Performance of borate-treated lumber in a protected, above-ground field test in Japan
2004 - IRG/WP 04-30344
This document is supplemental to the previous IRG document (Tsunoda et al., 2002). An experiment to simulate the sill plate (dodai) of the Japanese houses was conducted at the termite field test site of the Wood Research Institute in Kagoshima, Japan where two economically important subterranean termite species [Coptotermes formosanus Shiraki and Reticulitermes speratus (Kolbe)] are established. ...
K Tsunoda, A Byrne, P I Morris, J K Grace


Anti-sapstain chemicals for diffusion treatment of rubber wood
1986 - IRG/WP 3367
Performance of Sinesto B and Akzo EN 494, two formulated products of alkyl ammonium compounds, was tested as fungicidal additive in the boron solution to control mould and stain during diffusion storage of rubber wood. Sinesto B at 2.0% (a.i.) concentration has given good control over mould and its protection against sapstain was only satisfactory. Akzo EN 494 at 0.7% (a.i.) concentration has give...
R Gnanaharan


Gelatin encapsulated fumigants for wood fumigations: Current research status
1985 - IRG/WP 3336
The fumigants chloropicrin (trichloronitromethane) and methylisothiocyanate (MIT) were encapsulated in gelatin as an alternative to liquid fumigant treatments for control of decay fungi in wooden utility poles. Gelatin-encapsulated MIT was stored for over 2 years under dry conditions without significant fumigant leakage. Gelatin encapsulated MIT and chloropicrin were released from capsules when pl...
A R Zahora, M E Corden, J J Morrell


Moisture content of logs under sprinklers
2000 - IRG/WP 00-40157
Logs are kept under sprinklers during storage for avoiding the development of sapstain fungi. According to literature, sapstain fungi do not develop if the moisture content is above 120%. It is supposed that, the water sprinklers maintain the log's moisture content above this value, but, very often, sapstain is found on sawn lumber cut from these logs. Logs are harvested and transported t...
M C Rose, A M Briones, M Fernández


Formosan Subterranean Termite Resistance to Heat Treatment of Scots Pine and Norway Spruce
2003 - IRG/WP 03-40264
New challenges to the durability of wood building materials have arisen in the U.S. The Formosan subterranean termite (Coptotermes formosanus Shiraki) now infests sizable portions of the U.S. south and their range is extending. Heat treatments offer a unique opportunity for wood-based composites because many of the process techniques already employ various thermal applications and could be easil...
W R Smith, A O Rapp, C R Welzbacher, J E Winandy


A bioassay of remedially treated pole material
1987 - IRG/WP 3453
Stubs prepared from treated and untreated utility poles were installed in a test plot and pressure spade treated at the groundline with one of four preservative greases. At one and three year intervals, core samples were removed from the stubs and the improvement in the preservative efficacy due to the greases was assessed. The bioassay investigation showed that only bis(tributyltin) oxide (TBTO) ...
J N R Ruddick, L Parker


The future for chromium in wood preservation
1985 - IRG/WP 3332
Most water-borne preservatives contain CrVI compounds, originally to reduce corrosion although now also to improve toxicant fixation. Chromium contributes to preservation and this is recognised in, for example, New Zealand and USA where chromium contents are included in calculations of overall preservative activity of CCA formulations, but chromium may also have anti-stain and joinery (millwork) p...
B A Richardson, T R G Cox


COST Action E31: Management of Recovered Wood
2005 - IRG/WP 05-50224-26
The COST (European Co-operation in the Field of Scientific and Technical Research) Action E31 (2002 to 2006) is a multi-disciplinary forum for the exchange of information on “Management of Recovered Wood” with the main objective to improve the European management of recovered wood towards a higher common technical, economic and environmental standard. Researchers of 20 European countries – A...
G Jungmeier, B Hillring, A Frühwald, M Humar


Application of paint primers after light organic solvent preservative treatment
1986 - IRG/WP 3381
The application of three alternative paint primers is investigated, including a slow-drying oil-based primer, a fast-drying oil-based primer, and a fast-drying water-based primer. The treatment schedules employed, in particular the evacuation period after treatment, have a marked effect on subsequent paintability. Priming can potentially be carried out immediately after treatment with approved Tim...
P Vinden


Development of a commercial-scale CCA chemical sludge recycling system
1993 - IRG/WP 93-50001-19
The occurrence of fixation reactions in Copper Chromium Arsenate (CCA) treatment solutions is increased where the treatment of unseasoned and partially seasoned timbers in hot climates occurs. The by-products of the fixation reactions are predominantly insoluble chromium arsenate compounds, commonly referred to as CCA sludge. Historically, this material has been disposed of into toxic waste landfi...
A J B Butler


A field trial to assess the potential of antisapstain chemicals for long-term protection of sawn radiata pine
1986 - IRG/WP 3375
Seven chemical formulations were tested as antisapstain treatments for freshly sawn radiata pine sapwood (90x50 mm²). Each formulation was used with and without a water-repellent additive and was sprayed on to 1 m long boards. The boards were then stacked into "mini" packets and stored unprotected from the weather for 6 months. Haipen 50w (at 0.2 or 0.4% active) and NaPCP (1% active) plus 1.5% bo...
J A Drysdale


Selecting fumigants for treatment of internal decay in wood
1986 - IRG/WP 3370
A number of potential fumigants were screened with respect to their toxicity to decay fungi, (Poria carbonica, and Lentinus lepideus) and their sorption characteristics on Douglas Fir (Pseudotsuga menziesii Mirb. Franco) wood. Wafers of infected wood were exposed to different fumigant concentrations for various times then cultured to determine viability. The lethal concentration X time (ct) factor...
P A Cooper


Prevention of sapstain in logs using water barriers
1997 - IRG/WP 97-30147
Placing logs in ponds or under water sprinklers to keep moisture levels high enough to prevent oxygen tensions rising above inhibitory levels, is a proven method of preventing sapstain. The objective of this experiment was to determine if water barriers significantly reduce the rate of sapstain penetration into logs by maintaining moisture contents, and consequently oxygen tensions, at inhibitory ...
R N Wakeling, D R Eden, C M Chittenden, B Carpenter, I Dorset, J Wakeman, R Kuluz


Leaching of components from CCF treated timber in ground contact
1998 - IRG/WP 98-50108
In order to investigate the depletion of different CCF-salts during service small stakes (10*10*450mm³) were treated with five water-borne wood preservatives and after fixation brought into ground contact for several years. After failing some of the broken down stakes were used to determine the remaining concentration of relevant ions and their distribution in different segments of the stakes. A...
E Melcher


"XYLOPHENE ANTI-TERMITES" :A complete range of treatment products against termites
2000 - IRG/WP 00-30230
Dyrup-Xylochimie purpose for several years efficient treatment products for timber and wood materials, with its trade mark : "Xylophèn". As everybody know, termites become an important problem for construction in France. So important that, a national law was voted in May 1999, to define areas where termites are present, in order to protect future landowner. To prevent efficiently termites damages...
L Cubizolles, E Wozniak


Water transfer in wood in relation to fungal attack in building - Effect of condensation and diffusion
1992 - IRG/WP 92-1543
Wood is continuously exchanging moisture with the surrounding atmosphere, the temperature and relative humidity are important factors. Wood moisture in this case is not enough to provoque decay by fungi. However, when, during the night, condensation appears cyclically, wood absorbs water and moisture content may be sufficiently high to allow development if drying does not take place. The water tra...
D Dirol, J-M Vergnaud


A study of methanogenesis and sulphate-reduction: A possible source of explosive gas mixtures in a gold mine
1989 - IRG/WP 1399
Previous work isolated anaerobic bacteria from timbers and drainage water in a gold mine. The present work identifies the predominant methanogen in the mine ecosystem as Methanobacterium bryantii and sulphate-reducing isolates as Desulphovibrio desulphuricans and Desulphotomaculum antarcticum. Laboratory studies using model systems evaluate the activity of methanogenic and sulphate-reducing bacter...
L D Abraham, J F Putterill, A A W Baecker


Diagnostics methods and routes proposalsto define selective sorting of demolition wood wastes
2001 - IRG/WP 01-50177
Wood wastes are more and more often used in different wood waste valorisation industries (panels, wood energy, cement factories, ...). These industries are in progress to include in their processes, wood wastes coming from demolition wood. A state of the art and an analysis have been made to propose : (1) diagnostics methods to carry out a classification of wood wastes on demolition sites and in t...
G Labat, E Bucket, C Fréret, G Deroubaix


Borate diffusion from fused borate rods in douglas-fir transmission poles
1994 - IRG/WP 94-30042
Pressure-treated utility poles have given many years of excellent service, but their lifetime is often shortened by internal decay of the untreated heartwood center, particularly in refractory species, such as Douglas-fir. This paper reports the distribution of boron from fused borate rods installed in CCA-treated Douglas-fir transmission poles. The boric acid equivalent was roughly monitored by t...
T L Highley, W Finney, F Green III


Redistribution of boric acid in radiata pine during drying after preservative treatment
1993 - IRG/WP 93-40010
Samples of 100 x 50 mm² radiata pine were processed with a variety of options to produce dry, boron-treated wood. Concentrations of boric acid in the central one-ninth and in the whole of the wood cross-sections were determined by chemical analysis and compared. Diffusion treated material was dried by air, conventional kiln (70/60°C), or high temperature kiln (120/70°C). Four different predryin...
A J Bergervoet, D R Page, J A Drysdale


Wood cement composites using spent CCA treated wood
1999 - IRG/WP 99-50126
The feasibility of using spent or out-of-service CCA treated wood as a component of wood/cement composites was evaluated. Cold pressed wood particle cement boards were made using CCA treated particles from a red pine (Pinus resinosa Ait.) pole removed from service and from untreated red pine wood from a new pole. Boards were manufactured using a range of wood to cement ratios and water to cement r...
Chen Huang, P A Cooper


A novel method for evaluating the performance of water repellents
1987 - IRG/WP 2279
Application of water repellent formulations to timber surfaces offers protection from the weather, reducing degrade and movement. A novel test method has been developed to evaluate the comparative efficacy of such formulations when samples are exposed to weather. The method uses sapstain free sapwood of defect free, untreated, seasoned Radiata pine, (Pinus radiata D. Don.) Water Repellency was det...
A R Moffat


Penetration of oil-borne preservatives in American elm
1975 - IRG/WP 355
Pressure treatment of elm posts and cants by Rueping schedules resulted in erratic penetration. Instead of the expected gradual decrease in retention from surface inward in posts, inner zones frequently contained more preservative than the surface quarter inch. Heartwood was found penetrated when sapwood was not. There were numerous skips in treated zones. The prevalence and possible causes were i...
E A Behr


Experimental variations in the distribution of CCA preservative in lignin and holocellulose as a function of treating conditions (temperature, concentration, pH, species, and time)
1984 - IRG/WP 3277
The exact distributions between lignin and holocellulose and retentions on wood of copper, chromium and arsenic as a function of various sets of conditions in a 3x3x4x2 factorial experiment in which combinations of three temperatures of treatment, three CCA solution concentrations, four pH's of the initial CCA solution and two timber species, namely Pinus radiata and Eucalyptus grandis, a...
A Pizzi, E Orovan, M Singmin, A Jansen, M C Vogel


Conforming to European standards on preservative treatment
1998 - IRG/WP 98-20150
New European standards require that specifications for the preservative treatment of timber are written in terms of the penetration and retention of preservative within the treated commodity that result from the treatment process. In order to check compliance with this type of specification, suitable methods of quantitative analysis must be available. This paper presents the results of a study by ...
E D Suttie, R J Orsler


Previous Page | Next Page