IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 286 documents. Displaying 25 entries per page.


Application of roller-pressing method to the novel liquid impregnation treatment of green timber
2001 - IRG/WP 01-40198
A transverse compression technique enabled us to impregnate liquid into green timber through replacement of the free water in the timber with a treatment liquid without any critical physical damage to the timber by the roller-pressing method. The roller-pressing is supposed to remove free water the cell cavities and to concurrently introduce the treatment solution into green timber in the treatmen...
M Inoue, K Adachi, K Tsunoda, Y Imamura, S Kawai


Selective chromate elimination from the storage-drainage-water of a wood impregnation plant
1980 - IRG/WP 3153
With the Enviro-Chrom-Ex process it is possible to eliminate ecologically and economically hexavalent chromium (chromate) from water selectively. The process which is based on the principle of selective ion exchange works with different chromate concentrations and under the presence of other ions, irrespective of the water hardness. The values of water-offtake reach 0.1 mg CrVI at maximum, causing...
O Wälchli, R Ott, R Hugener, E Graf, B Lieberherr


A method for the preliminary assessment of timbers for their treatability with preservatives under pressure
1977 - IRG/WP 3100
President Maurice Fougerousse has provided the following references to a IUFRO report, published in English, French and German, which may be of interest to IRG members: 'A method for the preliminary assessment of timbers for their treatability with preservatives under pressure', PANS Vol 23, No 2, 153 158, June 1977. 'Une methode d'evaluation preliminaire de l...
M Fougerousse


Efficiency of wood impregnation processes
1980 - IRG/WP 3151
Many wood impregnation processes have been in use for a very long time, up to 150 years, but they have not been progressively modified. This paper considers impregnation processes in relation to current requirements, particularly impregnation efficiency and energy consumption. The term 'pore' is used throughout in its physical sense and is not confined to botanical 'pore...
B A Richardson


Treatability of waterstored poles of Norway spruce by sap-displacement and pressure treatment with Boliden K33 and creosote
1973 - IRG/WP 328
Poles of windthrown Norway spruce were stored in bark under water sprinklers for 11-20 months or fully submerged in a lake for 3 years (tab. 1 and 2). Water content after storage is shown in fig. 1 and 8. Treatment with Boliden K33 by sap-displacement (open tank suction) gave a poor result. The Danish requirements of delivery claim a penetration of 20 mm and a net retention of 12 kg/m³ in outer 2...
P Moltesen, E Borsholt, B Bang


Termite Field Tests of Various Timber Species Treated with permethrin using supercritical carbon dioxide
2005 - IRG/WP 05-10560
Termite field tests were conducted on permethrin-treated Eucalyptus obliqua heartwood, Pinus radiata sapwood and P. radiata LVL. The permethrin was impregnated using either supercritical carbon dioxide (scCO2) or light organic solvent preservative (LOSP) systems. Comparative permethrin retentions were most accurately achieved in P. radiata sapwood, where no difference between impregnation systems ...
A Qader, L J Cookson, J W Creffield, D Scown


The non-uniform uptake of chromium and copper during the impregnation of wood using the example of a CCB-salt
1998 - IRG/WP 98-20137
The correct impregnation of wood requires among other things a regular control of the concentration of the treating solution as this and/or its stoichometric composition can change as a result of the impregna-tion process and the treated wood. The preferential uptake of individual wood preservative components by the wood is of particular importance in this connection. Dipping and vacuum impregnat...
P Jüngel, E Melcher, R-D Peek


Volatile organic compounds (VOC) measured during drying of impregnated timber
2004 - IRG/WP 04-50216
Discussion about drying of impregnated timber has taken place in the Nordic countries under eighties and nineties and goes on nowadays. The drying increase the value of production and the customer gets fewer problems when handles the timber. This introduces a positive attitude to the impregnation as a process and its products. Beside the important information about the advantages of impregnated ti...
N Terziev, V Djokic


Preservative treatment and field test monitoring of spruce pole stock: Pressure and diffusible chemical treatments
1990 - IRG/WP 3605
One hundred and forty four spruce (test species) and southern yellow pine (reference species) poles were variously treated by center boring, incising, or kerfing, followed by pressure treatment with CCA and/or diffusible preservatives. The diffusible preservatives included NaF/creosote, borax and ammonium bifluoride. The poles were set at a test site and evaluated for preservative distribution and...
B Goodell, A J Pendlebury


Discoloration of pressure impregnated wood caused by Amorphotheca resinae
1990 - IRG/WP 1438
Amorphotheca resinae Parbery with the anamorph Cladosporium resinae (Lindau) von Arx & de Vries is a cosmopolitan fungus known from aviation kerosene, hydrocarbon contaminated soil and creosoted timbers. In Denmark it causes heavy discoloration on wood treated with waterborne chromate-containing preservatives e.g. CCA-oxide type. The teleomorph produces small spherical fruitbodies widespread o...
F Rune, A P Koch


Interim report on world survey of sap displacement impregnation of timber
1974 - IRG/WP 329
At the 4th Annual Meeting of the IRG held in West Berlin in October 1972 it was suggested that a survey of sap displacement impregnation of timber would be of interest. Accordingly through the courtesy and co-operation of the New Zealand Department of Trade and Industry a questionnaire was circulated to the Trade Commissioners for transmission to the relevant organisations in various parts of the ...
F B Shorland, C G W Mason


The suitability of high pressure sap-displacement for the retention of UK grown spruce and pine
1990 - IRG/WP 3595
The concentration and radial distribution of copper, chrome, arsenic (CCA), and the moisture content and depth of radial checking in UK grown, field exposed spruce and pine poles treated by high pressure sap-displacement are examined. The concentration of CCA elements in samples obtained from increment cores is similar in Norway spruce, Scots pine and Corsican pine but is significantly lower in Si...
P D Evans, S D Hainey, A Bruce, G M Smith, B King


Tendency of the preservative use for impregnation industries in Japan
1998 - IRG/WP 98-50101-05
In Japan, since 1997, the acceptable limit of the arsenic in the waste water become to 0,1 mg/l and the additional regional severer restriction can be established. In this reason, Japanese wood preservation industries intend to use other than CCA, like DDAC, ACQ, Tanalith CuAz, copper-naphthate and zinc-naphthenate, as replacing from CCA. In Jan-June 1997, the share of CCA preservatives was less t...
K Suzuki


Multiple-Phase Pressure (MPP) Process: Pilot plant trials for disposal of kickback using reverse osmosis membrane filtration
2001 - IRG/WP 01-40202
The MPP Process (a one-stage CCA treatment and accelerated fixation process) generates ~ 250 litres of kickback per cubic metre of timber treated. Composition of kickback is mainly wood sugars and traces of copper, chromium and arsenic. In pilot plant scale trials, MPP process kickback was filtered through a Reverse Osmosis (RO) membrane of a type found from earlier small-scale trials to be the mo...
H Pearson, G Durbin, M E Hedley


Metal Leaching from Pressure Treated Wood in Sanitary Landfill Leachate
2004 - IRG/WP 04-50220
Pressure treated wood products contain heavy metals to prevent biological decay. Scrap treated wood from construction activities and demolished structures containing treated wood are typically disposed in landfills. To examine the potential mobility of metals from pressure-treated wood disposed in landfills, wood samples were leached using leachate from lined landfills and the concentrations of ar...
B Dubey, T G Townsend, H M Solo-Gabriele


Cellular and fractural failure after supercritical fluid impregnation of four wood species
2004 - IRG/WP 04-10503
Supercritical fluids (SCFs) have been investigated for delivering biocides into sawn wood. Pressure differentials during treatment may exceed the compressive or tensile strength perpendicular to grain, creating a potential for transverse deformations that exceed elastic strain limits. Wood treated by SCF processing with CO2, a potential biocide carrier, was inspected macroscopically and microscopi...
M E Anderson, R J Leichti, J J Morrell


Remediation of a large CCA-impregnation plant
1998 - IRG/WP 98-50101-13
During 1949-85 the Swedish Telecom ran a plant for pressure impregnation of poles in Hjältevad, 80 km east of Jönköping in the southern part of Sweden. About one million poles were treated with CCA-preservaties. Leaks and accidential spills have contaminated soil and groundwater within the 5 ha large site. The total amount of released arsenic, the main pollutant, is estimated to 6-7 metric tons...
P Englöv


Penetration and distribution of styrene in pressure treated hardwoods
1997 - IRG/WP 97-40094
A styrene impregnation method was used to compare liquid distribution in several species as affected by flow direction, sapwood/heartwood, and method of impregnation. Twenty-five mm ( 1") cubes were cut from the sapwood and heartwood of red maple (Acer rubrum), white birch (Betula papyrifera), yellow poplar (Liriodendron tulipifera), trembling aspen (Populus tremuloides), red oak (Quercus rubra), ...
P A Cooper, T S Janezic, U Srinivasan, A Omidvar


The relationship between the electrical resistance and fixation of water-borne CCA salts and pressure-treated wood
1991 - IRG/WP 3657
Two investigations at 22°C and 30°C have been carried out. The electrical resistance in the treated wood and chemical analyses of the remaining amount of unfixed copper, chromium and arsenic were investigated. Samples impregnated with water were used as references. To hold the samples moist during the investigation, each sample was wrapped in a polyethylene plastic foil immediately after impregn...
F G Evans, B Nossen


Notes on a wood preservation industry in Medan, North Sumatera, Indonesia
1987 - IRG/WP 3405
This paper deals with a descriptive account on the development of a wood preservation industry in Medan, North Sumatera (Indonesia). The industry was established in 1974 when the State Owned Electicity Corporation decided to use wooden power poles for their distribution network in North Sumatera province. However, the use of wooden power poles was discontinued in 1981, so as the preservation indus...
N Supriana, A Murad


Wood Preservation in the United Kingdom
1979 - IRG/WP 385
This is only the first of several reports in English currently being prepared about wood preservation in Europe. The report deals with the extent of industrial impregnation and the number of impregnation plants in use today in Great Britain. Timbers which are treated for various end uses and their life expectancies are discussed. The market for wood preservatives, the size of the motorway fencing ...
R Cockcroft


Supercritical fluid impregnation of Douglas-fir heartwood with cyproconazole using temperature induced deposition
2003 - IRG/WP 03-40259
A limited understanding of the fundamental aspects of supercritical fluid (SCF) impregnation in wood remains an obstacle to the development of this technology. Developing a better understanding of the effects of various process parameters on treatment results would facilitate more rational development of SCF impregnation. In this project, the effect of treating period and specimen length on su...
Sung-Mo Kang, J J Morrell


A non-pressure method of protection based on hurdle theory to control the spectrum of internal environmental factors which affect the decay of poles in soil contact
1993 - IRG/WP 93-20005
A field trial was conducted to establish whether superficial barrier linings on poles in soil contact could function as environmental hurdles against the growth of biological agents and thus provide preventative methodology to preclude premature failure of vineyard poles under flood-irrigation. Assessment after 52 weeks exposure to the prevailing conditions and sub-tropical environment showed that...
A A W Baecker


Laboratory evaluation of copper naphthenate pressure treatments against the Formosan subterranean termite
1993 - IRG/WP 93-10005
Southern pine wafers and Douglas-fir cubes pressure treated with copper naphthenate in AWPA P9 Type A oil or in toluene were evaluated for resistance to attack by the Formosan subterranean termite, Coptotermes formosanus Shiraki (Isoptera: Rhinotermitidae). Wood samples were pressure treated to target copper retentions of 0.040, 0.075, 0.095, or 0.150 pcf, conditioned to simulate field exposure, a...
J K Grace, R T Yamamoto, P E Laks


Collaborative field trial out-of-ground contact
1982 - IRG/WP 2179
At the 12th meeting of the IRG in Sarajevo, Yugoslavia it was decided after considerable discussion that the best way to proceed with the work of the subgroup was to centre it around a co-operative field trial based on the L-joint test detailed in IRG/WP/2157. At the same time it was agreed that interested laboratories would also conduct their own methods, particularly the German planner test and ...
D J Dickinson, A F Bravery, J K Carey


Previous Page | Next Page