Performance of boron and fluoride based rods as remedial treatments in Douglas-fir poles
1995 - IRG/WP 95-30070
Boron and fluoride are widely used for remedial internal treatments, but their use in North America has been limited. Recently, however, interest in these chemicals has increased as the result of concerns about the risks of fumigant usage. The performance of boron or a boron/fluoride combination was assessed in Douglas-fir poles over 1 to 3 year periods. Both chemical formulations diffused well th...
J J Morrell, P F Schneider


The implementation of restrictions on the use of arsenic and chromium based wood preservatives in Sweden
1995 - IRG/WP 95-50062
In 1992 the Swedish National Chemicals Inspectorate introduced restrictions on the use of wood treated with arsenic and/or chromium based wood preservatives. Such wood is now in principle only allowed for use in ground contact or in water. These restrictions have had considerable influence on the use of wood preservatives for sawn timber for the Swedish domestic market. Thus only 35% of the preser...
J Jermer, M-L Edlund, K Nilsson


The degradation of wood surfaces by water
1984 - IRG/WP 3289
Thin radial/longitudinal sections (~100 µ) of Scots Pine (Pinus sylvestris) and lime (Tilia vulgaris), were exposed to deionised water over the temperature range 25-65°C. Losses in wet tensile strength and toughness occurred rapidly at temperatures from about 50°C upwards. After about 2 months' exposure pine lost some 10-30% of its tensile strength and 20-60% of its toughness. For lime...
W B Banks, P D Evans


Application of roller-pressing method to the novel liquid impregnation treatment of green timber
2001 - IRG/WP 01-40198
A transverse compression technique enabled us to impregnate liquid into green timber through replacement of the free water in the timber with a treatment liquid without any critical physical damage to the timber by the roller-pressing method. The roller-pressing is supposed to remove free water the cell cavities and to concurrently introduce the treatment solution into green timber in the treatmen...
M Inoue, K Adachi, K Tsunoda, Y Imamura, S Kawai


Evaluating the performance of preservative/water repellent emulsion systems
1997 - IRG/WP 97-20127
Water repellent emulsions are being combined with wood preservatives to improve the weathering properties of treated wood in service. Unfortunately, few standard procedures are available to objectively compare the performance of these systems and as a result quality issues are almost completely neglected. The value of swellometer tests, water immersion tests and accelerated weathering regimes in t...
K J Archer, F Cui


Soft rot - Soil burial - Tests. Influence of the water content of the soil on wood decay
1972 - IRG/WP 212
The decay of wood samples buried in the soil is influenced by various factors. Decisive are the water content, the content of organic substances, pH-value content of mineral nutritive substances etc. of the soil. For the tests, carried out by the EMPA until now, it was always started with a water content of 35%, refered to the dry weight of the EMPA-soil = 75% of its water capacity. In order to in...
O Wälchli


IRG/COIPM INTERNATIONAL MARINE TEST - to determine the effect of timber substrate on the effectiveness of water-borne salt preservatives in sea-water. Progress Report 1: Treatment of reference samples
1977 - IRG/WP 426
It was agreed in Wildhaus on 15 May 1976 that preparations for the test detailed in Document No: IRG/WP/414 should commence immediately, but that initially only two water-borne preservatives should be used - a copper/chrome/arsenic (CCA) and a copper/chrome/boron (CCB) formulation respectively. PRL, England (R Cockcroft) would be responsible for supplying samples of the reference timbers treated w...
R Cockcroft, T B Dearling, W O Schulz, H V Borck


Preliminary results of the treatment of wood with chlorosilanes
1981 - IRG/WP 3172
It is clear from the initial data reported here that the treatment of pine sapwood with chlorosilanes under the reaction conditions employed did not significantly reduce the decay by both white rot and brown rot fungi. Only the dichlorosilane compounds showed to possess some protective action against fungal attack. Before drawing conclusions on the application of organosilicon compounds as potenti...
M Stevens


The effect of water-repellent additives on the leaching of CCA from simulated southern Yellow pine decks
2000 - IRG/WP 00-50158
End-matched SYP boards were pressure-treated with CCA or CCA in combination with commercial water repellent additives. After fixation and drying, the boards were placed in plastic boxes and exposed outside in Harrisburg, NC. Plastic supports were used to keep the boards above the water collected. Over a period of five months, rain run-off water from 14 natural rainfalls were collected and analyzed...
F Cui, P J Walcheski


Serpula lacrymans, The Dry Rot Fungus and its Tolerance towards Copper-based Wood Preservatives
2005 - IRG/WP 05-10555
Serpula lacrymans (Wulfen : Fries) Schröter, the dry rot fungus, is considered the most economically important wood decay fungus in temperate regions of the world i.e. northern Europe, Japan and Australia. Previously copper based wood preservatives were the most commonly used preservatives for pressure treatment of wood for building constructions. Because of a suspicion about tolerance toward cop...
A C Steenkjær Hastrup, F Green III, C A Clausen, B Jensen


Selective chromate elimination from the storage-drainage-water of a wood impregnation plant
1980 - IRG/WP 3153
With the Enviro-Chrom-Ex process it is possible to eliminate ecologically and economically hexavalent chromium (chromate) from water selectively. The process which is based on the principle of selective ion exchange works with different chromate concentrations and under the presence of other ions, irrespective of the water hardness. The values of water-offtake reach 0.1 mg CrVI at maximum, causing...
O Wälchli, R Ott, R Hugener, E Graf, B Lieberherr


Determination of the water sorption properties and preliminary results from field tests above ground of thermally modified material from industrial scale processes
2004 - IRG/WP 04-40279
In this study the differences in moisture behavior and durability above ground of heat treated wood originating from different European industrial heat treatment plants by means of the water sorption properties as well as field tests were examined. The manufacturers of heat treated material were: PLATO Hout B.V./Netherlands, Thermo Wood (Premium wood)/ Finland and Menz Holz/ Germany, where Oil-...
C R Welzbacher; A O Rapp


Observations on the performance of copper-based wood preservatives in fungal cellar (soil-bed) tests
1994 - IRG/WP 94-20047
Fungal cellar (soil-bed) tests are considered to be an important tool for the evaluation of the performance of ground contact wood preservatives. Facilities of this type have been established world wide although caution has been exercised in their introduction into standard testing methods for the approval of wood preservatives. This is the result of concerns over the variability in the biological...
G R Williams, D Rudolph, M E Hedley, J A Drysdale, R F Fox


Vertical distribution of fouling and wood-boring organisms in the Trondheimsfjord (Western Norway)
1981 - IRG/WP 476
Results of a detailed study on the vertical distribution of fouling and wood-boring organisme of Trondheimefjord at an interval of 3 m from intertidal level to a depth of 30 m, has been presented, based on data collected from two series of panels, exposed from 15-3-1977 to 15-7-1977 (Series I) and from 22-7-1977 to 13-3-1978 (Series II). The intensity of fouling generally decreased with increasing...
L N Santhakumaran


Marine trials with ammoniacal wood preservatives
1980 - IRG/WP 423
Ammoniacal wood preservatives have been known for many years and are considered among the best water-borne systems for protecting wood in ground contact. In recent years attention has been increasingly focussed on these preservatives because of their ability to penetrate difficult-to-treat species better than most other fixed water-borne preservatives. This is particularly important for example, i...
M A Hulme, D P Ostaff


Treatability of waterstored poles of Norway spruce by sap-displacement and pressure treatment with Boliden K33 and creosote
1973 - IRG/WP 328
Poles of windthrown Norway spruce were stored in bark under water sprinklers for 11-20 months or fully submerged in a lake for 3 years (tab. 1 and 2). Water content after storage is shown in fig. 1 and 8. Treatment with Boliden K33 by sap-displacement (open tank suction) gave a poor result. The Danish requirements of delivery claim a penetration of 20 mm and a net retention of 12 kg/m³ in outer 2...
P Moltesen, E Borsholt, B Bang


A marine borer test with water-borne preservatives
1980 - IRG/WP 452
The use of preservative treated timber in sea-water where marine borers are active is of great economic importance, since untreated wood immediately will be damaged. Vacuum/pressure treated timber has been tested in several marine exposure trials on the Swedish west coast since the 1930s (Hager 1941, Hultman 1949, Sandstrom 1951, Nylinder-Norman et al. 1974). Since new interesting materials or pre...
B Henningsson, E Norman


Risk assessment of energetic valorization of treated wood - wooden recycling
1996 - IRG/WP 96-50072
The most useful method for the valorization of wood wastes and wooden wastes is energetic valorization. In France the percentage of wood treated by antisaptain products is around 30%. Currently with the growing regulation, there is a need for cleaner methods and technology to allow sustainable valorization. The preservatives concerned are common organochlorine compounds (NaPCP) less used nowadays ...
G Deroubaix, P Marchal, G Labat


Analysis of water repellents in wood treated with water borne formulations using FTIR
2000 - IRG/WP 00-40176
The use of aqueous water repellent emulsion formulations has increased significantly in the wood treatment industry. These products are primarily used to enhance the weathering characteristics of wood products treated with water borne preservatives systems used in exterior above ground applications. They are also used in pole treatments to improve climbing characteristics and in low VOC millwork t...
P J Walcheski, L Jin


Environmental fate of copper-based wood preservatives in different soil substrates - Part 2: Study of the metal sorption and migration potential under simulated rainfall
1998 - IRG/WP 98-50101-21 b
In order to examine the potential environmental impact of spillages of the saltborne wood preservative CCA in treatment plants, four large scale experiments are set-up so as to follow the water transport and ion mobility in various field soils. A plastic container is filled with a sand, silt, clay and potting soil, made up at their respective bulk density and wetted to a given moisture content. U...
G M F Van Eetvelde, R Hartmann, J M Mwangi, H S Öztürk, M Stevens


IRG/COIPM INTERNATIONAL MARINE TEST - to determine the effect of timber substrate on the effectiveness of water-borne salt preservatives in sea-water. Progress Report 21: Report of eighth inspection (7 years) in Australia
1985 - IRG/WP 4119
This report tabulates the seven year (86 month) inspection results, obtained on 28 Fabruary l985, of the IRG/COIPM International Marine Test at Goat Island, Australia. This test was installed in December 1977. The results are given in Tables 1-6. Table 7 lists the number of marine borers identified from blocks (2 cm and 6 cm long respectively) cut from the ends of specimens removed at the previous...
L J Cookson, J E Barnacle


Raising of the grain and deformation of Scots pine (Pinus sylvestris) treated with water-borne preservatives
1987 - IRG/WP 3456
In Sweden partial impregnation to 10 mm depth of the pine sapwood (class B in the Nordic preservation standard) of joineries was introduced during the seventies. To avoid product quality problems, organic solvent-based systems have been used. However, the Swedish industry today has problems with organic solvents, mainly for environmental reasons. We have studied raising of the grain and deformatio...
G Hägglund, T Sebring


Effects of two wood preservatives and one water repellant on the settlement of fouling communities in a tropical marine environment
2002 - IRG/WP 02-30293
Observations made on recruitment of fouling organisms on treated panels exposed at an Indian harbour, Krishnapatnam on the east coast (Lat: 13028’ to 13059’ N; Long: 80010’ to 80016’ E) during November, 1997 to October, 1999 are reported and compared with fouling communities on control panels. Wooden panels of Erythrina variegata, Paraserianthus falcataria, Tetrameles nudiflora an...
B Tarakanadha, K S Rao


X-ray photoelectron spectroscopic analysis of CCA treated wood
1992 - IRG/WP 92-3700
Ponderosa pine and Douglas-fir wood sections were treated with CCA preservative. To elucidate the mechanism of fixation of the CCA, the wood surface was analyzed by X-ray photoelectron spectroscopy (XPS). CCA treatment increased C1 (carbon bonded to carbon and/or hydrogen) and decreased C2 (carbon bonded to one oxygen) in XPS C1s spectra, both in unextracted and pre-extracted sections. This sugges...
J N R Ruddick, K Yamamoto, P C Wong, K A R Mitchell


Bacterial brown stain on sawn timber cut from water-stored logs
1992 - IRG/WP 92-1532
Brown stains which appear on the surface of sawn radiata pine cut from water-stored logs were identified as tannin-like compounds. They are derived from bacterial breakdown of flavanoid-glucosides. When timber is sawn from infected logs, the free flavanoids migrate to the wood surface as the timber dries. There, they condense and oxidise to form permanent brown discolourations. Stains occurred on ...
M E Hedley, R Meder