Performance of proprietary formulations of anti-sapstain preservatives on Hevea brasiliensis timbers in laboratory tests
1989 - IRG/WP 3532
A total of 10 proprietary and two experimental formulations were assessed for their effectiveness against sap-stain caused by Botryodiplodia theobromae on Rubberwood (Hevea brasiliensis). Sterilized wood samples 5x20x40 mm³ were dipped in the test chemicals for 60 seconds and then inoculated with 0.5 ml of culture filtrate of Botryodiplodia theobromae for incubation in sterile, damp petri dishes....
L T Hong


Microdistribution of water-borne preservatives in blue gum treated by full-cell process
1990 - IRG/WP 3617
The present work deals with the study of the microdistribution of copper, chrome and arsenic elements in Eucalyptus globulus Labill. sapwood, treated with a CCA water-borne preservative by full-cell process, with the help of scanning electron microscopy together with energy dispersion X-ray analysis technique. The work shows that the retention of CCA elements is high in vessels and vasicentric par...
D De Sousa Castro Reimão, J M Palacios


Field test of wood preservatives with Nasutitermes rippertii RAMBUR in Cuba
1996 - IRG/WP 96-10181
A field test of wood preservatives was carried out with Nasutitermes rippertii RAMBUR in the vicinity of the Material Testing Centre „Alexander von Humboldt" in Santiago de las Vegas/ Havana (Cuba) for 12 and 24 months. Test specimens of Pinus sylvestris L., Picea abies (L.) Karst. and Fagus sylvatica L. with dimensions of 25 x 25 x 490 mm³ were arranged vertically or horizontally in a circle o...
W Unger


Changes of EPR spectra of wood, impregnated with copper based preservatives, during exposure to Antrodia vaillantii
2000 - IRG/WP 00-10355
Spruce wood (Picea abies) samples were impregnated with two different aqueous solutions: copper(II) octanoate with ethanolamine or copper(II) sulfate (cCu = 1,0 x 10-2 mol/l). Impregnated and unimpregnated test pieces were exposed to wood rotting fungus Antrodia vaillantii. Some strains of this fungus are known as copper tolerant. After four weeks of exposure to A. vaillantii, we could not detect ...
M Humar, M Petric, F Pohleven, M Šentjurc


Influence of water-borne preservatives on water repellency and the impact of addition of water repellent additives
1992 - IRG/WP 92-3704
The primary goal of a desirable wood preservative system is to effectively control decay fungi and other biodeteriogens in service. The water repellent nature of a given system may play an important role in the protection of wood. In this study, the water repellency of several water-borne preservative systems has been evaluated by measurements of tangential swelling during immersion. The systems i...
L Jin, D M Roberts, A F Preston


Evaluation of a laboratory soft rot test on basis of weight loss and residual strength
1989 - IRG/WP 2336
Based on the principles of different previously reported experimental procedures dealing with laboratory soft rot testing, a study was conducted on treated poplar and beech. Preservatives used were CCA, CCF, AAC, Azaconazole and TCMTB. Treated samples were exposed for three months in a vermiculite substrate to Chaetomium globosum. Evaluation was based on absolute mass loss, percentage weight loss ...
W Verbeke, J Van Acker, M Stevens


Three-year field trials of polymeric formulations which provide a new basis for the invention and design of non-toxic wide-spectrum wood preservatives
1994 - IRG/WP 94-40029
Three types of non-toxic polymeric formulations invented using a new approach to wood preservation were challenged with termites and fungi in three-year ground-contact field trials in the sub-tropical climate of Natal. These formulations were copper soaps of carboxylic acid groups of unsaturated fatty acids of waxes and edible vegetable oils; of resin acids of rosin, and, of synthetic unsaturated ...
A A W Baecker, A Pizzi


Potential toxicants for controlling soft rot in preservative treated hardwoods. Part 2: Laboratory screening tests using sawdust
1977 - IRG/WP 2101
A technique is described for the rapid screening of toxicants against microorganisms, represented by the brown rot, Gloeophyllum trabeum, and a natural inoculum from soft rotted wood. Sawdust, in this case from sapwood of Eucalyptus maculata, is pretreated with the candidate formulation and moistened before inoculation. Visual scoring of growth can be used to discriminate suitable candidates as ea...
J D Thornton


Technologies for the Management of Wood Waste Containing Metals-Based Preservatives
2005 - IRG/WP 05-50224-16
Disposal of the metals from preservative treated wood can occur through two general strategies: “removal and confinement” or “dilution”. The acceptability of each of these two choices is typically dictated through the disposal regulations of a particular region. A considerable amount of research has been conducted to develop new and innovative “removal and confinement” technologies...
H M Solo-Gabriele, T G Townsend


A technique for measuring preservative loss or redistribution during leaching
1983 - IRG/WP 2199
Radiata pine sapwood stakes were treated with benzalkonium chloride (AAC) or copper-chrome-arsenate (CCA). After fixation and drying the outer 2 mm and 2-4 mm layers were removed from one radial longitudinal face. The planed face was coated with a waterproof coating and AAC-treated stakes were leached for 6, 12 or 18 weeks; 12 weeks for the CCA-treated stakes. After airdrying three 2 mm layers (0-...
J A Drysdale


Wood preservatives treatment of black spruce
1997 - IRG/WP 97-40092
A representative sample of black spruce logs from Central Newfoundland was harvested and processed to dressed 2"x4" lumber. Over 400 pieces of lumber were then incised and treated with ACQ preservative in a semi-industrial retort. 9 charges of 20 samples were used to determine treating parameters and 11 charges of 20 pieces were treated using the optimized process. This material was inspected by a...
A R Zahora, J P Hösli


Chemically modified tannin and tannin-copper complexes as preservatives for wood
2001 - IRG/WP 01-30271
The efficacy of Mimosa tannin, chemically modified tannin, and tannin-copper complexes as wood preservatives was studied. When the tannin-ammonia-CuCl2 solutions were impregnated into wood specimens in a one-step procedure, a large quantity of the tannin-copper complex was fixed in the specimens. Little of the complex was leached from specimens by a weathering treatment, and these specimens showed...
H Yamaguchi


Detoxification of salt impregnated wood by organic acids in a pulping process
1993 - IRG/WP 93-50012
The paper descibes a novel method to detoxify pine wood (Pinus silvestris L.) treated with CCB-, CCF- CC-, and Cu-HDO-type salt preservatives. In the process of biological detoxification organic acids produced by strains of Antrodia vaillantii and other brown rot fungi are used for the dissolution of the previously fixed inorganic compounds. These findings are the basis for applying an acid pulpin...
I Stephan, H H Nimz, R D Peek


Copper based wood preservative - A new approach using fixation with resin acids of rosin
2000 - IRG/WP 00-30249
Copper soaps with carboxylic acid groups of resin acids of rosin were shown to be potential long-term wood preservatives. The principle involved is the attachment of copper to the network formed by the inorganic part of the preservative (rosin) through the -COOH groups. The mechanisms of fixation have been studied, and it has been shown that this association could be obtained : (1) by forming the ...
C Roussel, J P Haluk, A Pizzi, M-F Thévenon


Experiences with environmental risk assessment within the Biocidal Products Directive
2005 - IRG/WP 05-50224-21
The Biocidal Products Directive (98/8/EC, the BPD) aims to authorize biocidal products based on risk assessment for both man and the environment. Active substances for wood preservation products and rodenticides were selected for the first list under the review program (Regulations EC 1896/2000 and EC 2032/2003) because several member states had experience with the evaluation and authorization of ...
P Blancquaert


A spectroscopic investigation of copper ethylenediamine fixation in wood
1999 - IRG/WP 99-20160
The fixation reaction which take place between copper ethylenediamine (Cu-en) solution and wood were expolored using X-ray photoelectron spectroscopy (XPS) and Fourier Transformed Infrared Spectroscopy (FTIR). The FTIR spectra revealed that copper reacts with the carboxylic acid and phenolic groups in wood to form stable complexes. The copper ethylenediamine complexes formed in wood were identifie...
Xiao Jiang, J N R Ruddick


Determination of toxicity data for preservatives against Basidiomycetes by measuring the reduction in compression strength of wood
1988 - IRG/WP 2297
Blocks of Pinus radiata D. Don were treated to 12 retention levels with CCA and NaPCP. These were exposed for 12 weeks in agar jars to the dry rot (brown rot) Serpula lacrymans (Schum. ex Fr.) S.F. Gray. After mass loss determination, the same blocks were tested for reduction in compression strength parallel to the grain. Using both these parameters, together with interpolated 6 week strength loss...
J Wazny, J D Thornton


Wood protecting chemicals for the 21st century
1993 - IRG/WP 93-30018
After assessing the past research with protection chemicals, this paper proposes future avenues for research and development in wood protection. Three scenarios are put forward for consideration. First, more is not better and future systems will emphasize combination formulations which enhance properties while providing biological efficacy. Second, current systems, especially those based on copper...
H M Barnes


The resistance of timbers to impregnation with wood preservatives
1979 - IRG/WP 3137
It is anatomical structure which determines liquid flow rate within different timber species. This cannot be deduced from properties such as density or rate of growth, and can only be found by experiment. A standard test has been in use at the Princes Risborough Laboratory for many years, employing a pressure-impregnation treatment, and a large number of timbers have been studied. The test consist...
Anonymous


Non agricultural biocide directive. Practical proposals of implementation in the case where biocides are wood preservatives
1995 - IRG/WP 95-50040-24
This project of non-agricultural biocide directive has currently an extremely wide scope of pre-marketing authorization of substances and preparations used in numerous applications, other than agricultural. Elaborated on the 86/414/EEC model of the phytopharmaceutical product directive, the "NAB" draft directive aims to cover situations as different as plant or wood protection: in the case of plan...
G Ozanne


Penetration and absorption of water-borne preservatives in conifers from the Western United States: A preliminary report
1988 - IRG/WP 3475
The treatment of most softwoods from the western United States with waterborne chemicals poses a major challenge. Although many of these species are commercially treated with waterbornes, there is considerable debate about their treatability. At present, there is little or no information on the treatability of western wood species with waterborne chemicals. The lack of accurate treatability inform...
S Kumar, J J Morrell


Less pollution due to technical approaches on accelerated steam fixation of chromated wood preservatives
1988 - IRG/WP 3487
Steaming of freshly treated wood at 100°C to 120°C initiates a spontaneous fixation of copper-chromate-containing wood preservatives. For the performance, a suitable anticorrosive equipment is necessary. Good results can be achieved using a separate steaming equipment which allows a rapid heating of the wood. While warming-up, in the wood some preservative solution extends and can be partly extr...
H Willeitner, R-D Peek


Depletion of preservatives from treated wood: Results from laboratory, fungus cellar and field test
1993 - IRG/WP 93-50001-07
This paper compares results of preservative component losses using a range of test procedures with several different water-borne preservatives. The data shows that laboratory leaching tests are in some cases comparable to, but in other cases significantly underestimate preservative component losses when compared with field or fungus cellar depletion tests. The results also suggest that preservativ...
L Jin, A F Preston


Effectiveness of wood preservatives and treatments against marine borers in Philippine waters
1976 - IRG/WP 416
A 5-year exposure test was conducted on the effectiveness of wood preservatives and treatments against marine borers in Philippine waters. Air-dried heartwood samples of apitong (Dipterocarpus grandiflorus) 76.2 x 88.9 x 609.6 mm³ (3 x 3.5 x 24 in³) in size were pressure treated with coal tar creosote and two types of CCA (copper/chrome/arsenic) and CuCZA (copperized chromated zinc arsenate) wat...
F R Siriban, M G Laxamana, P G Mata


IRG/COIPM INTERNATIONAL MARINE TEST - To determine the effect of timber substrate on the efectiveness of different preservatives in sea-water: Coding scheme
1976 - IRG/WP 420
It was agreed in Wildhaus on 15 May 1976 that preparations for the test detailed in Document No: IRG/WP/414 should commence immediately, but that initially only two water-borne preservatives should be used - a copper/chrome/arsenic (CCA) and a copper/chrome/boron (CCB) formulation respectively. PRL, England (R Cockcroft) would be responsible for supplying only the reference species treated with th...