IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 529 documents. Displaying 25 entries per page.


Treatment of particleboard with isocyanate resin to impart improved dimensional stability and water repellency
2000 - IRG/WP 00-40178
Standard particleboard panels (for interior use) of 16 mm nominal thickness were cut into samples measuring 6.4 mm x 78 mm2. The samples were divided into 4 end matched batches. Two batches were treated with isocyanate resin and cured. The other 2 batches were left untreated. One of the treated batched and 1 of the untreated batches were edge sealed with epoxy resin prior to isocyanate resin appli...
K M Filcock, P Vinden


Creosote movement from treated wood immersed in fresh water: Initial PAH migration
2003 - IRG/WP 03-50201
Creosote has a long history of successful use as a wood preservative, but polycyclic aromatic hydrocarbons (PAHs) in this preservative have raised environmental concerns, particularly when creosote-treated wood is used in aquatic environments. A number of models have been developed to predict the risk of creosote use in aquatic environments, but one limitation of these models is a lack of data o...
Sung-Mo Kang, J J Morrell, J Simonsen, S T Lebow


Copper based water-borne preservatives: The biological performance of wood treated with various formulations
1987 - IRG/WP 3451
Wood samples treated with the various components of CCA preservative singly and in combination were tested against a soft rot organism, a copper tolerant brown rot organism and in soil burial both unleached and after leaching. The results suggest that, of the elements tested, fixed copper is essential for preventing soft rot attack and fixed arsenic is essential for preventing attack by a copper t...
S M Gray, D J Dickinson


Examination of timbers from the Mary Rose in storage
1988 - IRG/WP 4149
Timbers from the Tudor ship, Mary Rose, have been examined for the presence of fungal fruiting structures. Wood specimens were also examined for the presence of microbial decay patterns using light and scanning electron microscopy. Structural timbers were surveyed using the Pilodyn for an overall picture of the extent of decay. Mary Rose timbers were predominantly inhabited by marine fungi. Fourte...
R Mouzouras


A comparison between methods for evaluating the water repellency of wood
1989 - IRG/WP 2328
Wood specimens treated with a number of water repellent formulations have been tested for their water repellency according to four laboratory test methods, based on weight increase, swelling and contact angle measurements, in order to assess the degree of agreement between the different methods. Treatments representing formulations with a wide range of water repellent efficiency were tested both i...
R Nussbaum


Testing wood in ground contact: An artificial soil
1977 - IRG/WP 280
This document is an interim report on the development of the artificial soil medium. It includes some information on the relationship between soil, wood and water which is of relevance in testing....
E F Baines, D J Dickinson, J F Levy


Waterborne silicones as wood preservatives
1995 - IRG/WP 95-30062
For more than thirty years silicones are used as water repellents for masonry. Their excellent properties make them also attractive for non-mineral substrates like wood. Although it was always thought that silicones are not able to perform on wood, a new type of aqueous silicone materials proofed the opposite: Excellent water repellency and astonishing durability were achieved. This paper describe...
R Hager


Practical testing of wood preservatives to prevent weathering damage and infection by micro-organisms on spruce and pine
1989 - IRG/WP 3530
Brush application, is generally used to prevent wooden window frames from decay caused by influence of weathering and fungi. Accordingly 10 boards of pine (Pinus sylvestris) and spruce (Picea abies) were treated with 10 commercially used wood preservatives. The efficiency of fungicides by using chiptest and blue stain test (EN 152), the effectiveness against weathering as well as the course of col...
R Gründlinger, O Janotta, H Melzer, K Messner


Assessment of contamination of soil and water at a CCA treatment plant: A demonstration project
1996 - IRG/WP 96-50067
Soil, sludge, dust and water samples were collected at a copper/chromium/arsenic wood preservation plant. Contamination of soil, sludge, dust and surface water with copper, chromium and arsenic was detected. Levels of contamination were sufficiently high to require remediation. Contamination originated from preservative solution dripping from recently treated wood. Migration of contaminants was vi...
P N Durrant, D C R Sinclair, G M Smith


Differential behaviour of wood rotters at water repellent Rubberwood
2000 - IRG/WP 00-10386
Rubberwood samples treated with different concentration of aqueous solution of chromic acid has induced significant increase in water repellency and attains dimensional stability. Though water repellency and dimensional stability was achieved by treatment, the fungal invasion could not be completely controlled. Differential level of decay of brown and white rot in wood treated with water repellent...
H C Nagaveni, S S Chauhan, K S Rao


Effect of leaching temperature and water acidity on the loss of metal elements from CCA treated timber in aquatic conditions. Part 2: Semi-industrial investigation
1995 - IRG/WP 95-50040-13
In continuation of previous leaching research on the quantification and modelling of metal elements released from CCA treated timber, a series of experiments has been carried out dealing with the influence of temperature and pH of the relative aquatic environment. The leaching method used is the Dutch prestandard for building materials, a long term static leaching test simulating practical bank-sh...
G M F Van Eetvelde, W J Homan, H Militz, M Stevens


Investigation of the fixation in wood of chromated zinc chloride and copperised chromated zinc chloride preservatives
1976 - IRG/WP 372
A biological method of evaluating the extent to which CZC and CCZC preparations are retained in wood in terms of the potential protection which they afford against destruction by Merulius lacrymans (dry rot) is given. CCZC is recommended for protection of wood under moderate leaching conditions, while the use of CZC under such conditions is not recommended....
V N Sozonova, D A Belenkov


An interim report on trials with 'Boliden K33' and 'Celcure A' in water of different salinities in the Baltic Sea and in the UK
1974 - IRG/WP 406
It was felt necessary to undertake field trials using large test samples exposed in natural water of different salinity in order to determine preservative leaching and to assess the degree of biological attack....
R A Eaton, D J Dickinson


Some observations on miniaturised soil/block tests
1988 - IRG/WP 2317
Results are presented for miniaturised soil/block tests carried out in 120 ml capacity glass jars. The four test fungi (Coniophora puteana, Coriolus versicolor, Gloeophyllum trabeum and Poria placenta) reacted differently to different moisture regimes established by varying the soil moisture content. Acceptable levels of decay were achieved by the three brown rot fungi with soil at 110% whc; howev...
J K Carey


Effect of double-vacuum and vacuum-pressure impregnation with water-borne preservatives on the dimensional characteristics of spruce
1990 - IRG/WP 3613
Air-dried planed spruce (Picea abies) samples were treated with a water-borne preservative (micro-emulsion) and one oil-borne type both containing azaconazole and deltamethrin. Each set of samples contained equal number of specimens with different growth ring orientation, heartwood content and density. In addition to the preservative retention and the penetration of a.i., the swelling of the sampl...
J Van Acker, M Stevens, G Rustenburg


Washboard effect: A surface deformation of spruce resulting from vacuum-pressure impregnation with water-borne preservatives
1987 - IRG/WP 3450
The washboard effect has been observed in sawn spruce after both commercial and laboratory based preservative treatments and is of increasing economic importance. The effect is defined as a specific phenomenon at the wood surface. It is distinct from internal collapse in the wood, but it may occur in association with internal collapse damage. Experimental investigations on the causes of washboardi...
H Willeitner, R J Murphy


Potential toxicants for controlling soft rot in preservative treated hardwoods. Part 4: Evaluation of combined diffusion and toxicity
1979 - IRG/WP 2129
A large number of inorganic and organic preservatives were evaluated as potential soft rot control chemicals, by their degree of inhibition of fungal growth after allowing them to diffuse through a 6 mm thick wood slab. The tests were inoculated with wood powder from soft-rotted CCA treated poles. Pentachlorophenol was unable to diffuse quickly through the wood slab, although formulations with hex...
E W B Da Costa, O Collett


Copper based water-borne preservatives: The use of a thin section technique to compare the protection of wood by copper based preservatives against soft-rot and bacterial decay
1987 - IRG/WP 2286
This paper describes the techniques developed and gives examples of results obtained for the performance of copper based wood preservatives against both the bacterial and fungal hazards....
A M Wyles, D J Dickinson


The potential for accelerated ageing to determine the persistence of active ingredients in timber
2006 - IRG/WP 06-20323
Fast screening methods for evaluating the persistence of active ingredients in timber are proposed. This is an outline proposal which is intended to provoke discussion and further development of the methods. Reliable and accurate analytical methods are key to these tests....
L D A Saunders, M R Powell


Agenda Special Seminar: Screening techniques for potential wood preservative chemicals
1978 - IRG/WP 2115
IRG Secretariat


Chapter 6 - Preservatives of bamboo
2007 - IRG/WP 07-10635-06
Almost all currently available oil-borne, water-borne and compound types of preservatives suitable for the preservation of bamboo or wood have been described along with their classifications, applications, formulations, merits and demerits, history of invention or discovery and development. The preservatives suitable for wood are also considered suitable for bamboo....
A K Lahiry


IRG/COIPM INTERNATIONAL MARINE TEST - to determine the effect of timber substrate on the effectiveness of water-borne salt preservatives in sea-water. 3rd Interim Report
1983 - IRG/WP 4101
This paper updates the results of microbiological examination and marine borer assessment of untreated wood samples (15 x 2 x 2 cm³) and samples treated with 3, 6 and 10% CCA and CCB preservatives. Three reference species - Alstonia scholaris, Fagus sylvatica, Pinus sylvestris were used at all the test sites in addition to local species chosen by participants in the test....
R A Eaton


Natural durability of some common Indian timbers and marine plywood against biodeterioration in Kochi waters (India)
1992 - IRG/WP 92-4177
Panels of thirty-eight timber species and marine plywood were tested in Kochi harbour (South-west India) for periods ranging from 3 to 21 months, so as to evaluate their natural resistance against marine borers. Results indicate that all the timber species studied are non-durable, 6 of them having undergone more than 50% internal destruction within 3 months; 14 species in 6 months, 13 species and ...
L N Santhakumaran, M V Rao


Leaching of inorganic wood preservatives – Investigating the relationship between leachability, dissociation characteristics and long-term leaching potential
2003 - IRG/WP 03-50199
Estimation of the leaching properties of preservative components is greatly affected by the leaching test method applied since not all methods equally consider the physical components responsible for leaching. These include: wetting of the wood and penetration of water (affected by dimensions, amount of end grain, permeability, duration and nature of water exposure); solution of preservative comp...
L Waldron, Y T Ung, P A Cooper


Water-borne preservative marine trials in Western Canada
1981 - IRG/WP 470
Red pine boards treated with chromated copper arsenate, ammoniacal copper arsenate, copper zinc arsenic additive, a modified ammoniacal copper arsenate, and zinc arsenic additive, have been installed in a marine field test at West Vancouver, British Columbia. After two and a quarter years exposure, all the test samples are in excellent condition with the exception of those treated with the zinc ar...
J N R Ruddick


Previous Page | Next Page