IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 607 documents. Displaying 25 entries per page.


Technologies for the Management of Wood Waste Containing Metals-Based Preservatives
2005 - IRG/WP 05-50224-16
Disposal of the metals from preservative treated wood can occur through two general strategies: “removal and confinement” or “dilution”. The acceptability of each of these two choices is typically dictated through the disposal regulations of a particular region. A considerable amount of research has been conducted to develop new and innovative “removal and confinement” technologies...
H M Solo-Gabriele, T G Townsend


Preliminary investigation on the natural durability of Guayule (Parthenium argentatum)-based wood products
2000 - IRG/WP 00-40154
Conventional preservatives used to protect wood from insect and microbial damages are presently of major concern to human health and the environment. Finding alternative and economical preservatives has not been successful. Previous studies have shown that the resinous material extracted from the guayule plant (Parthenium argentatum, Gray) has both insect- and microbial-resistant properties. Unfor...
F S Nakayama, P Chow, D S Bajwa, J A Youngquist, J H Muehl, A M Krzysik


Copper based wood preservative - A new approach using fixation with resin acids of rosin
2000 - IRG/WP 00-30249
Copper soaps with carboxylic acid groups of resin acids of rosin were shown to be potential long-term wood preservatives. The principle involved is the attachment of copper to the network formed by the inorganic part of the preservative (rosin) through the -COOH groups. The mechanisms of fixation have been studied, and it has been shown that this association could be obtained : (1) by forming the ...
C Roussel, J P Haluk, A Pizzi, M-F Thévenon


Preliminary desk research in the Netherlands on development of a Knowledge Based System for Life Cycle Assessment of wood products
1997 - IRG/WP 97-50093
TNO is currently coordinating an EC-project (LIFE-SYS WOOD) to develop a consistent approach to Life Cycle Assessment (LCA) of wood products. Existing and new LCA-inventory data of six wood products will be evaluated on reliability and consistency. After validation, LCA-results will be made available through a Knowledge Based System (by 1998-1999). The aim of the KBS is to make LCA-results availab...
P Esser, D Robson, R Vanhauten


Feeding response of field populations of Coptotermes species to softwood blocks treated with non-toxic water-proofing and anti-microbial products.
2003 - IRG/WP 03-10487
The feeding response of field populations of the subterranean termite, Coptotermes lacteus, to Pinus radiata wood blocks (50 x 40 x40 mm) treated with various combinations of non-toxic and odourless water-proofing materials based on natural high molecular weight esters (TimberTreatÒ) and a new water insoluble quaternary ammonium compound (‘anti-microbial’) is described. Treated wood blocks we...
J R J French, T Pynsent, M Susic


A technique for determining the efficacy of water diffusible preservative plugs for implanting in joinery in service
1987 - IRG/WP 2291
A technique is described for determining the efficacy of soluble, diffusible preservative plugs for eradicating decay in joinery. It uses blocks of Scots pine sapwood or heartwood adjusted to known moisture contents prior to the establishment of the test fungus Coniophora puteana, from a single longitudinal dowel and the subsequent introduction of the preservative plugs. Prevention of decay, eradi...
J K Carey, A F Bravery


The degradation of wood surfaces by dilute acids
1985 - IRG/WP 3326
Thin radial/longitudinal sections(~100 µ) of Corsican Pine (Pinus nigra) and Lime (Tilia vulgaris), were exposed to Sulphuric, Sulphurous, nitric, acetic, and formic acid at 40°C in the pH range 2-6. After about 3 months exposure to Sulphuric, nitric, acetic and formic acid at pH 2.0 Pine lost some 20-25% of its tensile strength. Losses in tensile strength due to sulphurous acid were greater bei...
P D Evans, W B Banks


Protection of cellulose string with biocide/water repellent mixtures
1997 - IRG/WP 97-30148
Protecting cellulosic materials in soil contact poses a formidable challenge. Many soil inhabiting bacteria and fungi that cannot degrade wood can nevertheless rapidly depolymerize cellulose once its protective lignin matrix is removed. As a result, cellulose based materials are rarely used in direct contact with soil. One exception, however, is the use of cellulose string to support climbing vine...
A B Chang, J J Morrell


Wood protecting chemicals for the 21st century
1993 - IRG/WP 93-30018
After assessing the past research with protection chemicals, this paper proposes future avenues for research and development in wood protection. Three scenarios are put forward for consideration. First, more is not better and future systems will emphasize combination formulations which enhance properties while providing biological efficacy. Second, current systems, especially those based on copper...
H M Barnes


Methods to determine the efficacy of three water repellent additives in waterborne preservatives
1997 - IRG/WP 97-30142
The paper describes the methods used to determine the efficacy of three different water repellent additives in waterborne preservatives. The wooden samples used are pine (Pinus sylvestris) and spruce (Picea abies) that are treated with 9 different waterborne preservatives in retention for hazard class 3 (above ground commodities). There are two sample sizes exposed, cladding boards (19 x 148 mm) w...
F G Evans, B Nossen, K M Jenssen, L R Wilhelmsen, G Fuglum


Permatek IM 30 as a termiticide treatment for veneer-based wood products
2003 - IRG/WP 03-30325
Permatek IM 30 is a termiticide designed for incorporation into wood products during manufacture. Whereas existing approved products in Australia are based predominantly on synthetic pyrethroids carried in solvents, Permatek IM 30 is based on imidacloprid, a neonicotinoid insecticide. The formulation has very low mammalian toxicity, is free of VOCs, and has been successfully tested as a glueline ...
J Doyle, K Webb, W R Rae, A F Siraa, J Malcolm-Black


Effect of leaching temperature and water acidity on the loss of metal elements from CCA treated timber in aquatic applications. Part 1: Laboratory scale investigation
1995 - IRG/WP 95-50046
In order to investigate the applicability of current prestandard leaching test methods, a series of experiments has been performed on CCA impregnated wood dealing with the influence of pH, temperature and agitation of the surrounding water. The leaching method used in this first part of the investigation is the European prestandard drafted by CEN/TC38/WG11, a short term dynamic leaching test under...
G M F Van Eetvelde, R J Orsler, G E Holland, M Stevens


Algal growth resistance of paints for coating of wood; a laboratory study
1997 - IRG/WP 97-10213
Twelve paints were tested for resistance against algae. In addition, one algicidal compound commercially used for remedial treatments of algal growth on paints was tested for its effectiveness for prevention of algal growth. An agar diffusion bioassay was employed in which paint films on filter paper discs were placed on mineral salt medium and sprayed with an algal suspension containing a mixture...
J Bjurman


Penetration and absorption of water-borne preservatives in conifers from the Western United States: A preliminary report
1988 - IRG/WP 3475
The treatment of most softwoods from the western United States with waterborne chemicals poses a major challenge. Although many of these species are commercially treated with waterbornes, there is considerable debate about their treatability. At present, there is little or no information on the treatability of western wood species with waterborne chemicals. The lack of accurate treatability inform...
S Kumar, J J Morrell


Aquatic toxicity research of structural materials
1998 - IRG/WP 98-50114
Continuing from preliminary results reported on the aquatic toxicity of some tropical hardwoods under high hazard conditions, a more comprehensive research study is set-up in order to assess the environmental toxicology of various structural materials in water applications. Hazard class 4 preservative treated wood is tested for its toxic response on a battery of aquatic test organisms, next to con...
G M F Van Eetvelde, S De Geyter, P Marchal, M Stevens


PCP in aquatic environments arising from historic contamination at wood processing and preservation sites
1995 - IRG/WP 95-50040-14
Three different studies are reported that assess the impacts of Pentachlorophenol (PCP) in aquatic environments arising from its historic use at sawmilling and wood preservation sites. These studies involved New Zealand wood processing facilities, and collectively they aimed to measure the transport of PCP from sawmill sites into the aquatic environment, determine the background environmental conc...
J S Gifford, P N McFarlane, M C Judd, S M Anderson


A model for attack at a distance from the hyphae based on studies with the brown rot Coniophora puteana
1995 - IRG/WP 95-10104
In timber infested by brown rot fungi, a rapid loss in strength is attributed to production of hydroxyl radicals (HO·) at a distance from the hyphae. The immediate precursor is Fenton's reagent (Fe(II)/H2O2), but the pathways leading to Fe(II) and H2O2 have remained unclear. Cellobiose dehydrogenase, purified from cultures of Coniophora puteana, will couple oxidation of cellodextrins to ...
S M Hyde, P M Wood


Influence of water soluble extractives on CCA fixation and leaching performance of red maple and red oak
1997 - IRG/WP 97-30133
We have observed several peculiarities in relation to CCA fixation in red maple and red oak woods such as high variability in fixation rates and leaching performance in maple and precipitate formation in solutions expressed from CCA treated red oak wood blocks at different stages of fixation. We have postulated that the extractives could be the factor of influence, as this has already been reporte...
T Stevanovic-Janezic, P A Cooper, Y T Ung


IRG/COIPM INTERNATIONAL MARINE TEST - To determine the effect of timber substrate on the efectiveness of different preservatives in sea-water: Coding scheme
1976 - IRG/WP 420
It was agreed in Wildhaus on 15 May 1976 that preparations for the test detailed in Document No: IRG/WP/414 should commence immediately, but that initially only two water-borne preservatives should be used - a copper/chrome/arsenic (CCA) and a copper/chrome/boron (CCB) formulation respectively. PRL, England (R Cockcroft) would be responsible for supplying only the reference species treated with th...
Anonymous


Leaching Characteristics of Alder Wood Treated with Copper Based Wood Preservatives
2005 - IRG/WP 05-50225
In this study, it was designed for determining leaching characteristics of CCA and alternatives wood preservatives. Alder wood blocks were treated with CCA (1 % and 2 %), ACQ-1900 (2 % and 3 %), ACQ-2200 (1 % and 2 %), Tanalith E 3491 (2 % and 2.8 %), Wolmanit CX-8 (% 1 and 2 %). Leaching studies were conducted according to AWPA E11-97. Copper analyses of leachate were determined Atomic absorption...
A Temiz, Ü C Yildiz, E D Gezer, S Yildiz, E Dizman


Moisture content of logs under sprinklers
2000 - IRG/WP 00-40157
Logs are kept under sprinklers during storage for avoiding the development of sapstain fungi. According to literature, sapstain fungi do not develop if the moisture content is above 120%. It is supposed that, the water sprinklers maintain the log's moisture content above this value, but, very often, sapstain is found on sawn lumber cut from these logs. Logs are harvested and transported t...
M C Rose, A M Briones, M Fernández


The future for chromium in wood preservation
1985 - IRG/WP 3332
Most water-borne preservatives contain CrVI compounds, originally to reduce corrosion although now also to improve toxicant fixation. Chromium contributes to preservation and this is recognised in, for example, New Zealand and USA where chromium contents are included in calculations of overall preservative activity of CCA formulations, but chromium may also have anti-stain and joinery (millwork) p...
B A Richardson, T R G Cox


Application of paint primers after light organic solvent preservative treatment
1986 - IRG/WP 3381
The application of three alternative paint primers is investigated, including a slow-drying oil-based primer, a fast-drying oil-based primer, and a fast-drying water-based primer. The treatment schedules employed, in particular the evacuation period after treatment, have a marked effect on subsequent paintability. Priming can potentially be carried out immediately after treatment with approved Tim...
P Vinden


A field trial to assess the potential of antisapstain chemicals for long-term protection of sawn radiata pine
1986 - IRG/WP 3375
Seven chemical formulations were tested as antisapstain treatments for freshly sawn radiata pine sapwood (90x50 mm²). Each formulation was used with and without a water-repellent additive and was sprayed on to 1 m long boards. The boards were then stacked into "mini" packets and stored unprotected from the weather for 6 months. Haipen 50w (at 0.2 or 0.4% active) and NaPCP (1% active) plus 1.5% bo...
J A Drysdale


Prevention of sapstain in logs using water barriers
1997 - IRG/WP 97-30147
Placing logs in ponds or under water sprinklers to keep moisture levels high enough to prevent oxygen tensions rising above inhibitory levels, is a proven method of preventing sapstain. The objective of this experiment was to determine if water barriers significantly reduce the rate of sapstain penetration into logs by maintaining moisture contents, and consequently oxygen tensions, at inhibitory ...
R N Wakeling, D R Eden, C M Chittenden, B Carpenter, I Dorset, J Wakeman, R Kuluz


Previous Page | Next Page