Your search resulted in 286 documents. Displaying 25 entries per page.


Beetle-Fungus Associations in Woody Substrates in the Context of International Trade
2007 - IRG/WP 07-10610
Interest in the role of insects in transmitting various fungi and in the potential for outbreaks of insects vectoring plant disease organisms has resulted in a large volume of literature on insect-fungi relationships. Mites are mentioned as an important third partner in these associations. This paper summarizes information and provides an update on major aspects of these intricate associations in ...
A Uzunovic


Comparison of permeability at different levels of moisture content in Bornmullerian fir (Abies bornmulleriana Mattf.) and Eastern spruce (Picea orientalis L.) impregnated under vacuum/pressure through full-cell method by using CCA and CCB of different concentrations
2007 - IRG/WP 07-40366
In this study, a comparison has been made in terms of the combined, longitudinal, tangential, and radial permeability of the species of Bornmullerian fir (Abies bornmulleriana Mattf.) and Eastern spruce (Picea orientalis L.) with moisture contents of 50 % and 15 %, which were impregnated under vacuum/pressure through full-cell method by using water-borne wood preservatives (impregnation materials)...
I Usta


Theoretic discussion on the way and driving forces of moisture migration in wood during vacuum drying
2011 - IRG/WP 10-40538
Most of parameters in conventional drying cannot explain a lot of phenomena appeared in vacuum condition, so it is necessary to further explore the moisture migration way and driving forces in wood under vacuum condition. For the water movement channel in wood is very narrow, the characteristic of heat and mass transfer in wood is similar to that in microscale. This article applies theory of liqui...
Zhengbin He, Xueli Yao, Liqiong Chen, Songlin Yi


The potential of silicone-based formulations to enhance wood properties through industrial treatment for outdoor use
2011 - IRG/WP 11-30578
High hygroscopicity is one of the main weaknesses of wood as far as its susceptibility to biodegradation, and specifically to fungal decay. New wood preservation technologies are constantly entering the wood protection market, competing with traditional, biocide-based preservation. Silicones are commercially used as hydrophobic agents on stones and concrete. They belong to the restricted number of...
F Simon, F Marchal, F Pochon, M Kutnik, I Le Bayon


Effect of preservative treatment on mechanical performance of round and square poles made of small diameter Scots pine
2012 - IRG/WP 12-40612
A growing proportion of harvested Scots pine (Pinus sylvestris L.) timber originates from the first or second commercial thinning stands. There is a need to find economically viable and high quality wood products that can be manufactured from this raw material. Small log volume means not only demands of increased efficiency for material handling in logistics and manufacturing processes, but also c...
V Möttönen, R Stöd, K Heikkilä, H Heräjärvi


Water absorption and desorption of non treated, pressure impregnated, and pine oil treated glulam made of small diameter Scots pine and Norway spruce
2012 - IRG/WP 12-40616
A growing proportion of harvested timber originates from the first or second commercial thinning stands in Finland, which means smaller average log volumes in comparison to final felling stands. Smaller log volume means challenging wood properties such as higher proportion of juvenile wood and sapwood. Due to these facts, products made of small diameter logs are prone to twist and check, and have ...
H Heräjärvi, V Möttönen, R Stöd


Functional silicones used as a potential tool for the development of non-biocidal wood treatments
2015 - IRG/WP 15-30665
The increase of wood resistance against biological agents for outdoor use is conventionally performed by deep impregnation with preservatives. However, some of the traditional wood preservatives, used for decades for wood protection and regarded as the most effective, are currently subjected to severe restrictions because of their toxicity. In fact, new preservation technologies are constantly ent...
F Lhumeau, C Delaite, F Marchal, F Pochon, M Kutnik


Impregnation of railway sleepers - Pressure gradient and transversal penetration
2016 - IRG/WP 16-40731
Based on the possible ban of creosote in the future, the need for oil based alternative products has gained in importance. Due to possible differences in impregnation properties compared to creosote the need for re-implementing former technology is given, to determine if momentarily used impregnation processes have to be modified. The here reported tests measure the pressure gradient during the im...
M Starck, A Gellerich, H Militz


Influence of pressure phase impregnation time on the uptake and distribution of wood preservatives in Scots pine material of diverse treatability
2016 - IRG/WP 16-40752
In spite of the general opinion that Scots pine sapwood is easy to impregnate considerable variations in treatability are reported. In order to study impregnation results of diverse Scots pine sapwood treated with increasing process times, Scots pine sapwood from two different predefined treatability groups was impregnated. A copper solution was used as impregnation agent in ten different vacuum p...
K Zimmer, B Kerfriden


Treatability of beechwood railway sleepers with potential creosote substitutes
2017 - IRG/WP 17-40790
Maintenance of an efficient railway infrastructure still requires the use of wooden railway sleepers, particularly because wooden sleepers have more favourable properties for intensified vibrations than concrete or steel sleepers. Creosote, used for decades for the impregnation of railway sleepers, will possibly no longer be available for this application due to European legislation. This reveals ...
N Pfabigan, E Habla, R Gründlinger


Non-vacuum/pressure ACQ treatment
2023 - IRG/WP 23-40971
Many developing countries are located in sub-tropical or tropical regions where rapid wood deterioration results in early failure of many structures. Whilst preservative treatment would help to reduce these losses and extend the forest resource commercial vacuum pressure treatment systems are often too expensive. The use of lower technology treatment systems, while not as quick as vacuum pressure ...
J Norton


Status of the research and development of a new preservative system (EFPL) for pressure treatment of spruce in Canada
1975 - IRG/WP 348
Our work has been to develop a system which would have the stability of the ACA system and the formulation flexibility of the CCA system enabling properties such as fixation of arsenic, water repellency, appearance and cost to be controlled. Our permeability studies of spruce using a method previously developed indicated that an ammoniacal solution of copper arsenate is an excellent candidate for ...
J Rak, M R Clarke


New technique to analyze impregnation processes
1988 - IRG/WP 2304
Equipment has been developed to measure liquid flow in wood during impregnation processes. Basic principles of flow measurements using directly heated negative temperature coefficient thermistors, and some characteristics of the hardware developed are presented in this paper....
J P Hösli


The use of pressure cycling to improve heartwood penetration in Pinus radiata (D. Don)
1995 - IRG/WP 95-40050
This study investigates the effect of cycling pressure on the treatability of radiata pine heartwood. The results indicate that liquid penetration into the heartwood is affected by the preconditioning method used and pressure treatment time. There is no significant improvement in the penetration of Pinus radiata (D. Don) heartwood when a cycling or pulsation process is used....
P R S Cobham, P Vinden


Non-pressure treatability of plywood by CCA, CCB and boron
2005 - IRG/WP 05-40295
Study on diffusibility and absorbability of CCA, CCB and boric acid in 3 mm thick 3-ply hardwood plywood at water saturated and air-dry conditions and dipped at same concentration (5%) and same duration of time (12 hours) revealed complete diffusion of all the preservatives at water saturated condition. Only the CCA-C was found absorbed by the plywood at air-dry condition. The rate of absorption a...
A K Lahiry


Field tests out of ground contact in France: Definition of the test procedure and preliminary results after 18 months
1981 - IRG/WP 2161
M Fougerousse


Studies of the distribution and degradation of tributyltin naphthenate in double-vacuum treated wood
1983 - IRG/WP 3230
The effects of forced solvent evaporation by kilning redwood (Pinus sylvestris) that has been double-vacuum treated with tributyltin naphthenate (TBTN) have been investigated. Contrary to previous studies reported, it has been shown that forced evaporation can have a considerable influence on the losses of the fungicide. It has been found that, whether the solvent is allowed to evaporate slowly or...
J Jermer, M-L Edlund, W Hintze, S V Ohlsson


Recycling of pressure impregnated timber and preservatives - incineration techniques
2001 - IRG/WP 01-50166-19
The object of the recycling research projects is to determine the technical and economical requirements of the recycling of CCA-impregnated wood. In the first recycling of impregnated timber project the amount and location of recyclable treated wood in Finland was determined and the costs of recycling were calculated. An incineration test was also made (1998). The conclusion of the first project i...
T Syrjänen, E Kangas


Light organic solvent preservative treatment schedules for New Zealand-grown radiata pine
1986 - IRG/WP 3379
The influence of pressure differential and treatment time on preservative uptake and distribution in radiata pine heartwood and sapwood is investigated. Treatment schedules are defined which minimise solvent usage but ensure complete sapwood penetration and optimise heartwood penetration....
P Vinden


Creosoted radiata pine by non-pressure methods
1988 - IRG/WP 3486
Posts of Pinus radiata have been impregnated with creosote by immersion for 1, 3, and 7 days, and by hot-and-cold open tank with hot bath temperatures at 40°C and 60°C. On the basis of the retention rates obtained, suitable procedures are described for wood elements that are going to be in ground contact, and an analysis is made of the way in which the variables tested affect the results....
M V Baonza Merino, C De Arana Moncada


Scientific development for prolonging the service life of timbers by impregnating with creosote or organic solvent type preservatives in which additive has been incorporated
1977 - IRG/WP 382
Chemically impregnated wood has played a prominent part in the Telephone and Electricity Distribution Industry during the past century and there is no doubt that it will play an equally prominent part in the future. The reasons why wood poles and wooden, structures predominate, are that when adequately chemically impregnated with a recognised timber preservative to ensure the expected service life...
P R B D De Bruin


Fire resistance of Alder wood treated with some chemicals. Part II. Effect of Other Chemicals on the Combustion Properties
2002 - IRG/WP 02-40235
Samples from alder wood (Alnus glutinosa (L.) Gaertn. subsp. barbata (C.A.Mey) Yalt.) were impregnated according to ASTM D 1413-88 with boron compounds (boric acid, borax, sodium perborate), vinyl monomers (styrene, methyl methacrylate), Tanalith-CBC, Phosphoric acid, Vacsol, Immersol, Polyethylene glycole (PEG-400) and their mixed solutions of chemicals in order to determine their combustion pro...
A Temiz, Ü C Yildiz


Long-term performance of a "wax" type additive for use with water-borne pressure preservative treatments
2000 - IRG/WP 00-40159
Field performance results are updated for matched CCA treated decking boards with and without an emulsion water repellent additive incorporated with the initial pressure treatment. Decks have been exposured for over 9 years in Harrisburg, NC. Boards were evaluated for in-service and laboratory performance for water repellent efficacy, as well as additive loadings in the boards after this exposure....
A R Zahora


The utilization of preserved rubberwood
1982 - IRG/WP 3186
The paper examines the use of processed and kiln-seasoned rubberwood for manufacturing furniture and doors and windows, discusses methods tested and found acceptable for preserving the timber as well as for drying the treated timber in conventional kilns. It considers a type of furniture where narrow width timber of preserved and kilned rubberwood has been used with great success. It recommends th...
V R Sonti, B Chatterjee, M S Ashraf


Multiple-Phase Pressure (MPP) Process: One-stage CCA treatment and accelerated fixation process. 5. Treatment of Sitka spruce and Scots pine
1999 - IRG/WP 99-40136
The suitability of the MPP Process for CCA treatment and accelerated fixation of species other than Radiata pine was assessed by pilot plant trials on UK-grown Sitka spruce (Picea sitchensis) and Scots pine (Pinus sylvestris). Pressure and vacuum kickbacks of spruce (14 l/m3) and Scots' pine (122 l/m3) were both substantially lower than that generated during treatment of radiata pine (369...
M E Hedley, K Nasheri, G Durbin


Previous Page | Next Page