The biological durability approach for wood product performance and service life prediction
2010 - IRG/WP 10-20457
The performance of wood-based products under conditions that enable biodegradation are of concern to all who envisage sustainable use of forest based products. This concern is also the basis of classification of wood species on the basis of their biological durability. Engineers are looking for options to transfer such classification into practical service life values for constructions and related...
J Van Acker, J Van den Bulcke, L De Boever


Improved analysis of field test data related to service life prediction of tropical wood species
2010 - IRG/WP 10-20458
Long field trials of wood in ground contact give valuable data on the natural durability of the material. The European Standard EN 350 gives guidance on how to perform these durability classification, but is limited to the use of averages of in-service life of a set of specimens compared to a reference set. Starting from a database of visual assessment of field stake testing, it is possible to obt...
J Van den Bulcke, A Wong, Ling Wang Choon, Yoon Soo Kim, J Van Acker


Assessment of Boracol 200RH (FrameSaver) as a remedial treatment to control decay in pre-decayed model timber frame units
2010 - IRG/WP 10-30529
Model timber frame units constructed from untreated radiata pine were pre-wetted to approximately 40% moisture content and inoculated with Coniophora puteana and Oligoporus placenta. Units were transferred to a controlled environment room maintained at 25°C and 95% RH for 7 and 10 weeks to allow two levels of decay to become established in units. Following pre-decay, units were disassembled, clea...
Mick Hedley, Dave Page, Jackie van der Waals


Accelerated L-joint performance testing of organosilicon treated wood
2010 - IRG/WP 10-30551
In this research Scots pine sapwood L-joints were treated with organosilicons and organosilicons in combination with biocides. These L-joints were prepared and exposed according to the accelerated L-joint method. They were inspected each season for fungal discolouration and removed from the rack after three years outdoor exposure. Subsequently the moisture content, mass loss and decaline uptake we...
L De Vetter, J Van Acker


Impact of wood species on the performance of exterior wood coatings
2010 - IRG/WP 10-40519
To prolong the service life of a wooden construction the protective function of a coating is of utmost importance. The chemical composition as well as the wood-coating interface affects the performance of this protective layer and obviously wood species have an impact too. This paper discusses the influence of wood species on the overall coating performance. Therefore, a range of opaque waterborne...
I De Windt, J Van den Bulcke, J Van Acker


Moisture dynamics of WPC as basis for biological durability
2010 - IRG/WP 10-40520
The largest market for wood-polymer composites (WPCs) is currently decking. Although many products are commercially available, a proper standard for the assessment of the biological durability of WPC does not exist. Recommended standards for testing resistance against basidiomycetes should be completed with a method to bring the specimens in a worst case situation, obtaining a moisture level high ...
N Defoirdt, J Van Acker, J Van den Bulcke


Non-destructive evaluation of wood decay
2011 - IRG/WP 11-20479
Evaluation of wood decay is often prone to subjective assessment. Standard rating scales are based on human perception of decay, often in addition to weight loss measurements. Especially the assessment of graveyard specimens or other long term testing material that has to be monitored regularly on a non-destructive basis, is challenging. In this paper two techniques are presented that can deliver ...
J Van den Bulcke, I De Windt, N Defoirdt, J Van Acker


The durability of acetylated radiata pine sapwood (Accoya). Results from five years testing
2011 - IRG/WP 11-30560
New Zealand grown radiata pine sapwood was modified using the Accsys PLC acetylation process (Accoya). Following treatment, various test samples were exposed in the Scion Accelerated Field Test facility (Fungus Cellar) and in exterior ground contact field tests. In the Fungus Cellar, performance was compared with that of radiata pine treated with CCA to Hazard Classes H3.2 (0.37% m/m Cu+Cr+As) and...
M Hedley, D Page, J van der Waals, K Nasheri, G Durbin


Limited variability in biological durability of thermally modified timber using vacuum based technology
2011 - IRG/WP 11-40567
The SmartHeat® thermal timber treatment is a new technology based on the process parameters being steered very precisely mainly due to the vacuum applied and heating system involved. Timber treated with this technology shows a potential for less variability of biological durability in one batch. Several batch treatments were sampled and assessed on statistical variability of decay resistance agai...
J Van Acker, S Michon, J Van den Bulcke, I De Windt, B Van Swaay, M Stevens


Coconut lumber for wood decks (Cocos nucifera L.): decay resistance against Basidiomycetes fungi
2012 - IRG/WP 12-10784
Since a couple of years, manufactured products of coconut wood for outdoor uses like wood decks have been proposed on the European market. These are presented as an alternative for traditional tropical timbers. In the past, coconut wood was neglected and burned for sanitary reasons and lack of interest at industrial scale. Plantation coconut trees at end of production of copra constitute a renewab...
B Jourez, C Verheyen, J Van Acker


Plywood under the scanner: linking moisture dynamics and 3D structure
2012 - IRG/WP 12-20491
Plywood is highly esteemed as a construction material. Yet, the influence of moisture on both strength and durability are important factors. Especially the dynamics of moisture desorption and absorption should be taken into account when assessing the quality of a panel, which is a fact for all panel materials. This paper therefore focuses on the monitoring of the moisture dynamics of plywood subje...
J Van den Bulcke, I De Windt, N Defoirdt, J Van Acker


Testing service life for use class 3: accelerated L-joint performance of commodities
2012 - IRG/WP 12-20500
Above ground testing is considered important for the assessment of treated wood intended for use class 3. Laboratory testing of efficacy of biocides as well as of natural durability focussing on such applications has to be linked to performance and service life. An accelerated L-joint test was some 15 years ago developed at the Ghent University to allow worst case assessment under semi-controlled ...
J Van Acker, J Van den Bulcke, I De Windt, L De Vetter


Protective nanoparticle coating reducing water absorption of wood species
2012 - IRG/WP 12-40614
Nanoparticle coatings were deposited onto different tropical wood samples for controlling the surface hydrophobicity. The styrene(maleimide) nanoparticles were synthesized in aqueous dispersions under pure conditions or in combination with 70 wt.-% palm oil. A first evaluation of the non-coated wood surfaces indicates a high dependence between the water contact angles, the average surface roughnes...
P Samyn, A Paredes, G Becker, H Van den Abbeele, L Vonck, D Stanssens


Detection of Aureobasidium as the dominant fungus on coated wood
2013 - IRG/WP 13-10796
Wood is often covered with a coating in order to protect the surface. Unwanted dark mold growth on paint covered surfaces in external conditions is a familiar phenomenon. Simple microbial techniques have commonly been used to determine the dominant fungal species present in the discoloured area, for example morphological analysis of microscopic preparations of fungal pieces sticking to an adhesive...
E J Van Nieuwenhuijzen, M F Sailer, R A Samson, O C G Adan


Statistical analysis of durability tests - Part 1: Principles of distribution fitting and application on laboratory tests
2013 - IRG/WP 13-20504
Service life prediction is an important topic in wood research, especially with regard to the Construction Products Regulation (CPR). Both laboratory tests as well as in-service performance testing are therefore essential in combination with proper monitoring and analysis tools. A crucial concept is variability in testing and analysis, especially for a biological material such as wood. The larger ...
I De Windt, J Van den Bulcke, C Brischke, C R Welzbacher, A Gellerich, S Bollmus, M Humar,


Determination of the natural durability of solid wood against wood-destroying fungi - a European round-robin test
2013 - IRG/WP 13-20511
In Europe the durability of wood against wood-destroying basidiomycetes is tested according to CEN/TS 15083-1 (2005). Hitherto existing experience with this standard is quite heterogeneous and results from previous round-robin tests have stayed unreported or have been reported incompletely. In particular the need for natural pre-weathering of the test specimens to allow potential detoxification of...
C Brischke, C R Welzbacher, A Gellerich, S Bollmus, M Humar, K Plaschkies, W Scheiding, G Alfredsen, J Van Acker, I De Windt


Statistical analysis of durability tests - Part 2: Principles of time-to-failure and application on field test data
2013 - IRG/WP 13-20512
Service life prediction is an important topic in wood research, especially with regard to the Construction Products Regulation (CPR). Both laboratory tests as well as in-service performance testing is therefore essential, in combination with proper monitoring and analysis tools. A crucial concept is variability and the incorporation of variability in tests and analysis. In this paper we focus on t...
J Van den Bulcke, I De Windt, C Brischke, C R Welzbacher, A O Rapp, J Van Acker


Performance standards for wood in construction – delivering customer service life requirements
2013 - IRG/WP 13-20537
There is increasing need for consideration of performance classification for wood products in construction, as evidenced by the CPR, warranty providers and end user demands for information. This means we need to radically consider how the tests we conduct on wood for durability (especially biological durability) can inform on service life and how they might if possible be translated into a perform...
E Suttie, C Brischke, F Englund, E Heisel, J Jermer, D Lorenzo, M Polášek, S Thelandersson, J Van Acker


Variability in durability of some selected South-American wood species
2014 - IRG/WP 14-10831
Within the scope of sustainable forest management one wants to encourage the proper use of lesser known wood species. Therefore the market has to shift from a demand-driven towards a supply-driven market without loss of wood quality. It is generally known that the durability from pith to bark varies thus, affecting the overall durability of wood species. Consequently, a detailed analysis is necess...
I De Windt, P ’t Hooft, J Van den Bulcke, J Van Acker


Performance classification of wood in construction – drafting a user friendly European standard
2014 - IRG/WP 14-20545
The performance classification for wood products in construction is an extremely important topic in Europe and beyond – warranty providers and end users demand service life and performance information in the face of competition with other materials. The European project PerformWOOD has formalised and drawn together the on-going research to focus on generation of a material resistance factor for ...
E Suttie, C Brischke, L Meyer, J Van Acker, M Kutnik, E Heisel, F Englund, J Jermer, S Thelandersson, M Polášek, D Lorenzo


Moisture dynamics of wood and wood-based products – Results from an inter-laboratory test
2014 - IRG/WP 14-20539
In the frame of the European research project PerformWOOD in close liaison with the CEN task group TG EN 350 of CEN TC 38 WG 21 in total six research institutes teamed up and initiated an inter-lab trial (Round Robin) to investigate the suitability of different test methods to determine the wetting ability of wood. The moisture performance of wood and wood-based products has been recognized as key...
C Brischke, L Meyer, C Hesse, J Van Acker, I De Windt, J Van den Bulcke, E Conti, M Humar, H Viitanen, M Kutnik, L Malassenet


The development of accelerated test systems to evaluate the durability of framing timber
2014 - IRG /WP 14-20547
Various accelerated decay resistance trials including small simulated wall units, samples exposed in enclosed tanks and ‘I’ samples in stacks have been explored and used to test the durability of treated and untreated radiata pine framing at Scion since 2001. These testing methods have been established to determine the effectiveness of commercial formulations in preventing decay in framing sub...
T Singh, D Page, J van der Waals


Statistical analysis of 40 years of preservative in-ground stake testing in Australia
2014 - IRG/WP 14-20552
Wood is widely recognized as a valuable material, yet the natural durability of some wood species limits its use for certain outdoor purposes. For decades, a wide range of methods and chemicals have been developed to increase the resistance of wood against degrading microorganisms and termites. Preservative treatment has a long and widespread tradition in wood protection. Proper testing of the eff...
J Van den Bulcke, L J Cookson, I De Windt, W Li, J Van Acker


Critical parameters on moisture dynamics in relation to time of wetness as factor in service life prediction
2014 - IRG/WP 14-20555
The concept of natural durability or enhanced durability based on the presence of active ingredients having an impact on both fungi and insects is not the only parameter steering the material resistance. Complementary resistance to getting wet (wetting ability) and consequently the ease of drying afterwards will lead to a parameter related to the time a piece of wood will remain under such wet con...
J Van Acker, I De Windt, W Li, J Van den Bulcke


Biological durability of natural fibre reinforced composites
2014 - IRG/WP 14-40681
Composite materials reinforced with wood or non-wood natural fibres have the potential to be a lighter and lower-cost alternative construction material. Until better availability and properties and a lower cost price of degradable polymers makes their use more prevalent, the application of natural fibre reinforcements in synthetic polymers is an intermediate step towards products that are complete...
N Defoirdt, I De Windt, J Van den Bulcke, J Van Acker


Previous Page | Next Page