IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 405 documents. Displaying 25 entries per page.


A comparative field test of the effectiveness of anti-sapstain treatments on radiata pine roundwood
1986 - IRG/WP 3376
Peeled radiata pine posts were sprayed with one of six antisapstain formulations, with and without a wax water-repellent additive, to evaluate the protection given by each treatment. After 3 months' outside storage the best treatments tested were 4% product Busan 30, 2% product Busan 1009, and 2% active sodium pentachlorophenoxide (NaPCP) with 1.5% borax. After 6 months' storage ...
J A Drysdale, R M Keirle


Studies on the biological improvement of permeability in New Zealand grown Douglas fir
1983 - IRG/WP 3231
This report outlines progress towards optimizing conditions for water storage of New Zealand grown Douglas fir with the aim of improving permeability to water-borne preservatives, in particular CCA. Small scale laboratory tests are in progress but the need to scale up to potential commercial applications is being considered. Mixed populations of bacteria isolated from 10 week water sprinkled Dougl...
K J Archer


Biodegradation of creosote/naphthalene-treated wood in the marine environment
1977 - IRG/WP 428
The present study was undertaken to determine the biodegradability of marine grade creosote and selected components, including naphtalene, and to determine the effectiveness of (up to 40%) creosote in protecting wood from microbial attack. Also, the impact(s) of creosote and naphtalene-enriched creosote on the microbial ecology os estuarine environments was examined....
P A Seesman, R R Colwell, A Zachary, A J Emery


Surface coatings for impregnated wood
1992 - IRG/WP 92-3684
The use of proper surface coatings enhances the aesthetic and protective properties of impregnated wood. Good results with especially water-borne coatings have been obtained for class-A impregnated L-joints and claddings in field tests started in 1982....
L Kotama


Experimental test site to prevent maritime pine logs from bluestaining: water-spraying and water-immersion methods
2003 - IRG/WP 03-10497
Following a storm which led to windfall wood, a research project was launched to develop preservation methods with a low environmental impact for maritime pine logs. These preservation methods are intended to be suitable for large-scale storage areas of maritime pine. In addition the aim was to maintain wood quality during long term storage. An experimental field test with 1 900 m3 of maritime pin...
I Le Bayon, H Callot, D Reuling, C Brunet, P Castéra


The rate of redistribution and loss of leachable preservatives under service conditions
1993 - IRG/WP 93-30026
This paper describes experiments carried out to determine patterns of preservative redistribution and any associated losses which occur when wood containing unfixed water-soluble wood preservatives is exposed to service conditions where leaching is possible. Scots pine sapwood treated with disodium octaborate was used as a model system. Results are recorded and discussed for trials representing pa...
R J Orsler, G E Holland


Report on marine borer attack on some timbers treated with CCA wood preservative and exposed for three months in sea-water
1985 - IRG/WP 4112
Destruction of timbers by marine borers has long been a problem for the coastal population of Thailand. The use of heavy durable timbers with frequent maintenance, or total replacement, is the only solution for fishermen with their fishing craft or marine installations, meanwhile wharves or other large scale constructions are usually made by using concrete pilings or concrete casings. In recogniti...
A Rananand, W Yoosukh, U Sittiphuprasert


Collaborative soft rot tests: Proposed amendments to Document No: IRG/WP/208
1973 - IRG/WP 224
J K Carey, J G Savory


300 years water-logged wood: Treatability with CCA-C
1998 - IRG/WP 98-40103
The treatability of 300 years water-logged and recent wood (Abies bornmülleriana M.) was assessed by dip treatment and vacuum and pressure cycling with CCA-C. Treatment runs were evaluated on the basis of weight gain retention and radial and tangential penetration measurements. The preservative penetration and retention levels in the 300 years water-logged wood were higher than in the recent wood...
S N Kartal, N Yilgör


Leaching tests - A paper for discussion
1973 - IRG/WP 221
J W W Morgan


IRG/COIPM INTERNATIONAL MARINE TEST - to determine the effect of timber substrate on the effectiveness of water-borne salt preservatives in sea-water: Final report
1987 - IRG/WP 4133
Three timbers chosen as reference species were treated with 3, 6 and 10% solutions of CCA and CCB preservatives and exposed for up to 93 months at 8 tropical and temperate marine sites. Eleven local species treated in the same way were exposed at 4 of the 8 sites. There was no apparent difference in performance between CCA and CCB treated specimens. The severest test site was Panama Canal but mari...
R A Eaton


Treatment of particleboard with isocyanate resin to impart improved dimensional stability and water repellency
2000 - IRG/WP 00-40178
Standard particleboard panels (for interior use) of 16 mm nominal thickness were cut into samples measuring 6.4 mm x 78 mm2. The samples were divided into 4 end matched batches. Two batches were treated with isocyanate resin and cured. The other 2 batches were left untreated. One of the treated batched and 1 of the untreated batches were edge sealed with epoxy resin prior to isocyanate resin appli...
K M Filcock, P Vinden


Creosote movement from treated wood immersed in fresh water: Initial PAH migration
2003 - IRG/WP 03-50201
Creosote has a long history of successful use as a wood preservative, but polycyclic aromatic hydrocarbons (PAHs) in this preservative have raised environmental concerns, particularly when creosote-treated wood is used in aquatic environments. A number of models have been developed to predict the risk of creosote use in aquatic environments, but one limitation of these models is a lack of data o...
Sung-Mo Kang, J J Morrell, J Simonsen, S T Lebow


Copper based water-borne preservatives: The biological performance of wood treated with various formulations
1987 - IRG/WP 3451
Wood samples treated with the various components of CCA preservative singly and in combination were tested against a soft rot organism, a copper tolerant brown rot organism and in soil burial both unleached and after leaching. The results suggest that, of the elements tested, fixed copper is essential for preventing soft rot attack and fixed arsenic is essential for preventing attack by a copper t...
S M Gray, D J Dickinson


Testing wood in ground contact: An artificial soil
1977 - IRG/WP 280
This document is an interim report on the development of the artificial soil medium. It includes some information on the relationship between soil, wood and water which is of relevance in testing....
E F Baines, D J Dickinson, J F Levy


Waterborne silicones as wood preservatives
1995 - IRG/WP 95-30062
For more than thirty years silicones are used as water repellents for masonry. Their excellent properties make them also attractive for non-mineral substrates like wood. Although it was always thought that silicones are not able to perform on wood, a new type of aqueous silicone materials proofed the opposite: Excellent water repellency and astonishing durability were achieved. This paper describe...
R Hager


Examination of timbers from the Mary Rose in storage
1988 - IRG/WP 4149
Timbers from the Tudor ship, Mary Rose, have been examined for the presence of fungal fruiting structures. Wood specimens were also examined for the presence of microbial decay patterns using light and scanning electron microscopy. Structural timbers were surveyed using the Pilodyn for an overall picture of the extent of decay. Mary Rose timbers were predominantly inhabited by marine fungi. Fourte...
R Mouzouras


Practical testing of wood preservatives to prevent weathering damage and infection by micro-organisms on spruce and pine
1989 - IRG/WP 3530
Brush application, is generally used to prevent wooden window frames from decay caused by influence of weathering and fungi. Accordingly 10 boards of pine (Pinus sylvestris) and spruce (Picea abies) were treated with 10 commercially used wood preservatives. The efficiency of fungicides by using chiptest and blue stain test (EN 152), the effectiveness against weathering as well as the course of col...
R Gründlinger, O Janotta, H Melzer, K Messner


Assessment of contamination of soil and water at a CCA treatment plant: A demonstration project
1996 - IRG/WP 96-50067
Soil, sludge, dust and water samples were collected at a copper/chromium/arsenic wood preservation plant. Contamination of soil, sludge, dust and surface water with copper, chromium and arsenic was detected. Levels of contamination were sufficiently high to require remediation. Contamination originated from preservative solution dripping from recently treated wood. Migration of contaminants was vi...
P N Durrant, D C R Sinclair, G M Smith


An interim report on trials with 'Boliden K33' and 'Celcure A' in water of different salinities in the Baltic Sea and in the UK
1974 - IRG/WP 406
It was felt necessary to undertake field trials using large test samples exposed in natural water of different salinity in order to determine preservative leaching and to assess the degree of biological attack....
R A Eaton, D J Dickinson


Copper based water-borne preservatives: The use of a thin section technique to compare the protection of wood by copper based preservatives against soft-rot and bacterial decay
1987 - IRG/WP 2286
This paper describes the techniques developed and gives examples of results obtained for the performance of copper based wood preservatives against both the bacterial and fungal hazards....
A M Wyles, D J Dickinson


Chapter 6 - Preservatives of bamboo
2007 - IRG/WP 07-10635-06
Almost all currently available oil-borne, water-borne and compound types of preservatives suitable for the preservation of bamboo or wood have been described along with their classifications, applications, formulations, merits and demerits, history of invention or discovery and development. The preservatives suitable for wood are also considered suitable for bamboo....
A K Lahiry


Differential behaviour of wood rotters at water repellent Rubberwood
2000 - IRG/WP 00-10386
Rubberwood samples treated with different concentration of aqueous solution of chromic acid has induced significant increase in water repellency and attains dimensional stability. Though water repellency and dimensional stability was achieved by treatment, the fungal invasion could not be completely controlled. Differential level of decay of brown and white rot in wood treated with water repellent...
H C Nagaveni, S S Chauhan, K S Rao


Effect of leaching temperature and water acidity on the loss of metal elements from CCA treated timber in aquatic conditions. Part 2: Semi-industrial investigation
1995 - IRG/WP 95-50040-13
In continuation of previous leaching research on the quantification and modelling of metal elements released from CCA treated timber, a series of experiments has been carried out dealing with the influence of temperature and pH of the relative aquatic environment. The leaching method used is the Dutch prestandard for building materials, a long term static leaching test simulating practical bank-sh...
G M F Van Eetvelde, W J Homan, H Militz, M Stevens


Some observations on miniaturised soil/block tests
1988 - IRG/WP 2317
Results are presented for miniaturised soil/block tests carried out in 120 ml capacity glass jars. The four test fungi (Coniophora puteana, Coriolus versicolor, Gloeophyllum trabeum and Poria placenta) reacted differently to different moisture regimes established by varying the soil moisture content. Acceptable levels of decay were achieved by the three brown rot fungi with soil at 110% whc; howev...
J K Carey


Previous Page | Next Page