IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 558 documents. Displaying 25 entries per page.


Promoting Commercially Available Epoxy Resins for Non-biocidal Wood Preservation
2019 - IRG/WP 19-40877
Commercially available epoxy and polyamine resins were evaluated with the aim of developing new non-biocidal wood preservation treatments. A simple method allowing the impregnation of wood by vacuum double impregnation followed by a curing process was developed for two reference species, beech Fagus sylvatica and Scots pine Pinus sylvestris. The tested products were evaluated for their ability to ...
P Poveda, M Mubarok, S Dumarcay, M Montibus, I Le Bayon, M Kutnik, P Gerardin, F Simon


Alternative products enhancing dimensional stability comparing to conventional treated products in Japan
2019 - IRG/WP 19-40885
The Act on the Promotion of the Utilization of Wood in Public Buildings (2010) in Japan has made a new stream of the utilization field of timber from housing constructions to larger scale non-housing constructions. After the act, the performance of dimensional stability in preservative treated products becomes more important factor than before. Therefore, various technologies have been developed, ...
K Yamamoto, D Tezuka, Y Sugai, S Maeda, I Momohara


Wood veneer with high flexible decorated with nanoparticles for highly efficient water treatment
2019 - IRG/WP 19-50347
Natural wood is mainly comprised of numerous long, partially aligned channels (lumens) as well as nanochannels. Wood with these quick and effective passages is suitable for a membrane/separation material. However, a suitable thickness range of wood along its growth direction is essential to effectively separate small molecular, and the wood membrane is too thick to clean easily. In this paper, woo...
S Chang, D Xu, G Liu, J Hu, X Li, Y Liu


Effect of long-term immersion in fresh and salt water on mould growth on Scots pine (Pinus Sylvestris L.) wood
2020 - IRG/WP 20-10962
Wood exposed outdoors will eventually be degraded by fungi, depending on exposure and material characteristics. Numerous wooden constructions in the Røros municipality have existed since the 17th century, but wood used in recent repairs have decayed faster than expected. Before 1970 timber was mainly transported by log driving or rafting, and the logs were immersed in water for longer or shorter ...
M Sand Austigard, J Mattsson


Water interactions in wood polyesterified with sorbitol and citric acid
2020 - IRG/WP 20-40888
Polyesterifcation of wood with sorbitol and citric acid seems to be a promising chemical wood modification technique that is both low-cost and produced from bio-based chemicals. An interesting aspect of the modification is the interaction of water with the polyesterified wood since the relationship with moisture appears to be unique compared to other wood modification systems. This communication p...
G Beck, A Treu, E Larnøy


Performance of a water-borne stain on beech, spruce, MDF and OSB improved by plasma pre-treatment
2020 - IRG/WP 20-40897
Coatings are an important part of wood protection, especially for outdoor applications. In order to provide a good protection, protective coatings need to exhibit good adhesion, mechanical resistance, and weathering resistance. Plasma pre-treatments are an established method to increase the performance of existing coatings including those on wood and wood-based substrates. Moreover, plasma deposit...
S Dahle, J Žigon, I Uranjek, M Petrič


Comprehensive protection of timber in seawater
2020 - IRG/WP 20-10970
The hazard of wood in seawater can be divided into two areas: Below the water level, shipworm (Teredo navalis) and gribble (Limnoria lignorum) can attack non-resistant or insufficiently protected wood; above the water level, there is a risk by wood-destroying fungi and, to a lesser extent, insects. In a national project funded by the Deutsche Bundesstiftung Umwelt (DBU, German Federal Environmenta...
E Melcher, J Müller, T Huckfeldt


Silicate coatings for wood substrates
2020 - IRG/WP 20-40906
Silicate coatings are surface finishing products containing alkali metal silicates or ethyl silicates as main binders. They are traditionally designed and well established for mineral substrates or corrosion protection of steel. The interest for these coatings in wood field is growing because of the benefits they could provide such as high durability, weathering resistance and fireproofing and sus...
A M Cheumani Yona, M Pavlič, M Petrič


Surface morphology and short-term water uptake of charred and coated wood
2021 - IRG/WP 21-40916
Charring of the wood surface represents a traditional alternative surface treatment technique with the purpose of aesthetics and protection. By the treatment with flame the surface of wood becomes carbonized and a few millimetres thick charred layer is formed on the top of the wooden element. Further, the charred layer can be removed by brushing, which accentuates the structure of the surface. Add...
J Zigon


Studies on the material resistance and moisture dynamics of Douglas fir and Sitka spruce from Slovenia
2021 - IRG/WP 21-20677
Wood in outdoor applications is subject to various decomposition factors. Wood degradation can be prevented by construction details, biocide protection of wood, wood modification, or selection of naturally durable wood species. Unfortunately, the majority of timber species in Europe do not have naturally durable wood. Imported tree species represent a new pool from which we can draw wood species w...
M Humar, B Lesar, D Krzisnik, E Kerzic, R Brus


Preliminary investigation for preservation method of CLT using non-pressure treatment
2021 - IRG/WP 21-40919
Cross-laminated Timber (CLT) is increasingly being used in residential and non-residential construction around the world, and some of these areas are at high risk of biodeterioration. Addition to moisture management of construction, preservative treatment of CLT may be needed to prevent decay and termite attack in the area. Pressure treatment being most reliable, is not feasible due to the large d...
T Miyauchi, Y Ohashi, J Miyazaki, R Takanashi, H Shibui, S Isaji, T Shigeyama, Y Sugai, A Yamamoto, T Hramiishi, T Mori, H Matsunaga


Treatability of South African-grown Eucalyptus grandis with water-borne copper azole and disodium octaborate tetrahydrate wood preservatives
2021 - IRG/WP 21-40920
This study investigated the treatability of the sapwood and heartwood of sawn Eucalyptus grandis with copper-azole (CuAz) and disodium octaborate tetrahydrate (DOT) water-borne preservatives towards improving its durability for enhanced use in structural solid wood applications. The results obtained showed that, at a moisture content of 12 ± 1%, sawn E. grandis sapwood can be impregnated to a mea...
A A Alade, Z Naghizadeh, C B Wessels


Effect of a Water Repellent Treatment on Moisture Behavior of Three Australian Hardwoods: A Preliminary Report
2021 - IRG/WP 21-40921
Wood is inherently hygroscopic and will sorb moisture either directly from the atmosphere or via capillary action. Moisture can have marked effects on wood properties and repeated wetting and drying creates dimensional changes that lead to physical damage. Exposure to elevated moisture levels also increases the risk of fungal attack. Wood preservatives have long been used to minimize the risk of ...
B Hassan, J J Morrell, K Wood


Evaluation of weathering and termite resistance of the Myoung-oil as a Korean traditional coating agent
2022 - IRG/WP 22-10996
This study investigated the applicability of Myoung-oil (MO) as an eco-friendly preservative of Korean wooden cultural properties and buildings. Wood test specimens painted with various concentrations of MO were exposed in the external environment. Then color change and wettability of the wood surface were evaluated and compared depending on the exposure time. As a result of exposure for 12 months...
S-M Yoon, Y Park, W-S Jeon, H-M Lee, J-G Park, K Dal Nam, W-J Hwang


Properties of Iron (II) Sulphate treated Norway Spruce
2022 - IRG/WP 22-30765
Exterior wood is exposed to various environmental factors that cause weathering. Weathering is important primarily from an aesthetic standpoint. However, not all parts of the building are equally susceptible to weathering. Parts exposed to moisture will discolour faster than protected parts, such as wood under roof overhangs. To achieve fast and uniform artificial greying, a surface treatment with...
B Lesar, M Humar, M Škamlec


Field tests of different tropical wood species in sea water
2022 - IRG/WP 22-30773
A number of tropical timbers have been tested according to EN 275 at Kristineberg Marine Research Station in Sweden since 1999. Most of these tests have started during the last 5-8 years. Wood species included have been Lophira alata (Azobé/Ekki), Minquartia guianensis (Manwood/Acaria), Chlorocardium rodiei (Greenheart), Cyclodiscus gabonensis (Okan/Denya), Shorea spp. (Bankirai), Dicorynia guia...
M Westin, P Larsson Brelid


A novel wood preservation technology improving durability and water-related properties
2022 - IRG/WP 22-40926
A newly developed silicone oil (Archroma Management GmbH, Switzerland) was tested for wood modification purposes. Scots pine sapwood was treated with aqueous solutions of this silicone oil and showed a penetration of the modification agent into the wood cell wall. Both, biological durability and moisture-related properties, experienced significant improvements by the modification. Besides, the mod...
L Emmerich, H Militz, M Vila


The influence of thermal modification and surface charring to different levels on wettability of Norway spruce wood
2022 - IRG/WP 22-40942
The wood can alternatively be protected from water absorption by thermal modification and charring. Both techniques cause certain chemical and physical changes in the wood, the extent of which depends on the level of temperature applied. The objective of this study was to determine how the combination of charring to different levels and thermal modification affects the chemical, morphological, and...
J Žigon, C Gerardin, M E P Wålinder, P Gerardin


Moisture sorption behaviour of poplar and thermally modified poplar using dynamic vapour sorption (DVS)
2022 - IRG/WP 22-40947
The moisture sorption behaviour of wood has a critical impact on service life. In Europe, softwood is mostly used to manufacture engineered wood products such as cross-laminated timber (CLT) or glue-laminated timber (GLT or glulam). Yet fast-growing and widespread tree species such as hybrid poplar with or without modification, have potential to meet the increasing demand. This study shows the moi...
X Jiang, J Van den Bulcke, L De Boever, M Minsart, A Mignon, J Van Acker


Utilization of Pressure Treated Lumber in Cross Laminated Timber Manufacture and its Impact on Bondline
2022 - IRG/WP 22-40953
Mass timber building construction is increasing dramatically across North America which presents challenges to these structures not seen in Northern Europe. Large parts of the United States harbor termites and existing mass timber building technologies that rely solely on moisture exclusion to increase durability are insufficient in these areas. The successful expansion of mass timber construction...
G Presley, C Wainscott, J Valenti, S Noble


Assessment of the Material Durability and Structural Integrity of the Wooden Velodrome in Češča vas, Slovenia
2023 - IRG/WP 23-11012
Wood is a widely used material in the construction industry, and it has been utilized for thousands of years to create buildings and other structures. When wooden structures are designed, built, and maintained properly, they can be safe and long-lasting. Sports facilities, which provide athletes with a space to train, compete, and improve their abilities, are crucial in creating a strong and susta...
D Kržišnik, M Humar, B Lesar


Identifying compatible waterborne timber preservatives and fire retardants for use in a VPI system: a practical approach
2023 - IRG/WP 23-30796
To enhance the use and suitability of timber in all applications in both exterior and interior settings, timber typically needs to be treated with a preservative and/or a fire retardant chemical. Combining fire retardants with preservatives into a single treatment process has been a long-term aim of researchers in the timber preservative industry because of the significant logistic and economic ad...
R Robinson, S Meldrum


Biological durability and wood-water interactions of sorbitol and citric acid modified wood – Effects on the expected service life
2023 - IRG/WP 23-40960
A high level of research activities on sorbitol and citric acid (SorCA) modified wood has been recognized in Europe over the last few years. As this treatment is close to entering an industrial-scale production, it is of interest to investigate how such treated wood performs upon long-term outdoor exposure. Hence, in this study Scots pine (Pinus sylvestris L.) sapwood was modified with aqueous sol...
K Kurkowiak, L Emmerich, H Militz


Non-vacuum/pressure ACQ treatment
2023 - IRG/WP 23-40971
Many developing countries are located in sub-tropical or tropical regions where rapid wood deterioration results in early failure of many structures. Whilst preservative treatment would help to reduce these losses and extend the forest resource commercial vacuum pressure treatment systems are often too expensive. The use of lower technology treatment systems, while not as quick as vacuum pressure ...
J Norton


Short-term absorption of water and coatings on thermally modified blue-stained spruce wood
2023 - IRG/WP 23-40984
The importance of wood has been increasing in the last decades. Among conifers, predominantly spruce (Picea abies) wood is often used in building constructions in Europe. Namely for construction and facades of buildings, decking and fences. Due to the increased public concerns about biocides, alternative techniques for protection, such as thermal modification and protection by construction, are ga...
R Hasanagic, M Bahmani, M Humar, L Fathi, L Cai


Previous Page | Next Page