Preservative treatement of muli bamboo (Melocanna baccifera) by pressure process
2001 - IRG/WP 01-40194
This study was carried out in order to investigate the possibility of preservative treatment of split bamboo by pressure process. Whole bamboo is very difficult to treat by pressure process, which is the best and most dependable of all treating processes. Because it surface has a coat of impervious cutiular which make it very resistance to the penetration of liquid. Beside this it is prone to deve...
K Akhter, M Younusuzzaman, M H Chowdhury


Rapid analytical methods for wood waste - An overview
1998 - IRG/WP 98-50104
The proper handling of wood after service is a today's problem. Untreated wood could be reused or may be used as fuel. For treated wood special care is demanded to avoid environmental impacts. Thus, analytical methods are requested to detect rapidly whether and to what extend wood is contaminated, covering a wide spectrum of organic and inorganic agents used during the last 50 years. Trad...
A Peylo, R-D Peek


The dip diffusion treatment of tropical building timbers in Papua New Guinea
1972 - IRG/WP 310
In Papua New Guinea a dip diffusion process using a multi salt preservative developed by C.S.I.R.0. has been in commercial use for 8 years. Over 200 million super feet (236,000 m³ ) of timber has been treated during this period and current rate of treatment is 34 million super feet (80,400 m³ ) of timber per year in 70 licenced treatment plants. The process has been found to be simple to apply, ...
C R Levy, S J Colwell, K A Garbutt


Effect of treatment process on performance of copper-chrome-arsenate. Part 2: Field stake tests
1995 - IRG/WP 95-40046
Pinus radiata sapwood stakes 20 x 20 x 400 mm³ were treated with CCA Type C using a range of concentrations and three treatment processes; Bethell, Lowry and Rueping. Preservative retention was determined by chemical analysis of treated material. Following fixation stakes were installed in a randomised plot in the Whaka graveyard located on the FRI campus. Stakes were inspected at yearly interval...
M E Hedley, J Anderson, J B Foster, B E Patterson


Acceleration of the fixation of chromated wood preservatives by UV-radiation
1989 - IRG/WP 3544
Preliminary laboratory tests demonstrated that the fixation of chromated water-borne wood preservatives may be accelerated by UV-radiation. The degree of fixation depends on the intensity of radiation and the prevailing temperature. Three hours radiation at 20°C in a device for artificial weathering diminished the leaching of chromium to 43% and of copper to 23% compared to not-radiated samples. ...
H M Illner, H Willeitner, K Brandt


A Preliminary Report on the Properties of Engineered Wood Composite Panels Treated with Copper Naphthenate
2005 - IRG/WP 05-40294
This paper reports on our preliminary investigation of the properties of randomly oriented strandboard which had waterborne or powdered copper naphthenate (CuN) incorporated into the board during manufacture. When compared to zinc borate-treated controls (ZnB), the mechanical properties of strandboard (MOR, MOE, work-to-maximum load, internal bond strength) were not adversely affected by treatmen...
J W Kirkpatrick, H M Barnes


Bending properties of TCMTB-treated Southern pine sapwood using supercritical carbon dioxide impregnation process
1997 - IRG/WP 97-40080
The effects of elevated pressure and treatment with thiocyanomethylthiobenzothiazole (TCMTB) on the bending properties of Southern pine sapwood were evaluated at pressures ranging from 1,800 to 3,600 psi. All bending properties were affected to some extent by supercritical fluid treatment. Modulus of elasticity and work to maximum load were not significantly affected by pressure levels. Modulus of...
Gyu-Hyeok Kim, S Kumar, E S Demessie, K L Levien, J J Morrell


An environmental assessment of timber treatment plants in Australia
1999 - IRG/WP 99-50124
Australian Standard AS 2843 Timber Preservation Plant Safety Code, sets the specifications for the design and operation of timber treatment plants in Australia. The Timber Preservers' Association of Australia has carried out an environmental survey of timber treatment plants throughout Australia using the operational checklist provided in Appendix C of Part 2 of the Standard. Third party ...
J Norton, K Riley


Decrease of the antidecay resistance of beech wood treated with organotin fungicides after its natural ageing
1998 - IRG/WP 98-30185
The antidecay resistance of beech-wood samples (120 x 8.5 x 8.5 (MM)) treated with tributyltin fungicides gradually decreased due to prolongation of their natural ageing: tributyltin fungicides (TBTO, TBTS, TBTCA, TBT-DEDTK were applied by pressure impregnation technique in ethanole solutions (c = 0. 1%, 0.33% or 1%); treated beech-wood samples were naturally aged without their contact with grou...
L Reinprecht


Study of the degradation of retified wood through ultrasonic and gravimetric techniques
1994 - IRG/WP 94-40030
One of the non-polluting processes that increase the natural durability of wood is a thermal treatment in an atmosphere poor in oxygen, producing what is normally denominated "retified wood". In this study the validity of a non-destructive technique (ultrasound) in order to determine the biodegradation suffered by wood across time has been studied. For this reason, the behavior of a wood species (...
D T De Troya, A M Navarrete


Treatment of wood-based panel products with volatile borate
1990 - IRG/WP 3616
The paper presents recent developments in the use of volatile borate esters for the preservative treatment of wood based board materials. Several advances on previous reports are discussed. In laboratory studies, treatment times of approximately ten minutes at 20°C on boards at equilibrium moisture content provided full penetration and retentions of 1% wt/wt boric acid. Biological tests have been...
P Turner, R J Murphy, D J Dickinson


Soil-bed studies. Part 2: The efficacy of wood preservative
1983 - IRG/WP 2205
Various methods of decay assessment were investigated. Three stages or phases of decay were identified which could be used to describe the efficacy of a preservative system or virulence of a soil-bed testing medium. These included the lag, decay, and senescent phase. Premature senescence could arise if wood samples became waterlogged. It was concluded that time to failure was unsuitable as a metho...
P Vinden, J F Levy, D J Dickinson


Microwave conditioning of Pinus radiata D. Don for preservative treatment
2000 - IRG/WP 00-40182
This paper reviews the effect of pressure steam conditioning on the permeability and treatability of green radiata pine heartwood and the potential for substituting microwave conditioning for steaming. The penetration of liquids into radiata pine occurs mainly in the radial tissue. The permeability of green radiata pine improves following steam conditioning by blowing out the soft radial tissue. T...
P Vinden, G Torgovnikov, J Romero


Anatomical Characteristics to the Distribution of Water-borne Copper Wood Preservatives in Wood
2004 - IRG/WP 04-40277
The objective of this study was to understand the micro-distribution of a copper-based preservative in wood in connection with anatomical morphology and to consider the fixation of copper in wood. Bulk specimens and semi-ultra thin sections (0.5µm) obtained from Japanese cedar were treated with a CuAz preservative solution. After fixation, SEM-EDXA was used to investigate the micro-distribution...
H Matsunaga, J Matsumura, K Oda


Moisture condition in treated wood exposed outdoors. A progress report
1989 - IRG/WP 3533
Wood treated with water-borne preservatives, mainly CCA (copper/chromium/arsenic), CCB (copper/chrome/boron) or CC (copper/chrome) is often said among users in Sweden to absorb more water than untreated wood. In laboratory tests this statement has not been confirmed but no field tests have been carried out in Sweden to study this phenomenon. In 1986 a project was started to compare water absorptio...
M-L Edlund, C E Sundman


Sampling rates and the probability of detecting defective treatment in the sampling of preservative treated timber
1987 - IRG/WP 2277
When attempting to enforce standards of penetration and retention set for treated timber, the regulating authority must establish a sampling or inspection scheme which will prevent large quantities of substandard product entering the market. On the other hand, the scheme should not penalise treaters for the small quantities of such material which are inevitably produced by any industrial process. ...
M J Kennedy, L E Leightley


Durability of surface preserved wood particle boards submitted to atmospherical influence
1995 - IRG/WP 95-40039
The worldwide problem of the continuously growing deficit of high quality natural wood material has caused the attempts of many research workers to find effective composites such as wood particle boards (WPBs) for replacing the massive wood for constructive purposes, depending on where the boards are exploited - in the open or under a shed, they are submitted to various climatic factors such as he...
L Valcheva


Determination of fixation properties by bioassays - A proposal for the assessment of safety indexes in wood protection
1990 - IRG/WP 3566
In the determination of environmental effects of chemicals tests with fishes, daphnia and algae have proved to be practicable. With respect to wood protection such bioassays are suitable to control effects of treated timber against aquatic organisms. By using the fish-acute-toxicity-test the development of a laboratory test method is described for the checking of the fixation rate of a copper-chro...
H-W Wegen


Risk reduction from curative treatments, restoration and maintenance of building and individual housing - simple precautions that make the difference
2005 - IRG/WP 05-50224-15
This document explores the potentialities of risk reduction, from activities of remediation in construction, developped at small scale by professionals or individuals on targets like moulds, rots, termites and other wood destroying insects, with products distributed for professional or do-it-yourself purposes. At the first stage, an inventory of the type / interest of products / processes is carri...
G Ozanne


Optimum growth conditions for the metal-tolerant wood decay fungus, Meruliporia incrassata TFFH 294
1999 - IRG/WP 99-50142
There is a worldwide need for alternative methods for the treatment and disposal of CCA-treated waste wood. Illman and Highley (IRG/WP 96-10163) reported the isolation of a unique strain of Meruliporia incrassata (TFFH 294) with tolerance to CCA. The strain is capable of degrading CCA treated waste wood, giving a 40% weight loss in the ASTM soil block test. The strain is an ideal candidate for deg...
V W Yang, B Illman


Traitement des matériaux lignocellulosiques en présence des composés halogénés (Risques toxiques des produits de combustion)
1995 - IRG/WP 95-50040-17
From the point of view of the combustion products toxicity, the highest environmental hazard comes from the combustion of materials creating toxic products such as dioxins and dilbenzofurans. 95% of these are formed during incineration of different materials. The aromatics result essentially from the products of paper industry and from wood treatment. Formation of halogenated products during the c...
I Surina, M Slimak, S Vodny, A Périchaud, K Balog


Treatment of wood with formaldehyde. Acid catalysis of the reaction between formaldehyde and wood
1980 - IRG/WP 3146
Formaldehyde reacts with the free OH-groups in wood forming cross-linking bonds. The reaction can be brought about without any catalyst but in that case the activation energy is very high and high temperatures and long reaction times are needed. Normally, the reaction is catalysed by different acids. Acid catalysts, however, tend to degrade the cellulose and the wood matrix causing reduction in th...
T Vihavainen, K Piispanen, P Mansikkamäki


Practical consequences of the clarification of the chemical mechanism of CCA fixation to wood
1983 - IRG/WP 3220
Practical consequences derived from the chemical investigation of the mechanism of fixation of CCA to the wood constituents are discussed. Among these, formulas for the calculation of the time of hexavalent chrome fixation are presented. Furthermore, three parameters are shown to be important to the long-term effectiveness of CCA-treated timber: (i) the temperature of treatment, (ii) the initial p...
A Pizzi


Serviceability modeling-Predicting and extending the useful service life of FRT-plywood roof sheathing
2000 - IRG/WP 00-20210
One of the most, if not the most, efficient methods of extending our existing forest resource is to prolong the service life of wood currently in-service by using those existing structures to meet our future needs (Hamilton and Winandy 1998). It is currently estimated that over 7 x 109 m3 (3 trillion bd. ft) of wood is currently in service within the United States of America (PATH 1999). Research ...
J E Winandy


The effect of wick action on the moisture distribution in heartwood and sapwood stakes of Pinus radiata D. Don.
1999 - IRG/WP 99-40139
The pattern of moisture distribution in stakes of Pinus radiata D. Don. subjected to "wick action" is investigated. There was incomplete saturation of the stakes even after 93 days of continual soaking. Maximum moisture absorption occurred at the base of the stake and at the air/water interface of the stake. Incomplete saturation of the stake was thought to be due to air embolism within the wood. ...
J Hann, P Vinden