IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 558 documents. Displaying 25 entries per page.


Impact of water holding capacity and moisture content of soil substrates on the moisture content of wood in terrestrial microcosms
2019 - IRG/WP 19-20662
Terrestrial microcosms (TMC) are frequently used for testing the durability of wood and wood-based materials as well as the protective effectiveness of wood preservatives. In contrary to experiments in soil ecology sciences, the experimental set-up is usually rather simple. However, for service life prediction of wood exposed in ground, it is of immanent interest to better understand the different...
C Brischke, F L Wegener


COPPER NAPHTHENATE: A Product for All Seasons: Protecting the Americas’ Infrastructure for Over 100 Years and Potential for Expanded Usage in Europe
2019 - IRG/WP 19-30738
This paper is a brief review of the history and use of the wood preservative Copper Naphthenate, with a focus on use patterns within the USA and opportunities for expansion in Europe and Canada. This paper reviews how copper naphthenate has performed to preserve and protect cellulosic and wooden items essential to critical infrastructure, and why it is the ideal choice for use in the replacement o...
M H Freeman, J A Brient, M Manning


Chemical Analysis of Southern Pine Pole Stubs Sixty Months Following Treatment with a Methylisothiocyanate-Based Solid Fumigant Stick
2019 - IRG/WP 19-30740
Methylisothiocyanate-based fumigants have been commercially used in the United States for over 35 years to control internal decay in utility poles and other wooden structures with little technological advancement. The most recently commercialized methylisothiocyanate-based fumigant is chemically known as dazomet. Dazomet is a free-flowing powder or granule that decomposes in the presence of mois...
D J Herdman, T Pope, R R Browning


Antifouling wood matrix with natural water transfer and micro reaction channels for water treatment
2019 - IRG/WP 19-40853
Wood with abundant nutrition transport channels could be considered as a kind of natural water purifier due to quick and effective passages for separation. Nevertheless, microporosity as main porous structure of initial wood are not enough to effectively separate small molecular, such as organic dye pollutants. Meanwhile, like most filters the fouling resulting in blocking and poor water flux will...
G Liu, D Xu, S Chang, J Hu, Xianjun Li5, Y Liu


Promoting Commercially Available Epoxy Resins for Non-biocidal Wood Preservation
2019 - IRG/WP 19-40877
Commercially available epoxy and polyamine resins were evaluated with the aim of developing new non-biocidal wood preservation treatments. A simple method allowing the impregnation of wood by vacuum double impregnation followed by a curing process was developed for two reference species, beech Fagus sylvatica and Scots pine Pinus sylvestris. The tested products were evaluated for their ability to ...
P Poveda, M Mubarok, S Dumarcay, M Montibus, I Le Bayon, M Kutnik, P Gerardin, F Simon


Wood veneer with high flexible decorated with nanoparticles for highly efficient water treatment
2019 - IRG/WP 19-50347
Natural wood is mainly comprised of numerous long, partially aligned channels (lumens) as well as nanochannels. Wood with these quick and effective passages is suitable for a membrane/separation material. However, a suitable thickness range of wood along its growth direction is essential to effectively separate small molecular, and the wood membrane is too thick to clean easily. In this paper, woo...
S Chang, D Xu, G Liu, J Hu, X Li, Y Liu


Effect of long-term immersion in fresh and salt water on mould growth on Scots pine (Pinus Sylvestris L.) wood
2020 - IRG/WP 20-10962
Wood exposed outdoors will eventually be degraded by fungi, depending on exposure and material characteristics. Numerous wooden constructions in the Røros municipality have existed since the 17th century, but wood used in recent repairs have decayed faster than expected. Before 1970 timber was mainly transported by log driving or rafting, and the logs were immersed in water for longer or shorter ...
M Sand Austigard, J Mattsson


Water interactions in wood polyesterified with sorbitol and citric acid
2020 - IRG/WP 20-40888
Polyesterifcation of wood with sorbitol and citric acid seems to be a promising chemical wood modification technique that is both low-cost and produced from bio-based chemicals. An interesting aspect of the modification is the interaction of water with the polyesterified wood since the relationship with moisture appears to be unique compared to other wood modification systems. This communication p...
G Beck, A Treu, E Larnøy


Studying amount, location and state of water in modified wood at moisture levels relevant for fungal degradation
2020 - IRG/WP 20-40889
Water is an essential parameter for fungal degradation of wood, but degradation primarily occurs at high moisture levels at water potential in the range of -4 to -0.1 MPa, which corresponds to 97-99.9% relative humidity. At these moisture levels, water is present in the wood structure both in and outside of cell walls. The majority of previous studies on the interaction between wood and water for ...
M Fredriksson, E Engelund Thybring, Ramunas Digaitis


Performance of a water-borne stain on beech, spruce, MDF and OSB improved by plasma pre-treatment
2020 - IRG/WP 20-40897
Coatings are an important part of wood protection, especially for outdoor applications. In order to provide a good protection, protective coatings need to exhibit good adhesion, mechanical resistance, and weathering resistance. Plasma pre-treatments are an established method to increase the performance of existing coatings including those on wood and wood-based substrates. Moreover, plasma deposit...
S Dahle, J Žigon, I Uranjek, M Petrič


Comprehensive protection of timber in seawater
2020 - IRG/WP 20-10970
The hazard of wood in seawater can be divided into two areas: Below the water level, shipworm (Teredo navalis) and gribble (Limnoria lignorum) can attack non-resistant or insufficiently protected wood; above the water level, there is a risk by wood-destroying fungi and, to a lesser extent, insects. In a national project funded by the Deutsche Bundesstiftung Umwelt (DBU, German Federal Environmenta...
E Melcher, J Müller, T Huckfeldt


Silicate coatings for wood substrates
2020 - IRG/WP 20-40906
Silicate coatings are surface finishing products containing alkali metal silicates or ethyl silicates as main binders. They are traditionally designed and well established for mineral substrates or corrosion protection of steel. The interest for these coatings in wood field is growing because of the benefits they could provide such as high durability, weathering resistance and fireproofing and sus...
A M Cheumani Yona, M Pavlič, M Petrič


Surface morphology and short-term water uptake of charred and coated wood
2021 - IRG/WP 21-40916
Charring of the wood surface represents a traditional alternative surface treatment technique with the purpose of aesthetics and protection. By the treatment with flame the surface of wood becomes carbonized and a few millimetres thick charred layer is formed on the top of the wooden element. Further, the charred layer can be removed by brushing, which accentuates the structure of the surface. Add...
J Zigon


Treatability of South African-grown Eucalyptus grandis with water-borne copper azole and disodium octaborate tetrahydrate wood preservatives
2021 - IRG/WP 21-40920
This study investigated the treatability of the sapwood and heartwood of sawn Eucalyptus grandis with copper-azole (CuAz) and disodium octaborate tetrahydrate (DOT) water-borne preservatives towards improving its durability for enhanced use in structural solid wood applications. The results obtained showed that, at a moisture content of 12 ± 1%, sawn E. grandis sapwood can be impregnated to a mea...
A A Alade, Z Naghizadeh, C B Wessels


Effect of a Water Repellent Treatment on Moisture Behavior of Three Australian Hardwoods: A Preliminary Report
2021 - IRG/WP 21-40921
Wood is inherently hygroscopic and will sorb moisture either directly from the atmosphere or via capillary action. Moisture can have marked effects on wood properties and repeated wetting and drying creates dimensional changes that lead to physical damage. Exposure to elevated moisture levels also increases the risk of fungal attack. Wood preservatives have long been used to minimize the risk of ...
B Hassan, J J Morrell, K Wood


Evaluation of weathering and termite resistance of the Myoung-oil as a Korean traditional coating agent
2022 - IRG/WP 22-10996
This study investigated the applicability of Myoung-oil (MO) as an eco-friendly preservative of Korean wooden cultural properties and buildings. Wood test specimens painted with various concentrations of MO were exposed in the external environment. Then color change and wettability of the wood surface were evaluated and compared depending on the exposure time. As a result of exposure for 12 months...
S-M Yoon, Y Park, W-S Jeon, H-M Lee, J-G Park, K Dal Nam, W-J Hwang


Comparative study on the efficacy of biobased wood preservative over conventional wood preservatives against fungi and termites
2022 - IRG/WP 22-30761
The current focus of wood preservation research is on developing wood preservatives from natural and environmentally compatible compounds for industrial application. Liquefaction of wood is one of the promising approaches to utilize woody waste where the wood powder is converted into a chemically active liquid with the help of a liquefying agent like phenol, cresol, plant-based solvent as CNSL and...
A Kumar, A John, B N Hazarika


Properties of Iron (II) Sulphate treated Norway Spruce
2022 - IRG/WP 22-30765
Exterior wood is exposed to various environmental factors that cause weathering. Weathering is important primarily from an aesthetic standpoint. However, not all parts of the building are equally susceptible to weathering. Parts exposed to moisture will discolour faster than protected parts, such as wood under roof overhangs. To achieve fast and uniform artificial greying, a surface treatment with...
B Lesar, M Humar, M Škamlec


Field tests of different tropical wood species in sea water
2022 - IRG/WP 22-30773
A number of tropical timbers have been tested according to EN 275 at Kristineberg Marine Research Station in Sweden since 1999. Most of these tests have started during the last 5-8 years. Wood species included have been Lophira alata (Azobé/Ekki), Minquartia guianensis (Manwood/Acaria), Chlorocardium rodiei (Greenheart), Cyclodiscus gabonensis (Okan/Denya), Shorea spp. (Bankirai), Dicorynia guia...
M Westin, P Larsson Brelid


A novel wood preservation technology improving durability and water-related properties
2022 - IRG/WP 22-40926
A newly developed silicone oil (Archroma Management GmbH, Switzerland) was tested for wood modification purposes. Scots pine sapwood was treated with aqueous solutions of this silicone oil and showed a penetration of the modification agent into the wood cell wall. Both, biological durability and moisture-related properties, experienced significant improvements by the modification. Besides, the mod...
L Emmerich, H Militz, M Vila


The influence of thermal modification and surface charring to different levels on wettability of Norway spruce wood
2022 - IRG/WP 22-40942
The wood can alternatively be protected from water absorption by thermal modification and charring. Both techniques cause certain chemical and physical changes in the wood, the extent of which depends on the level of temperature applied. The objective of this study was to determine how the combination of charring to different levels and thermal modification affects the chemical, morphological, and...
J Žigon, C Gerardin, M E P Wålinder, P Gerardin


Assessment of the Material Durability and Structural Integrity of the Wooden Velodrome in Češča vas, Slovenia
2023 - IRG/WP 23-11012
Wood is a widely used material in the construction industry, and it has been utilized for thousands of years to create buildings and other structures. When wooden structures are designed, built, and maintained properly, they can be safe and long-lasting. Sports facilities, which provide athletes with a space to train, compete, and improve their abilities, are crucial in creating a strong and susta...
D Kržišnik, M Humar, B Lesar


Efficacy of a wide-spectrum plant bio-based anti-termite product - Laboratory trials
2023 - IRG/WP 23-11024
Compared to the number of timbers available, the list of wood species resistant to termites is rather limited and largely composed of tropical timbers. In addition, due to climate change and environmental degradation, together with global trade, a significant global expansion of termites is predicted along with the economic losses due to their activities. Therefore, there is a demand to find produ...
M-F Thévenon, F Chopinet, J Vuillemin, A Robert, S Lafay, D Messaoudi


Biological durability and wood-water interactions of sorbitol and citric acid modified wood – Effects on the expected service life
2023 - IRG/WP 23-40960
A high level of research activities on sorbitol and citric acid (SorCA) modified wood has been recognized in Europe over the last few years. As this treatment is close to entering an industrial-scale production, it is of interest to investigate how such treated wood performs upon long-term outdoor exposure. Hence, in this study Scots pine (Pinus sylvestris L.) sapwood was modified with aqueous sol...
K Kurkowiak, L Emmerich, H Militz


Evaluation of the efficacy of silver nanoparticles and chitosan oligomer composites as poplar wood protective treatments against termites
2023 - IRG/WP 23-40963
Populus × euramericana ‘I-214’ (poplar) is a fast-growing species widely distributed throughout the world, and in the Castile-Leon region of Spain it accounts for more than 50% of all plantations. Its wood is becoming increasingly appreciated, yet its low durability against xylophagous agents —termites being one of the most aggressive and destructive in warm climates— continues to be a li...
E Spavento, M T Troya, M Casado-Sanz, J Martín-Gil, P Matín-Ramos, L Robertson, L Acuña-Rello


Previous Page | Next Page