Your search resulted in 646 documents. Displaying 25 entries per page.
Procedure for a collaborative study of leaching from CCA-treated timber in the sea
1988 - IRG/WP 4143
As a follow-up to the collaborative IRG/COIPM marine trial of CCA and CCB preservatives, a further trial is proposed with the objective of measuring the degree of leaching of CCA components from three timber species at marine sites in Malaysia and the U.K.. Details of the planned procedure are given....
S M Cragg, J E Barnacle, J D Bultman, R A Eaton, B R Johnson, L E Leightley, K D Singh
Natural Resistance of timbers to marine borer attack. COIPM/IRG CO-OPERATION. Final report concerning panels exposed in the sea at Sekondi, Ghana
1979 - IRG/WP 449
The test was carried out according to Document COIPM/72.044, Revised procedure for the testing of naturally durable timbers against marine borers. The panels of the three species remaining in the test at the end of 1978 were removed and assessed visually. An average rating was given to the panels of each species....
F F K Ampong
Treatment of dried sawn spruce and redwood building timbers with water-borne preservatives under a scheme for the quality control of the preservation and preserved wood in the Netherlands
1978 - IRG/WP 3123
Treatment of dried sawn spruce and redwood Building Timbers with water-borne preservatives under a scheme for the quality control of the preservation and preserved wood in the Netherlands. The aim of this article is to give the reader a modest description of the evaluation of fundamental research in wood preservation into a practical application....
H F M Nijman, N Burgers
Evaluation of wood treated with copper-based preservatives for Cu loss during exposure to heat and copper-tolerant Bacillus licheniformis
1999 - IRG/WP 99-20155
Copper-based wood preservatives need to be effective against exposure to all types of microorganisms. Wood treated with six copper-based preservatives was exposed to 121°C and 20 psi pressure for 15 minutes under standard autoclave conditions and the copper-tolerant bacterium, Bacillus licheniformis CC01, for 10 d at 28°C and 150 rpm. Sixteen to 37 percent of the copper was released from the woo...
D M Crawford, C A Clausen
The collaborative developement of soil acceptance criteria for timber treatment chemicals in New Zealand
1995 - IRG/WP 95-50040-34
In New Zealand, the issue of potential contamination on timber treatment sites arose in the late 80's due to the long history of use of PCP by the industry. One of the recommendations from the task group set up to investigate the issue was the development of a set of acceptance criteria to define trigger levels for remediation. A technical group from the government, industry and regional ...
H C Boyd
Fungal defacement of water-stored softwoods
1993 - IRG/WP 93-10009
Sapstain, mould and basidiomycete defacement of untreated sawn boards of Scots and Corsican pine was recorded during a 14 week field trial. Boards were cut from freshly felled logs and from logs previously maintained under water sprinklers for 6 months and ca. 4 years. The incidence of sapstain defacement or the freshly felled wood was very servere aftcr 2 weeks and remained so throughout the boar...
M A Powell, R A Eaton
Some thoughts on the future strategy for eradicating Serpula lacrymans from a building
1989 - IRG/WP 1405
We now have a clear view of the mechanism of translocation of nutrients in the mycelium of Serpula lacrymans which is one of the physiological processes underlying the remarkable capacity of this fungus to spread through a building. Here the elements of the mechanism of translocation are dissected out to suggest avenues which might be followed in the search for new ways for eradicating the fungus ...
D H Jennings
Microbial biofouling of 10-40% naphthalene in creosote treated and untreated wooden pilings in the marine environment
1978 - IRG/WP 442
R R Colwell, P L Fish, D A Webb, A J Emery
Volatile borates in the treatment of wood and wood based panel products against subterranean termites
1995 - IRG/WP 95-30094
Blocks of pine solid wood, oriented strand board and plywood were treated with trimethyl borate by vapour treatment. It was meant to obtain either a full impregnation of the specimens or a shell treatment of the outer three millimetres. The efficacy of the treatments against subterranean termites (Reticulitermes lucifugus) was evaluated using an European Standard method....
L Nunes, D J Dickinson, R J Murphy
Long-term performance of a "wax" type additive for use with water-borne pressure preservative treatments
2000 - IRG/WP 00-40159
Field performance results are updated for matched CCA treated decking boards with and without an emulsion water repellent additive incorporated with the initial pressure treatment. Decks have been exposured for over 9 years in Harrisburg, NC. Boards were evaluated for in-service and laboratory performance for water repellent efficacy, as well as additive loadings in the boards after this exposure....
A R Zahora
Migration of active ingredients from treated timber into fresh water
1991 - IRG/WP 3669
Spruce roundwoods and segments were treated with three different wood preservatives. Two of them containing copper and chromium the other one free of chromium. After fixation (3 weeks, 20°C) the specimens were leached by using artifical rain or by shaking the segments for one hour in contact with demineralized water. The water was analysed for the relevant elements of the preservative tested. Lea...
H Klipp, H Willeitner, K Brandt, A Müller-Grimm
About the water and biological resistance of some new chemically modified wood composites
1997 - IRG/WP 97-40077
As well known, wood represents a valuable natural composite material with a very large utilisation as solid wood or in wood based composite materials. Its qualities but also its defects as the dimensional instability, the susceptibility to biological attack, the anisotropy, are due to its complex structure. Research has demonstrated that the chemical modification of wood, meaning the involving of ...
M C Timar, M D Mihai, G Baciu
The effect of storage or simulated internal use on the durability of wood based panels to decay fungi
1997 - IRG/WP 97-20106
Wood based panels such as particleboard and medium density fibreboard are experiencing a steady increase in use, in areas from structural to decorative applications. Understanding the "natural" durability of these panel products against basidiomycete fungal decay is therefore of great importance. Various methods have been proposed or are under development to test the durability/susceptibility of v...
S F Curling, R J Murphy, J K Carey
Evaluation of polystyrene as a protective of wood in sea-water
1986 - IRG/WP 4129
A test is described on the biological protection of wood by treatment with polystyrene. The results, obtained in marine trials, after 18 months, show that the treatment with polystyrene is not all that effective in preventing the attack of marine borers....
A Gambetta
Marine borers and marine wood protection - Some answers and some outstanding questions - A comment
1990 - IRG/WP 4163
A brief description of the nature of hazards encountered in different parts of the marine environment is given. An attempt is then made to assess what were the essential findings of selected areas of research in the marine wood protection field and what still needs to be done. That is, if we are to more adequately understand what we are attempting to do in this field of study!...
J E Barnacle
Wood preservation in the Australian beekeeping industry
1988 - IRG/WP 3473
This paper reports the results of a survey of Australian commercial beekeepers working 200 or more hives in June/July 1985. Nine hundred and forty seven apiarists were asked to participate and to provide information on their wood preservation methods, painting procedures and maintenance of bee boxes. Three hundred and eighty-four apiarists returned completed questionnaires (41%). The main wood pre...
P J Robinson, J R J French
Effect of sterilization method on germination of spores of wood decay fungi observed by contact agar block method
1978 - IRG/WP 2117
Previous studies of germination of spores of wood decay fungi on wood have generally concluded that method of wood sterilization has little significant effect on germination response. This study expands the numbers of test fungi as well as number of sterilization methods employed to determine the influence of sterilization method on spore germination response of decay fungi. Germination was assess...
E L Schmidt, D W French
Combined effects of the treatment of wood with formaldehyde
1978 - IRG/WP 3117
Treatment of fibrous materials with reagents in a vapor phase is neither new nor unique. Numerous examples exist in literature of vapor phase experiments on cellulose fibers and fabrics, and on wood. For many years the textile research and industry have used vapor phase processes for the treatment of textiles. The chemical modification of cellulose is based on different types of reactions e.g. est...
M Stevens, J Schalck
A comparative field test of the effectiveness of anti-sapstain treatments on radiata pine roundwood
1986 - IRG/WP 3376
Peeled radiata pine posts were sprayed with one of six antisapstain formulations, with and without a wax water-repellent additive, to evaluate the protection given by each treatment. After 3 months' outside storage the best treatments tested were 4% product Busan 30, 2% product Busan 1009, and 2% active sodium pentachlorophenoxide (NaPCP) with 1.5% borax. After 6 months' storage ...
J A Drysdale, R M Keirle
A bibliography of organic solvent-based wood preservatives
1973 - IRG/WP 322
H Alliot
Water-repellent additive for CCA
1991 - IRG/WP 3655
Hickson have developed a water repellent additive for incorporation into copper-chromium-arsenate timber treatment solutions. The water repellent emulsion shows good stability in the treatment solution, is easily incorporated and applied in a single stage treatment. No modifications to the additive is safe to treatment schedule are usually needed and use. Weathering of the treated wood is substant...
P Warburton, R F Fox, J A Cornfield
The isolation of actinomycetes from wood in ground contact and the sea
1980 - IRG/WP 1110
M S Cavalcante, R A Eaton
Biodegradation of creosote/naphthalene-treated wood in the marine environment
1977 - IRG/WP 428
The present study was undertaken to determine the biodegradability of marine grade creosote and selected components, including naphtalene, and to determine the effectiveness of (up to 40%) creosote in protecting wood from microbial attack. Also, the impact(s) of creosote and naphtalene-enriched creosote on the microbial ecology os estuarine environments was examined....
P A Seesman, R R Colwell, A Zachary, A J Emery
Studies on the biological improvement of permeability in New Zealand grown Douglas fir
1983 - IRG/WP 3231
This report outlines progress towards optimizing conditions for water storage of New Zealand grown Douglas fir with the aim of improving permeability to water-borne preservatives, in particular CCA. Small scale laboratory tests are in progress but the need to scale up to potential commercial applications is being considered. Mixed populations of bacteria isolated from 10 week water sprinkled Dougl...
K J Archer
Experimental test site to prevent maritime pine logs from bluestaining: water-spraying and water-immersion methods
2003 - IRG/WP 03-10497
Following a storm which led to windfall wood, a research project was launched to develop preservation methods with a low environmental impact for maritime pine logs. These preservation methods are intended to be suitable for large-scale storage areas of maritime pine. In addition the aim was to maintain wood quality during long term storage. An experimental field test with 1 900 m3 of maritime pin...
I Le Bayon, H Callot, D Reuling, C Brunet, P Castéra