Effectiveness of Water Based Bentonite-Borate Slurry for In-situ Remedial Protection of Historic Wooden Piles: The Eurobor Protocol, Part 2
2011 - IRG/WP 11-30574
The study of the biocide product Eurobor®, water mixture of boric acid, borax and sodium bentonite, aimed to verify previous findings regarding borates penetration from a clay-water mixture of foundation timber. The product was applied on samples from 100 year old timber foundation from the city of Göteborg. Although in ground for this long the timber was in acceptable god condition due to groun...
M. Theorin, K. Fimmerstad, K-M. Bandh


The potential of propolis and other naturally occurring products for preventing biological decay
2011 - IRG/WP 11-30575
The potential of using a range of naturally occurring plant extracts and propolis from bee hives for enhancing the durability of timber in service as well as helping with the conservation of archaeological timbers is considered in this paper. Results reported demonstrate that there is some degree of protective effect noted, suggesting a viable treatment option might be developed based on a deeper ...
D Jones, N Howard, E Suttie


The potential of silicone-based formulations to enhance wood properties through industrial treatment for outdoor use
2011 - IRG/WP 11-30578
High hygroscopicity is one of the main weaknesses of wood as far as its susceptibility to biodegradation, and specifically to fungal decay. New wood preservation technologies are constantly entering the wood protection market, competing with traditional, biocide-based preservation. Silicones are commercially used as hydrophobic agents on stones and concrete. They belong to the restricted number of...
F Simon, F Marchal, F Pochon, M Kutnik, I Le Bayon


Evaluation of an optimized industrial process aiming to improve the natural durability and mechanical behavior of bamboo for outdoor use
2011 - IRG/WP 11-40554
Mao Bamboo (Phyllostachys pubescens) is characterized by high contents of sugar and starch and by high hygroscopicity, which makes it susceptible to biodegradation, and specifically to fungal decay. Still, many bamboo based products regularly enter the European wood construction market, competing with traditional solid wood products used for outdoor decking and cladding. The performance of a heat ...
F Simon, M Kutnik, I Le Bayon, G Moisset, V Gatimel


Ambient-temperature borate dip-diffusion treatment of green railroad crossties
2011 - IRG/WP 11-40556
In the USA, borates are increasingly being applied prior to air seasoning and creosote treatment of railroad ties (railway sleepers). Borates are typically applied to green ties by vacuum pressure application at 1 to 10% disodium octaborate tetrahydrate (DOT) concentration or by traditional dip-diffusion treatments at elevated temperatures. Higher temperatures are used to maintain the 30 to 50% so...
Jae-Woo Kim, A M Taylor, C Köse


Utilization of thermodesorption coupled to GC-MS to study kinetics of thermodegradation of different wood species
2011 - IRG/WP 11-40559
Thermdesorption coupled to Gas Chromatography coupled to Mass Spectroscopy (TD-GC-MS) has been investigated to identify volatile degradation products generated during wood heat treatment by mild pyrolysis. For this purpose, wood samples of different softwood and hardwood species have been heat treated under nitrogen for different temperatures comprised between 180 and 230°C during 15 min. in the ...
K Candelier, M Chaouch, S Dumarçay, A Pétrissans, M Pétrissans, P Gérardin


Optimization of the bi-oleothermal treatment process for wood preservation and fireproofing
2011 - IRG/WP 11-40566
The bi-oleothermal© process (combination of oil and heat treatment) is a well mastered alternative method for wood protection. However, the fire behavior and resistance to decay of bi-oleothermally treated wood are not good enough to ensure performance which meets the service standards for outdoor applications such as cladding or decking expected by the market. The aim of the present research pro...
F Simon, M Kutnik, M Goyer, M-F Thévenon, C Alfos, M Céron


Limited variability in biological durability of thermally modified timber using vacuum based technology
2011 - IRG/WP 11-40567
The SmartHeat® thermal timber treatment is a new technology based on the process parameters being steered very precisely mainly due to the vacuum applied and heating system involved. Timber treated with this technology shows a potential for less variability of biological durability in one batch. Several batch treatments were sampled and assessed on statistical variability of decay resistance agai...
J Van Acker, S Michon, J Van den Bulcke, I De Windt, B Van Swaay, M Stevens


Effect of Nano-silver Treatment on Densified Poplar Wood Properties. Part Two: Spring Back, Compression set, Impact Load Resistance and Hardness
2011 - IRG/WP 11-40568
This paper is the second part of the study of applying nano-silver treatment before densification of poplar wood (Popolus alba). The specimens were prepared in four groups of: 1) nano-silver impregnated 2) water impregnated 3) dried with no impregnation and 4) the control specimens. The impregnation process was done by empty cell process. Then, the groups of 1 to 3 were compressed in a hot press a...
G Rassam, H Reza Taghiyari, B Jamnani, M Ali Khajeh


Effects of nano-silver on brittleness of heat-treated solid woods
2011 - IRG/WP 11-40572
The present study is aimed at the effect of heat-treatment of normal as well as nano-silver-impregnated Populus nigra, Populus deltoides, and Fagus orientalis on brittleness. Specimens were impregnated with 200 ppm water-based solution of nano-silver particles under 3 bars in a pressure vessel using empty-cell process. For heat treatment, both nano-silver-impregnated and normal specimens were kept...
H Reza Taghiyari, B Moradi Malek, A Karimi


The overview of ISPM 15 implementation in Croatian wood-working companies
2011 - IRG/WP 11-30576
Croatia is a small European county, but in the same time a great country according to it’s tradition in the forestry and wood working industry. However, around 48% of it’s territory is afforested. As the export is one of the main directions in the Croatian development conception, the production and distribution of wood package intended for the international trade, is one of the most important ...
R Despot, V Jambrekovic, M Hasan


TRU-CORE Process for Treatment of Refractory Species and Engineered Wood Products
2011 - IRG/WP 11-40573
The TRU-CORE Process is a novel, chemically-based technology for rapidly delivering globally accepted wood preservatives and insecticides deep into the core of wood and wood-based composites in a waterborne carrier. Protectant materials which can be utilized with the TRU-CORE Process include a variety of carbon-based fungicides and insecticides. An important feature of the TRU-CORE Process is it...
A S Ross


In-situ experimental treatment and consolidation of degraded timber elements from a XIX century building
2012 - IRG/WP 12-10767
This paper presents the in situ experimental conservation work performed on three timber structural elements from a XIX century building: two floor beams and one roof beam. The palace was built in 1877 in the centre of Lisbon initially with residential purposes. It has four floors, with timber structural horizontal elements, stairs and roof beams (generally of Pinus sylvestris L.). The exterior wa...
D F Henriques, J de Brito, L Nunes


Preliminary laboratory bioassay to evaluate engineered Fibre-boards against subterranean termites C. acinaciformis (Isoptera: Rhinotermitidae)
2012 - IRG/WP 12-10768
In Australia, laboratory bioassays with subterranean termites typically contain groups of workers and soldiers in a substrate of moist mound material. This termite substrate may affect termite consumption, and the test materials create a favorable termite condition for the test. The main purpose of this test is to examine the effect of a melamine formaldehyde treatment of wood panels to evaluate t...
B M Ahmed (Shiday), H Militz, B Ozarska, I Ali, L Kloeser


Antifungal activity of wood extractives from waste products of steam distillation of Aniba rosaeodora
2012 - IRG/WP 12-10779
Aniba rosaeodora, is a slow growing evergreens of the Lauraceae family which are indigenous over a wide range of the Greater Amazon Region (the Guianas and Venezuela, Brazilian Amazon…). The essential oil obtained from the wood has a characteristic aroma and is a long-established ingredient in the more expensive perfumes. Around the olfactive characteristic of the essential oil is due to the pre...
N Amusant, A Digeon, E Hoüel, J Beauchène


A survey on Bio-Resistance of Oak and Elm in Caspian Sea Water
2012 - IRG/WP 12-20483
Logs of Oak (Quercus castanifolia) and Elm (Zelkova carpinifolia) have been cut to lumbers with dimensions of 300×100×30 mm. The oven dried samples have been impregnated with CCA (Chrome–Cupper-Arsenic). Treated and untreated (natural as a control) woods have been established for 3, 6, 9 and 12 months in Amirabad beach of Behshare under fishing environment. The observation results shows that i...
S M Kazemi


Performance superiority of CCA-C treated wooden jetty poles and piles used for 30 years in Bangladesh against marine borers
2012 - IRG/WP 12-30582
Observational study along with previous investigation and records revealed that chromated copper arsenate type C (CCA-C) impregnated southern pine poles and piles of jetty constructed in most vulnerable brackish water in Bangladesh are stable and resistant to attack of all types of marine borers after 30 years of use. It is evident from the service records of other construction materials that CCA-...
A K Lahiry


Mold Control for Treated Lumber in Block-Stack Storage Conditions
2012 - IRG/WP 12-30588
The mold development and control for freshly treated and block-stacked wood have been evaluated using a green house mold testing method. The results for the mold resistance of several commonly used water boron preservative treatment systems, such as ACQ, Copper Azole, and borates with and without inclusion of mold inhibitors are presented. The data suggest that the different preservative treatme...
L Jin, P Walcheski, A Preston


Supercritical impregnation of wood with siloxane
2012 - IRG/WP 12-30595
This paper describes the effect of supercritical impregnation with siloxane on the water repellency of Scots pine (Pinus sylvestris) sapwood samples. Samples were impregnated with a low amount of siloxane dissolved in supercritical carbon dioxide using isopropanol as a co-solvent. Siloxane retention (i.e. weight percent gain (WPG)) of the treated samples was 1.3 % (w/w) as found by mass balance. T...
A Kjellow, F Imsgard, J Fernandes, O Henriksen, E Klaassen, R Wagner, J Delis


Effects of oil types and treatment temperature on the properties of wood subjected to thermal modification in oil medium
2012 - IRG/WP 12-40574
The effect of the use of oil as a medium of heat transfer during thermal modification of different species of wood has been widely investigated with different results accruing with regards to the various end-use properties of the materials. However very little have been done on the effect of oil types as well as its interaction with treatment temperature on the resultant properties of the material...
L Awoyemi, M M Apetogbor, A A Oteng-Amoako


Effects of Nano-Zycosil on Liquid and Gas Permeability of MDF
2012 - IRG/WP 12-40578
Effects were studied of zycosil nanoparticles, with size range from 30 to 90 nm, on liquid and gas permeability of medium density fiberboard. 100 g of nanozycosil was added to each kg of dry fibers. Density was kept constant at 0.67 g/cm3. The obtained results indicated that addition of zycosil to the mat resulted in a significant increase in gas permeability due to the lower fiber-content in the ...
H Reza Taghiyari, K Heidarhaee, P Noori, A Karimi


The effect of press time on springback and water absorption of acetylated particleboard
2012 - IRG/WP 12-40579
In this study the effect of press time on springback, thickness swelling and water absorption was investigated. After 24 hours soaking in acetic anhydride, in order to achieving WPG 17%, acetylated particles were heated in an oven at 120 0C for 360 minutes. Acetylated and nonacetylated (control) particleboards were produced with 10% melamine urea formaldehyde (based on the oven-dry weight of part...
F Bavaneghi, M Ghorbani, A Kargarfard


Water uptake of wood surfaces with and without coating: influence of weathering
2012 - IRG/WP 12-40580
The objective of this study was to compare liquid water absorption of wood surfaces with and without coating, before and after artificial weathering. Samples of spruce, oak and sapelli were exposed to the EN 927-6 cycle for 1500 and 1850 hours and to the weathering produced by the Garner wheel for 1000 hours. Two highly pigmented coatings (solventborne and waterborne) and two semi-transparent stai...
L Podgorski, S Collignan, J D Lanvin


Study on the Effect of Combined Nanosilver-Hygrothermal Treatment on Wood Properties
2012 - IRG/WP 12-40581
In this study, the impregnation process with nanosilver solution, before hygrothermal treatment was carried out to investigate its effect on some physical and mechanical properties of Iranian beech (Fagus orientalis Lipsky) and Russian imported spruce (Picea abies). Wood specimens were impregnated with nanosilver solution (400ppm) in an impregnation tank under pressure of 0.25 Mpa, for 20 minutes....
G Rassam, H Reza Taghiyari, A Karimi, B Jamnani, M Ebrahimi


Influence of heat treatment intensity on the structural integrity of 14 timber species
2012 - IRG/WP 12-40586
Thermally modified timber (TMT) is characterized by improved durability and dimensionally stability, but strength properties, especially the dynamic ones, are compromised at the same time. Because dynamic standard tests require high efforts and time, the high-energy multiple impact (HEMI) –test was developed for the fast and reliable characterisation of the structural integrity of TMT, showing a...