber deterioration and its prevention in marine environment
2005 - IRG/WP 05-10559
Wood-borer activity is an established fact in Mumbai harbour that leads to severe deterioration of timber. In order to prevent the deterioration caused by wood borers three resin preservatives containing Zinc borate, Organo-copper polymer (4 wt% Cu) and Organo-Tin polymer &#61531;Copoly(TBTM-MMA)&#61533; were used for timber treatment. Test panels were treated using standard method and the...
B S Swami, M Udhayakumar, P Kumar, A B Samui


Rapid loss of lignin at wood surfaces during natural weathering
1992 - IRG/WP 92-2390
Thin veneers of radiata pine (Pinus radiata D. Don) were exposed to natural weathering over a period of 30 days. Incident UV radiation was monitored at the test site. FTIR internal reflectance spectroscopy was used to study the chemical changes taking place at the veneer surface during weathering. Spectra obtained show that after only 3 days exposure there was substantial delignification at veneer...
P D Evans, K J Schmalzl, A J Michell


Permanence of permethrin and bifenthrin in framing timbers subjected to hazard class 3 exposure
2005 - IRG/WP 05-30383
End-sealed Pinus radiata specimens measuring 235 x 90 x 35 mm were treated using a modified Lowry schedule with permethrin or bifenthrin in white spirit to Hazard Class 2 (H2) retentions. After conditioning, the specimens were exposed at 45o on north facing racks near Melbourne (Australia). Samples of the specimens were taken before installation, and after three and six months exposure. Analyses o...
A C Hunt, D G Humphrey, R Wearne, L J Cookson


The performance of metal-chromium-arsenic formulations after 32 to 38 years' in-ground exposure in Australia
2000 - IRG/WP 00-30240
Two trials of metal-chromium-arsenic preservatives were exposed in-ground in Australia. In Trial 1, Pinus radiata stakes treated with Boliden K.33, Boliden S.25, Celcure A, Tanalith C and Tanalith CA were installed at Sydney and Narrandera in 1961/1962. In Trial 2, P. radiata and Eucalyptus regnans sapwood were treated with Celcure A, Celcure A21-N, Celcure A 21-O and Tanalith CA (new) and install...
G C Johnson, J D Thornton, J Beesley


Blue stain in timber in service. Results of further IRG collaborative tests to compare different artificial weathering systems
1981 - IRG/WP 2146
The previous work described in Document No IRG/WP/286 examined 3 preservatives (1% phenyl mercury succinate - PMS, 5% pentachlorophenol - PCP and 1.5% Preventol A4 - PA4) subjected to 5 different artificial weathering systems (BAM Xenotest, Cuprinol Marr, EMPA Xenotest, Gori Atlas and PRL Marr) and after natural weathering at 5 sites (BAM, Cuprinol, EMPA, Gori and PRL). Results showed good correla...
A F Bravery, D J Dickinson


Performance of different treatments and finishes on wood out of ground contact. Preliminary results
1984 - IRG/WP 2221
Pinus and Eucalyptus L-joints treated with CCA, a water dispersable PCP and untreated ones were painted according to seven different finish&apos;s schedules and exposed at two sites in State of Sao Paulo. After ten months of exposure, it was possible to verify that preservative treatment improve the performance of both wood and finish. It was also possible to observe that wood substrate, prese...
S Milano


Performance of Paraserianthus falcataria treated with ACZA, ACQ, CC or CCA and exposed in Krishnapatnam harbour, India
2005 - IRG/WP 05-30382
Paraserianthus falcataria (=Albizia falcataria) treated to two retentions with ammoniacal copper zinc arsenate (ACZA), ammoniacal copper quaternary (ACQ), ammoniacal copper citrate (CC) and chromated copper arsenate (CCA) was assessed over 34 months in a tropical marine waters at Krishnapatnam harbour on the east coast of India. ACZA treatment showed comparatively better resistance than CCA, ACQ a...
B Tarakanadha, K S Rao, J J Morrell


Water-borne DNBP wood preservatives - Preparation and performance
1987 - IRG/WP 3407
Three waterborne wide-spectrum ground-contact DNBP (2-sec-butyl-4,6-dinitrophenol) wood preservative formulations and their performance are presented. Two are double-treatment formulations in which insolubilization and precipitation of the preservative is attained by salt formation or by formation of a water insoluble Cu/NH3/DNBP complex of formula [DNBP]2 [Cu(NH3)2]2 the clarified structure of wh...
W E Conradie, A Pizzi


Water-based silicones on wood
1997 - IRG/WP 97-30144
Five waterbased silicones commonly used on masonry where tested as water repellents for wood. The Water Repellent Effectiveness was determined by swellometer-tests and by measuring the water uptake of samples after 24 hours complete immersion and by immersion in a water level of 4 mm for 24 hours. The different methods are compared and discussed. Artificial and natural weathering was performed to ...
D Lukowsky, R D Peek, A O Rapp


Comparison of performance of wood preservatives in laboratory and field tests of treated commodities
1993 - IRG/WP 93-20010
The purpose of laboratory tests for evaluating efficacy of wood preservatives is usually to establish toxic values against standard strains of wood decay fungi. Exposure conditions are usually chosen as optimal for fungal growth. Toxic values so determined serve as a guide as to expected performance of the preservative in field stake tests or in above ground exposure tests. Test material is select...
M E Hedley


Modification of wood by graft treatment
2003 - IRG/WP 03-40257
New water-repellent systems for wood are needed to improve the weathering characteristics. This study found that treatment of wood with chemical grafting systems imparted substantial water repellency. Different direct oxidative grafting systems were examined. Specifically, KMnO4, Fe(NH4)(SO4)2·12H2O, Fe2(SO4)3·5H2O, and (NH4)2Ce(NO3)6 were used as initiators and styrene as the monomer. All the...
M M Morshed, D D Nicholas, C Pittman Jr, T Schultz


Performance of preservative-treated wood not in ground contact
1975 - IRG/WP 254
Experimental sash units of Pinus strobus L. and Pinus resinosa Ait. wood were removed from a test fence at Ottawa, Canada after outdoor exposure of over 20 years. The units were superficially treated, prior to painting, with preservatives containing either copper naphthenate, pentachlorophenol or a combination of zinc naphthenate and pentachlorophenol. Results indicated that all treatments were ef...
J K Shields, J Krzyzewski


Previous Page | Next Page